901 resultados para GOLD-SILVER NANOPARTICLES
Resumo:
Uses of plants extracts are found to be more advantageous over chemical, physical and microbial (bacterial, fungal, algal) methods for silver nanoparticles (AgNPs) synthesis. In phytonanosynthesis, biochemical diversity of plant extract, non-pathogenicity, low cost and flexibility in reaction parameters are accounted for high rate of AgNPs production with different shape, size and applications. At the same time, care has to be taken to select suitable phytofactory for AgNPs synthesis based on certain parameters such as easy availability, large-scale nanosynthesis potential and non-toxic nature of plant extract. This review focuses on synthesis of AgNPs with particular emphasis on biological synthesis using plant extracts. Some points have been given on selection of plant extract for AgNPs synthesis and case studies on AgNPs synthesis using different plant extracts. Reaction parameters contributing to higher yield of nanoparticles are presented here. Synthesis mechanisms and overview of present and future applications of plant-extract-synthesized AgNPs are also discussed here. Limitations associated with use of AgNPs are summarised in the present review.
Resumo:
Modification of citrate and hydroxylamine reduced Ag colloids with thiocholine bromide, a thiol functionalized quaternary ammonium salt, creates particles where the zeta potential is switched from the normal values of ca. -50 mV to ca. + 50 mV. These colloids are stable but can be aggregated with metal salts in much the same way as the parent colloids. They are excellent SERS substrates for detection of anionic targets since their positive zeta potentials promote adsorption of negatively charged ions. This is important because the vast majority of published SERS studies involve cationic or neutral targets. Moreover, the fact that the modifier is a quaternary ammonium ion means that the negative surface charge is maintained even at alkaline pH. The modified colloids can be used to detect compounds which cannot be detected using conventional negatively-charged citrate or hydroxylamine reduced metal nanoparticles, for example the detection limit was 5.0 x 10(-5) M for perchlorate and
Resumo:
Silver nanoparticles (AgNP) have been produced and applied in a variety of products ranging from personal care products to food package containers, clothing and medicine utilities. The antimicrobial function of AgNP makes it very useful to be applied for such purposes. Silver (Ag) is a non-essential metal for organisms, and it has been historically present in the environment at low concentrations. Those concentrations of silver increased in the last century due to the use of Ag in the photographic industry and lately are expected to increase due to the use of AgNPs in consumer products. The presence of AgNP in the aquatic environment may pose a risk for aquatic species, and the effects can vary from lethal to sublethal effects. Moreover, the contact of aquatic organisms with AgNP may not cause immediately the death of individuals but it can be accumulated inside the animals and consequently transferred within the food chain. Considering this, the objective of this work was to study the transfer of silver nanoparticles in comparison to silver ions, which was used as silver nitrate, within an aquatic food chain model. To achieve this goal, this study was divided into four steps: the toxicity assessment of AgNP and AgNO3 to aquatic test-species, the bioaccumulation assessment of AgNP and AgNO3 by Pseudokirchneriella subcapitata and Daphnia magna under different exposure scenarios, and finally the evaluation of the trophic transfer of Ag through an experimental design that included the goldfish Carassius auratus in a model trophic chain in which all the species were exposed to the worse-case scenario. We observed that the bioconcentration of Ag by P. subcapitata is mainly driven by ionic silver, and that algae cannot internalize these AgNPs, but it does internalizes dissolved Ag. Daphnia magna was exposed to AgNP and AgNO3 through different exposure routes: water, food and both water and food. The worse-case scenario for Daphnia Ag bioaccumulation was by the joint exposure of contaminated water and food, showing that Ag body burdens were higher for AgNPs than for AgNO3. Finally, by exposing C. auratus for 10 days through contaminated water and food (supplied as D. magna), with another 7 days of depuration phase, it was concluded that the 10 days of exposure were not enough for fish to reach a plateau on Ag internal concentration, and neither the 7 days of elimination were sufficient to cause total depuration of the accumulated Ag. Moreover, a higher concentration of Ag was found in the intestine of fish when compared with other organs, and the elimination rate constant of AgNP in the intestine was very low. Although a potential for trophic transfer of AgNP cannot be suggested based in the data acquired in this study, there is still a potential environmental risk for aquatic species.
Resumo:
Nanoporous materials with large surface area and well-ordered pore structure have been synthesized. Thiol groups were grafted on the materials' surface to make heavy metal ion pre-concentration media. The adsorption properties ofthe materials were explored. Mercury, gold and silver can be strongly adsorbed by these materials, even in the presence of alkaline earth metal ion. Though the materials can adsorb other heavy metal ions such as lead and copper, they show differential adsorption ability when several ions are present in solution. The adsorption sequence is: mercury> == silver> copper » lead and cadmium. In the second part of this work, the memory effects of mercury, gold, silver and boron were investigated. The addition of 2% L-cysteine and 1% thiourea eliminates the problems of the three metal ions completely. The wash-out time for mercury dropped from more than 20 minutes to 18 seconds, and the wash-out time for gold decreased from more than 30 minutes to 49 seconds. The memory effect of boron can be reduced by the use of mannitol.
