918 resultados para Cotton yarn
Resumo:
The question posed in the title has been addressed by studying the swelling of celluloses at 20 C by twenty protic solvents, including water; linear- and branched-chain aliphatic alcohols; unsaturated aliphatic alcohols, and alkoxyalcohols. The biopolymers investigated included microcrystalline cellulose, MC, native and never-dried mercerized cotton cellulose, cotton and M-cotton, and native and never-dried mercerized eucalyptus cellulose, eucalyptus and M-eucalyptus, respectively. In most cases, better correlations with the physico-chemical properties of the solvents were obtained when the swelling was expressed as number of moles of solvent/anhydroglucose unit, nSw, rather than as % increase in sample weight. The descriptors employed in these correlations included, where available, Hildebrand`s solubility parameters, Gutmann`s acceptor and donor numbers, solvent molar volume, V(S), as well as solvatochromic parameters. The latter, employed for the first time for correlating the swelling of biopolymers, included empirical solvent polarity, E(T)(30), solvent ""acidity"", alpha(S), ""basicity"", beta(S), and dipolarity/polarizability, pi(S)*, respectively. Small regression coefficients and large sums of the squares of the residues were obtained when values of nSw were correlated with two solvent parameters. Much better correlations were obtained with three solvent parameters. The most statistically significant descriptor in the correlation equation depends on the cellulose, being pi(S)* for MC, cotton, and eucalyptus, and V(S) for M-cotton and M-eucalyptus. The best correlations were obtained with the same set of four parameters for all celluloses, namely, solvent pKa (or alpha(S)) beta(S), pi(S)*, and V(S), respectively. These results indicate that the supra-molecular structure of the biopolymer, in particular the average sizes of crystallites and micro-pores, and the presence of its chains in parallel (cellulose I) or anti-parallel (cellulose II) arrangements control its swelling. At least for the present biopolymer/solvent systems, use of solvatochromic parameters is a superior alternative to Hildebrand`s solubility parameters and/or Gutmann`s acceptor and donor numbers. The relevance of these results to the accessibility of the hydroxyl groups of cellulose, hence to its reactivity, is briefly discussed.
Resumo:
The acylation of three cellulose samples by acetic anhydride, Ac(2)O, in the solvent system LiCl/N,N-dimethylacetamide, DMAc (4 h, 110 A degrees C), has been revisited in order to investigate the dependence of the reaction efficiency on the structural characteristics of cellulose, and its aggregation in solution. The cellulose samples employed included microcrystalline, MCC; mercerized cotton linters, M-cotton, and mercerized sisal, M-sisal. The reaction efficiency expresses the relationship between the degree of substitution, DS, of the ester obtained, and the molar ratio Ac(2)O/AGU (anhydroglucose unit of the biopolymer); 100% efficiency means obtaining DS = 3 at Ac(2)O/AGU = 3. For all celluloses, the dependence of DS on Ac(2)O/AGU is described by an exponential decay equation: DS = DS(o) - Ae(-[(Ac2O/AGU)/B]); (A) and (B) are regression coefficients, and DS(o) is the calculated maximum degree of substitution, achieved under the conditions of each experiment. Values of (B) are clearly dependent on the cellulose employed: B((M-cotton)) > B((M-sisal)) > B((MCC)); they correlate qualitatively with the degree of polymerization of cellulose, and linearly with the aggregation number, N(agg), of the dissolved biopolymer, as calculated from static light scattering measurements: (B) = 1.709 + 0.034 N(agg). To our knowledge, this is the first report on the latter correlation; it shows the importance of the physical state of dissolved cellulose, and serves to explain, in part, the need to use distinct reaction conditions for MCC and fibrous celluloses, in particular Ac(2)O/AGU, time, temperature.
Resumo:
The effects of alkali treatment on the structural characteristics of cotton linters and sisal cellulose samples have been studied. Mercerization results in a decrease in the indices of crystallinity and the degrees of polymerization, and an increase in the alpha-cellulose contents of the samples. The relevance of the structural properties of cellulose to its dissolution is probed by studying the kinetics of cellulose decrystallization, prior to its solubilization in LiCl/N,N-dimethylacetamide (DMAc). Our data show that the decrystallization rate constants and activation parameters are only slightly dependent on the physico-chemical properties of the starting celluloses. This multi-step reaction is accompanied by a small enthalpy and large, negative, entropy of activation. These results are analyzed in terms of the interactions within the biopolymer chains during decrystallization, as well as those between the two ions of the electrolyte and both DMAc and cellulose.