900 resultados para THERMO-LUMINESCENCE
Resumo:
Intense photoluminescence in highly disordered strontium titanate amorphous thin films prepared by the polymeric precursor method was observed at room temperature (300 K). The luminescence spectra of SrTiO3 amorphous thin films at room temperature revealed an intense single-emission band in the visible region. X-ray absorption near edge structure was used to probe the local atomic structure of SrTiO3 amorphous and crystalline thin films. Photoluminescence intensity in the 535 nm range was found to be correlated with the presence of non-bridging oxygen defects. A discussion is presented of the nature of this photoluminescence, which may be related to the disordered structure in SrTiO3 amorphous thin films. (C) 2002 Elsevier B.V. B.V. All rights reserved.
Resumo:
Luminescent properties of scandium and yttrium phosphates are discussed and mechanisms involving their emissions proposed.
Resumo:
The mechanism of the Yb(3+)-->Er(3+) energy transfer as a function of the donor and the acceptor concentration was investigated in Yb(3+)-Er(3+) codoped fluorozirconate glass. The luminescence decay curves were measured and analyzed by monitoring the Er(3+)((4)I(11/2)) fluorescence induced by the Yb(3+)((2)F(5/2)) excitation. The energy transfer microparameters were determined and used to estimate the Yb-Er transfer rate of an energy transfer process assisted by excitation migration among donors state (diffusion model). The experimental transfer rates were determined from the best fitting of the acceptor luminescence decay obtained using a theoretical approach analog to that one used in the Inokuti-Hirayama model for the donor luminescence decay. The obtained values of transfer parameter gamma [gamma(exp)] were always higher than that predicted by the Inokuti-Hirayama model. Also, the experimental transfer rate, gamma(2)(exp), was observed to be higher than the transfer rate predicted by the migration model. Assuming a random distribution among excited donors at the initial time (t=0) and that a fast excitation migration, which occurs in a very short time (t
Resumo:
Monolithic silica xerogels doped with different concentrations of Er3+, Yb3+ and Al3+ were prepared by sol-gel route. Densification was achieved by thermal treatment in air at 950degreesC for 120 h with a heating rate of 0.1degreesC/min. We studied the luminescence properties of the I-4(13/2)-->I-4(15/2) emission band of Er3+ as a function of the Al/Er/Yb concentration and we paid particular attention to the alumina effects. Raman spectroscopy and Vis-NIR absorption were used to monitor the degree of densification of the glasses and the residual OH content.
Resumo:
This work reports on the preparation, structural and luminescent studies of nanosized up-converter phosphors Y2O2S:Yb(4%), Er(0.1%) and Y2O2S:Yb(4%), Tm(0.1%),both from polymeric and basic carbonate precursors. The precursors were submitted to a sulphuration process that was previously developed for oxysulfide preparation from basic carbonate. From XRD data, all phosphors presented the oxysulfide phase and the mean crystallite size estimated from the Scherrer formula in the range of 15-20 nm. Polymeric precursor leads to the smallest crystallite size independent on the doping ion. SEM and TEM results confirmed that basic carbonate leads to spherical particles with narrow size distribution and mean diameter of 150 nm, and polymeric precursor smaller spherical particles with diameter between 20 and 40 nm. Up-conversion studies under 980 nm laser excitation showed that Er-doped phosphors present strong green emission related to H-2(11/2), S-4(3/2) --> I-4(15/2) Er transitions as well as the red ones, F-4(9/2) --> I-4(15/2). Tm-doped samples show strong blue emission assigned to (1)G(4) --> H-3(6) and also the red ones, related to (1)G(4) --> F-3(4). Therefore, the sulphuration method was successfully applied to prepare nanosized and nanostructured blue and green up-converter oxysulfide phosphors starting from basic carbonate and polymeric precursors. (C) 2003 Elsevier B.V. All rights reserved.
