987 resultados para POLY(AMIDE-IMIDE)
Resumo:
We synthesized a series of polymers: poly(ether ether ketone ketone)(PEEKK), poly(ether biphenyl ether ketone ketone) (PEBEKK) and their copolymer by polycondensation, We also prepared a series of PEEKK-PEBEKK blends, By using DSC method, we found that T-g of the copolymers and the blends rose with the increasing of biphenyl contents in the polymers, T-c of the copolymers and the blends is higher than the corresponding homopolymer. From the results, we think that PEEKK-PEBEKK copolymer and blends are miscible and the copolymer is random.
Resumo:
Flexural fatigue tests were conducted on injection-molded short fiber composites, carbon fiber/poly(phenylene ether ketone) (PEK-C) and glass fiber/PEK-C (with addition of polyphenylene sulfide for improving adhesion between matrix and fibers), using four-point bending at stress ratio of 0.1. The fatigue behavior of these materials was presented. By comparing the S-N curves and analyzing the fracture surfaces of the two materials, the similarity and difference of the failure mechanisms in the two materials were discussed. It is shown that the flexural fatigue failure of the studied materials is governed by their respective tensile properties. The matrix yielding is main failure mechanism at high stress, while at lower stress the fatigue properties appear fiber and interface dominated. (C) 1997 John Wiley & Sons, Inc.
Resumo:
Prepolymers of poly(ethylene oxide) (Pre-PEG) were synthesized by reacting azoisobutyronitrile (AIBN) with poly(ethylene glycol) (PEG), and their structures were characterized by IR and UV. The molecular weight of pre-PEG was related to the feed ratio and reaction time. These prepolymers can be used to prepare block copolymers - poly(ethylene oxide)-block-poly(butyl acrylate) (PEO-b-PBA) by radical polymerization in the presence of butyl acrylate (BA). Solution polymerization was a suitable technique for this step. The yield and the molecular weight of the product were related to the ratio of the prepolymer to BA, the reaction time, and temperature. GPC showed that the molecular weight increased with a higher ratio of BA to pre-PEO. The intrinsic viscosity of the copolymers was only slightly dependent on reaction time, but decreased at higher reaction temperatures, as did the amount of PEA homopolymer. (C) 1997 John Wiley & Sons, Inc.
Resumo:
Blends of a liquid crystalline thermotropic copolyester (LCP70) and an amorphous phenolphthalein based poly(ether-ketone)(PEK-C) with two viscosities were prepared by melt blending. The blends' morphology, rheological and mechanical properties were investigated by DSC, SEM, mechanical and rheological tests. It was observed that the optimum composition of the PEK-C/LCP70 blend was 10 wt% LCP for both mechanical and rheological properties. When the LCP content was less than 10%, the LCP phase existed as finely dispersed fibrous domains with a diameter of about 1 mu m in the matrix, and both tensile and flexural properties were improved. In contrast, when the LCP content reached 20% or more, the LCP domains coalesced to ellipsoidal particles with a diameter of about 5 mu m, and the mechanical properties decreased as a result. It is demonstrated that pure PEK-C with a high viscosity which was difficult to process by melt extrusion, could be extruded conveniently when 10% LCP70 was incorporated. It is emphasized that LCP not only can be used as a reinforcing phase but also an effective processing agent for engineering thermoplastics, especially for those with high viscosity and narrow processing window. (C) 1997 Elsevier Science Ltd.
Resumo:
Para-para linked aromatic poly(amic ester) precursors of rodlike polyimide (PI) BPDA-PDA and polyetherimide (PEI) HQDPA-ODA were synthesized. The para-para linked poly(amic ester)s were employed in this work to obtain, in theory, full-imidized polyimides. The two precursors were mixed by dissolving them in N, N'-dimethyl acetamide and subsequently coagulating in methanol. After thermal imidization, the miscibility behaviour of the resulting composites has been studied by means of dynamic mechanical analysis (d.m.a.) and differential scanning calorimetry (d.s.c.). The composites show a single glass transition temperature (T-g) at both d.m.a. and d.s.c. in which the T-g increases with increasing PI content. These Tg values are reproducible in repeated heating cycles, suggesting the true miscibility of the blends. (C) 1997 Elsevier Science Ltd.
