524 resultados para Polyurethane hemimandibles
Resumo:
Aqueous-based polyurethane dispersions have been widely utilized as lubricants in textile, shoes, automotive, biomaterial and many other industries because they are less aggressive to surrounding environment. In this work thin films with different thickness were deposited on biocompatible polyurethane by plasma polymerization process using diethylene glycol dimethyl ether (Diglyme) as monomer. Molecular structure of the films was analyzed by Fourier Transform Infrared spectroscopy. The spectra exhibited absorption bands of O-H (3500-3200cm(-1)), C-H (3000-2900cm(-1)), C=O (1730-1650cm(-1)), C-O and C-O-C bonds at 1200-1600cm(-1). The samples wettability was evaluated by measurements of contact angle using different liquids such as water, glycerol, poly-ethane and CMC. The polyurethane surface showed hydrophilic behavior after diglyme plasma-deposition with contact angle dropping from 85(0) to 22(0). Scanning Electron Microscopy revealed that diglyme films covered uniformly the polyurethane surfaces ensuring to it a biocompatible characteristic.
Resumo:
Conselho Nacional de Desenvolvimento Científico e Tecnológico (CNPq)
Resumo:
Dynamic mechanical properties of a polyurethane (PU) elastomer and a mortar processed with the same elastomer (modified polytetramethylene ether glycol (PTMEG)) were studied. The results obtained showed that the liquid aromatic amine ETHACURE (R) 300, used as cure agent, can be used to substitute the aromatic amine MOCA (R), which is usually used as cure agent in high performance elastomers. The resulting mortar produced with ETHACURE (R) 300 presents similar dynamic-mechanical thermal properties when compared with MOCA (R). However, dynamic-mechanical thermal analysis studies showed that the mortar developed with ETHACURE (R) 300 presents some advantages such as the low values of tan d, indicating a good capacity of recovery of the strain after retreating an applied force. (c) 2012 Wiley Periodicals, Inc. J Appl Polym Sci, 2012
Resumo:
Conselho Nacional de Desenvolvimento Científico e Tecnológico (CNPq)
Resumo:
Molecular mobility in castor oil based polyurethane was investigated with thermally stimulated depolarization current (TSDC) measurements and alternating-current (ac) dielectric relaxation spectroscopy. Three peaks could be observed in TSDC thermograms from 173 to 373 K. The relaxation located at 213 K could be attributed to the change in the molecular chain due to the interaction between the isocyanate and the solvent, and it was well fitted with the Vogel-Fulcher-Tammann equation. The other two peaks were located at 274 and 365 K and could be attributed to interfacial polarization and space charge, respectively. (c) 2005 Wiley Periodicals, Inc.
Resumo:
Flexible and free-standing films from blends of polyurethane, based on castor oil, and polyaniline were obtained with various compositions by casting. Significant increase on conductivity followed by a considerable decrease on doping time was obtained by doping the films in N,N-dimethylformamide (DMF) solution with p-toluene sulphonic acid (TSA) or HCl instead of the conventional doping in aqueous solution. This doping efficiency is proposed to be due to an improved swelling of the blend structure caused by the solvent. The electrical conductivity increases significantly upon polyaniline content increase reaching 10(-2) S/cm for a polyaniline content of about 10% (w/w).
Resumo:
Vegetable-based polyurethane (PU) was prepared in the thin film form by spin coating. This polymer is synthesised from castor oil, which can be extracted from the seeds of a native plant in Brazil called mamona. This polymer is biocompatible and is being used as material for artificial bone. The PU was characterised by dielectric spectroscopy in a wide range of frequency (10(-5) Hz to 10(5) Hz) and by thermally stimulated discharge current (TSDC) measurements. The glass transition temperature (T-g=39degreesC) was determined and using the initial rise method the activation energy was found to be 1.58 eV. (C) 2003 Kluwer Academic Publishers.
