976 resultados para CRYSTALLINE TELLURIUM


Relevância:

10.00% 10.00%

Publicador:

Resumo:

The proton NMR spectral complexity arising due to severe overlap of peaks hampers their analyses in diverse situations, even by the application of two-dimensional experiments. The selective or complete removal of the couplings and retention of only the chemical shift interactions in indirect dimension aids in the simplification of the spectrum to a large extent with little investment of the instrument time. The present study provides precise enantiodiscrimination employing more anisotropic NMR parameters in the chiral liquid crystalline medium and differentiates the overlapped peaks of many organic molecules and peptides dissolved in isotropic solvents.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

ZnO nanostructures were deposited on flexible polymer sheet and cotton fabrics at room temperature by activated reactive evaporation. Room-temperature photoluminescence spectrum of ZnO nanostructured film exhibited a week intrinsic UV emission and a strong broad yellow-orange visible emission. TEM and HRTEM studies show that the grown nanostructures are crystalline in nature and their growth direction was indentified to be along [002]. ZnO nanostructures grown on the copper-coated flexible polymer sheets exhibited stable field-emissio characteristics with a threshold voltage of 2.74 V/mu m (250 mu A) and a very large field enhancement factor (beta) of 23,213. Cotton fabric coated with ZnO nanostructures show an excellent antimicrobial activity against Staphylococcus aureus bacteria (Gram positive), and similar to 73% reduction in the bacterial population is achieved compared to uncoated fabrics after 4 h in viability. Using a shadow mask technique, we also selectively deposited the nanostructures at room temperature on polymer substrates.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Hydrothermal treatment of a slurry of badly crystalline (beta(bc)) nickel hydroxide at different temperatures (65-170 degrees C) results in the progressive ordering of the structure by the step-wise elimination of disorders. Interstratification is eliminated at 140 degrees C, while cation vacancies are eliminated at 170 degrees C. A small percentage of stacking faults continue to persist even in `crystalline' samples. Electrochemical investigations show that the crystalline nickel hydroxide has a very low (0.4 e/Ni) reversible charge storage capacity. An incidence of at least 15% stacking faults combined with cation vacancies is essential for nickel hydroxide to perform close to its theoretical (1 e/ Ni) discharge capacity. (c) 2005 The Electrochemical Society.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Previously, it was reported from this laboratory that the heme groups of hemoglobin are “buried” within globin at pH 4.0 and not dissociated, on the basis of the obiligatory requirement of urea for the reaction of N-bromosuccinimide with the heme groups of hemoglobin at pH4.0, and also on the basis of the “normalization” of the spectrum of hemoglobin at this pH in the presence of urea or sucrose. In the present study, it has been shown that the behaviour of sperm whale myoglobin with respect to its reaction with N-bromosuccinimide and with respect to spectral “normalization” in urea or sucrose are essentially similar to that of hemoglobin. It has also been demonstrated that the spectral “normalization” obtained with crystalline hemin is not identical with that obtained with either hemoglobin or myoglobin. The bearing of the results of the present study on the earlier work on hemoglobin is indicated.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

The Raman spectrum of crystalline boric acid is recorded using mercuryλ2537 excitation. Fifteen Raman lines, three of them belonging to the lattice spectrum, are reported. Satisfactory assignments of all the observed Raman frequencies are made using the available X-ray crystal structure data. From the presence of a new high frequency Raman band at about 3420 cm.−1 it is suggested that there might be a small number of long, weak O-H....O hydrogen bonds in the crystal, in addition to the hydrogen bonds of moderate strength reported from X-ray diffraction data.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

