959 resultados para MATERIALS SCIENCE - Radiation Effects
Resumo:
The mechanical properties of a typical sintered aluminium alloy (Al-4.4Cu-0.8Si-0.5Mg) have been improved by the simultaneous use of trace additions of Sn, high sintering temperatures and modified heat treatments. Tin increases densification, but the Sn concentration is limited to less than or equal to 0.1wt% because incipient melting occurs during solution treatment at higher Sn levels. A sintering temperature of 620 degrees C increases the liquid volume over that formed at the conventional 590 degrees C sintering temperature. However, the higher sintering temperature results in the formation of an embrittling phase which can be eliminated if solution treatment is incorporated into the sintering cycle (a modified TS heat treatment). These conditions produce a tensile strength of 375 MPa, an increase of nearly 20% over the unmodified alloy. (C) 1999 Elsevier Science S.A. All rights reserved.
Theoretical and numerical analyses of convective instability in porous media with upward throughflow
Resumo:
Exact analytical solutions have been obtained for a hydrothermal system consisting of a horizontal porous layer with upward throughflow. The boundary conditions considered are constant temperature, constant pressure at the top, and constant vertical temperature gradient, constant Darcy velocity at the bottom of the layer. After deriving the exact analytical solutions, we examine the stability of the solutions using linear stability theory and the Galerkin method. It has been found that the exact solutions for such a hydrothermal system become unstable when the Rayleigh number of the system is equal to or greater than the corresponding critical Rayleigh number. For small and moderate Peclet numbers (Pe less than or equal to 6), an increase in upward throughflow destabilizes the convective flow in the horizontal layer. To confirm these findings, the finite element method with the progressive asymptotic approach procedure is used to compute the convective cells in such a hydrothermal system. Copyright (C) 1999 John Wiley & Sons, Ltd.
Resumo:
Freeform fabrication methods allow the direct formation of parts built layer by layer, under the control of a CAD drawing. Most of these methods form parts in thermoplastic or thermoset polymers, but there would be many applications for freeform fabrication of fully functional metal or ceramic parts. We describe here the freeforming of sinterable aluminium alloys. In addition, the building approach allows different materials to be positioned within a monolithic part for an optimal combination of properties. This is illustrated here with the formation of an aluminium gear with a metal-matrix composite wear surface. (C) 1999 Kluwer Academic Publishers.
Resumo:
The effect of alumina on the liquidus temperatures of fayalite slags at iron saturation has been investigated experimentally. Equilibrated synthetic slags were quenched, and the samples were subsequently examined using optical microscopy and electron probe microanalysis (EPMA). The isotherms in the fayalite primary field and boundary lines were determined, and the results were presented in the form of pseudo-ternary phase diagrams of FeO-CaO-SiO2 with 0, 2, 4, and 6 wt pet Al2O3 in the slag. The experimental results show that the alumina addition expands the fayalite primary phase field and decreases the liquidus temperatures in the fayalite primary phase field.
Resumo:
This is the first paper in a study on the influence of the environment on the crack tip strain field for AISI 4340. A stressing stage for the environmental scanning electron microscope (ESEM) was constructed which was capable of applying loads up to 60 kN to fracture-mechanics samples. The measurement of the crack tip strain field required preparation (by electron lithography or chemical etching) of a system of reference points spaced at similar to 5 mu m intervals on the sample surface, loading the sample inside an electron microscope, image processing procedures to measure the displacement at each reference point and calculation of the strain field. Two algorithms to calculate strain were evaluated. Possible sources of errors were calculation errors due to the algorithm, errors inherent in the image processing procedure and errors due to the limited precision of the displacement measurements. Estimation of the contribution of each source of error was performed. The technique allows measurement of the crack tip strain field over an area of 50 x 40 mu m with a strain precision better than +/- 0.02 at distances larger than 5 mu m from the crack tip. (C) 1999 Kluwer Academic Publishers.
