965 resultados para Dental prosthesis


Relevância:

20.00% 20.00%

Publicador:

Resumo:

The aim of this study was to determine the cutting ability of chemical vapor deposition (CVD) diamond burs coupled to an ultrasonic dental unit handpiece for minimally invasive cavity preparation. One standard cavity was prepared on the mesial and distal surfaces of 40 extracted human third molars either with cylindrical or with spherical CVD burs. The cutting ability was compared regarding type of substrate (enamel and dentin) and direction of handpiece motion. The morphological characteristics, width and depth of the cavities were analyzed and measured using scanning electron micrographs. Statistical analysis using the Kruskal-Wallis test (p < 0.05) revealed that the width and depth of the cavities were significantly greater when they were prepared on dentin. Wider cavities were prepared when the cylindrical CVD bur was used, and deeper cavities resulted from preparation with the spherical CVD bur. The direction of handpiece motion did not influence the size of the cavities, and the CVD burs produced precise and conservative cutting.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Purpose: To evaluate the fatigue resistance of the bond between dentin and glass-infiltrated alumina ceramic, using different luting protocols. Materials and Methods: The null hypothesis is that the fatigue resistance varies with the luting strategy. Forty blocks of In-Ceram Alumina were prepared, and one surface of each block was abraded with 110-μm aluminum oxide particles. Then, the blocks were luted to flat dentin surfaces of 40 human third molars, using 4 different luting strategies (luting system [LS]/ceramic surface conditioning [CSC]) (n=10): (G1) [LS] RelyX-Unicem/[CSC] airborne abrasion with 110-μm Al2O3 particles; (G2) [LS] One-Step + Duo-Link (bis-GMA-based resin)/[CSC] etching with 4% hydrofluoric acid + silane agent; (G3) [LS] ED-Primer + Panavia F (MDP-based resin)/[CSC] Al2O 3; (G4) [LS] Scotchbond1+RelyX-ARC (bis-GMA-based resin)/[CSC] chairside tribochemical silica coating (air abrasion with 30-μm SiO x particles + silane). After 24 h of water storage at 37°C, the specimens were subjected to 106 fatigue cycles in shear with a sinusoidal load (0 to 21 N, 8 Hz frequency, 37°C water). A fatigue survivor score was given, considering the number of the fatigue cycles until fracture. The failure modes of failed specimens were observed in a SEM. Results: G3 (score = 5.9, 1 failure) and G4 (score = 6, no failures) were statistically similar (p = 0.33) and had significantly higher fatigue resistance than G1 (score = 3.9, 5 failures) and G2 (score = 3.7, 6 failures) (p < 0.03). SEM analysis of fractured specimens of G1 and G2 showed that almost all the failures were between ceramic and cement. Conclusion: The MDP-based resin cement + sandblasting with Al2O3 particles (G3) and bis-GMA-based resin cement + tribochemical silica coating (G4), both using the respective dentin bonding systems, were the best luting protocols for the alumina ceramic. The null hypothesis was confirmed.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

A histological study was conducted of the alveolar bone healing process following tooth extraction of dehydrated rats after the implantation of fibrin adhesive (TISSUCOL™) associated to previous irrigation of the wound with a 5% epsilon aminocaproic acid solution (EACA). Seventy two rats were used, divided into three groups receiving different treatments after the surgical procedure. In group I, the gingival mucosa was sutured after extraction of the right upper incisor. In groups II and III, chronic dehydration was produced by water deprivation for 9 days (3 days in the preoperative period and 6 days in the postoperative period). In the animals of Group II, after tooth extraction, the gingival mucosa was sutured in the same way as performed in group I. In group III, after extraction, the dental socket was irrigated with 5% EACA, followed by implantation of the fibrin adhesive (TISSUCOL™). The mucosa was sutured in the same way as performed in the other groups. At 3, 7, 15 and 21 postoperative days, the animals were sacrificed in number of 6 for each group. Specimens containing the dental socket were removed and fixed in 10% formalin and decalcified in an equal part formic acid and sodium citrate solution. After routine processing, the specimens were embedded in paraffin for microtomy. We obtained 6 μm semi-serial slices that were stained with hematoxylin and eosin for histological evaluation. The results showed that the water deprivation in the pre- and postoperative periods caused a delay in the alveolar bone healing process. The use of the fibrin adhesive (TISSUCOL™) produced an improvement in the fibrinolytic picture caused by dehydration.