ORANGE red and amorphous peroxy-titanium complexes of oxalic, malonic and maleic acids1-3, when vacuum-dried, have co-ordinated water molecules firmly bonded to the central titanium atom as shown in formula (I). The peroxy-oxygen from these compounds is slowly lost even at room temperature because of the strained peroxy-group3,4. The compounds, when kept at 95°-100°C. for about three days, give deperoxygenated compounds of the type (II). However, a sample of peroxy-titanium oxalate sealed in a glass tube lost all its peroxy-oxygen in about four years and gave a white crystalline basic oxalate (II). The amorphous nature of the compounds may be due to random hydrogen bonding in the complexes. The crystallinity observed in one of the deperoxygenated titanyl oxalates may be due to the rearrangement of the molecules during ageing for more than four years. The infra-red absorption of these compounds was studied to find out the effect of co-ordination and hydrogen bonding on the infra-red bands of the free water.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Most new drug molecules discovered today suffer from poor bioavailability. Poor oral bioavailability results mainly from poor dissolution properties of hydrophobic drug molecules, because the drug dissolution is often the rate-limiting event of the drug’s absorption through the intestinal wall into the systemic circulation. During the last few years, the use of mesoporous silica and silicon particles as oral drug delivery vehicles has been widely studied, and there have been promising results of their suitability to enhance the physicochemical properties of poorly soluble drug molecules. Mesoporous silica and silicon particles can be used to enhance the solubility and dissolution rate of a drug by incorporating the drug inside the pores, which are only a few times larger than the drug molecules, and thus, breaking the crystalline structure into a disordered, amorphous form with better dissolution properties. Also, the high surface area of the mesoporous particles improves the dissolution rate of the incorporated drug. In addition, the mesoporous materials can also enhance the permeability of large, hydrophilic drug substances across biological barriers. T he loading process of drugs into silica and silicon mesopores is mainly based on the adsorption of drug molecules from a loading solution into the silica or silicon pore walls. There are several factors that affect the loading process: the surface area, the pore size, the total pore volume, the pore geometry and surface chemistry of the mesoporous material, as well as the chemical nature of the drugs and the solvents. Furthermore, both the pore and the surface structure of the particles also affect the drug release kinetics. In this study, the loading of itraconazole into mesoporous silica (Syloid AL-1 and Syloid 244) and silicon (TOPSi and TCPSi) microparticles was studied, as well as the release of itraconazole from the microparticles and its stability after loading. Itraconazole was selected for this study because of its highly hydrophobic and poorly soluble nature. Different mesoporous materials with different surface structures, pore volumes and surface areas were selected in order to evaluate the structural effect of the particles on the loading degree and dissolution behaviour of the drug using different loading parameters. The loaded particles were characterized with various analytical methods, and the drug release from the particles was assessed by in vitro dissolution tests. The results showed that the loaded drug was apparently in amorphous form after loading, and that the loading process did not alter the chemical structure of the silica or silicon surface. Both the mesoporous silica and silicon microparticles enhanced the solubility and dissolution rate of itraconazole. Moreover, the physicochemical properties of the particles and the loading procedure were shown to have an effect on the drug loading efficiency and drug release kinetics. Finally, the mesoporous silicon particles loaded with itraconazole were found to be unstable under stressed conditions (at 38 qC and 70 % relative humidity).

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Thermotropic liquid crystals are known to display rich phase behavior on temperature variation. Although the nematic phase is orientationally ordered but translationally disordered, a smectic phase is characterized by the appearance of a partial translational order in addition to a further increase in orientational order. In an attempt to understand the interplay between orientational and translational order in the mesophases that thermotropic liquid crystals typically exhibit upon cooling from the high-temperature isotropic phase, we investigate the potential energy landscapes of a family of model liquid crystalline systems. The configurations of the system corresponding to the local potential energy minima, known as the inherent structures, are determined from computer simulations across the mesophases. We find that the depth of the potential energy minima explored by the system along an isochor grows through the nematic phase as temperature drops in contrast to its insensitivity to temperature in the isotropic and smectic phases. The onset of the growth of the orientational order in the parent phase is found to induce a translational order, resulting in a smectic-like layer in the underlying inherent structures; the inherent structures, surprisingly, never seem to sustain orientational order alone if the parent nematic phase is sandwiched between the high-temperature isotropic phase and the low-temperature smectic phase. The Arrhenius temperature dependence of the orientational relaxation time breaks down near the isotropic-nematic transition. We find that this breakdown occurs at a temperature below which the system explores increasingly deeper potential energy minima.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Crystalline Bi5NbO10 nanoparticles have been achieved through a modified sol–gel process using a mixture of ethylenediamine and ethanolamine as a solvent. The Bi5NbO10 nanoparticles were characterized by X-ray diffraction (XRD), differential scanning calorimetry/thermogravimetry (DSC/TG), Fourier transform infrared spectroscopy (FT-IR), transmission electron microscopy (TEM) and Raman spectroscopy. The results showed that well-dispersed 5–60 nm Bi5NbO10 nanoparticles were prepared through heat-treating the precursor at 650 °C and the high density pellets were obtained at temperatures lower than those commonly employed. The frequency and temperature dependence of the dielectric constant and the electrical conductivity of the Bi5NbO10 solid solutions were investigated in the 0.1 Hz to 1 MHz frequency range. Two distinct relaxation mechanisms were observed in the plots of dielectric loss and the imaginary part of impedance (Z″) versus frequency in the temperature range of 200–350 °C. The dielectric constant and the loss in the low frequency regime were electrode dependent. The ionic conductivity of Bi5NbO10 solid solutions at 700 °C is 2.86 Ω−1 m−1 which is in same order of magnitude for Y2O3-stabilized ZrO2 ceramics at same temperature. These results suggest that Bi5NbO10 is a promising material for an oxygen ion conductor.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

