[EN] What is Braulio asking from Eugenius in this passage: that he requires a Mass to be celebrated (where?) in honour of San Millán, or that Eugenius himself writes the Mass, or, simply, some parts or prayers for it? Firstly, translations and interpretations provided by scholars to date are checked and criticized; then an interpretation of the passage is proposed, being based on textual criticism approaches, on the work context and on the cultural environment in which this work takes place.
Resumo:
This publication gives fishery statistics relating to the landings of the Ivorian trawlers in Abidjan in 1983. The data used are the inquiries made by the C.R.O. on the boats and the auction sheets of the fishing harbour. The data processing was executed on the C.R.O. computer.
Resumo:
This publication gives the results of the bottom trawlings made during the cruises Togo 5 and Togo 6 by the oceanographic research vessel "Andre Nizery" on the continental shelf of Togo during the estimation program of halieutic resources. The report includes: 1 - the report of the cruises Togo 5 and Togo 6; 2 - Some information on the presentation of the results; 3 - the trawl recording maps for the 2 cruises; 4 - The length frequency distributions of the measured samples.
Resumo:
采用提拉法生长了Yb掺杂原子数分数为0.5%的Yb:Y3Al5O12。(Yb2YAG)晶体,对晶体的吸收光谱和荧光光谱进行了分析。与Yb掺杂原子数分数为5%的Yb:YAG晶体进行了对比,得出采用940nm激光二极管(LD)抽运晶体最为合适。原子数分数为0.5%的Yb:YAG晶体相对于原子数分数为5%的Yb:YAG晶体白吸收效应的影响要小。测量了原子数分数为0.5%的Yb:YAG晶体的荧光寿命为0.95ms,与理论值很接近。因此采用原子数分数为0.5%的Yb:YAG晶体作为激光工作物质将有利于高效、小型集成
Resumo:
In this work, microwave dielectric properties of A-site substitution by La3+ in (Pb0.45Ca0.55) (Fe0.5Nb0.5) 03 system were investigated. Microwave dielectric properties of A-site charge unbalance substitution of [(Pb0.45Ca0.55)(1-x) La-x] (Fe0.5Nb0.5)O-3(+) (P45CLFN) were improved because the solid solution of small amount of surplus La3+ with (Pb, Ca)(2+) could eliminate oxygen vacancies, and the formation of secondary phase (pyrochlore) was also caused by surplus La3+. The decreasing of dielectric constant with the increase of La3+ content is due to the formation of pyrochlore. The grain size is changed slightly and Q(f) values (7000 similar to 7300 GHz) are almost unchanged at x = 0.02 similar to 0.10, but the temperature coefficient of resonant frequency (TCF) are increased and changed from negative to positive. TCF is zero at x 0.075 with Q(f) = 7267 GHz and K = 89. TCF of all specimens are within +/- 5 x 10(-6)degrees C-1.
Resumo:
For the first time, a quaternary doping system of Er3+, Yb3+, Ce3+, Na+:CaF2 single crystal was demonstrated to have high fluorescence yield in the eye-safe 1.5 mu m region under 980 nm laser diode pumping, with relatively broad and flat gain curves. A simplified model was established to illustrate the effect of Ce3+ on the branching ratio for the Er3+4I11/2 -> I-4(13/2) transition. With 0.2-at.% Er3+ and 2.0-at.% Ce3+ in the quaternary-doped CaF2 crystal, the branching ratio was estimated to be improved more than 40 times by the deactivating effect of Ce3+ on the Er3+ 4I11/2 level. The quaternary-doped CaF2, system shows great potential to achieve high laser performance in the 1.5 mu m region. (c) 2006 Elsevier B.V. All rights reserved.