Resumo:
Flexible and free-standing films of piezoelectric composites made up of lead zirconate titanate (PZT) ceramic powder dispersed in a castor oil-based polyurethane (PU) matrix were obtained by spin coating and characterised as materials for sensor applications. The piezoelectric coefficients d(31) and d(33) were measured with the usual technique. The piezoelectric charge constant d(33) yields values up to less than or equal to 24 pC/N, even at lower PZT content (33 vol%). Some desirable properties like piezoelectricity, flexibility and good mechanical resistance show this new material to be a good alternative for use as sensors and actuators.
Resumo:
Composite made of Lead Zirconate Titranate (PZT) ceramic powder and castor oil based polyurethane (PU) were prepared in the thin film form with 0-3 connectivity by spin coating. The composite films were obtained in the thickness range of 100 mum to 300 mum using 33-vol.% of ceramic. The samples mechanical resistance. The material was characterised by dielectric spectroscopy, thermally stimulated discharge current (TSDC), hysteresis measurements and laser-intensity-modulation method (LIMM). The pyroelectric coefficient at 343 K was 7x10(-5) C.m(-2) K-1 for the sample poled with 10 MV/m at 373 K for Ih. The results show that this new composite can be used as suitable piezo and pyroelectric sensors.
Resumo:
Flexible piezo- and pyroelectric composite was made in the thin film form by spin coating. Lead Zirconate Titanate (PZT) ceramic powder was dispersed in a castor oil-based polyurethane (PU) matrix, providing a composite with 0-3 connectivity. The dielectric data, measured over a wide range of frequency (10(-5) Hz to 105 Hz), shows a loss peak around 100 Hz related with impurities in the polymer matrix. There is also an evidence of a peak in the range 10(-4) Hz, possibly originating from the glass transition temperature T of the polymer. The pyroelectric coefficient at 34 K is 7.0x10(-5) C(.)m(-2.)K(-1) which is higher than that of P-PVDF (1X10(-5) C(.)m(-2.)K(-1)).
Resumo:
Thin films of blend made up of castor oil-based polyurethane (PU) and polyaniline (PANI) were obtained by casting. The molecular mobility was studied using dielectric spectroscopy and thermally stimulated depolarization current (TSDC) for blends with two different compositions (90/10, 80/20) and the results were compared with PU pure. The peak located around -60 degrees C in TSDC thermograms of PU/PANI blend has dipolar behavior and might be attributed to the change in the molecular chain due to the interaction between isocyanate and the solvent. Vogel-Fulcher Tammann fits was performed on the observed relaxation and the result shows a alpha-relaxation-like. (c) 2005 Springer Science + Business Media, Inc.
Resumo:
Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)
Resumo:
Coordenação de Aperfeiçoamento de Pessoal de Nível Superior (CAPES)
Resumo:
Conselho Nacional de Desenvolvimento Científico e Tecnológico (CNPq)
Resumo:
Innocuous biocompatible materials have been searched to repair or reconstruct bone defects. Their goal is to restore the function of live or dead tissues. This study compared connective tissue and bone reaction when exposed to demineralized bovine bone matrix and a polyurethane resin derived from castor bean (Ricinus communis). Forty-five rats were assigned to 3 groups of 15 animals (control, bovine bone and polyurethane). A cylindrical defect was created on mandible base and filled with bovine bone matrix and the polyurethane. Control group received no treatment. Analyses were performed after 15, 45 and 60 days (5 animals each). Histological analysis revealed connective tissue tolerance to bovine bone with local inflammatory response similar to that of the control group. After 15 days, all groups demonstrated similar outcomes, with mild inflammatory reaction, probably due to the surgical procedure rather than to the material. In the polymer group, after 60 days, scarce multinucleated cells could still be observed. In general, all groups showed good stability and osteogenic connective tissue with blood vessels into the surgical area. The results suggest biocompatibility of both materials, seen by their integration into rat mandible. Moreover, the polyurethane seems to be an alternative in bone reconstruction and it is an inexhaustible source of biomaterial.