Non-stoichiometric mixed-valent molybdenum(VI, V) oxide film was grown on carbon substrates by the electrodeposition method. Responses of the prepared molybdenum oxide thin films to potential and to different solution acidities were studied by cyclic voltammetry, and the corresponding morphological changes of the film were monitored by atomic force microscopy (AFM). AFM images of the molybdenum oxide film show that the characteristic domed structure on the film surface increased during the transition from the oxidized state to the reduced state without signification change in the KMS surface roughness value. Furthermore, AFM studies show that the solution acidity has great effect on the morphology of the films, and the films undergo a homogenizing process with increasing pH of the solutions. (C) 1999 Elsevier Science S.A. All rights reserved.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

In this paper we focus on the surface morphology of polypyrrole film by using in situ atomic force microscopy (AFM). The formation process of polypyrrole film and the transformation process of the film from the oxidized to reduced state were clearly observed.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

对基于扫描隧道显微镜(Scanning tunnel microscope,STM)及原子力显微镜(Atomicforcemicroscope,AFM)的纳米操作技术发展进行阐述,针对其中存在的主要问题,引述出机器人化纳米操作的必要性。接着,对国内外机器人化纳米操作系统的研究进展、现状及存在的主要问题进行详细分析,提出基于AFM的机器人化纳米操作系统的结构原型,并指出实现机器人化纳米操作所需解决的关键技术问题及相应的解决方案之一,为进行深入的机器人化纳米操作研究提供了可以借鉴的研究方向。

Relevância:

100.00% 100.00%

Publicador:

Resumo:

针对原子力显微镜(AFM)纳米成像中存在的失真问题,研究了通过探针建模实现AFM扫描图像重构方法.目前探针盲建模算法在重构AFM图像时存在较大误差,因此提出基于探针模型预估计的AFM扫描图像重构方法.该方法采用分区探针针尖建模,并通过基于该探针模型的反卷积运算实现AFM扫描图像重构,获得比较接近真实形貌的AFM扫描图像.文中介绍了算法的具体步骤,通过仿真和实验结果证明,该方法能够有效降低AFM图像重构时引入的误差,得到的图像更能反映样品表面真实的形貌。

Relevância:

100.00% 100.00%

Publicador:

Resumo:

针对基于原子力显微镜(AFM)的机器人化纳米操作,对探针作用下探针—基片—微粒之间纳观力的作用规律进行了初步分析.指出起主要作用的纳观力为范德华力、接触斥力、纳米摩擦力、毛细作用力以及纳米静电力等五种,并初步推导了各种纳观力的表达形式.通过力—距离曲线仿真与实验验证了所进行分析的合理性;该分析有助于进行纳米操作的精确控制.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