Resumo:
Crack tip strain maps have been measured for AISI 4340 high strength steel. No significant creep was observed. The measured values of CTOD were greater than expected from the HRR model. Crack tip branching was observed in every experiment. The direction of crack branching was in the same direction as a major ridge'' of epsilon(yy) strain, which in turn was in the same direction as predicted by the HRR model. Furthermore, the measured magnitudes of the epsilon(y)y strain in this same direction were in general greater than the values predicted by the HRR model. This indicates more plasticity in the crack tip region than expected from the HRR model. This greater plasticity could be related to the larger than expected CTOD values. The following discrepancies between the measured strain fields for AISI 4340 and the HRR predictions are noteworthy: (1) The crack branching. (2) Values of CTOD significantly higher than predicted by HRR. (3) The major ridge'' of epsilon(yy) strain an angle of about 60 degrees with the direction of overall propagation of the fatigue precrack, in which the measured magnitudes of the epsilon(yy) strain were greater than the values predicted by the HRR model. (4) Asymmetric shape of the plastic zone as measured by the epsilon(yy) strain. (5) Values of shear strain gamma(xy) significantly higher than predicted by the HRR model. (C) 1999 Kluwer Academic Publishers.
Resumo:
This paper studied the influence of hydrogen and water vapour environments on the plastic behaviour in the vicinity of the crack tip for AISI 4340. Hydrogen and water vapour (at a pressure of 15 Torr) significantly increased the crack tip opening displacement. The crack tip strain distribution in 15 Torr hydrogen was significantly different to that measured in vacuum. In the presence of sufficient hydrogen, the plastic zone was larger, was elongated in the direction of crack propagation and moreover there was significant creep. These observations support the hydrogen enhanced localised plasticity model for hydrogen embrittlement in this steel. The strain distribution in the presence of water vapour also suggests that SCC in AISI 4340 occurs via the hydrogen enhanced localised plasticity mechanism. (C) 1999 Kluwer Academic Publishers.
Resumo:
An extensive research program focused on the characterization of various metallurgical complex smelting and coal combustion slags is being undertaken. The research combines both experimental and thermodynamic modeling studies. The approach is illustrated by work on the PbO-ZnO-Al2O3-FeO-Fe2O3-CaO-SiO2 system. Experimental measurements of the liquidus and solidus have been undertaken under oxidizing and reducing conditions using equilibration, quenching, and electron probe X-ray microanalysis. The experimental program has been planned so as to obtain data for thermodynamic model development as well as for pseudo-ternary Liquidus diagrams that can be used directly by process operators. Thermodynamic modeling has been carried out using the computer system FACT, which contains thermodynamic databases with over 5000 compounds and evaluated solution models. The FACT package is used for the calculation of multiphase equilibria in multicomponent systems of industrial interest. A modified quasi-chemical solution model is used for the liquid slag phase. New optimizations have been carried out, which significantly improve the accuracy of the thermodynamic models for lead/zinc smelting and coal combustion processes. Examples of experimentally determined and calculated liquidus diagrams are presented. These examples provide information of direct relevance to various metallurgical smelting and coal combustion processes.
Resumo:
Hypoeutectic AI-Si alloys represent the most widely used alloy system for cast aluminium applications. This system has a unique behaviour with respect to grain formation where an increase in silicon content results in a transition to larger grain sizes after a minimum at an intermediate concentration. As a result of the already large solute content, grain refinement by solute additions is inefficient and nucleant particles from the common aluminium grain refiners are not as effective as in wrought alloys. However, casting conditions, such as a low pouring temperature, that promote the formation of wall crystals tie. crystals nucleated in the thermally undercooled layer at or next to mould walls) are very effective in yielding a small grain size. This paper presents results of an investigation of the effect of low superheat and mould preheat temperature on grain size. It was found that pouring temperature controls the effectiveness of the wall mechanism while mould preheat has little effect until high preheat temperatures at which a large increase in grain size occurs. The observed changes in grain size are explained in terms of the balance between nucleation rate and survival rate of crystal nuclei resulting from changes in superheat and mould temperature.
