926 resultados para Optical scanners


Relevância:

20.00% 20.00%

Publicador:

Resumo:

Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Coordenação de Aperfeiçoamento de Pessoal de Nível Superior (CAPES)

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Coordenação de Aperfeiçoamento de Pessoal de Nível Superior (CAPES)

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Objectives: This study evaluated the marginal gaps on several surfaces of onlays created with the Cerec 3D system using one intraoral and two extraoral optical impression methods. Methods: A human molar (#19) was mounted with its adjacent teeth on a typodont (Frasaco) and prepared for a MODL onlay. The typodont was assembled in the mannequin head in order to simulate clinical conditions. The same operator took 36 individual optical impressions using a CEREC 3D camera. For group 1 (IP), a thin layer of titanium dioxide powder (CEREC powder-VITA) was applied directly onto the surface of the preparation for imaging (n=12). For group 2 (EP), a sectional impression was taken with hydrocolloid Identic Syringable (Dux Dental), a die made with polyvinylsiloxane KwikkModel Scan (R-dental Dentalerzeugnisse GmbH) and powdered with titanium dioxide for imaging (n=12). For group 3 (ES), a sectional impression was taken with PVS and a sectional stock tray, a die fabricated in stone (Diamond die- HI-TEC Dental Products) and the die being imaged without powdering (n=12). One operator designed and machined the onlays in Vita Blocks Mark II for Cerec (VITA) using a CEREC 3D. The marginal gaps (pm) were measured with an optical microscope (50x) at 12 points, three on each surface of the MODL. The results were analyzed by two-way ANOVA/Tukey's (p=0.05). Results: The overall mean marginal gaps (mu m) for the three methods were: IP=111.6 (+/- 34.0); EP=161.4 (+/- 37.6) and ES=116.8 (+/- 42.3). IP and ES were equal, but both were significantly less than EP. The pooled mean marginal gaps (mu m) for the occlusal = 110.5 (+/- 39) and lingual = 111.5 (+/- 30.5) surfaces were equivalent and significantly less than the distal = 136.5 (+/- 42.5) and mesial = 161.1 (+/- 43.3). Conclusion: The marginal gap of CEREC 3D onlay restorations was not different when the optical impression was taken intraorally vs extraorally using a stone cast that does not require powdering. The lingual and occlusal surfaces showed the lowest gaps.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Coordenação de Aperfeiçoamento de Pessoal de Nível Superior (CAPES)

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Conselho Nacional de Desenvolvimento Científico e Tecnológico (CNPq)

Relevância:

20.00% 20.00%

Publicador:

Resumo:

We report the fabrication and characterization of the first guiding chalcogenide As(2)S(3) microstructured optical fibers (MOFs) with a suspended core. At 1.55 mu m, the measured losses are approximately 0.7 dB/m or 0.35 dB/m according to the MOF core size. The fibers have been designed to present a zero dispersion wavelength (ZDW) around 2 mu m. By pumping the fibers at 1.55 mu m, strong spectral broadenings are obtained in both 1.8 and 45-m-long fibers by using a picosecond fiber laser. (C) 2010 Optical Society of America

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Conselho Nacional de Desenvolvimento Científico e Tecnológico (CNPq)

Relevância:

20.00% 20.00%

Publicador:

Resumo:

We present photoluminescence and decay of photo excited conductivity data for sol-gel SnO(2) thin films doped with rare earth ions Eu(3+) and Er(3+), a material with nanoscopic crystallites. Photoluminescence spectra are obtained under excitation with several monochromatic light sources, such as Kr(+) and Ar(+) lasers, Xe lamp plus a selective monochromator with UV grating, and the fourth harmonic of a Nd: YAG laser (4.65eV), which assures band-to-band transition and energy transfer to the ion located at matrix sites, substitutional to Sn(4+). The luminescence structure is rather different depending on the location of the rare-earth doping, at lattice symmetric sites or segregated at grain boundary layer, where it is placed in asymmetric sites. The decay of photo-excited conductivity also shows different trapping rate depending on the rare-earth concentration. For Er-doped films, above the saturation limit, the evaluated capture energy is higher than for films with concentration below the limit, in good agreement with the different behaviour obtained from luminescence data. For Eu-doped films, the difference between capture energy and grain boundary barrier is not so evident, even though the luminescence spectra are rather distinct.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Fluoroindate glasses containing 1, 2, 3, and 4 mol% ErF3 were prepared in a dry box under an argon atmosphere. Absorption spectra of these glasses at room temperature were obtained. The Judd-Ofelt parameters Ωλ (λ = 2, 4, 6) for f-f transitions of Er3+ ions as well as transition probabilities, branching ratios, radiative lifetimes, and peak cross-sections for stimulated emission of each band were determined. The concentration effect on the intensities is analyzed. The optical properties of the fluoroindate glasses doped with Er3+ ions are compared with those of other glasses described in the literature. © 1995.