Resumo:
采用提拉法生长Y3Al5O12(YAG)晶体和Yb3+掺杂原子数分数分别为5%, 10%, 15%, 20%, 25%, 50%和100%的Yb∶Y3Al5O12(Yb∶YAG)晶体。系统表征和分析了Yb3+掺杂浓度对拉曼光谱的影响。随着Yb3+掺杂浓度的增加,晶体的振动模式没有明显的变化,晶体结构没有改变;在370 cm-1和785 cm-1附近,振动吸收峰的半峰全宽逐渐增大。分析得出,Yb3+掺杂浓度对晶体的晶格、对称性、荧光寿命均有影响,从而可能影响到晶体的光谱和激光性能。
Resumo:
The effects of gamma-irradiation on the air-annealed 10 at.% Yb:Y3Al5O12 (YAG) and air annealing on the gamma-irradiated 10at.% Yb:YAG have been studied by the difference absorption spectra before and after treatment. The gamma-irradiation and air annealing led to opposite changes of the absorption properties of the Yb:YAG crystal. After air annealing, the gamma-irradiation induced centers were totally removed and the concentration of Fe3+ and Yb3+ were lightly increased. For the first time, the gamma-irradiation induced valence changes between Yb3+ and Yb2+ ions in Yb:YAG crystals have been observed. (C) 2007 Elsevier B.V. All rights reserved.
Resumo:
Er3+ -doped Gd2SiO5 (Er:GSO) single crystal with dimensions of circle divide 35 x 40 mm(3) has been grown by the Czochralski method. The absorption and fluorescence spectra of the Er:GSO crystal were measured at room temperature. The spectral parameters were calculated based on Judd-Ofelt theory, and the intensity parameters Omega(2), Omega(4) and Omega 6 are obtained to be 6.168 x 10(-20), 1.878 x 10(-20), and 1.255 x 10(-20) cm(2), respectively. The emission cross-section has been calculated by Fuechtbauer-Ladenbury formula. (c) 2007 Elsevier B.V. All rights reserved.
Resumo:
High optical quality Lu2SiO5 (LSO) and (Lu0.5Gd0.5)(2)SiO5 (LGSO) laser crystals codoped with Er3+ and Yb3+ have been fabricated by the Czochralski method. Intense upconversion (UC) and infrared emission (1543 nm) are observed under excitation of 975 nm. The luminescence processes are explained and the emission efficiencies are quantitatively obtained by measuring the UC efficiency and calculating the emission cross section. The temperature-dependent optical properties of the crystals are also investigated. Our study indicates that Er3+-Yb3+ : LSO and Er3+-Yb3+: LGSO crystals are promising gain media for developing the solid-state 1.5 mu m optical amplifiers and tunable UC lasers. (c) 2008 American Institute of Physics.
Resumo:
This paper reports that the TM3+:Lu2SiO5 (Tm:LSO) crystal is grown by Czochralski technique. The room-temperature absorption spectra of Tm:LSO crystal are measured on a b-cut sample with 4 at.% thulium. According to the obtained Judd-Ofelt intensity parameters Omega(2)=9.3155 x 10(-20) cm(2), Omega(4)=8.4103 x 10(-20) cm(2), Omega(6)=1.5908 x 10(-20) cm(2), the fluorescence lifetime is calculated to be 2.03 ms for F-3(4) -> H-3(6) transition, and the integrated emission cross section is 5.81 x 10(-18) cm(2). Room-temperature laser action near 2 mu m under diode pumping is experimentally evaluated in Tm:LSO. An optical-optical conversion efficiency of 9.1% and a slope efficiency of 16.2% are obtained with continuous-wave maximum output power of 0.67 W. The emission wavelengths of Tm:LSO laser are centred around 2.06 mu m with spectral bandwidth of similar to 13.6 nm.
Resumo:
A bulk crystal of Yb:Sc2SiO5 (Yb:SSO) with favorable thermal properties was successfully obtained by the Czochralski method. The energy level diagrams for Yb:SSO crystal were determined by optical spectroscopic analysis and semi-empirical crystal-field calculations using the simple overlap model. The full width at half maximum of the absorption band centering at 976 nm was calculated to be 24 nm with a peak absorption cross-section of 9.2x10(-21) cm(2). The largest ground-state splitting of Yb3+ ions is up to 1027 cm(-1) in a SSO crystal host. Efficient diode-pumped laser performance of Yb:SSO was primarily demonstrated with a slope efficiency of 45% and output power of 3.55 W.