928 resultados para Mesoporous Zeolite
Resumo:
Two porous zirconium methylphosphonates (designated as ZMPmi and ZMPme respectively) were synthesized by using dibutyl methylphosphonate (DBMP) as a template. Two efficient post-synthetic treatments were developed to remove the incorporated template without destroying the hybrid structures. The materials were characterized by SEM, EPMA, TG, DTA, FTIR, and NMR. Specific surface area and porosity were evaluated by BET, alpha(s)-plots and DFT methods based on N-2 adsorption-desorption isotherms. The specific surface areas of ZMPmi and ZMPme are determined to be 279 and 403 m(2) g(-1) and the maxima of pore size distributions are at 0.7 and 1.3 nm respectively. (c) 2005 Elsevier Inc. All rights reserved.
Resumo:
The production of ethylbenzene from the alkylation of dilute ethylene in fee off-gases with benzene has been commercialized in China over a newly developed catalyst composed of ZSM-5/ZSM-11 co-crystallized zeolite. The duration of an operation cycle of the commercial catalyst could be as long as 180 days. The conversion of ethylene could attain higher than 95%, while the amount of coke deposited on the catalyst was only about 10 wt.%. Thermogravimetry (TG) was used to study the coking behavior of the catalyst during the alkylation of fee off-gas with benzene to ethylbenzene. Based on effects of reaction time, reaction temperature, reactants and products on coking during the alkylation process, it is found that the coking rate during the alkylation procedure follows the order: ethylbenzene > ethylene > propylene > benzene for single component, and benzene-ethylene > benzene-propylene for bi-components under the same reaction condition. Furthermore, the coking kinetic equations for benzene-ethylene, benzene-propylene and ethylbenzene were established. (C) 2003 Elsevier B.V. All rights reserved.
Resumo:
It was explored by density functional calculations that exchanged La or P species exert great influence on the local Al sites as well as on the adjacent exchanged species. In partially exchanged La- or P/H-ZSM-5 zeolite, some of the Al sites will fall off from the zeolite framework even more easily than in H-form ZSM-5, consistent with our XRF experiments. However, when exchanged by both La and P species, Al at either of the two exchanged sites shows better stability compared to H-from. zeolite. La and P species will interact strongly with each other, as evidenced by the charge donation process and the shortening of P-O-1 bond length. It was just the cooperation of La and P species that enabled RSCC catalysts worked normally under severe conditions. (C) 2004 Elsevier B.V. All rights reserved.
Resumo:
ZSM-5 zeolites with similar SUM ratio were synthesized successfully using various templates (n-butylamine (BTA), ethylamine (ETA), isopropylamine (IPA), ethylenediamine (EDA), ethanol (ETL), ethanol-ammonium (ETL-AM) and no template (NT)) under hydrothermal conditions. The samples were characterized by XRD, SEM, XRF, NH3-TPD and BET surface area measurements in order to understand the template effects and the differences of the ZSM-5 samples. The synthesis of ZSM-5 with organic templates was relatively easier than those with inorganic templates and without template. SEM results revealed that ZSM-5 synthesized with different templates had different morphology and particle size. The Si/Al ratio and BET specific surface area of the sample with ethanol as template was the lowest. NH3-TPD results showed that the sample synthesized without template had fewer strong acid sites than others. n-Hexane cracking reaction was carried out over the samples to evaluate the catalytic properties. All ZSM-5 zeolites were effective in n-hexane cracking reaction, especially for the sample synthesized without template. (C) 2004 Elsevier B.V. All rights reserved.
