This study evaluated the potential of plasma treatments to modify the surface chemistry and hydrophobicity of a denture base acrylic resin to reduce the Candida glabrata adhesion. Specimens (n=54) with smooth surfaces were made and divided into three groups (n=18): control - non-treated; experimental groups - submitted to plasma treatment (Ar/50W; AAt/130W). The effects of these treatments on chemical composition and surface topography of the acrylic resin were evaluated. Surface free energy measurements (SFE) were performed after the treatments and after 48h of immersion in water. For each group, half (n=9) of the specimens were preconditionated with saliva before the adhesion assay. The number of adhered C. glabrata was evaluated by cell counting after crystal violet staining. The Ar/50W and AAt/130W treatments altered the chemistry composition, hydrophobicity and topography of acrylic surface. The Ar/50W group showed significantly lower C. glabrata adherence than the control group, in the absence of saliva. After preconditioning with saliva, C. glabrata adherence in experimental and control groups did not differ significantly. There were significant changes in the SFE after immersion in water. The results demonstrated that Ar/50W treated surfaces have potential for reducing C. glabrata adhesion to denture base resins and deserve further investigation, especially to tailor the parameters to prolong the increased wettability. © 2012 Blackwell Verlag GmbH.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

In order to prolong the clinical longevity of resilient denture relining materials and reduce plaque accumulation, incorporation of antimicrobial agents into these materials has been proposed. However, this addition may affect their properties. Objective: This study evaluated the effect of the addition of antimicrobial agents into one soft liner (Soft Confort, Dencril) on its peel bond strength to one denture base (QC 20, Dentsply). Material and Methods: Acrylic specimens (n=9) were made (75x10x3 mm) and stored in distilled water at 37 degrees C for 48 h. The drug powder concentrations (nystatin 500,000U - G2; nystatin 1,000,000U - G3; miconazole 125 mg - G4; miconazole 250 mg - G5; ketoconazole 100 mg - G6; ketoconazole 200 mg - G7; chlorhexidine diacetate 5% - G8; and 10% chlorhexidine diacetate - G9) were blended with the soft liner powder before the addition of the soft liner liquid. A group (G1) without any drug incorporation was used as control. Specimens (n=9) (75x10x6 mm) were plasticized according to the manufacturers' instructions and stored in distilled water at 37 degrees C for 24 h. Relined specimens were then submitted to a 180-degree peel test at a crosshead speed of 10 mm/min. Data (MPa) were analyzed by analysis of variance (alpha=0.05) and the failure modes were visually classified. Results: No significant difference was found among experimental groups (p=0.148). Cohesive failure located within the resilient material was predominantly observed in all tested groups. Conclusions: Peel bond strength between the denture base and the modified soft liner was not affected by the addition of antimicrobial agents.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Purpose: Adequate denture hygiene can prevent and treat infection in edentulous patients, who are frequently elderly and have difficulty brushing their teeth. This study evaluated the efficacy of complete denture biofilm removal using a chlorhexidine solution in two concentrations: 0.12% and 2.0%. Materials and Methods: Sixty complete denture wearers participated in a trial for 21 days after receiving brushing instructions. They were distributed into three groups, according to the tested solution and regimen (n = 20): (G1) Control (daily overnight soaking in water); (G2) daily immersion at home in 0.12% chlorhexidine for 20 minutes after dinner; and (G3) a single immersion in 2.0% chlorhexidine for 5 minutes at the end of the experimental period, performed by a professional. Biofilm coverage area (%) was quantified on the internal surface of maxillary dentures at baseline and after 21 days. Afterward, the differences between initial and posttreatment results were compared by means of the Kruskal-Wallis test (a = 0.05). Results: Median values for biofilm coverage area after treatment were: (G1) 36.0%; (G2) 5.3%; and (G3) 1.4%. Differences were significant (KW = 35.25; p < 0.001), although G2 and G3 presented similar efficacy in terms of biofilm removal. Conclusions: Both chlorhexidine-based treatments had a similar ability to remove denture biofilm. Immersion in 0.12% or 2.0% chlorhexidine solutions can be used as an auxiliary method for cleaning complete dentures.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