© 2015 The American Physiological Society

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Cette thèse rapporte le greffage chimique de brosses de polymères neutres de poly(acrylate de tert-butyle) (PtBA) et de brosses chargées d’acide polyacrylique (PAA) sur des substrats de mica afin d’étudier leur conformation en fonction de la densité de greffage, du pH et de la force ionique. Le greffage est réalisé par polymérisation contrôlée par transfert d’atome (ATRP) initiée depuis la surface de mica afin de contrôler la croissance du polymère et sa densité de greffage. L’étude de la conformation des brosses de PtBA et de PAA a été menée avec la technique AFM en mesurant les épaisseurs des films à sec et gonflés sous différentes conditions de solvant, de pH et de force ionique. Une monocouche d’amorceurs est tout d’abord greffée sur du mica porteur de groupes hydroxyles créés par plasma (Ar/H2O). Cette couche a été caractérisée par des mesures d’angle de contact et par la technique TOF-SIMS. L’amorceur greffé a ensuite permis d’initier l’ATRP directement depuis la surface pour former des brosses neutres de PtBA liés de façon covalente au mica. La croissance linéaire de l’épaisseur du film avec la masse molaire du polymère en solution et le taux de conversion montre que la polymérisation est contrôlée. De plus, la ré-initiation des chaînes greffées atteste du caractère vivant de la polymérisation. L’hydrolyse des brosses de PtBA, confirmée par des mesures d’angle de contact, d’épaisseur et par FT-IR, conduit à des brosses de PAA. Les différentes couches greffées sont stables à l’air, en milieu organique et en milieu aqueux et leur gonflement est réversible. Le degreffage de la couche de PAA est observé suite à une longue exposition à pH basique. Cette étude représente le premier exemple de brosses greffées chimiquement sur du mica par polymérisation initiée depuis la surface. La variation des paramètres de la réaction de greffage de l’amorceur, tels que la concentration et la durée de réaction, a permis de contrôler le taux de recouvrement de l’amorceur et la densité de greffage du polymère. Une grande gamme de taux de recouvrement de l’amorceur est accessible et se traduit par un intervalle de densités de greffage allant de faibles à élevées (e.g. 0,04 chaîne/nm2 à 0,5 chaîne/nm2). L’étude de la conformation des chaînes de PtBA dans le DMF montre que cet intervalle de densités recouvre le régime crêpe au régime brosse. Le gonflement de brosses de PAA et la variation de la hauteur de la brosse L ont été étudiés en fonction de la densité de greffage, du pH et du sel ajouté cs (NaCl). Une transition brusque de collapsée à étirée est observée avec l’augmentation du pH, indépendamment de la densité de greffage. A pH neutre, les brosses sont collapsées et se comportent comme des brosses neutres en mauvais solvant. A pH basique, les brosses sont gonflées et chargées et se trouvent dans un régime de Pincus caractéristique des polyélectrolytes forts. En présence de sel, les charges sont partiellement écrantées et les répulsions électrostatiques dominent toujours dans la brosse. Cette étude contribue à une meilleure compréhension du comportement complexe des brosses de polyélectrolytes faibles et apporte un soutien expérimental à la théorie sur le comportement de ces brosses.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Ellipsometry and atomic force microscopy (AFM) were used to study the film thickness and the surface roughness of both 'soft' and solid thin films. 'Soft' polymer thin films of polystyrene and poly(styrene-ethylene/butylene-styrene) block copolymer were prepared by spin-coating onto planar silicon wafers. Ellipsometric parameters were fitted by the Cauchy approach using a two-layer model with planar boundaries between the layers. The smooth surfaces of the prepared polymer films were confirmed by AFM. There is good agreement between AFM and ellipsometry in the 80-130 nm thickness range. Semiconductor surfaces (Si) obtained by anisotropic chemical etching were investigated as an example of a randomly rough surface. To define roughness parameters by ellipsometry, the top rough layers were treated as thin films according to the Bruggeman effective medium approximation (BEMA). Surface roughness values measured by AFM and ellipsometry show the same tendency of increasing roughness with increased etching time, although AFM results depend on the used window size. The combined use of both methods appears to offer the most comprehensive route to quantitative surface roughness characterisation of solid films. Copyright (c) 2007 John Wiley & Sons, Ltd.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Asymmetric poly(styrene-b-methyl methacrylate) (PS-b-PMMA) diblock copolymers of molecular weight M-n = 29,700g mol(-1) (M-PS = 9300 g mol(-1) M-PMMA = 20,100 g mol(-1), PD = 1.15, chi(PS) = 0.323, chi(PMMA) = 0.677) and M-n = 63,900 g mol(-1) (M-PS = 50,500 g mol(-1), M-PMMA = 13,400 g mol(-1), PD = 1.18, chi(PS) = 0.790, chi(PMMA) = 0.210) were prepared via reversible addition-fragmentation chain transfer (RAFT) polymerization. Atomic force microscopy (AFM) was used to investigate the surface structure of thin films, prepared by spin-coating the diblock copolymers on a silicon substrate. We show that the nanostructure of the diblock copolymer depends on the molecular weight and volume fraction of the diblock copolymers. We observed a perpendicular lamellar structure for the high molar mass sample and a hexagonal-packed cylindrical patterning for the lower molar mass one. Small-angle X-ray scattering investigation of these samples without annealing did not reveal any ordered structure. Annealing of PS-b-PMMA samples at 160 degrees C for 24 h led to a change in surface structure.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Antarctic biodiversity is evolutionarily complex, reflecting the extreme ambient conditions. Therefore, Antarctic organisms exhibit sophisticated adaptations in all organization levels, including organs, tissues, and cells. Since red blood cells (RBCs) travel through the vertebrates blood delivering O(2) to all tissues and organs and purging the unwanted CO(2), they represent an interesting model to investigate biological adaptations. We have used atomic force microscopy (AFM) to compare the shape and size of RBCs of the Pygoscelid penguins. A total of 18 landmarks were measured in AFM images. When analyzed individually, the parameters were not capable of discriminating the RBCs of each species. However, the simultaneous use of multiple parameters discriminated (74%) among the RBCs. In addition, the use of RBC measurements was sufficient to hierarchically cluster the species in accordance to other common and reliable phylogenetic strategies. In light of these results, the use of RBC characters could effectively benefit taxonomic inferences.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

The purpose of this in vitro study was to test a new methodology to evaluate the effects of 35% hydrogen peroxide agent on the microtopography of sound enamel using an atomic force microscope (AFM). The buccal sound surfaces of three extracted human lower incisors were used, without polishing the surfaces to maintain them with natural morphology. These unpolished surfaces were subjected to bleaching procedure with 35% hydrogen peroxide that consisted of 4 applications of the bleaching agent on enamel surfaces for 10 min each application. Surface images were obtained in a 15 mu m x 15 mu m area using an AFM. The roughness (Ra and RMS) and the power spectral density (PSD) were obtained before and after the bleaching treatment. As results we could inquire that the PSD analyses were very suitable to identifying the morphological changes on the surfaces, while the Ra and RMS parameters were insufficient to represent the morphological alterations promoted by bleaching procedure on enamel. The morphological wavelength in the range of visible light spectrum(380-750 nm) was analyzed, showing a considerable increase of the PSD with the bleaching treatment. (C) 2009 Elsevier B. V. All rights reserved.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

