Resumo:

The rigid backbone of the poly(3-butylthiophene) molecule adopts a perpendicular orientation with respect to the substrate by using a solvent-vapor treatment (see figure). Small and closely contacting spherulites instead of conventional whisker-like crystals are achieved. This could be utilized to improve charge-carrier mobility particularly in the direction normal to the film plane by designing and constructing thick crystalline domains in the functional layer.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The dewetting evolution process of polymethyl methacrylate (PMMA) film on the flat and prepatterned polydimethylsiloxane (PDMS) substrates (with square microwells) by the saturated solvent of methyl ethyl ketone (MEK) treatment has been investigated at room temperature by the optical microscope (OM) and atomic force microscope (AFM). The final dewetting on the flat PDMS substrate led to polygonal liquid droplets, similar to that by temperature annealing. However, on the patterned PDMS substrate, depending on the microwells' structure of PDMS substrate and defect positions that initiated the rupture and dewetting of PMMA, two different kinds of dewetting phenomena, one initiated around the edge of the microwells and another initiated outside the microwells, were observed. The forming mechanism of these two different dewetting phenomena has been discussed. The microwells were filled with liquid droplets of PMMA after dewetting due to the formation of fingers caused by the pinning of the three-phase-line at the edge of the microwells and their rupture.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The self-assembly processes of the rod-coil diblock oligomer thin film of tetra-aniline (TANI)-block-poly(L-lactide) (PLLA) with different film thicknesses induced in the coil-selective solvent of acetone vapor at room temperature were studied. The morphologies of the oligomer films were determined by the film thickness. For the thicker film (232 nm), the nonextinct concentric ring-banded textures could form. While for the thinner and appropriate film (about 6 nm), multistacked diamond-shaped appearances with the periodic thickness being about 8.5 nm(6-nm-thick extended PLLA chain and 2.5-nm-thick p-pi conjugating TANI bimolecular layer) formed. The possible formation models of those two regular morphologies were presented in detail.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

We have followed the time development of the microdomain structure in symmetric diblock copolymer poly(styrene-b-methyl methacrylate), P(S-b-MMA), ultrathin films via PMMA-selective solvent vapor treatment by atomic force microscopy (AFM). After preparation on a substrate preferentially attracting the PMMA block, PS forms a continuous layer at a film's free surface. With subsequent solvent vapor treatment, the film gradually shows a well-ordered hexagonally packed nanocylinders structure. It is shown that only when the film thickness is less than the 1/2L(0) (lamellar repeat spacing), and exposed to PMMA block selective solvent for an appropriate time, can the well-ordered hexagonally packed nanocylinders form. On an extended solvent vapor treatment, a mixed morphology containing nanocylinders and stripes appears, followed by the striped morphologies. When the annealing time is long enough, the film comes back to the flat surface again, however, with PMMA instead of PS dominating the free surface.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

A simple thermal process for the preparation of small Pt nanoparticles is presented, carried out by heating a H-2-PtCl6/3- thiophenemalonic acid aqueous solution. The following treatment of such colloidal Pt solution with Ru( bpy)(3)(2+) causes the assembly of Pt nanoparticles into aggregates. Most importantly, directly placing such aggregates on bare solid electrode surfaces can produce very stable films exhibiting excellent electrochemiluminescence behaviors.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

A new orthorhombic phase of BaEu2Mn2O7 with the space group of Ccmm (no.63) was identified for single crystals after heat treatment and its Crystal Structure was determined by single crystal X-ray diffractometry. The volume Of the unit cell has twice the fundamental tetragonal cell and corner-shared MnO6 octahedra are slightly distorted and Mn-O-Mn angle between the neighboring octahedra tilts with an angle by around 3 degrees from b-axis. It is concluded from the results of the heat treatment of single crystals at various temperatures that this orthorhombic phase changes into a tetragonal One With superstructure (P4(2)/mnm) at 402 K and changes once more into the fundamental tetragonal phase (I4/mmm) above 552 K. The tetragonal phase with superstructure which has been expected to be an unstable one is stable between the two temperatures.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Dendrimer-protected gold nanoparticles have been facilely obtained by heating an aqueous solution containing third generation poly(propyleneimine) dendrimers and HAuCl4 without the additional step of introducing other reducing agents. Transmission electron microscopy (TEM) and UV vis data indicate the size the nucleation and growth kinetics of gold nanoparticles thus formed which can be tuned by changing the initial molar ratio of dendrimer to gold.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Measurement of iron and manganese is very important in evaluating the quality of natural waters. We have constructed an automated Fe(II), total dissolved iron(TDI), Mn(II), and total dissolved manganese(TDM) analysis system for the quality control of underground drinking water by reverse flow injection analysis and chemiluminescence detection(rFIA-CL), The method is based on the measurement of the metal-catalyzed light emission from luminol oxidation by potassium periodate. The typical signal is a narrow peak, in which the height is proportional to light emitted and hence to the concentration of metal ions. The detection limits were 3 x 10(-6) mu g ml(-1) for Fe(II) and the linear range extents up to 1.0 x 10(-4) and 5 x 10(-6) mu g ml(-1) for Mn(II) cover a linear range to 1.0 x 10(-4) mu g ml(-1). This method was used for automated in-situ monitoring of total dissolved iron and total dissolved in underground water during water treatment. (C) 1997 Elsevier Science B.V.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Using the wide-angle X-ray diffraction method, the variation of crystallographic parameters of poly(aryl ether ether ketone ketone) (PEEKK) has been studied in different heat treatment temperatures. All the reflections and their intensities as well as their Miller indices are presented in detail according to an orthorhombic system. The investigation indicates that the unit cell parameters a, b, c and the unit cell volume V systematically decrease with increasing heat treatment temperature. This variation is interpreted by the change of conformation of polymer molecular chains during thermal treatment. The results calculated from the formula of degree of crystallinity (W-c,W-x) for PEEKK, which was derived based on X-ray scattering intensity theory and the graphic multipeak resolution method, are compatible with the density measurement (W-c,W-d) and calorimetry (W-c,W-h) values. (C) 1997 Elesevier Science Ltd.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The structural parameters of the aggregated state of polyamide (PA)-1010 annealed at various temperatures were computed by means of the desmearing intensity from Smalt Angle X-ray Scattering (SAXS) measurements and by using the concept of the distance distribution function. The results indicated that the structural parameters of the aggregated state were strongly dependent upon heat treatment conditions and the maximum values of the structural parameters were obtained for the samples annealed at T = 175 degrees C. The particle size Z annealed at different temperature was ranged between 8.1-12.8nm, and the values of the distance distribution function P-max(Z) were obtained when Z = 4.0-6.8 nm. Using one dimension electron density correlation function (1D EDCF) method long period (L) and thickness of the lamellar (d(0)) were estimated and were found to increase with the increase of the degree of crystallinity.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The variations of unit cell parameters and crystallite size of nine PEEK samples treated at various temperatures have been studied by using Wide-Angle X-ray Diffraction (WAXD), The results indicate a decrease in unit cell parameter a,b and c but an increase in crystallite size L(hkl) With the increase beat treatment temperature. Based on X-ray scattering intensity theory and using the graphic multipeak resolution method, the formula of degree of crystallinity (W-c,W-X) for PEEK is derived. The results calculated are compatible with the density measurement and calorimetry.