978 resultados para CVD (Chemical Vapor Deposition)
Resumo:
The gas-phase ion/molecule reactions of F(-) and EtO(-) with Ge(OEt)(4) yield readily and exclusively pentacoordinated complexes XGe(OEt)(4)(-) (X = F, EtO) at pressures in the 10(-8) T range as observed by FT-ICR techniques. These hypervalent species are prone to undergo sequential fragmentations induced by infrared multiphoton excitation that lead to a variety of germyl and germanate anions. In the case of FGe(OEt)(4)(-), three primary competitive channels are observed in the IRMPD process that can be identified as (EtO)(3)GeO(-), F(EtO)(2)GeO(-) and (EtO)(3)Ge(-). Ab initio calculations have been carried out to characterize the primary fragmentation paths induced by IRMPD and the most favorable structure of the resulting anions. The gas-phase acidity of a number of these germanium-containing ions have been estimated by bracketing experiments and by theoretical calculations. Germanate anions such as (EtO)(3)GeO(-) undergo some interesting reactions with H(2)S to give rise to anions such as (EtO)(3)GeS(-) and (EtO)(2)Ge(OH)S(-). (C) 2010 Elsevier B.V. All rights reserved.
Resumo:
Boron-doped diamond (BDD) films grown on the titanium substrate were used to study the electrochemical degradation of Reactive Orange (RO) 16 Dye. The films were produced by hot filament chemical vapor deposition (HFCVD) technique using two different boron concentrations. The growth parameters were controlled to obtain heavily doped diamond films. They were named as E1 and E2 electrodes, with acceptor concentrations of 4.0 and 8.0 x 10(21) atoms cm(-3), respectively. The boron levels were evaluated from Mott-Schottky plots also corroborated by Raman`s spectra, which characterized the film quality as well as its physical property. Scanning Electron Microscopy showed well-defined microcrystalline grain morphologies with crystal orientation mixtures of (1 1 1) and (1 00). The electrode efficiencies were studied from the advanced oxidation process (AOP) to degrade electrochemically the Reactive Orange 16 azo-dye (RO16). The results were analyzed by UV/VIS spectroscopy, total organic carbon (TOC) and high-performance liquid chromatography (HPLC) techniques. From UV/VIS spectra the highest doped electrode (E2) showed the best efficiency for both, the aromaticity reduction and the azo group fracture. These tendencies were confirmed by the TOC and chromatographic measurements. Besides, the results showed a direct relationship among the BDD morphology, physical property, and its performance during the degradation process. (C) 2011 Elsevier B.V. All rights reserved.
Resumo:
Foram estudadas as propriedades elétricas de estruturas MOS envolvendo materiais com Zr e Hf: Al/HfO2/Si, Al/HfAlO/Si, Al/ZrO2/Si e Al/ZrAlO/Si depositadas por JVD (Jet Vapor Deposition) submetidas a diferentes doses de implantação de nitrogênio e tratamentos térmicos; Au/HfO2/Si e Au/HfxSiyOz/Si preparadas por MOCVD (Metal-Organic Chemical Vapor Deposition) e Au/HfxSiyOz/SiO2/Si preparadas por sputtering reativo em O2 submetidas a tratamentos térmicos distintos. Para isso, além das medidas de C-V e I-V padrão, foi desenvolvido o método da condutância para estudo da densidade de estados na interface dielétrico/Si, o qual mostrou-se mais viável para as estruturas com dielétricos alternativos. A inclusão de Al na camada de dielétrico, bombardeamento por íons de nitrogênio, e tratamentos térmicos rápidos em atmosferas de O2 e N2 foram responsáveis por mudanças nas propriedades das amostras. Diversos mecanismos físicos que influenciam as propriedades elétricas dessas estruturas foram identificados e discutidos. Foi constatado que as interfaces com menores densidades de estados foram as das amostras preparadas por MOCVD e sputtering reativo.
Resumo:
Amorphous hydrogenated chlorinated carbon (a-C:H:Cl) films were produced by the plasma polymerization of chloroform-acetylene-argon mixtures in a radiofrequency plasma enhanced chemical vapor deposition system. The main parameter of interest was the proportion of chloroform in the feed, R(C), which was varied from 0 to 80%. Deposition rates of 80 nm min (1) were typical for the chlorinated films. Infrared reflection-absorption spectroscopy revealed the presence of C-Cl groups in all the films produced with chloroform in the feed. X-ray photoelectron spectroscopy confirmed this finding, and revealed a saturation of the chlorine content at similar to 47 at.% for R(C)>= 40%. The refractive index and optical gap, E(04), of the films were roughly in the 1.6 to 1.7, and the 2.8 to 3.7 eV range. These values were calculated from transmission ultraviolet-visible-near infrared spectra. Chlorination leads to an increase in the water surface contact angle from similar to 40 degrees to similar to 77 degrees. (C) 2011 Elsevier B.V. All rights reserved.