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Dental bleaching is a simple and conservative procedure for aesthetic restoration of vital and non-vital discolored teeth. Nevertheless, a number of studies have demonstrated the risk of tissue damage from the contact of these agents with the oral mucosa. In the current study, the genotoxic potential associated with exposure to dental bleaching agents was assessed by the single cell gel (comet) assay in vitro. Chinese hamster ovary (CHO) cells in vitro were exposed to six commercial dental bleaching agents (Clarigel Gold - Dentsply; Whitespeed - Discus Dental; Nite White - Discus Dental; Magic Bleaching - Vigodent; Whiteness HP - FGM and Lase Peroxide - DMC). The results pointed out that all dental bleaching agents tested contributed to DNA damage as depicted by the mean tail moment, being the strongest effect observed with the highest dose of hydrogen peroxide (Whiteness HP and Lase peroxide, at a 35% concentration). On the other hand, Magic Bleaching (Vigodent) induced the lowest level of DNA breakage. Negative and positive controls displayed absence and presence of DNA-damaging, respectively. Taken together, these results suggest that dental bleaching agents may be a factor that increases the level of DNA damage. A higher concentration of hydrogen peroxide produced higher noxious activities in the genome as detected by single cell gel (comet) assay.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Purpose: This article reports preliminary clinical results of the Speed Master system, a method for immediate loading of implants for the treatment of mandibular edentulism. Materials and Methods: Fifteen patients with edentulous mandibles were consecutively included in the study. Each received 4 implants between the mental foramina placed using the system's surgical guides. Permanent fixed prostheses fabricated over premanufactured titanium bars were attached to the implants on the day of implant placement. The patients were followed for 15 to 27 months (mean, 19 months). Peri-implant tissues were periodically evaluated. Marginal bone loss was monitored with periapical radiographs using a computerized technique. Satisfaction was assessed by means of a questionnaire. Results: The overall implant and prosthetic survival rates were 100%. At the time of the final follow-up visit, mean marginal bone loss was 1.11 mm, and bleeding on probing was not observed. Only 6.7% of the patients reported any discomfort during treatment, and all patients would recommend the procedure to others. Discussion: The immediate loading of implants placed in the edentulous mandible with the Speed Master surgical and prosthetic protocol reduces treatment time and number of surgical procedures in comparison to classic delayed loading protocols. Conclusion: The rehabilitation of the mandible with an immediately delivered occlusally loaded hybrid prosthesis supported by 4 implants does not appear to jeopardize the success of the osseointegration and represents a viable treatment option.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Objectives: The objectives of this study were to assess the fluoride concentration in the public water supply and the prevalence of dental fluorosis in schoolchildren between 7 and 15 years old, living in a peripheral district of the municipality of Bauru. Material and Methods: For this, fifty two water samples were collected on three different days of one week. These samples were analyzed for fluoride by means of the ion-sensitive electrode method (Orion 9609) coupled to a potentiometer (Procyon, model 720). In this method, 1.0 mL of TISAB II (Orion) was added to 1.0 mL of the sample. For the epidemiological survey of fluorosis, 52 schoolchildren of both genders, aged between 7 and 15 were assessed, with prior authorization from their caretakers. Only one person examined the children, after supervised toothbrushing and drying with cotton wool rolls. The TF index was used. Results: The fluoride concentrations in the water samples ranged from 0.62 to 1.20 mg/L, with a mean of 0.9 mg/L. The prevalence of dental fluorosis was 33%, with severity ranging from TF1 to TF4 (Kappa of 0.73 and concordance of 83.33%). Conclusions: The results from the analysis of water samples indicated a fluoride concentration greater than recommended for Bauru. The fluorosis levels found were higher than expected for a peripheral district, in which water is one of the few sources of fluoride.