Resumo:

By carrying out contact-arc vaporization of graphite in a partial atmosphere of Fe(CO)5, an iron-adduct with C60 has been obtained. The adduct has been characterized by various techniques including mass spectrometry, Fe-57 Mossbauer spectroscopy and Fe K-EXAFS. Properties of this adduct are compared with those of an adduct prepared by solution method where Fe is clearly outside the cage. Results suggest that FeC60 obtained from the gas phase reaction has the Fe atom in the cage.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

We have investigated tunneling conductances in disordered, normally conducting perovskite oxides close to the metal�insulator transition. We show that the normal state tunneling conductance of perovskite oxides can be cast in a general form G(V) = G0[1 + curly logical orV/V*curly logical orn] with 1?n?0.5 and where V* is an intrinsic energy scale. The exponent n graduall y increases from 0.5 to 1 as the metal-insulator (M-I) transition is approached. In the high-Tc Bi(2212) cuprates, the normally observed, linear G(V)(n=1) can be made sub-linear (n<1) by substitution of Ca with Y. From the similarity of the linear conductances, we suggest proximity to the M-I transition as a likely cause for this G(V)logical or, bar below V dependence. In systems showing linear conductances (nreverse similar, equals1), we find that ?G/?Vreverse similar, equalsG?0 with ?reverse similar, equals 1 and the intrinsic energy scale V*reverse similar, equals25�75 meV in the different oxides investigated.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The influence of strain rate and state-of-stress on the formation of ferrite in stainless steel type AISI 304L, 304 and 304 as-cast, during hot working has been studied. Compression and torsion tests were conducted in the temperature range 1100 to 1250 degrees C and strain rate range 0.001 to 100 s(-1) on these materials, Ferrite formation occurs during deformation at temperatures above 1150 degrees C and strain rates above 10 s(-1), in stainless steel type AISI 304L and 304. The tendency for the formation of ferrite is more in as-cast 304 than in wrought 304, In as-cast 304 the ferrite forms at lower temperatures and strain rates, The tendency for the ferrite formation is more in torsion than in compression.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

he chemical potential of carbon in diamond, relative to its value in graphite, has been directly determined using a solid state electrochemical cell incorporating single crystal CaF2 as the solid electrolyte. The cell can be represented as Pt, C(graphite) + CaC2 + CaF2double vertical barCaF2double vertical barCaF2 + CaC2 + C(diamond), Pt The reversible emf of this cell is directly related by the Nernst equation to the Gibbs free energy change for the conversion of diamond to graphite. The difference in the chemical potential of carbon in the two crystal structures varies linearly with temperature in the range 940 to 1260 K ?C(diamond) ? ?C(graphite) = 1100 + 4.64T (±50) J mol?1 On the average, the values given by the equation are 320 J mol?1 less positive than the currently accepted ones based on calorimetric studies. The difference is primarily in the enthalpy term.