Ultrafine full-vulcanized polybutadiene rubber (UFBR) in particle sizes of ca. 50-100 nm has been used for modifying mechanical and processing performances of polypropylene (PP), and PP-g-maleic anhydride (PP-MA) has been used as a compatibilizer for enhancing the interfacial adhesion between the two components. The results show that PP/UFBR possesses rheological behaviors such as highly branched PP when UFBR content in blends reaches 10 wt%, while in contrast, the much low content of UFBR combining small amount of PP-MA endows the material with rheological characteristics of high melt strength materials like highly branched PP.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

La2Zr2O7 (LZ) and La-2(Zr0.7Ce0.3)(2)O-7 (LZ7C3) as novel candidate materials for thermal barrier coatings (TBCs) were prepared by electron beam-physical vapor deposition (EB-PVD). The adhesive strength of the as-deposited LZ and LZ7C3 coatings were evaluated by transverse scratch test. Meanwhile, the factors affecting the critical load value were also investigated. The critical load value of LZ7C3 coating is larger than that of LZ coating, whereas both values of these two coatings are lower than that of the traditional coating material, i.e. 8 wt% yttria stabilized zirconia (8YSZ). The micro-cracks formed in the scratch channel can partially release the stress in the coating and then enhance the adhesive strength of the coating. The width of the scratch channel and the surface spallation after transverse scratch test are effective factors to evaluate the adhesive strength of LZ and LZ7C3 coatings.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Aim: To investigate (a) variability in powder/liquid proportioning (b) effect of the extremes of any such variability on diametral tensile strength (DTS), in a commercial zinc phosphate cement. Statistical analyses (a = 0.05) were by Student's t-test in the case of powder/liquid ratio and one-way ANOVA and Tukey HSD for for pair-wise comparisons of mean DTS. The Null hypotheses were that (a) the powder-liquid mixing ratios observed would not differ from the manufacturer's recommended ratio (b) DTS of the set cement samples using the extreme powder/liquid ratios observed would not differ from those made using the manufacturer's recommended ratio. Methodology: Thirty-four undergraduate dental students dispensed the components according to the manufacturer's instructions. The maximum and minimum powder/liquid ratios (m/m), together with the manufacturer's recommended ratio (m/m), were used to prepare cylindrical samples (n = 3 x 34) for DTS testing. Results: Powder/liquid ratios ranged from 2.386 to 1.018.The mean ratio (1.644 (341) m/m) was not significantly different from the manufacturer's recommended value of 1.718 (p=0.189). DTS values for the maximum and minimum ratios (m/m), respectively, were both significantly different from each other (p<0.001) and from the mean value obtained from the manufacturer's recommended ratio (m/m) (p<0.001). Conclusions: Variability exists in powder/liquid ratio (m/m) for hand dispensed zinc phosphate cement. This variability can affect the DTS of the set material.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Transport of particulate clay occurs during some extremely cold weather conditions typically in the winter in the far North area. During the transport and temporary storage time, the clay may cake inside a rail or road wagon or in a silo, and consequently be difficult to be discharged from the containers. This paper studied caking strength of a granulated clay powder with a certain water moisture content of 18% for influences of temperature, packing stress and freezing time. The temperature tested was -5 oC, -10 oC and -20 oC. Because the clay powder may be packed at different bed depth, the study was undertaken across the packing stress range at 8.3 kPa (1 m bed depth), 25.0 kPa (3 m) and 75.0 kPa (9 m). Freezing time varied between 4 hours (transport) and 18 hours (overnight). During the tests, failure of caked materials was measured using a QTS texture analyzer and the caking strength of frozen samples was calculated. Influences on freeze caking of granular clay in storage or transport are discussed briefly. Some conclusions are made at the end of the paper,including recommendations for practical methods for mitigating these problems.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

This paper presents a study of the residual strength of Pinus sylvestris, which has been subject to attack by the furniture beetle (Anobium punctatum). It is relatively easy to stop the infestation, but difficult to assess the structural soundness of the remaining timber. Removal and replacement of affected structural elements is usually difficult and expensive, particularly in buildings of historic interest. Current on-site assessment procedures are limited. The main object of the study was to develop an on-site test of timber quality: a test which can be carried out on the surface and also at varying depths into the timber. It is based on a probe pull-out technique using a portable load-measuring device. Pull-out force values have been correlated with both strength and energy absorbed as measured by compression testing on laboratory samples of both sound and infested timber. These two relationships are significant and could be used to assess whether remedial work is needed. In addition, work on the use of artificial borings to simulate the natural worming of timber is presented and the findings discussed.