Resumo:
This study reports on the effects of growth temperature on the secretion and some properties of the xylanase and beta-xylosidase activities produced by a thermotolerant Aspergillus phoenicis. Marked differences were observed when the organism was grown on xylan-supplemented medium at 25 degreesC or 42 degreesC. Production of xylanolytic enzymes reached maximum levels after 72 h of growth at 42 degreesC; and levels were three- to five-fold higher than at 25 degreesC. Secretion of xylanase and beta-xylosidase was also strongly stimulated at the higher temperature. The optimal temperature was 85 degreesC for extracellular and 90 degreesC for intracellular beta-xylosidase activity, independent of the growth temperature. The optimum temperature for extracellular xylanase increased from 50 degreesC to 55 degreesC when the fungus was cultivated at 42 degreesC. At the higher temperature, the xylanolytic enzymes produced by A. phoenicis showed increased thermo stability, with changes in the profiles of pH optima. The chromatographic profiles were distinct when samples obtained from cultures grown at different temperatures were eluted from DEAE-cellulose and Biogel P-60 columns.
Resumo:
Temperature investigation of infrared-to-visible frequency upconversion in erbium-doped tellurite glasses excited by CW laser radiation at 1540 nm and under cryogenic temperatures is reported. Intense upconversion emission signals around 530, 550 and 660 nm corresponding to the H-2(11/2), S-4(3/2), and F-4(9/2) transitions to the I-4(15/2) ground state were generated and studied as a function of the laser intensity and temperature. The upconversion excitation mechanism of the Er3+ ions emitting energy levels was accomplished via stepwise multiphoton absorption. The green upconversion luminescence exhibited a fivefold intensity enhancement when the temperature of the sample was varied in the range between 5 and 300 K. A maximum green upconversion intensity was attained around 120 K and a steady decreasing behavior for higher temperatures up to 300 K was observed. A model based upon conventional rate equations was used to model the observed temperature evolution of the upconversion luminescence. (C) 2002 Elsevier B.V. B.V. All rights reserved.
Resumo:
Upconversion luminescence and thermal effects in Pr3+/Yb3+- and Er3+/Yb3+-codoped 60TeO(2)-10GeO(2)-10K(2)O-10Li(2)O-10Nb(2)O(5) tellurite glasses excited by CW infrared radiation at 1.064 mum is reported. Generation of intense green and red fluorescence emission in Er3+/Yb3+-codoped samples and appreciable upconversion luminescence in the wavelength region of 450-680 nm in Pr3+/Yb3+-codoped samples is observed. Temperature-induced enhancement of X12 in the upconversion efficiency in Er3+/Yb3+- and X10 in the Pr3+/Yb3+-doped samples is demonstrated. (C) 2002 Elsevier B.V. B.V. All rights reserved.
Resumo:
Intense red upconversion emission around 650 nm in PbGeO3-PbF2-CdF2 transparent glass ceramic containing beta-PbF2:Ho3+ nanocrystals, is presented. The holmium-doped vitroceramic samples were excited by a 980 nm diode laser source. The 650 nm upconversion signal was assigned to the F-5(5) --> I-5(8) transition of holmium ions. Very low intensity signals around 490 and 540 nm corresponding to the F-5(2,3) --> I-5(8) and S-4(2), F-5(4) --> I-5(8) transitions, respectively, were also detected. The upconversion excitation mechanism was achieved through a combination of stepwise phonon-assisted multiphoton absorption, cross-relaxation processes involving pairs of holmium ions, and excited-state absorption. Using a diode laser pump source around 850 nm green upconversion emission around 540 nm was the observed predominant signal. (C) 2004 Elsevier B.V. All rights reserved.
Resumo:
Luminescent spectra of Eu3+-doped sol-gel glasses have been analyzed during the densification process and compared according to the presence or not of aluminum as a codoping ion. A transition temperature from hydrated to dehydroxyled environments has been found different for doped and codoped samples. However, only slight modifications have been displayed from luminescence measurements beyond this transition. To support the experimental analysis, molecular dynamics simulations have been performed to model the doped and codoped glass structures. Despite no evidence of rare earth clustering reduction due to aluminum has been found, the modeled structures have shown that the luminescent ions are mainly located in aluminum-rich domains. The synthesis of both experimental and numerical analyses has lead us to interpret the aluminum effect as responsible for differences in structure of the luminescent sites rather than for an effective dispersion of the rare earth ions. (C) 2004 Elsevier B.V. All rights reserved.