Resumo:
The present work investigates the effects of cyclic fatigue loading on the residual properties of an injection-molded composite, carbon-fiber-reinforced poly(phenylene ether ketone) (CF/PEK-C), and damage development in this material under fatigue lending. Test specimens, which had been conditioned to various preselected fatigue damage stages, were measured for their residual properties. The results indicated that cyclic fatigue loading alters the constitutive behavior of the injection-molded composite, especially in the non-linear portion of the stress/strain curve. The residual strength decreases with increase in the number of fatigue cycles as a consequence of the accumulation of fatigue damage, which is dominated by the growth of microcracks. While the residual modulus increases slightly with cyclic fatigue loading, this is probably due to the oriented hardening resulting from creep deformation which is induced during cyclic loading. (C) 1997 Elsevier Science Limited.
Resumo:
The mechanical properties of wollastonite-filled phenolphthalein poly(ether ketone) (PEK-C) composites have been studied at room temperature and 200 degrees C. The dispersion of wollastonite particles in PEK-C matrix were investigated by means of scanning electron microscope. The modulus and strength of the composites increased with filler content. The reinforced effect of wollastonite on PEK-C is more marked at elevated temperature. The glass transition temperature of the composites is higher than that of PEK-C and is independent of filler content. The restriction effect of tiller particles on the molecular mobility of the polymer matrix should be attributed to the reinforcement. (C) 1997 John Wiley & Sons, Inc.
Resumo:
Polyamide 1010/poly(propylene) (PA1010/PP) blends were investigated with and without the addition of poly(propylene)-graft-glycidyl methacrylate (PP-g-GMA). The effect of the compatibilizer on the thermal properties and crystallization behavior was determined by differential scanning calorimetry and wide-angle X-ray diffraction. From the results it is found that the crystallization of PA 1010 is significantly affected by the presence of PP-g-GMA. PP/PA 1010 (75/25) blends containing higher amounts of PP-g-GMA show concurrent crystallization at the crystallization temperature of PP. Isothermal crystallization kinetics also were performed in order to investigate the influence of the compatibilized process on the nucleation and growth mechanism. In the PP/PA 1010 (25/75) blends, concurrent crystallization behavior was not observed, even though the amount of PPg-GMA was high.
Resumo:
The novel poly(aryl ether ketone)s containing chloro-side group were synthesized by nucleophilic substitution reactions of 4,4'-biphenol and chlorohydroquinone with either 4,4'-difluorobenzophenone(BP/CH/DF) or 1,4-bis(p-fluorobenzoyl)benzene (BP/CH/BF) and their thermotropic liquid crystalline properties were characterized by a variety of experimental techniques. The thermotropic liquid crystalline behavior was observed in the copolymers containing 50 and 70% biphenol. Melting transition (Tm) and isotropization transition (Ti) both appeared in the DSC thermograms. A banded texture was formed after shearing the sample in the liquid crystalline state. The novel poly(aryl ether ketone)s had relatively higher glass transition temperature (Tg) in the range of 168 similar to 200 degrees C and lower melting temperature (Tm) in the range of 290 similar to 340 degrees C. The thermal stability (Td) was in the range of 430 similar to 490 degrees C.
Resumo:
Two etching techniques are used to reveal the morphology of PC/PBA-cs-PMMA blend. One is based on acetic acid (CH3COOH) solutions, whereas the other uses CCl4/ C2H5OH (3/1 v/v). The latter approach shows to be more appropriate and successful for revealing the morphology of PC/PBA-cs-PMMA blend.
Resumo:
The thermal properties and crystalline structure of the amphiphilic graft copolymers CR-g-PEG600, CR-g-PEG2000, and CR-g-PEG6000 using chloroprene rubber (CR) as the hydrophobic backbone and poly(ethylene glycol) (PEG) with different molecular weights as the hydrophilic side chains were studied by DSC and WAXD. The results showed that a distinct phase-separated structure existed in CR-g-PEGs because of the incompatibility between the backbone segments and the side-chain segments. For all the polymers studied, T-m2, which is the melting point of PEG crystalline domains in CR-g-PEG, decreased compared to that of the corresponding pure PEG and varied little with PEG content. For CR-g-PEG600 and CR-g-PEG2000, T-m1, which is the melting point of the CR crystalline domains, increased with increasing PEG content when the PEG content was not high enough, and at constant PEG content, the longer were the PEG side chains the higher was the T-m1. The crystallite size L-011 of CR in CR-g-PEGs increased compared to that of the pure CR and decreased with increasing PEG content. (C) 1997 John Wiley & Sons, Inc.