An unfavorable denture-bearing area could compromise denture retention and stability, limit mastication, and possibly alter masticatory motion. The purpose of this study was to evaluate the masticatory movements of denture wearers with normal and resorbed denture-bearing areas. Completely edentulous participants who received new complete dentures were selected and divided into 2 groups (n=15) according to the condition of their denture-bearing areas as classified by the Kapur method: a normal group (control) (mean age, 65.9 ± 7.8 years) and a resorbed group (mean age, 70.2 ± 7.6 years). Masticatory motion was recorded and analyzed with a kinesiographic device. The patients masticated peanuts and Optocal. The masticatory movements evaluated were the durations of opening, closing, and occlusion; duration of the masticatory cycle; maximum velocities and angles of opening and closing; total masticatory area; and amplitudes of the masticatory cycle. The data were analyzed by 2-way ANOVA and the Tukey honestly significant difference post hoc test (α=.05). The group with a resorbed denture-bearing area had a smaller total masticatory area in the frontal plane and shorter horizontal masticatory amplitude than the group with normal denture-bearing area (P<.05). Denture wearers with resorbed denture-bearing areas showed reduced jaw motion during mastication.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Candida biofilms on denture surfaces are substantially reduced after a single immersion in denture cleanser. However, whether this effect is maintained when dentures are immersed in cleanser daily is unclear. The purpose of this study was to evaluate the effect of the daily use of enzymatic cleanser on Candida albicans biofilms on denture base materials. The surfaces of polyamide and poly(methyl methacrylate) resin specimens (n=54) were standardized and divided into 12 groups (n=9 per group), according to study factors (material type, treatment type, and periods of treatment). Candida albicans biofilms were allowed to form over 72 hours, after which the specimens were treated with enzymatic cleanser once daily for 1, 4, or 7 days. Thereafter, residual biofilm was ultrasonically removed and analyzed for viable cells (colony forming units/mm(2)) and enzymatic activity (phospholipase, aspartyl-protease, and hemolysin). Factors that interfered with the response variables were analyzed by 3-way ANOVA with the Holm-Sidak multiple comparison method (α=.05). Polyamide resin presented more viable cells of Candida albicans (P<.001) for both the evaluated treatment types and periods. Although enzymatic cleansing significantly (P<.001) reduced viable cells, daily use did not maintain this reduction (P<.001). Phospholipase activity significantly increased with time (P<.001) for both materials and treatments. However, poly(methyl methacrylate) based resin (P<.001) and enzymatic cleansing treatment (P<.001) contributed to lower phospholipase activity. Aspartyl-protease and hemolysin activities were not influenced by study factors (P>.05). Although daily use of an enzymatic cleanser reduced the number of viable cells and phospholipase activity, this treatment was not effective against residual biofilm over time.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Different surface treatment protocols of poly(methyl methacrylate) have been proposed to improve the adhesion of silicone-based resilient denture liners to poly(methyl methacrylate) surfaces. The purpose of this study was to evaluate the effect of different poly(methyl methacrylate) surface treatments on the adhesion of silicone-based resilient denture liners. Poly(methyl methacrylate) specimens were prepared and divided into 4 treatment groups: no treatment (control), methyl methacrylate for 180 seconds, acetone for 30 seconds, and ethyl acetate for 60 seconds. Poly(methyl methacrylate) disks (30.0 × 5.0 mm; n = 10) were evaluated regarding surface roughness and surface free energy. To evaluate tensile bond strength, the resilient material was applied between 2 treated poly(methyl methacrylate) bars (60.0 × 5.0 × 5.0 mm; n = 20 for each group) to form a 2-mm-thick layer. Data were analyzed by 1-way ANOVA and the Tukey honestly significant difference tests (α = .05). A Pearson correlation test verified the influence of surface properties on tensile bond strength. Failure type was assessed, and the poly(methyl methacrylate) surface treatment modifications were visualized with scanning electron microscopy. The surface roughness was increased (P < .05) by methyl methacrylate treatment. For the acetone and ethyl acetate groups, the surface free energy decreased (P < .05). The tensile bond strength was higher for the methyl methacrylate and ethyl acetate groups (P < .05). No correlation was found regarding surface properties and tensile bond strength. Specimens treated with acetone and methyl methacrylate presented a cleaner surface, whereas the ethyl acetate treatment produced a porous topography. The methyl methacrylate and ethyl acetate surface treatment protocols improved the adhesion of a silicone-based resilient denture liner to poly(methyl methacrylate).

