990 resultados para 188-1166
Resumo:
The nonisothermal crystallization behavior of poly (L-lactide)-poly(ethylene glycol) ( PLLA-PEG) diblock copolymer was studied by means of real-time WAXD, DSC and POM, and Ozawa equation was used to analyze the kinetics of PLLA-PEG under nonisothermal crystallization conditions. During the crystallization of the high-T-m block (PLLA), the low-T-m block (PEG) acts as a noncrystalline diluent, and the crystallization behavior of PLLA obeys the Ozawa theory. When the PEG block begins to crystallize, the PLLA phase is always partially solidified and the presence of the spherulitic microstructure of PLLA profoundly restricts its crystallization behavior, which results in that the overall crystallization process does not obey the Ozawa equation. Furthermore, the study of the crystalline morphology of PLLA-PEG at different cooling rates indicates that when the cooling rate is from low to high, the crystalline morphology undergoes a transformation from the ring-banded spherulites to the typical Maltese cross spherulites, which experiences the mixed crystalline morphologies of ring-banded and typical Maltese cross spherulites, and the spherulitic size becomes smaller.
Resumo:
The miscibility and structure of A-B copolymer/C homopolymer blends with special interactions were studied by a Monte Carlo simulation in two dimensions. The interaction between segment A and segment C was repulsive, whereas it was attractive between segment B and segment C. In order to study the effect of copolymer chain structure on the morphology and structure of A-B copolymer/C homopolymer blends, the alternating, random and block A-B copolymers were introduced into the blends, respectively. The simulation results indicated that the miscibility of A-B block copolymer/C homopolymer blends depended on the chain structure of the A-B copolymer. Compared with alternating or random copolymer, the block copolymer, especially the diblock copolymer, could lead to a poor miscibility of A-B copolymer/C homopolymer blends. Moreover, for diblock A-B copolymer/C homopolymer blends, obvious self-organized core-shell structure was observed in the segment B composition region from 20% to 60%. However, if diblock copolymer composition in the blends is less than 40%, obvious self-organized core-shell structure could be formed in the B-segment component region from 10 to 90%. Furthermore, computer statistical analysis for the simulation results showed that the core sizes tended to increase continuously and their distribution became wider with decreasing B-segment component.
Resumo:
采用高温固相反应合成了Sr4Al14O25∶RE3+(RE=Eu,Ce,Tb)样品,研究了其中Eu3+,Ce3+和Tb3+的光谱性质,以及Ce3+与Tb3+共掺时的能量传递现象;发现Eu3+,Ce3+和Tb3+占有两个格位,与Eu2+在此基质中的情况相似;在Tb3+的发射光谱中同时观察到了来自5D3与5D4的发射,表明两能级间无辐射跃迁过程不显著;Ce3+对Tb3+有敏化作用。
Resumo:
Rare earth complex (C5H9C9H6)(3)SmCl-Li+ (THF)(4)( I ) was synthesized by reacting anhydrous SmCl3 with two equivalents of C5H9C9H6Li. From mix-solvent of THF and hexane, red color single crystals were obtained. The crystal belongs to a cubic system, space group P2(1)3 with unit cell parameters a= b=c= 1. 754 0(2) nm, alpha=beta=gamma=90degrees, V=5. 396 4(11) nm(3), Z = 4. The ten-coordinated samarium atom is bonded to three cyclopentylindenyl rings and a chlorine atom to form the anionic part of the title complex, ring centroids and the chlorine atom form a tortured tetrahedron around samarium. In the cationic part, lithium atom coordinates to four oxygen atoms of THF molecules to form a normal tetrahedron. The Sm-C(within the same ring) distance varies from 0. 268 to 0. 299 nm.
Resumo:
以醋酸铅 ,硝酸氧锆 ,钛酸四丁酯为原料用溶胶 -凝胶法制备了纳米 Pb( Zr0 .52 Ti0 .48) O3 ( PZT)。结果表明 ,随溶剂中乙二醇单甲醚与水的比例的增大 ,PZT粉体的晶化温度增高 ,晶粒的粒径尺寸也增大 ,当V( C3 H8O2 ) / V( H2 O) =4 .4 7时 ,不仅凝胶完成时间短 ,且可得到粒度分布集中、晶化温度低的 PZT粉体。用原子力显微镜测定 PZT的粒径为 6 0~ 70 nm,用 TG-DTA分析确定在 4 43℃即可发生晶化反应 ,在 5 0 0℃下结晶完善。通过对不同温度下热处理的粉体的红外光谱和 X射线衍射的分析 ,对溶胶 -凝胶法制备 PZT粉体形成钙钛矿结构的过程进行了研究。
Resumo:
稀土配合物能使极性和非极性单体聚合[1] .虽然目前已测定了几乎所有的三 (环戊二烯基 )稀土配合物及部分三 (取代环戊二烯基 )稀土配合物的晶体结构 ,但有关三 (茚基 )稀土配合物的报道较少 .第一个三 (茚基 )稀土配合物是无水三氯化稀土与 3倍物质的量的茚基钠 C9H7Na在四氢呋喃中反应而得 ,但未报道其晶体结构[2 ] .后来用同样的反应却分离出以氯为桥的二聚体离子对配合物[Na( THF) 6][Ln( η5- C9H7) 3μ( Cl) Ln( η5- C9H7) 3]( Ln=Nd,Sm) [3] .无水三氯化稀土与 Mg( C9H7) 2 或C9H7K等物质的量反应则生成非溶剂化的 ( C9H7) 3Sm[4 ] ,而与茚基钠和环辛四烯钾 ( C8H8K)以 1∶ 2∶ 1物质的量比反应时 ,则得到 ( C9H7) 3Ln( THF) ( Ln=Nd,Gd) [5] .Bottomley[6] 曾用 ( C9Me7) K(七甲基茚基钾 )与 L n Cl3(物质的量比 3∶ 1 )反应制备 ( C9Me7) 3Nd( THF) 5和 ( C9Me7) 3Er· ( THF) 3,但未报道晶...