Resumo:
This work was performed to verify the chemical structure, mechanical and hydrophilic properties of amorphous hydrogenated carbon films prepared by plasma enhanced chemical vapor deposition, using acetylene/argon mixture as monomer. Films were prepared in a cylindrical quartz reactor, fed by 13.56 MHz radiofrequency. The films were grown during 5 min, for power varying from 25 to 125 W at a fixed pressure of 9.5 Pa. After deposition, all samples were treated by SF(6) plasma with the aim of changing their hydrophilic character. Film chemical structure investigated by Raman spectroscopy, revealed the increase of sp(3) hybridized carbon bonds as the plasma power increases. Hardness measurements performed by the nanoindentation technique showed an improvement from 5 GPa to 14 GPa following the increase discharge power. The untreated films presented a hydrophilic character, which slightly diminished after SF(6) plasma treatment.
Resumo:
Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)
Resumo:
Conselho Nacional de Desenvolvimento Científico e Tecnológico (CNPq)
Resumo:
Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)
Resumo:
This work describes an XPS investigation of plasma-deposited polysiloxane films irradiated with 170 keV He+ ions at fluences, Phi, ranging from 1 x 10(14) to 1 x 10(16) cm(-2). Modifications in the atomic concentrations of the surface atoms with (D were revealed by changes in the [O]/[Si], [O]/[C] and [C]/[Si] atomic ratios. Surface chemical structure modifications were evidenced by the increasing C1s peak width and asymmetry as Phi was increased, due to the formation of ether and carboxyl functionalities. Moreover, structural transformations were indicated by the positive binding energy shift of the Si2p peaks, due to the increasing Si oxidation. Correlations of the XPS data with other results from previous work on polysiloxanes illustrate the role of ion beam-induced bond breaking on the structural modifications.
Resumo:
This work illustrates the advantages of using p-polarized radiation at an incidence angle of 70 degrees in contrast to the conventional unpolarized beam at normal (or near-normal) incidence for the infrared spectroscopic study of polycarbosilane, polysilazane and polysiloxane thin films synthesized by plasma enhanced chemical vapor deposition (PECVD) and subsequently irradiated with 170 keV He+ ions at fluences from 1 x 10(14) to 1 x 10(16) cm(-2). Several bands not seen using the conventional mode could be observed in the polarized mode. (c) 2006 Elsevier B.V. All rights reserved.
Resumo:
In this work films were produced by the plasma enhanced chemical vapor deposition (PECVD) of titanium tetraisopropoxide-oxygen-helium mixtures and irradiated with 150 keV singly-charged nitrogen ions (N(+)) at fluences, phi, between 10(14) and 10(16) cm(-2). Irradiation resulted in compaction, which reached about 40% (measured via the film thickness) at the highest fluence. Infrared reflection-absorption spectroscopy (IRRAS) revealed the presence of Ti-O bonds in all films. Both O-H and C-H groups were present in the as-deposited films, but the density of each of these decreased with increasing phi and was absent at high phi, indicating a loss of hydrogen. X-ray photoelectron spectroscopy (XPS) analyses revealed an increase in the C to Ti atomic ratio as phi increased, while the O to Ti ratio hardly altered, remaining at around 2.8. The optical gap of the films, derived from data obtained by ultraviolet-visible spectroscopy (UVS), remained at about 3.6 eV for all fluences except the highest, for which an abrupt fall to around 1.0 eV was observed. For the irradiated films, the electrical conductivity, measured using the two-point method, showed a systematic increase with increasing phi. (c) 2008 Elsevier B.V. All rights reserved.
Resumo:
Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)
Resumo:
Strontium barium niobate (SBN) thin films were crystallized by conventional electric furnace annealing and by rapid-thermal annealing (RTA) at different temperatures. The average grain size of films was 70 nm and thickness around 500 nm. Using x-ray diffraction, we identified the presence of polycrystalline SBN phase for films annealed from 500 to 700 °C in both cases. Phases such as SrNb2O6 and BaNb2O6 were predominantly crystallized in films annealed at 500 °C, disappearing at higher temperatures. Dielectric and ferroelectric parameters obtained from films crystallized by conventional furnace and RTA presented essentially the same values.
Resumo:
Thin films of lithium niobate were deposited on the Pt/Ti/SiO2 (111) substrates by the polymeric precursor method (Pechini process). Annealing in static air and oxygen atmosphere was performed at 500°C for 3 hours. The films obtained were characterized by X-ray diffraction, scanning electron microscopy and transmission electron microscopy. The dielectric constant, dissipation factor and resistance were measured in frequency region from 10 Hz to 10 MHz. Electrical characterizations of the films pointed to ferroelectricity via hysteresis loop. The influence of oxygen atmosphere on crystallization and properties of LiNbO3 thin films is discussed.
Resumo:
Conselho Nacional de Desenvolvimento Científico e Tecnológico (CNPq)