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The wear resistance of denture teeth is important to the longevity of removable prostheses of edentulous patients. The ability of denture teeth to maintain a stable occlusal relationship over time may be influenced by this property. The purpose of this in vitro study was to evaluate the wear resistance of polymethyl methacrylate (PMMA) denture teeth based on their chemical composition when opposed by a ceramic antagonist. The maxillary canines (n=10) of 3 PMMA denture teeth (Trubyte Biotone, cross-linked PMMA; Trilux, highly cross-linked IPN (interpenetrating polymer network)-PMMA; and Vivodent, highly cross-linked PMMA) were secured in an in vitro 2-body wear-testing apparatus that produced sliding contact of the specimens (4.5 cycles/s, sliding distance of 20 mm, under 37°C running water) against glazed or airborne particle abraded ceramic. Wear resistance was measured as height loss (mm) under 300 g (sliding force) after 100,000 cycles, using a digital measuring microscope. Mean values were analyzed by 2-way ANOVA and Tukey's test (a=0.05). The wear of Trubyte Biotone (0.93 ± 0.14 mm) was significantly higher than that of both other types of teeth tested against abraded ceramic (p<0.05). The Vivodent tooth (0.64 ± 0.17 mm) exhibited the best wear resistance among the denture teeth tested against airborne particle abraded ceramic. There were no statistically significant differences (p>0.05) in wear among the 3 denture teeth evaluated against glazed ceramic. Trilux and Vivodent teeth tested against either glazed or airborne particle abraded ceramic did not differ significantly from each other (p<0.05). All teeth showed significantly more wear against airborne particle abraded ceramic than against glazed ceramic (p<0.05). In conclusion, the three types of PMMA denture teeth presented significantly different wear resistance against the abraded ceramic. The high-strength PMMA denture teeth were more wear-resistant than the conventional PMMA denture tooth.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The maintenance of masticatory function is especially important for patients wearing complete dentures due to their limitations. Thus, the bilateral balanced occlusal concept is used to achieve greater masticatory efficiency. However, a critical review of the literature reveals that there is not sufficient scientific evidence to support bilateral balanced occlusion as the most appropriate occlusal concept in complete dentures. Therefore, the aim of this study was to evaluate the masticatory efficiency in complete dentures wearers with bilateral balanced occlusion and canine guidance. A double-blinded controlled crossover clinical trial was conducted. The sample was composed by 24 edentulous patients who wore sets of complete dentures with both occlusal concepts during equal periods of 3 months. Objective data were collected through the masticatory efficiency test performed by the colorimetric method with the beads, in which capsules of a synthetic material enclosing fuchsine-containing granules were used. Subjective data were recorded by patient's ratings of their chewing function. No significant statistical difference was found for masticatory efficiency (p=0.095) between the two occlusal concepts studied. The results suggest that bilateral balanced occlusion does not improve the masticatory efficiency in complete denture wearers.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Fluorinated denture base acrylic resins can present more stable physical properties when compared with conventional polymers. This study evaluated the incorporation of a fluoroalkyl methacrylate (FMA) mixture in a denture base material and its effect on roughness and flexural strength. A swelling behavior assessment of acrylic resin specimens (n=3, per substance) after 12 h of FMA or methyl methacrylate (MMA) immersion was conducted to determine the solvent properties. Rectangular specimens (n=30) were allocated to three groups, according to the concentration of FMA substituted into the monomer component of a heat-polymerized acrylic resin (Lucitone 550), as follows: 0% (control), 10% and 20% (v/v). Acrylic resin mixed with concentrations of 25% or more did not reach the dough stage and was not viable. The surface roughness and flexural strength of the specimens were tested. Variables were analyzed by ANOVA and Tukey's test (a=0.05). Immersion in FMA produced negligible swelling, and MMA produced obvious swelling and dissolution of the specimens. Surface roughness at concentrations of 0%, 10% and 20% were: 0.25 ± 0.04, 0.24 ± 0.04, 0.22 ± 0.03 mm (F=1.78; p=0.189, not significant). Significant differences were found for flexural strength (F=15.92; p<0.001) and modulus of elasticity (F=7.67; p=0.002), with the following results: 96 ± 6, 82 ± 5, 84 ± 6 MPa, and 2,717 ± 79, 2,558 ± 128, 2574 ± 87 MPa, respectively. The solvent properties of FMA against acrylic resin are weak, which would explain why concentrations over 20% were not viable. Surface changes were not detected after the incorporation of FMA in the denture base acrylic resin tested. The addition of FMA into denture base resin may lower the flexural strength and modulus of elasticity, regardless of the tested concentration.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