Resumo:
The Cochin estuary (CE), which is one of the largest wetland ecosystems, extends from Thanneermukkam bund in the south to Azhikode in the north. It functions as an effluent repository for more than 240 industries, the characteristics of which includes fertilizer, pesticide, radioactive mineral processing, chemical and allied industries, petroleum refining and heavy metal processing industries (Thyagarajan, 2004). Studies in the CE have been mostly on the spatial and temporal variations in the physical, chemical and biological characteristics of the estuary (Balachandran et al., 2006; Madhu et al., 2007; Menon et al., 2000; Qasim 2003;Qasim and Gopinathan 1969) . Although several monitoring programs have been initiated in the CE to understand the level of heavy metal pollution, these were restricted to trace metals distribution (Balachandran et al., 2005) or the influence of anthropogenic inputs on the benthos and phytoplankton (Madhu et al., 2007;Jayaraj, 2006). Recently, few studies were carried out on microbial ecology in the CE(Thottathil et al 2008a and b;Parvathi et al., 2009and 2011; Thomas et al., 2006;Chandran and Hatha, 2003). However, studies on metal - microbe interaction are hitherto not undertaken in this estuary. Hence, a study was undertaken at 3 sites with different level of heavy metal concentration tounderstand the abundance, diversity and mechanisms of resistance in metal resistant bacteria and its impact on the nutrient regeneration. The present work has also focused on the response of heavy metal resistant bacteria towards antibacterial agent’s antibiotics and silver nanoparticles
Resumo:
In this work a systematic study of the dependence of the structural, electronic, and vibrational properties on nanoparticle size is performed. Based on our total energy calculations we identified three characteristic regimes associated with the nanoparticle`s dimensions: (i) below 1.5 nm (100 atoms) where remarkable molecular aspects are observed; (ii) between 1.5 and 2.0 nm (100 and 300 atoms) where the molecular behavior is influenced by the inner core crystal properties; and (iii) above 2.0 nm (more than 300 atoms) where the crystal properties are preponderant. In all considered regimes the nanoparticle`s surface modulates its properties. This modulation decreases with the increasing of the nanoparticle`s size.
Resumo:
Carboxylic acid groups in PAH/PAA-based multilayers bind silver cations by ion exchange with the acid protons. The aggregation and spatial distribution of the nanoparticles proved to be dependent oil the process used to reduce the silver acetate aqueous solution. The reducing method with ambient light formed larger nanoparticles with diameters ranging from 4-50 nm in comparison with the reduction method using UV light, which gave particles with diameters of 2-4 nm The high toughness of samples reduced by ambient light is a result of two population distributions of particle sizes caused by different mechanisms when compared with the UV light process. According to these phenomena, a judicious choice of the spectral source call be used as a way to control the type and size of silver nanoparticles formed on PEMs. Depending on the energy of the light source, the Ag nanoparticles present cubic and/or hexagonal crystallographic structures, as confirmed by XRD. Beyond the kinetically controlled process of UV photoinduced cluster formation, the annealing produced by UV light allowed a second mechanism to modify the growth rates, spatial distribution, and phases.
Resumo:
Coordenação de Aperfeiçoamento de Pessoal de Nível Superior (CAPES)
Resumo:
Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)
Resumo:
Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)
Resumo:
Synthesis of silver nanoparticles by thermal treatment of a silver-aspartarne complex under inert atmosphere is described. Spherical metallic silver naroparticles with average diameter of 5 +/-2 nm were obtained by thermal treatment of the complex [Ag(C14H17N2O5)] 1/2H(2)O at 185 degrees C. Thermogravimetric and infrared analysis of the product show the occurrence of an ester bond cleavage of the aspartame ligand followed by rearrangement and release of a molecule of formaldehyde (H2CO), which is transformed in two strong reducing molecules, H-2 and CO. For silver reduction, the presence of the formaldehyde molecules seems to be the key process for the metallic nanoparticles fort-nation. The maintenance of the ligand crystalline structure, with the exception of the ester group loss, was noted as essential for nanoparticles formation and size control. The ligand crystalline structure was completely lost at 200 degrees C and particle growth and coalescence were observed above 250 degrees C. (C) 2005 Elsevier B.V. All rights reserved.
Resumo:
Conselho Nacional de Desenvolvimento Científico e Tecnológico (CNPq)
Resumo:
Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)
Resumo:
Hydrated bacterial cellulose (BC) membranes obtained from cultures of Acetobacter xylinum were used in the preparation of silver nanoparticles containing cellulose membranes. In situ preparation of Ag nanoparticles was achieved from the hydrolytic decomposition of silver triethanolamine (TEA) complexes. Scanning electron microscopy (SEM) images and X-ray diffraction (XRD) patterns both lead to the observation of spherical metallic silver particles with mean diameter of 8 nm well adsorbed onto the BC fibriles. (c) 2007 Elsevier B.V. All rights reserved.