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Concrete used for underwater repair is often proportioned to spread readily into place and self-consolidate, and to develop high resistance to segregation and water dilution. An investigation was carried out to determine the effect of the dosage of antiwashout admixture, water-cementitious materials ratio (w/cm), and binder composition on the relative residual strength of highly flowable underwater concrete. Two types of antiwashout admixtures were used: a powdered welan gum at 0.07 and 0.15% by mass of binder, and a liquid-based cellulosic admixture employed at a high dosage of 1 to 1.65 L/100 kg of cementitious materials. The w/cms were set at 0.41 and 0.47 to secure adequate performance of underwater concrete for construction and repair. Four binder compositions were used: a Canadian Type 10 cement; a cement with 10% silica fume replacement; a cement with 50% replacement of granulated blast-furnace slag; and a ternary binder containing 6% silica fume and 20% Class F fly ash. Test results indicate that for a given washout mass loss and slump flow consistency, greater relative residual strength can be secured when the dosage of antiwashout admixture is increased, the w/cm is reduced, and a binary binder with 10% silica fume substitution or the ternary binder are employed. Such mixtures can develop relative residual compressive strengths of 85 and 80%, compared to mixtures cast in air, when the value of washout loss is limited to 4 and 6% for mixtures with slump flow values of 450 and 550 mm, respectively.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Objectives: To determine, by means of static fracture testing the effect of the tooth preparation design and the elastic modulus of the cement on the structural integrity of the cemented machined ceramic crown-tooth complex. 
Methods: Human maxillary extracted premolar teeth were prepared for all-ceramic crowns using two preparation designs; a standard preparation in accordance with established protocols and a novel design with a flat occlusal design. All-ceramic feldspathic (Vita MK II) crowns were milled for all the preparations using a CAD/CAM system (CEREC-3). The machined all-ceramic crowns were resin bonded to the tooth structure using one of three cements with different elastic moduli: Super-Bond C&B, Rely X Unicem and Panavia F 2.0. The specimens were subjected to compressive force through a 4 mm diameter steel ball at a crosshead speed of 1 mm/min using a universal test machine (Loyds Instrument Model LRX.). The load at the fracture point was recorded for each specimen in Newtons (N). These values were compared to a control group of unprepared/unrestored teeth. 
Results: There was a significant difference between the control group, with higher fracture strength, and the cemented samples regardless of the occlusal design and the type of resin cement. There was no significant difference in mean fracture load between the two designs of occlusal preparation using Super-Bond C&B. For the Rely X Unicem and Panavia F 2.0 cements, the proposed preparation design with a flat occlusal morphology provides a system with increased fracture strength
Significance: The proposed novel flat design showed less dependency on the resin cement selection in relation to the fracture strength of the restored tooth. The choice of the cement resin, with respect to its modulus of elasticity, is more important in the anatomic design than in the flat design. © 2013 Academy of Dental Materials.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Objective: The aim of this research is to use finite element analysis (FEA) to quantify the effect of the sample shape and the imperfections induced during the manufacturing process of samples on the bond strength and modes of failure of dental adhesive systems through microtensile test. Using the FEA prediction for individual parameters effect, estimation of expected variation and spread of the microtensile bond strength results for different sample geometries is made. Methods: The estimated stress distributions for three different sample shapes, hourglass, stick and dumbbell predicted by FEA are used to predict the strength for different fracture modes. Parameters such as the adhesive thickness, uneven interface of the adhesive and composite and dentin, misalignment of axis of loading, the existence of flaws such as induced cracks during shaping the samples or bubbles created during application of the adhesive are considered. Microtensile experiments are performed simultaneously to measure bond strength and modes of failure. These are compared with the FEA results. Results: The relative bonding strength and its standard deviation for the specimens with different geometries measured through the microtensile tests confirm the findings of the FEA. The hourglass shape samples show lower tensile bond strength and standard deviation compared to the stick and dumbbell shape samples. ANOVA analysis confirms no significant difference between dumbbell and stick geometry results, and major differences of these two geometries compared to hourglass shape measured values. Induced flaws in the adhesive and misalignment of the angle of application of load have significant effect on the microtensile bond strength. Using adhesive with higher modulus the differences between the bond strength of the three sample geometries increase. Significance: The result of the research clarifies the importance of the sample geometry chosen in measuring the bond strength. It quantifies the effect of the imperfections on the bond strength for each of the sample geometries through a systematic and all embracing study. The results explain the reasons of the large spread of the microtensile test results reported by various researchers working in different labs and the need for standardization of the test method and sample shape used in evaluation of the dentin-adhesive bonding system. © 2007 Academy of Dental Materials.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