TiO2 thin films have been deposited on glass and indium tin oxide (ITO) coated glass substrates by sol-gel technique. the influence of annealing temperature on the structural , morphological and optical properties has been examined. X-ray diffraction (XRD) results reveal the amorphous nature of the as-deposited film whereas the annealed films are found to be in the crystalline anatase phase. The surface morphology of the films at different annealing temperatures has been examined by atomic force microscopy (AFM). The in situ surface morphology of the as-deposited and annealed TiO2 films has also been examined by optical polaromicrograph (OPM). TiO2 films infatuated different structural and surface features with variation of annealing temperature. The optical studies on these films suggest their possible usage in sun-shielding applications.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Stiffness, strength, and toughness are the three primary attributes of a material, in terms of its mechanical properties. Bulk metallic glasses (BMGs) are known to exhibit elastic moduli at a fraction lower than crystalline alloys and have extraordinary strength. However, the reported values of fracture toughness of BMGs are highly variable; some BMGs such as the Zr-based ones have toughness values that are comparable to some high strength steels and titanium alloys, whereas there are also BMGs that are almost as brittle as silicate glasses. Invariably, monolithic BMGs exhibit no or low crack growth resistance and tend to become brittle upon structural relaxation. Despite its critical importance for the use of BMGs as structural materials, the fracture toughness of BMGs is relatively poorly understood. In this paper, we review the available literature to summarize the current understanding of the mechanics and micromechanisms of BMG toughness and highlight the needs for future research in this important area.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Large quantities of single-crystalline ZnO nanorods and nanotubes have been prepared by the microwave, irradiation of a metalorganic complex of zinc, in the presence of a surfactant. The method is simple, fast, and inexpensive (as it uses a domestic microwave oven), and yields pure nanostructures of the hexagonal wurtzite phase of ZnO in min, and requires no conventional templating. The ZnO nanotubes formed have a hollow core with inner diameter varying from 140-160 nm and a wall of thickness, 40-50 nm. The length of nanorods and nanotubes varies in the narrow range of 500-600 nm. These nanostructures have been characterized by X-ray diffraction (XRD), scanning electron microscopy (SEM), transmission electron microscopy (TEM), and selected area electron diffraction (SAED). The ZnO nanorods and nanotubes are found by SAED to be single-crystalline. The growth process of ZnO nanorods and nanotubes has been investigated by varying the surfactant concentration and microwave irradiation time. Based on the various results obtained, a tentative and plausible mechanism for the formation of ZnO nanostructures is proposed.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

By roller quenching and water quenching melts of Bi2(Ca, Sr)3Cu2O8+δ, glasses have been obtained. These glasses exhibit two glass transitions as well as two crystallization transitions. Microwave absorption studies show the glass to be weakly superconducting at 77 K, probably due to the presence of ultramicrocrystallites. The glass on crystallization at 870 K gives the crystalline n=1 member of the homologous series Bi2(Ca, Sr)n+1CunO 2n+4 and the n=2 member on annealing at 1100 K. The glass route provides a unique means of obtaining the n=2 member of the series. On prolonged annealing of the glass at 1120 K, the n=3 member seems to be formed.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Cellobiohydrolases I and II were purified to homogeneity from culture filtrates of a thermophilic fungus, Chaetomium thermophile var. coprophile, by using a combination of ion-exchange and gel filtration chromatographic procedures. The molecular weights of cellobiohydrolase I and II were estimated to be 60000 and 40000 and the enzymes were found to be glycoproteins containing 17 and 22.8% carbohydrate, respectively. The two forms differed in their amino-acid composition mainly with respect to threonine, alanine, methionine and arginine. Antibodies produced against either form of cellobiohydrolases failed to cross-react with the other. The tryptic maps of the two enzymes were found to be different. The temperature optima for cellobiohydrolase I and II were 75 and 70°C, and they were optimally active at pH 5.8 and 6.4, respectively. Both enzymes were stable at higher temperatures and were able to degrade crystalline cellulosic materals.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

The activity of gallium in liquid Ga-Te alloys has been measured at 1120 K using a solid state galvanic cell incorporating yttria-stabilized thoria as the solid electrolyte. The cell can be schematically represented as (−) W,Re,Ga(1)+Ga2O3(s)|(Y2O3) ThO2|Ga-Te(1) + Ga2O3(s), Re, W (+) The activity of tellurium was derived by Gibbs-Duhem integration. The activity of gallium shows negative deviation from Raoult's law for XGa < 0.6 and positive deviation from ideality for XGa > 0.6. The activity of gallium was constant in the composition range 0.73 < XGa < 0.89, indicating liquid state immiscibility in this region. The Gibbs energy of mixing and the concentration-concentration structure factor at long wavelength limit show a minimum at XGa ≈ 0.4, suggesting strong interactions in the liquid phase with formation of ‘Ga2Te3‘-type complexes