Resumo:
By characterizing fresh and used Mo/HMCM-22 catalysts with ICP-AES, XRD, NH3-TPD technique, UV - Vis DRS and UV Raman spectroscopy, the reactivity of Mo species for methane partial oxidation into formaldehyde were directly studied with a new point of view. By comparing the fresh and used catalysts, it was found that the tetrahedral Mo species bonding chemically to the support surface were practically unchanged after the reaction, while the polymolybdate octahedral Mo species, which had a rather weak interaction with the MCM-22 zeolite, leached out during the reaction, especially when the Mo loading was high. Correspondingly, it was found from the time-on-stream reaction data that the HCHO yield remained unchanged, while COx decreased with the reaction time during the reaction. By combining the characterization results and the reaction data, it can be drawn that the isolated tetrahedral molybdenum oxo-species (T-d) is responsible for HCHO formation, while the octahedral polyoxomolybdate species (O-h) will lead to the total oxidation of methane.
Resumo:
The role of acid strength of zeolites in liquid-phase alkylation of benzene with ethylene was studied over beta, MCM-22, and USY zeolites by means of adsorbing NH3 at different temperatures. The strong acid sites are active centers, while the weak acid sites are inactive. The selectivity behavior of the strong acid sites varies with the relative acid strength as well as the types of the zeolites.
Resumo:
The transformation of olefin to aromatics over ZSM-5 catalysts with different K-loadings has been investigated both in a continuous flow fixed-bed reactor and in a pulse microreactor. Investigation of variation of olefin aromatization activity with K-loadings shows that strong acid sites are indispensable for the converting of olefin to aromatics. As intermediates of olefin aromatization process, butadiene and cyclopentene not only show much higher aromatization activity than mono-olefins, but also can be transformed into aromatics over relatively weak acid sites of K/ZSM-5. A proposal is put forward, stating that among all the steps experienced in olefins aromatization, the formation of diene or cycloolfin from mono-olefins through hydrogen transfer is the key step and can be catalyzed by strong acid sites.
Resumo:
The oxidative dehydrogenation of ethane (ODE) with CO2 to C2H4 has been studied over a series of Cr-based catalysts using SiO2, Al2O3, (MCM-41 zeolite) MCM-41, MgO and Silicate-2 (Si-2) as the supports. TPR, NH3-TPD, and EPR characterizations of catalysts were carried out to investigate the reduction property of Cr species on different supports, the acidities of catalysts and Cr species of 6Cr/SiO2 catalysts, respectively.
Resumo:
The role of Bronsted acidity of titanium silicalite zeolite (with different ratios of Si/Ti) in oxidation reactions of styrene has been investigated and discussed. For zeolites with Si/Ti > 42, most of the titanium is in the zeolite framework. These framework titanium species, which act both as the isolated titanium centers and as Bronsted acidity centers (together with the Bronsted acidity produced by the tetrahedral aluminum impurity introduced during synthesis), can catalyze both the epoxidation and the succeeding rearrangement reactions, thus promoting the formation of phenylacetaldehyde. With an increase in the titanium content of the zeolite, titanium will tend to stay outside the zeolite lattice, except for the TiOx nanophases which can be occluded in the zeolite channels or on the external surface. These non-framework titanium species are favorable for the carbon-carbon bond scission, leading to the production of additional benzaldehyde. The catalytic performances of these zeolites with different Si/Ti ratios are correlated here with their structural information by using solid-state NMR and UV-Vis methods. (C) 2003 Elsevier B.V. All rights reserved.
Resumo:
Silver impregnated H-ZSM-5 zeolite catalysts with silver loading from 3 to 15 wt.% were investigated for the selective catalytic reduction (SCR) of NOx with CH4 in the excess of oxygen. X-ray diffraction (XRD) and UV-Vis measurements established the structure of silver catalysts. A relationship between the structure of silver catalysts and their catalytic functions for the SCR of NOx by CH4 was clarified. The NO conversion to N-2 showed a S-shape dependence on the increase of Ag loading. No linear dependence of catalytic activity on the amount of silver ions in the zeolite cation sites was observed. Contrastively, the activity was significantly enhanced by the nano-sized silver particles formed on the higher Ag loading samples (greater than or equal to7 wt.%). Temperature programmed desorption (TPD) and temperature programmed reduction (TPR) studies showed that nano-silver particles provided much stronger adsorption centers for active intermediates NO3-(s) on which adsorbed NO3-(s) could be effectively reduced by the activated methane. Silver ions in the zeolite cation sites might catalyze the reaction through activation of CH4 at lower temperatures. Activated CH4 reacted with NO3-(s) adsorbed on nano-silver particles to produce N-2 and CO2. (C) 2003 Elsevier B.V. All rights reserved.