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Purpose: The aim of this study was to evaluate the effect of two surface conditioning methods on the microtensile bond strength of a resin cement to three high-strength core ceramics: high alumina-based (In-Ceram Alumina, Procera AllCeram) and zirconia-reinforced alumina-based (In-Ceram Zirconia) ceramics. Materials and Methods: Ten blocks (5 ×6 × 8 mm) of In-Ceram Alumina (AL), In-Ceram Zirconia (ZR), and Procera (PR) ceramics were fabricated according to each manufacturer's instructions and duplicated in composite. The specimens were assigned to one of the two following treatment conditions: (1) airborne particle abrasion with 110-μm Al2O3 particles + silanization, (2) silica coating with 30 μm SiOx particles (CoJet, 3M ESPE) + silanization. Each ceramic block was duplicated in composite resin (W3D-Master, Wilcos, Petrópolis, RJ, Brazil) using a mold made out of silicon impression material. Composite resin layers were incrementally condensed into the mold to fill up the mold and each layer was light polymerized for 40 s. The composite blocks were bonded to the surface-conditioned ceramic blocks using a resin cement system (Panavia F, Kuraray, Okayama, Japan). One composite resin block was fabricated for each ceramic block. The ceramic-composite was stored at 37°C in distilled water for 7 days prior to bond tests. The blocks were cut under water cooling to produce bar specimens (n = 30) with a bonding area of approximately 0.6 mm2. The bond strength tests were performed in a universal testing machine (crosshead speed: 1 mm/min). Bond strength values were statistically analyzed using two-way ANOVA and Tukey's test (≤ 0.05). Results: Silica coating with silanization increased the bond strength significantly for all three high-strength ceramics (18.5 to 31.2 MPa) compared to that of airborne particle abrasion with 110-μm Al2O3 (12.7-17.3 MPa) (ANOVA, p < 0.05). PR exhibited the lowest bond strengths after both Al2O3 and silica coating (12.7 and 18.5 MPa, respectively). Conclusion: Conditioning the high-strength ceramic surfaces with silica coating and silanization provided higher bond strengths of the resin cement than with airborne particle abrasion with 110-μm Al2O3 and silanization.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The aim of this study was to evaluate the effects of the autogenous demineralized dentin matrix (ADDM) on the third molar socket wound healing process in humans, using the guided bone regeneration technique and a polytetrafluoroethylene barrier (PTFE). Twenty-seven dental sockets were divided into three groups: dental socket (Control), dental socket with PTFE barrier (PTFE), and dental socket with ADDM slices associated to PTFE banier (ADDM + PTFE). The dental sockets were submitted to radiographic bone densitometry analysis and statistical analysis on the 15th, 30th, 60th and 90th days using analysis of variance (ANOVA) and Tukey's test (p ≤ 0.05). The radiographic analysis of the ADDM + PTFE group showed greater homogeneity of bone radiopacity than the Control group and the PTFE group, during all the observation times. The dentin matrix gradually disappeared from the dental socket during the course of the repair process, suggesting its resorption during the bone remodeling process. It was concluded that the radiographic bone density of the dental sockets treated with ADDM was similar to that of the surrounding normal bone on the 90th day. The ADDM was biocompatible with the bone tissue of the surgical wounds of human dental sockets. The radiographic analysis revealed that the repair process was discreetly faster in the ADDM + PTFE group than in the Control and PTFE groups, although the difference was not statistically significant. In addition, the radiographic image of the ADDM + PTFE group suggested that its bone architecture was better than that of the Control and PFTE groups.