OBJECTIVE: Removable partial dentures (RPD) require different hygiene care, and association of brushing and chemical cleansing is the most recommended to control biofilm formation. However, the effect of cleansers has not been evaluated in RPD metallic components. The aim of this study was to evaluate in vitro the effect of different denture cleansers on the weight and ion release of RPD. MATERIAL AND METHODS: Five specimens (12x3 mm metallic disc positioned in a 38x18x4 mm mould filled with resin), 7 cleanser agents [Periogard (PE), Cepacol (CE), Corega Tabs (CT), Medical Interporous (MI), Polident (PO), 0.05% sodium hypochlorite (NaOCl), and distilled water (DW) (control)] and 2 cobalt-chromium alloys [DeguDent (DD), and VeraPDI (VPDI)] were used for each experimental situation. One hundred and eighty immersions were performed and the weight was analyzed with a high precision analytic balance. Data were recorded before and after the immersions. The ion release was analyzed using mass spectrometry with inductively coupled plasma. Data were analyzed by two-way ANOVA and Tukey HSD post hoc test at 5% significance level. RESULTS: Statistical analysis showed that CT and MI had higher values of weight loss with higher change in VPDI alloy compared to DD. The solutions that caused more ion release were NaOCl and MI. CONCLUSIONS: It may be concluded that 0.05% NaOCl and Medical Interporous tablets are not suitable as auxiliary chemical solutions for RPD care.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Removable partial dentures (RPD) demand specific hygienic cleaning and the combination of brushing with immersion in chemical solutions has been the most recommended method for control of biofilm. However, the effect of the cleansers on metallic components has not been widely investigated. This study evaluated the effect of different cleansers on the surface of RPD. Five disc specimens (12 mm x 3 mm metallic disc centered in a 38 x 18 x 4 mm mould filled with resin) were obtained for each experimental situation: 6 solutions [Periogard (PE), Cepacol (CE), Corega Tabs (CT), Medical Interporous (MI), Polident (PO), 0.05% sodium hypochlorite (NaOCl), and distilled water (DW) control] and 2 Co-Cr alloys [DeguDent (DD) and VeraPDI (VPDI)] were used for each experimental situation. A 180-day immersion was simulated and the measurements of roughness (Ra, µm) of metal and resin were analyzed using 2-way ANOVA and Tukey’s test. The surface changes and tarnishes were examined with a scanning electronic microscopy (SEM). In addition, energy dispersive x-ray spectrometry (EDS) analysis was carried out at representative areas. Visually, NaOCl and MI specimens presented surface tarnishes. The roughness of materials was not affected by the solutions (p>0.05). SEM images showed that NaOCl and MI provided surface changes. EDS analysis revealed the presence of oxygen for specimens in contact with both MI and NaOCl solutions, which might suggest that the two solutions promoted the oxidation of the surfaces, thus leading to spot corrosion. Within the limitations of this study, it may be concluded that the NaOCl and MI may not be suitable for cleaning of RPD.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

In this study, a questionnaire was applied to patients from Ribeirão Preto Dental School, University of São Paulo, Brazil, to evaluate the hygiene methods and habits concerning the use of complete dentures, the age of dentures, and whether patients have been instructed on how to clean their dentures. The mean age of patients was 63.35 years, and most of them were females (82.08%). The results showed that 62.26% of the respondents had been using the same maxillary complete denture for more than 5 years, and 49.06% used the same mandible complete denture for more than 5 years. Of the patients interviewed, 58.49% slept with the dentures. Mechanical brushing was the most used cleaning method by the patients (100%), using water, dentifrice and toothbrush (84.91%). Most patients (51.89%) reported never having been instructed by their dentists as to how to clean their dentures. Based on the limitations of this study, it was concluded that the patients interviewed had limited knowledge about prosthetic hygiene and oral care. The method more used by patients was the mechanical method of brushing, most patients used the same complete dentures for more than 5 years and slept with the dentures.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

