钢基身管镀铬层在高温腐蚀性气体中服役,采用YAG激光器对身管内表面作螺旋线状离散淬火预处理后再电镀铬的复合工艺,形成了基体界面呈激光淬火区/激光未处理区周期性变化的铬层/基体结构.对该身管进行高温腐蚀介质为火药气体的靶场实验.对实验后的基体界面腐蚀形貌与铬层剥落的关系研究表明:次界面裂纹的形成是基体界面高温气体腐蚀的根本原因,基体界面腐蚀的结果是形成基体烧蚀坑,烧蚀坑上的铬层以断裂形式剥落.激光淬火预处理钢基体通过抑制次界面裂纹的形成避免了基体界面高温气体腐蚀损伤,提高了铬层的抗剥落能力.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

The finite element method is used to analyze the elastodynamic response of a columnar thermal barrier coating due to normal impact and oblique impact by an erosive particle. An assessment is made of the erosion by crack growth from preexisting flaws at the edge of each column: it is demonstrated that particle impacts can be sufficiently severe to give rise to columnar cracking. First, the transient stress state induced by the normal impact of a circular cylinder or a sphere is calculated in order to assess whether a 2D calculation adequately captures the more realistic 3D behavior. It is found that the transient stress states for the plane strain and axisymmetric models are similar. The sensitivity of response to particle diameter and to impact velocity is determined for both the cylinder and the sphere. Second, the transient stress state is explored for 2D oblique impact by a circular cylindrical particle and by an angular cylindrical particle. The sensitivity of transient tensile stress within the columns to particle shape (circular and angular), impact angle, impact location, orientation of the angular particle, and to the level of friction is explored in turn. The paper concludes with an evaluation of the effect of inclining the thermal barrier coating columns upon their erosion resistance. © 2011 The American Ceramic Society.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

热浸镀铝钢材在铝铁界面处易产成FeAl冶金结合层。本文就FeAl层对铝镀层等离子体电解氧化(PEO)陶瓷层的表面形貌、截面组织、相结构和元素分布的影响进行了研究。结果表明:由于FeAl参与,PEO陶瓷层局部区域出现了50μm~80μm的贯穿性孔洞,在孔洞/FeAl界面处出现了许多微观裂纹。EDS结果显示孔洞周围的Fe、Na元素含量增高了近8倍。陶瓷层主要由γ-Al_2O_3、莫来石相、α-Al_2O_3和Fe_3O_4相组成。与FeAl层相比,PEO陶瓷层具有较高的硬度和塑性变形能力。