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Purpose: Selecting artificial teeth for edentulous patients is difficult when pre-extraction records are not available. Various guidelines have been suggested for determining the width of the maxillary anterior denture teeth. This study was undertaken to evaluate the use of the nasal width as a guide for the selection of proper width maxillary anterior denture teeth in four racial groups of the Brazilian population. Materials and Methods: One hundred and sixty subjects (40 Whites, 40 Mulattos, 40 Blacks, and 40 Asians) were selected. Using a sliding caliper, the nasal width and the intercanine distance were measured. The Pearson product-moment correlation coefficient was used to determine the relationship between the above measurements. A prediction was made of the percentage of subjects of the White, Mulatto, Black, and Asian populations in which the selection error due to the clinical application of the method of the nasal width would be within 0 to 2 mm, within 2 to 4 mm, and greater than 4 mm. Results: The four racial groups showed a weak correlation between the intercanine distance and the nasal width. In 39.7% of the White, 55.7% of the Mulatto, 81.9% of the Black, and 48.2% of the Asian populations, errors greater than 4 mm would be present with the use of the nasal width. Conclusions: The correlation found between the intercanine distance and the nasal width was not high enough to be used as a predictive factor. The relationship between natural tooth width and artificial tooth width as predicted by the nasal width showed that the nasal width method is not accurate for all the studied groups. Copyright © 2006 by The American College of Prosthodontists.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Purpose: The purpose of this study was to quantitatively evaluate the effect of 10% carbamide peroxide on the microhardness of pit and fissure sealant materials. Methods: Fluroshield, Vitroseal Alfa, and one unfilled (Clinpro) sealants were placed in Teflon matrices (4 mm in diameter by 2 mm in height) and polymerized for 40 seconds. A total of 20 specimens were prepared for each material, in which half were assigned as the control group (stored in artificial saliva and no bleaching treatment). For the remaining half, Clarigel Gold bleaching agent (10% carbamide peroxide) was placed over the specimen surface for 4 hours/day during 4 weeks. When specimens were not under bleaching treatment, they were kept in artificial saliva. Afterwards, specimens were subjected to Knoop microhardness testing using a 25-g load for 5 seconds. Five measurements were made on the sealants' surfaces and then calculated in Knoop hardness values. The data were statistically analyzed by two-way analysis of variance and Tukey's tests with a 5% confidence level. Results: The results of this in vitro study showed that the application of a carbamide peroxide-based bleaching material significantly affected the microhardness values of filled sealant materials. The bleaching agent did not affect the microhardness of the unfilled sealant. CLINICAL SIGNIFICANCE: The results of this in vitro study suggest that the bleaching agents altered the surface hardness of filled sealant restorative materials. This could possibly lead to increased wear and surface roughness. © 2006, Copyright the authors.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The purpose of this study was to test the hypothesis that mechanical polishing methods of ceramic surfaces allow similar superficial roughness to that of glazed surfaces. Twenty-five Vitadur Alpha ceramic discs (5 mm x 2 mm) were prepared according to the manufacturer's specifications. All specimens were glazed and randomly assigned to 5 groups (n=5), according to finishing and polishing protocols: G1: glazed (control); G2: diamond bur finishing; G3: G2 + silicon rubber tip polishing; G4: G3 + felt disc/diamond polishing paste; G5: G3 + felt disc impregnated with fine-particle diamond paste. Next, surface roughness means (Ra - μm) were calculated. Qualitative analysis was made by scanning electron microscopy. Surface roughness data were submitted to ANOVA and Tukey's test at 5% significance level. G1 and G4 were statistically similar (p>0.05). G2 presented the highest roughness means (p<0.05) followed by groups G3, G5, G4 and G1 in a decreasing order. The hypothesis was partially confirmed as only the mechanical polishing (G4) produced similar superficial roughness to that of surface glazing, although finishing and polishing are technically critical procedures.