Resumo:
The enzymatic degradation of poly(epsilon-caprolactone) (PCL) films in phosphate buffer solution containing lipases has been studied by DSC, WAXD and SEM. Three lipases, pseudomonas lipase (PS), porcine pancreatic lipase (PP), and candida cylindracea lipase (AY), were used. The results showed that the degradation of PCL films in phosphate buffer solution containing PP or AY was very slow: no weight loss could be found within 1 week. However, PCL film could degrade rapidly and completely within 4 days in phosphate buffer solution containing PS lipase. (C) 1997 Elsevier Science Limited.
Resumo:
The miscibility and crystallization behavior of poly(beta-hydroxybutyrate) (PHB) and poly(p-vinylphenol) (PVPh) blends were studied by differential scanning calorimetry and optical microscopy (OM). The blends exhibit a single composition-dependent glass transition temperature, characteristic of miscible systems, A depression of the equilibrium melting temperature of PHB is observed. The interaction parameter values obtained from analysis of the melting point depression are of large negative values, which suggests that PHB and PVPh blends are thermodynamically miscible in the melt. Isothermal crystallization kinetics in the miscible blend system PHB/PVPh was examined by OM. The presence of the amorphous PVPh component results in a reduction in the rate of spherulite growth of PHB. The spherulite growth rate is analyzed using the Lauritzen-Hoffman model, The isothermally crystallized blends of PHB/PVPh were examined by wide-angle X-ray diffraction and smell-angle X-ray scattering (SAXS). The long period obtained from SAXS increases with the increase in PVPh component, which implies that the amorphous PVPh is squeezed into the interlamallar region of PHB.
Resumo:
Isothermal melt and cold crystallization kinetics of PEDEKmK linked by meta-phenyl and biphenyl were investigated by differential scanning calorimetry in two temperature regions. Avrami analysis is used to describe the primary stages of the melt and cold crystallization, with exponent n = 2 and n = 4, respectively. The activation energies are -118 kJ/mol and 510 kJ/mol for crystallization from the melt and the glassy states, respectively. The equilibrium melting point T-m(0) is estimated to be 309 degrees C by using the Hoffman-Weeks approach, which compares favorably with determination from the Thomson-Gibbs method. The lateral and end surface free energies derived from the Lauritzen-Hoffman spherulitic growth rate equation are sigma = 8.45 erg/cm(2) and sigma(e) = 45.17 erg/cm(2), respectively. The work of chain folding q is determined as 3.06 kcal/mol. These observed crystallization characteristics of PEDEKmK are compared with those of the other members of poly(aryl ether ketone) family. (C) 1997 John Wiley & Sons, Inc.
Resumo:
The gas transport of hydrogen, oxygen, nitrogen, carbon dioxide, and methane gases in a series of poly(aryl ether ketone)s was examined. These polymer membranes have a wide range of permeability coefficients and permselectivity coefficients, showing excellent gas-transport properties. The enhanced interchain interaction in the polymers due to intermolecular hydrogen bonds and ionic bonds results in a considerable increase in permselectivity but a decrease in permeability. On the contrary, the polymers with bulky arkyl substituents show significantly increased permeability. The causes of this trend are interpreted in terms of the free volume, interchain distance, and glass transition temperature together with the respective contribution of gas solubility and diffusivity to the overall permeability. Of interest is the observation that the ionomer IMPEK-K+, which simultaneously contains bulky isopropyl substituents and pendant carboxylate groups, exhibits over twice higher CO2 permeability and 15% higher CO2/CH4 permselectivity than those of bisphenol-A p'olysulfone (PSF). The possibility of using the new synthesized poly(aryl ether ketone)s in gas separation membrane application is also discussed. (C) 1997 John Wiley & Sons, Inc.