Resumo:
Extraction and separation of Eu3+ and Zn2+ in sulfuric acid solution was investigated by hollow fiber membrane with cyanex 302 (bis (2,4,4-trimethylpentyl) monothiophosphinic acid) in counter-currently circulating operation. Reaction mechanism of membrane extraction and effect of extractant concentration and H+ concentration in aqueous phase on the mass transfer coefficient were discussed. It can be concluded that Zn2+ can be extracted completely from Eu3+ sulfate solution according to the kinetics competing difference. In one extractor process, extraction percentage of Zn2+ was not completely and Eu3+ was not extracted. Extraction percentage of Zn2+ reached 94.92%, but Eu3+ only reached 8.59% after 100 minutes extraction in two series connectors and that of Zn2+ and Eu3+ reached 99.9% and 6.53% respectively after 40 minutes extraction in three series connectors.
Resumo:
利用中空纤维膜器,采用逆流循环萃取法,用二(2,4,4-三甲基戊基)硫代膦酸(Cyanex302)从硫酸溶液中萃取分离锌和铕。探讨了膜萃取的反应机制,考察了料液酸度、萃取剂浓度等因素对传质系数的影响,提出利用动力学竞争可以实现锌、铕混合组分的分离。研究了不同酸度、不同配比以及膜器串联的不同级数等条件对锌、铕混合物分离的影响。采用单级萃取时,只有锌被萃取,而铕不被萃取,且锌的萃取不完全;当采用膜器二级串联,经过 100min后锌的萃取率达到 94.92%,而铕的萃取率仅为8.59%;当采用膜器三级串联时,经过 40min后,锌的萃取率达到 99.9%以上,而铕的萃取率仅为6.53%。
Resumo:
鉴于变量选择在 QSAR/QSPR研究中的重要性 ,比较了遗传算法和几种传统的方法 ,如前进法、后退法及逐步回归法 .结果表明 ,对于研究中所用数据 ,遗传算法较几种传统的方法为好 ,其原因可能由于传统的方法陷入了局部最优 .遗传算法在变量较多的情况下方可显示出效率高和得到较好结果的优越性 .对于变量的选择 ,遗传算法是一值得推荐的有效的方法
Resumo:
Dodecanethiol-capped gold nanoparticles could spread on water subphase and be transferred by LB technique. The superlattice structure of gold nanoparticles multilayer was discussed.
Resumo:
A new series of mixed conducting oxides, Sr10-n/2BinFe20Om (n = 4, 6, 8, 10), were synthesized by a solid state reaction method, and they have high oxygen permeability. The oxygen permeation rate at 1150 K is 0.41 ml(STD)/ cm(2).min for n = 6 and 0.90 ml(STD)/cm(2).min for n = 10, which is two times higher than that for Sr1-xBixFeO3 (x = 0.5). For the Sr1-xBixFeO3 (x = 0.1, 0.3, 0.5) series, the oxygen flux increases with increasing Bi content. (C) 1998 Elsevier Science Ltd.
Resumo:
探讨了石墨炉原子吸收法测定钢铁及合金中微量钒的各种实验条件及影响因素。 实验表明,采用热解涂层管与光控升温相结合并在温度稳定的情况下原子化,可改善信号峰 形,提高灵敏度,消除记忆效应。方法用于钢铁及合金中钒的分析,结果令人满意。
Resumo:
The effect of physical aging at 210 degrees C on the mechanical properties of phenolphthalein polyether sulfone (PES-C) and a PES-C/poly(phenylene sulfide) (PPS) blend, with 5% content of PPS, were studied using DMA, tensile experiments, an instrumented impact tester, and SEM observations. The blend shows good mechanical properties in comparison with the corresponding PES-C. The mechanical properties of both materials exhibit characteristics of physical aging, with only the aging rate of the blend relatively slower, which should be attributed to the constraint effect of PPS particles and the good interfacial adhesion. The morphology of the PPS phase in the blend did not change with aging time. The principal role of PPS particles is to induce crazes, which dissipate energy, under applied loading; thus, the blend shows good toughness. On the other hand, the multiple crazing mechanism depends on the molecular mobility or structural state of the matrix. (C) 1996 John Wiley & Sons, Inc.
Resumo:
Functionalized polypyrrole films were prepared electrochemically in the presence of indigo-carmine from aqueous solution. The film shows a couple of reversible redox peaks superimposed on a large background of polypyrrole. The redox reaction is pH dependent. The film has good stability in air and can be cycled between -0.1 and 0.4 V (Ag/AgCl) for several hours without any significant changes in the voltammograms. UV-visible spectra indicate the incorporation of indigo-carmine into the polymer matrix.