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Several pathologies have been diagnosed in children of hypertensive mothers; however, some studies that evaluated the alterations in their oral health are not conclusive. This study analyzed the salivary gland activity and dental mineralization of offsprings of spontaneously hypertensive rats (SHR). Thirty-day-old SHR males and Wistar rats were studied. The salivary flow was evaluated by injection of pilocarpine, the protein concentration and salivary amylase activity, by the Lowry method and kinetic method at 405 nm, respectively. Enamel and dentin mineralization of the mandibular incisors was quantified with aid of the microhardness meter. The results were analyzed by the ANOVA or Student's t test (p<0.05). It was noticed that the salivary flow rate (0.026 mL/min/100 g±0.002) and salivary protein concentration (2.26mg/mL±0.14) of SHR offspring were reduced compared to Wistar normotensive offspring (0.036 mL/min/100 g±0.003 and 2.91 mg/mL±0.27, respectively), yet there was no alteration in amylase activity (SHR: 242.4 U/mL±36.9; Wistar: 163.8 U/mL±14.1). Microhardness was lower both in enamel (255.8 KHN±2.6) and dentin (59.9 KHN±0.8) for the SHR teeth compared to the Wistar teeth (enamel: 328.7 KHN±3.3 and dentin: 67.1 KHN±1.0). These results suggest that the SHR offspring are more susceptible to development of pathologies impairing oral health, once they presented lesser flow and salivary protein concentration and lower dental mineralization.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Purpose: This study compared the microtensile bond strength of resin-based cement (Panavia F) to silica-coated, silanized, glass-infiltrated high-alumina zirconia (In-Ceram Zirconia) ceramic in dry conditions and after various aging regimens. Materials and Methods: The specimens were placed in 1 of 4 groups: group 1: dry conditions (immediate testing without aging); group 2: water storage at 37°C for 150 days; group 3: 150 days of water storage followed by thermocycling (× 12,000, 5°C to 55°C); group 4: water storage for 300 days; group 5: water storage for 300 days followed by thermocycling. Results: Group 1 showed a significantly higher microtensile bond strength value (26.2 ± 1 MPa) than the other aging regimens (6.5 ± 1, 6.2 ± 2, 4.5 ± 1, 4.3 ± 1 MPa for groups 2, 3, 4, and 5, respectively) (P < .01). Conclusion: Satisfactory results were seen in dry conditions, but water storage and thermocycling resulted in significantly weaker bonds between the resin cement and the zirconia.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Objective: To evaluate the prevalence of dental fluorosis in scholars aging 12 to 15 years old, residents in the city of Bauru, State of São Paulo, Brazil. Methods: 1318 volunteers were enrolled in this study and examined in 18 public schools of the State of São Paulo. The examinations were performed in the schools' court by three dentists (with a Master's degree in Public Health), after toothbrushing supervised by another dentist. The teeth were dried with cotton pellets and examined under natural light by visual inspection, using an explorer as recommended by the WHO, a plane mirror and a tongue depressor. The Thylstrup-Fejerskov (TF) index was used for rating fluorosis. Intra and inter-examiner reproducibility was calculated and data were submitted to descriptive analysis. Results: Approximately 36% of the children presented dental fluorosis, of which 28% was diagnosed as TF1 while the remaining received scores between TF2 and TF4. Conclusion: The prevalence of dental fluorosis in Bauru is within the expected range, based on previous studies. Although fluoride is an important resource for caries control, its use must be adequate to the needs of each specific population.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

This study aimed to evaluate the durability of adhesion between acrylic teeth and denture base acrylic resin. The base surfaces of 24 acrylic teeth were flatted and submitted to 4 surface treatment methods: SM1 (control): No SM; SM2: application of a methyl methacrylate-based bonding agent (Vitacol); SM3: air abrasion with 30-μm silicone oxide plus silane; SM4: SM3 plus SM2. A heat-polymerized acrylic resin was applied to the teeth. Thereafter, bar specimens were produced for the microtensile test at dry and thermocyled conditions (60 days water storage followed by 12,000 cycles). The results showed that bond strength was significantly affected by the SM (P < .0001) (SM4 = SM2 > SM3 > SM1) and storage regimens (P < .0001) (dry > thermocycled). The methyl methacrylate-based adhesive showed the highest bond strength.