Resumo:
Porphyrin was incorporated in a silicate network, via a covalent bond, by grafting a functional group with 3-aminopropyltriethoxysilane, using a sol-gel process. We have carried out the synthesis and measured the absorption spectra, nuclear magnetic resonance spectra, infrared (IR) spectra, luminescence spectra and lifetime of these hybrid silicates, porphyrinosilicas. These samples contained the following free-base porphyrins: meso-tetrakis-p-chlorobenzoylporphyrin, meso-tetrakis-2,6-dichloro-3-chlorosulfonylphenylporphyrin. The obtained porphyrinosilicas have similar absorption and luminescence spectra to the free base porphyrins in solution. IR spectra confirm the formation of monomeric species. Lifetime measurement for porphyrinosilica reveals that 32% +/- 2% of porphyrin is covalently bonded to the silica network. (C) 1999 Elsevier B.V. B.V. All rights reserved.
Resumo:
In this work, the polymeric precursor method Was used to obtain disordered Zn2TiO4 powders, either Undoped or doped with Sn4+, Cr3+ and V5+, to be applied its photoluininescent material. The characterization was undertaken by means of thermal analysis (TG and DTA), X-ray diffraction (XRD), infrared spectroscopy (IR) and photoluminescence (PL). Previous works stated that titanate octahedra containing a short Ti-O distance show efficient luminescence at roorn temperature if these octahedra are isolated from each other. In the present work, the phenomenon was observed in condensed octahedra, sharing edges. The room temperature PL noticed in undoped Zn2TiO4 had its intensity increased by the dopant addition-the increase was of about 300% for V5+ doping 400% for Cr3+ and 800% for Sn4+. (c) 2005 Elsevier B.V. All rights reserved.
Resumo:
We investigate the linear optical properties and energy transfer processes in tungstate fluorophosphate glass doped with thulium (Tm3+) and neodymium (Nd3+) ions. The linear absorption spectra from 370 to 3000 nm were obtained. Transitions probabilities, radiative lifetimes, and transition branching ratios were determined using the Judd-Ofelt [Phys. Rev. 127, 750 (1962); J. Chem. Phys. 37, 511 (1962)] theory. Frequency up-conversion to the blue region and fluorescence in the infrared were observed upon pulsed excitation in the range of 630-700 nm. The excitation spectra of the luminescence were obtained to understand the origin of the signals. The temporal decay of the fluorescence was measured for different concentrations of the doping ions. Energy transfer rates among the Tm3+ and Nd3+ ions were also determined.
Resumo:
In this paper we investigate the energy transfer processes in TM3+/Er3+ doped telluride glass pumped at the commercial diode laser pump wavelength similar to 800 nm. Tailoring the rare-earths content in the glass matrix, seven main energy transfer channels within the doping range considered were identified, A 6-fold enhancement of the Er3+ visible frequency upconversion fluorescence at similar to 660 nm is observed due to the inclusion of Tm3+ ions. This is evidence of the relevant contribution of the route Er-1(I-4(11/2)) + Er-2(I-4(13/2)) -> Er-1(I-4(15/2)) + Er-2(F-4(9/2)) to the process. Energy migration among pumped I-4(9/2) level reducing the efficiency of the upconversion emission rate (H-3(11/2), S-4(3/2), and F-4(9/2)) is observed for Er3+ above 1.5 wt%. The rate equations regarding the observed energy transfer routes are determined and a qualitative analysis of the observed processes is reported. (c) 2006 Elsevier B.V. All rights reserved.
Resumo:
Parabolic quantum wells (PQWs) have been studied by temperature dependent photoluminescence (PL). Two kind of samples have been studied. Concerning the undoped sample, the dominant luminescences were the bulk GaAs and the fundamental transition of the PQW. The evolution on temperature of the energy position of both PL emissions follows the well known Varshing formula. For the doped samples strong radiative recombination of the electron gas with photogenerated holes was observed. At low temperature strong Fermi level enhancement occurs in the luminescence as a result of the multi-electron-hole scattering, which is smear out increasing the temperature.