This article reports the case of a 55-year-old female patient who presented with unsatisfactory temporary crowns in the right mandibular premolars and molars, and a premolar-to-molar fixed partial denture in the left side. The clinical and radiographic examinations revealed a fracture of the left first premolar that was a retainer of the fixed partial denture and required extraction. Initially, the acrylic resin crowns were replaced by new ones, and a provisional RPD was made using acrylic resin and orthodontic wire clasps to resolve the problem arising from the loss of the fixed partial denture. Considering the patient's high esthetic demands, the treatment options for the definitive prosthetic treatment were discussed with her and rehabilitation with implant-supported dentures was proposed because the clinical conditions of the residual alveolar ridge were suitable for implant installation, and the patient's general health was excellent. However, the patient did not agree because she knew of a failed case of implant-retained denture in a diabetic individual and was concerned. The patient was fully informed that implant installation was the best indication for her case, but the arguments were not sufficient to change her decision. The treatment possibilities were presented and the patient opted for a clasp-retained removable partial denture (RPD) associated with the placement of crowns in the pillar teeth. The temporary RPD was replaced by the definitive RPD constructed subsequently. Although RPD was not the first choice, satisfactory esthetic and functional outcomes were achieved, overcaming the patient's expectations. This case report illustrates that the dentist must be prepared to deal with situations where, for reasons that cannot be managed, the patient does not accept the treatment considered as the most indicated for his/her case. Alternatives must be proposed and the functional and esthetic requirements must be fulfilled in the best possible manner.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

OBJECTIVES: To evaluate the color stability and hardness of two denture liners obtained by direct and indirect techniques, after thermal cycling and immersion in beverages that can cause staining of teeth. MATERIAL AND METHODS: Seventy disc-shaped specimens (18 x 3 mm) processed by direct (DT) and indirect techniques (IT) were made from Elite soft (n=35) and Kooliner (n=35) denture liners. For each material and technique, 10 specimens were subjected to thermal cycling (3,000 cycles) and 25 specimens were stored in water, coffee, tea, soda and red wine for 36 days. The values of color change, Shore A hardness (Elite soft) and Knoop hardness (Kooliner) were obtained. The data were subjected to ANOVA, Tukey's multiple-comparison test, and Kruskal-Wallis test (P<0.05). RESULTS: The thermal cycling promoted a decrease on hardness of Kooliner regardless of the technique used (Initial: 9.09± 1.61; Thermal cycling: 7.77± 1.47) and promoted an increase in the hardness in the DT for Elite Soft (Initial: 40.63± 1.07; Thermal cycling: 43.53± 1.03); hardness of Kooliner (DT: 8.76± 0.95; IT: 7.70± 1.62) and Elite Soft (DT: 42.75± 1.54; IT=39.30± 2.31) from the DT suffered an increase after the immersion in the beverages. The thermal cycling promoted color change only for Kooliner in the IT. Immersion in the beverages did not promote color change for Elite in both techniques. The control group of the DT of Kooliner showed a significant color change. Wine and coffee produced the greatest color change in the DT only for Elite Soft when compared to the other beverages. CONCLUSION: The three variation factors promoted alteration on hardness and color of the tested denture lining materials.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The present study evaluated the effect of repeated simulated microwave disinfection on physical and mechanical properties of Clássico, Onda-Cryl and QC-20 denture base acrylic resins. Aluminum patterns were included in metallic or plastic flasks with dental stone following the traditional packing method. The powder/liquid mixing ratio was established according to the manufacturer's instructions. After water-bath polymerization at 74ºC for 9 h, boiling water for 20 min or microwave energy at 900 W for 10 min, the specimens were deflasked after flask cooling and finished. Each specimen was immersed in 150 mL of distilled water and underwent 5 disinfection cycles in a microwave oven set at 650 W for 3 min. Non-disinfected and disinfected specimens were subjected to the following tets: Knoop hardness test was performed with 25 g load for 10 s, impact strength test was done using the Charpy system with 40 kpcm, and 3-point bending test (flexural strength) was performed at a crosshead speed of 0.5 mm/min until fracture. Data were analyzed statistically by ANOVA and Tukey's test (α= 0.05%). Repeated simulated microwave disinfections decreased the Knoop hardness of Clássico and Onda-Cryl resins and had no effect on the impact strength of QC-20. The flexural strength was similar for all tested resins.