The effect of colloidal nanosilica on the fresh and rheological parameters, plastic shrinkage, heat of hydration, and compressive strength of cement-based grouts is investigated in this paper. The fresh and rheological properties were evaluated by the minislump flow, Marsh cone flow time, Lombardi plate cohesion meter, yield value, and plastic viscosity. The key parameters investigated were the dosages of nanosilica and superplasticizer and temperature of mixing water. Statistical models and isoresponse curves were developed to capture the significant trends. The dosage of nanosilica had a significant effect on the results. The increase in the dosage of nanosilica led to increasing the values of flow time, plate cohesion meter, yield stress, plastic viscosity, heat of hydration at 1 day and 3 days, and compressive strength at 1 day, while reducing the minislump, plastic shrinkage up 24 h, and compressive strength at 3, 7, and 28 days. Conversely, the increase in the dosage of superplasticizer led to decreasing the values of flow time, plate cohesion meter, yield stress, plastic viscosity, heat of hydration at 1 day and 3 days, and compressive strength at 1 day, while increasing the minislump, plastic shrinkage, and compressive strength at 3 and 7 days. Increasing the temperature of mixing water led to a notable increase in the results of minislump, flow time, plastic viscosity, heat of hydration at 3 days, and compressive strength at 1 day, while it reduced the plate cohesion, compressive strength at 3, 7, and 28 days. The statistical models developed in this study can facilitate optimizing the mixture proportions of grouts for target performance by reducing the number of trial batches needed.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Low-velocity impact damage can drastically reduce the residual mechanical properties of the composite structure even when there is barely visible impact damage. The ability to computationally predict the extent of damage and compression after impact (CAI) strength of a composite structure can potentially lead to the exploration of a larger design space without incurring significant development time and cost penalties. A three-dimensional damage model, to predict both low-velocity impact damage and compression after impact CAI strength of composite laminates, has been developed and implemented as a user material subroutine in the commercial finite element package, ABAQUS/Explicit. The virtual tests were executed in two steps, one to capture the impact damage and the other to predict the CAI strength. The observed intra-laminar damage features, delamination damage area as well as residual strength are discussed. It is shown that the predicted results for impact damage and CAI strength correlated well with experimental testing.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Low-velocity impact damage can drastically reduce the residual mechanical properties of the composite structure even when there is barely visible impact damage. The ability to computationally predict the extent of damage and compression after impact (CAI) strength of a composite structure can potentially lead to the exploration of a larger design space without incurring significant development time and cost penalties. A three-dimensional damage model, to predict both low-velocity impact damage and compression after impact CAI strength of composite laminates, has been developed and implemented as a user material subroutine in the commercial finite element package, ABAQUS/Explicit. The virtual tests were executed in two steps, one to capture the impact damage and the other to predict the CAI strength. The observed intra-laminar damage features, delamination damage area as well as residual strength are discussed. It is shown that the predicted results for impact damage and CAI strength correlated well with experimental testing.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Interest in polyethylene and polypropylene bonding has increased in the last years. However, adhesive joints with adherends which are of low surface energy and which are chemically inert present several difficulties. Generally, their high degree of chemical resistance to solvents and dissimilar solubility parameters limit the usefulness of solvent bonding as a viable assembly technique. One successful approach to adhesive bonding of these materials involves proper selection of surface pre-treatment prior to bonding. With the correct pre-treatment it is possible to glue these materials with one or more of several adhesives required by the applications involved. A second approach is the use of adhesives without surface pre-treatment, such as hot melts, high tack pressure-sensitive adhesives, solvent-based specialty adhesives and, more recently, structural acrylic adhesives as such 3M DP-8005® and Loctite 3030®. In this paper, the shear strengths of two acrylic adhesives were evaluated using the lap shear test method ASTM D3163 and the block shear test method ASTM D4501. Two different industrial polyolefins (polyethylene and polypropylene) were used for adherends. However, the focus of this study was to measure the shear strength of polyethylene joints with acrylic adhesives. The effect of abrasion was also studied. Some test specimens were manually abraded using 180 and 320 grade abrasive paper. An additional goal of this work was to examine the effect of temperature and moisture on mechanical strength of adhesive joints.