In this paper we report here new considerations about the relationship between the mass and charge variations (m/z relationship) in underpotential deposition (UPD), bulk deposition and also in the H(2)Se formation reaction. Nanogravimetric experiments were able to show the adsorption of H(2)SeO(3) on the AuO surface prior to the voltammetric sweep and that, after the AuO reduction, 0.40 monolayer of H(2)SeO(3) remains adsorbed on the newly reduced Au surface, which was enough to gives rise to the UPD layer. The UPD results indicate that the maximum coverage with Se(ads) on polycrystalline gold surface corresponds to approximately 0.40 monolayer, in good agreement with charge density results. The cyclic voltammetry experiments demonstrated that the amount of bulk Se obtained during the potential scan to approximately 2 Se monolayers, which was further confirmed by electrochemical quartz crystal microbalance (EQCM) measurements that pointed out a mass variation corresponding of 3 monolayers of Se. In addition, the Se thin films were obtained by chronoamperometric experiments, where the Au electrode was polarized at +0.10V during different times in 1.0 M H(2)SO(4) + 1.0 mM SeO(2). The topologic aspects of the electrodeposits were observed in Atomic Force Microscope (AFM) measurements. Finally, in highly negative potential polarizations, the H(2)Se formation was analyzed by voltammetric and nanogravimetric measurements. These finding brings a new light on the selenium electrodeposition and point up to a proposed electrochemical model for molecule controlled surface engineering. (c) 2009 Elsevier Ltd. All rights reserved.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

The adhesion force between an atomic force microscope (AFM) tip and sample surfaces, mica and quartz substrates, was measured in air and water. The force curves show that the adhesion has a strong dependence on both the surface roughness and the environmental conditions surrounding the sample. The variability of the adhesion force was examined in a series of measurements taken at the same point, as well as at different places on the sample surface. The adhesion maps obtained from the distribution of the measured forces indicated regions contaminated by either organic compounds or adsorbed water. Using simple mathematical expressions we could quantitatively predict the adhesion force behavior in both air and water. The experimental results are in good agreement with theoretical calculations, where the adhesion forces in air and water were mostly associated with capillary and van der Waals forces, respectively. A small long-range repulsive force is also observed in water due to the overlapping electrical double-layers formed on both the tip and sample surfaces.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

The influence of small amounts of bovine serum albumin (BSA) (nM concentration) on the lateral organization of phospholipid monolayers at the air-water interface and transferred onto solid substrates as one-layer Langmuir-Blodgett (LB) films was investigated. The kinetics of adsorption of BSA onto the phospholipid monolayers was monitored with surface pressure isotherms in a Langmuir trough, for the zwitterionic dipalmitoylphosphatidyl ethanolamine (N,N-dimethyl-PE) and the anionic dimyristoylphosphatidic acid (DMPA). A monolayer of N,N-dimethyl-PE or DMPA incorporating BSA was transferred onto a solid substrate using the Langmuir-Blodgett technique. Atomic force microscopy (AFM) images of one-layer LB films displayed protein-phospholipid domains, whose morphology was characterized using dynamic scaling theories to calculate roughness exponents. For DMPA-BSA films the surface is characteristic of self-affine fractals, which may be described with the Kardar-Parisi-Zhang (KPZ) equation. on the other hand, for N,N-dimethyl-PE-BSA films, the results indicate a relatively flat surface within the globule. The height profile and the number and size of globules varied with the type of phospholipid. The overall results, from kinetics of adsorption on Langmuir monolayers and surface morphology in LB films, could be interpreted in terms of the higher affinity of BSA to the anionic DMPA than to the zwitterionic N,N-dimethyl-PE. Furthermore, the effects from such small amounts of BSA in the monolayer point to a cooperative response of DMPA and N,N-dimethyl-PE monolayers to the protein. (c) 2005 Elsevier B.V. All rights reserved.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

This in vitro study evaluated the marginal gap at the composite tooth/resin interface in class V cavities under the influence of two insertion techniques and a curing system by means of atomic force microscopy (AFM). Forty enamel and dentin cavities were prepared on the buccal surface in bovine teeth with quadratic forms measuring 2 mm X 2 mm and depth of 1.5 mm. The teeth were then divided into four groups: group A, 10 cavities were restored in one increment, light cured by halogen light; group B, 10 cavities filled with bulk filling, light cured by the light emitting diodes (LED); group C, 10 cavities were restored by the incremental technique, light cured by halogen light; group D, 10 cavities were restored by the incremental technique, light cured by the LED. The teeth underwent the polishing procedure and were analyzed by AFM for tooth/restoration interface evaluation. The data were compared between groups using the nonparametric Kruskall-Wallis and Mann-Whitney tests (p < 0.05). The results showed a statistically significant difference between groups A and B and groups A and C. It was concluded that no insertion and polymerization technique was able to completely seal the cavity.