Resumo:
The solution treatment stage of the T6 heat-treatment of Al-7%Si-Mg foundry alloys influences microstructural features such as Mg2Si dissolution, and eutectic silicon spheroidisation and coarsening. Microstructural and microanalytical studies have been conducted across a range of Sr-modified Al-7%Si alloys, with an Fe content of 0.12% and Mg contents ranging from 0.3-0.7wt%. Qualitative and quantitative metallography have shown that, in addition to the above changes, solution treatment also results in changes to the relative proportions of iron-containing intermetallic particles and that these changes are composition-dependent. While solution treatment causes a substantial transformation of pi phase to beta phase in low Mg alloys (0.3-0.4%), this change is not readily apparent at higher Mg levels (0.6-0.7%). The pi to beta transformation is accompanied by a release of Mg into the aluminum matrix over and above that which arises from the rapid dissolution of Mg2Si. Since the level of matrix Mg retained after quenching controls an alloy's subsequent precipitation hardening response, a proper understanding of this phase transformation is crucial if tensile properties are to be maximised.
Resumo:
The high strength to weight ratio of magnesium alloys makes them extremely attractive for applications in transport or aerospace technology. However, their corrosion behavior is a major issue and one reason why they are still not as popular as aluminum alloys. This papers reviews the corrosion mechanisms of magnesium and provides the basis for the design of new alloys with improved corrosion properties.
Resumo:
First of all, we would like to clarify that the passive to active transition was determined not by using Solgasmix [1], but by combining thermodynamic equilibrium and mass balance for the oxidation of SiC under pure CO2 and pure CO. The model used in our paper [2]was an extension ofWagner’s model [3], in a similar way as Balat et al. [4] did for the oxidation of SiC in oxygen.
Resumo:
Mesoporous Mobil catalytic materials of number 41 (MCM-41) silica was chemically modified using both inorganic and organic precursors and characterized using the techniques, XRD, XPS, MAS NMR, FTIR, W-Vis, and physical adsorption of nitrogen, hydrocarbons (hexane, benzene, acetone, and methanol) and water vapor. Modification using organic reagents was found to result in a significant loss in porosity and a shape change of surface properties (increased hydrophobicity and decreased acidity). With inorganic modifying reagents, the decrease in porosity was also observed while the surface properties were not significantly altered as reflected by the adsorption isotherms of organics and water vapors. Chemical modifications can greatly improve the hydrothermal stability of MCM-41 material because of the enhanced surface hydrophobicity (with organic modifiers) or increased pore wall thickness (with inorganic modifiers). (C) 2000 Elsevier Science B.V. All rights reserved.
Resumo:
The reported experimental work on the systems Fe-Zn-O and Fe-Zn-Si-O in equilibrium with metallic iron is part of a wider research program that combines experimental and thermodynamic computer modeling techniques to characterize zinc/lead industrial slags and sinters in the system PbO-ZnO-SiO2-CaO-FeO-Fe2O3. Extensive experimental,investigations using high-temperature equilibration and quenching techniques followed by electron probe X-ray microanalysis (EPMA) were carried out. Special experimental; procedures were developed to enable accurate measurements in these ZnO-containing systems to be performed in equilibrium with metallic iron; The systems Fe-Zn-O and FeZn-Si-O were experimentally investigated in equilibrium with metallic iron in the temperature ranges 900 degreesC to 1200 degreesC (1173 to 1473 K) and from 1000 degreesC to 1350 degreesC (1273 to 1623 K), respectively. The liquidus surface in the system Fe-Zn-Si-O in equilibrium with metallic iron was characterized in the composition ranges 0 to 33 wt pet ZnO and 0 to 40 wt pet SiO2. The wustite (Fe,Zn)O, zincite (Zn,Fe)O, willemite (Zn,Fe)(2)SiO4, arid fayalite: (Fe,Zn)(2)SiO4 solid solutions in equilibrium with metallic iron were measured.