Resumo:
Post-steaming treatment of Mo/HZSM-5 catalysts results in more molybdenum species migrating into and residing in the HZSM-5 zeolite channels. This is confirmed by XRF and XPS measurements. H-1 MAS NMR and Si-29 MAS NMR also demonstrate that the number of free Bronsted acid sites decreases in the Mo/HZSM-5 catalysts that underwent post-steaming treatment, compared to untreated Mo/HZSM-5 catalysts. As a result, the deactivation rate constant (kd) on the Mo/HZSM-5 catalyst after post-steaming treatment for 0.5 h is much smaller, and the catalyst therefore shows remarkable stability in the probe reaction of methane dehydro-aromatization. The results suggest that a more beneficial bi-functional balance between active Mo species for methane activation and acid sites for the following aromatization is developed over those Mo/HZSM-5 catalysts that have experienced post-steaming treatment for 0.5 h, in comparison with the untreated Mo/HZSM-5 catalysts.
Resumo:
The surface properties, porosities, and adsorption capacities of activated carbons (AC) are modified by the oxidation treatment using concentrated H2SO4 at temperatures 150-270 degreesC. The modified AC was characterized by N-2 adsorption, base titration, FTIR, and the adsorption of iodine, chlorophenol, methylene blue, and dibenzothiophene. The treatment of AC with concentrated H2SO4 at 250 degreesC greatly increases the mesoporous volume from 0.243 mL/g to 0.452 mL/g, specific surface areas from 393 m(2)/g to 745 m(2)/g, and acidic surface oxygen complexes from 0.071 meq/g to 1.986 meq/g as compared with the unmodified AC. The base titration results indicate that the amount of acidic surface oxygen groups on the modified AC increases with increasing the treatment temperatures and carboxyls and phenols are the most abundant carbon-oxygen functional groups. The carboxyl groups, COO- species, and hydroxyl groups are detected mainly for the sample treated at 250 degreesC. The mesoporous properties of the AC modified by concentrated H2SO4 were further tested by the adsorption of methylene blue and dibenzothiophene. The AC modified by concentrated H2SO4 at 250 degreesC has much higher adsorption capacities for large molecules (e.g., methylene blue and dibenzothiophene) than the unmodified AC but less adsorption capacities for small molecules (e.g., iodine). The adsorption results from aqueous solutions have been interpreted using Freundlich adsorption models.
Resumo:
A metal ions (Ag, Bi, V, Mo) modified sol-gel method was used to prepare a mesoporous Ag0.01Bi0.85V0.54Mo0.45O4 catalytic membrane which was used in the selective oxidation of propane to acrolein. By optimizing the preparation parameters, a thin and perfect catalytically active membrane was successfully prepared. SEM results showed that the membrane thickness is similar to5 mum. XRD results revealed that Ag0.01Bi0.85V0.54Mo0.45O4 with a Scheelite structure, which is catalytically active for the selective oxidation of propane to acrolein, was formed in the catalytic membrane only when AgBiVMoO concentrations were higher than 40%. Catalytic reaction results demonstrated that the selective oxidation of propane could be controlled to a certain degree, such as to acrolein, in the catalytic membrane reactor (CMR) compared to the fixed bed reactor (FBR). For example, a selectivity of 54.85% for acrolein in the liquid phase was obtained in the CMR, while only 8.31% was achieved in the FBR. (C) 2003 Elsevier B.V. All rights reserved.