978 resultados para Colloidal Crystallization


Relevância:

20.00% 20.00%

Publicador:

Resumo:

Transparent glasses of BaNaB9O15 (BNBO) were fabricated via the conventional melt-quenching technique. The amorphous and the glassy nature of the as-quenched samples were, respectively, confirmed by x-ray powder diffraction and differential scanning calorimetry (DSC). The glass transition and crystallization parameters were evaluated under non-isothermal conditions using DSC. The correlation between the heating rate dependent glass transition and the crystallization temperatures was studied and the Kauzmann temperature was deduced for BNBO glass plates and powdered samples. The values of the Kauzmann temperature for the plates and powdered samples were 776 K and 768 K, respectively. An approximation- free method was used to evaluate the crystallization kinetic parameters for the BNBO glass samples. The effect of the sample thickness on the crystallization kinetics of BNBO glasses was also investigated.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The basic lectin from winged bean (Psophocarpus tetragonolobus) could be crystallized using polyethyleneglycol (PEG) 4000 (I), PEG 8000 (II) and 2-methylpentane-2,4-diol (MPD) (III) as precipitants. Crystal forms I and II grew in the presence of methyl-α-Image -galactopyranoside or N -acetylgalactosamine while III grew in the absence of sugar. The three forms have the same space group (P21212) and similar unit cell dimensions with two dimeric molecules in the asymmetric unit. The unit cell dimensions are a = 156·8 Å, b = 89·0 Å, c = 73·3 Å for I, a = 155·5 Å, b = 92·3 Å, c = 72·5 Å for II and a = 148·3 Å, b = 90·7 Å, c = 73·8 Å for III. The crystals, particularly those grown using PEG 8000, are suitable for high resolution X-ray analysis, which is in progress.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Fabrication of multilayer microcapsules via layer-by-layer approach through hydrogen bonding has attracted enormous interest due to its strong response to pH. In this communication, we have prepared hydrogen-bonded multilayer microcapsule without using any cross-linking agent by using DNA base pair (adenine and thymine) modified biocompatible polymers. The growth of the self-assembly on colloidal (melamine formaldehyde: MF) particles has been monitored with zeta potential measurement. The capsules were obtained on dissolution of MF particles at 0.1N HCl. The capsules were characterized with scanning electron microscopy. Moreover, we have observed the salt induced microscopic change in self-assembly of this system on the surface of colloidal particles.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The thermal degradation behavior of banana fiber and polypropylene/banana fiber composites has been studied by thermogravimetric analysis. Banana fiber was found to be decomposing in two stages, first one around 320 degrees C and the second one around 450 degrees C. For chemically treated banana fiber, the decomposition process has been at a higher temperature, indicating thermal stability for the treated fiber. Activation energies for thermal degradation were estimated using Coats and Redfern method. Calorific value of the banana fiber was measured using a constant volume isothermal bomb calorimeter. rystallization studies exhibited an increase in the crystallization temperature and crystallinity of polypropylene upon the addition of banana fiber. POLYM. COMPOS., 31:1113-1123, 2010. (C) 2009 Society of Plastics Engineers.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Bacillus subtilis BacB is an oxidase that is involved in the production of the antibiotic bacilysin. This protein contains two double-stranded beta-helix (cupin) domains fused in a compact arrangement. BacB crystallizes in three crystal forms under similar crystallization conditions. An interesting observation was that a slight perturbation of the crystallization droplet resulted in the nucleation of a different crystal form. An X-ray absorption scan of BacB suggested the presence of cobalt and iron in the crystal. Here, a comparative analysis of the different crystal forms of BacB is presented in an effort to identify the basis for the different lattices. It is noted that metal ions mediating interactions across the asymmetric unit dominate the different packing arrangements. Furthermore, a normalized B-factor analysis of all the crystal structures suggests that the solvent-exposed metal ions decrease the flexibility of a loop segment, perhaps influencing the choice of crystal form. The residues coordinating the surface metal ion are similar in the triclinic and monoclinic crystal forms. The coordinating ligands for the corresponding metal ion in the tetragonal crystal form are different, leading to a tighter packing arrangement. Although BacB is a monomer in solution, a dimer of BacB serves as a template on which higher order symmetrical arrangements are formed. The different crystal forms of BacB thus provide experimental evidence for metal-ion-mediated lattice formation and crystal packing.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The study of proteins involved in de novo biosynthesis of purine nucleotides is central in the development of antibiotics and anticancer drugs. In view of this, a protein from the hyperthermophile Pyrococcus horikoshii OT3 was isolated, purified and crystallized using the microbatch method. Its primary structure was found to be similar to that of SAICAR synthetase, which catalyses the seventh step of de novo purine biosynthesis. A diffraction-quality crystal was obtained using Hampton Research Crystal Screen II condition No. 34, consisting of 0.05 M cadmium sulfate hydrate, 0.1 M HEPES buffer pH 7.5 and 1.0 M sodium acetate trihydrate, with 40%(v/v) 1,4-butanediol as an additive. The crystal belonged to space group P3(1), with unit-cell parameters a = b = 95.62, c = 149.13 angstrom. Assuming the presence of a hexamer in the asymmetric unit resulted in a Matthews coefficient (V-M) of 2.3 angstrom(3) Da(-1), corresponding to a solvent content of about 46%. A detailed study of this protein will yield insights into structural stability at high temperatures and should be highly relevant to the development of antibiotics and anticancer drugs targeting the biosynthesis of purine nucleotides.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The purpose of this study is to experimentally investigate the interaction of inelastic deformation and microstructural changes of two Zr-based bulk metallic glasses (BMGs): Zr41.25Ti13.75Cu12.5Ni10Be22.5 (commercially designated as Vitreloy 1 or Vit1) and Zr46.75Ti8.25Cu7.5Ni10Be27.5 (Vitreloy 4, Vit4). High-temperature uniaxial compression tests were performed on the two Zr alloys at various strain rates, followed by structural characterization using differential scanning calorimetry (DSC) and transmission electron microscopy (TEM). Two distinct modes of mechanically induced atomic disordering in the two alloys were observed, with Vit1 featuring clear phase separation and crystallization after deformation as observed with TEM, while Vit4 showing only structural relaxation with no crystallization. The influence of the structural changes on the mechanical behaviors of the two materials was further investigated by jump-in-strain-rate tests, and flow softening was observed in Vit4. A free volume theory was applied to explain the deformation behaviors, and the activation volumes were calculated for both alloys.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Biofunctionalization of noble metal nanoparticles like Ag, Au is essential to obtain biocompatibility for specific biomedical applications. Silver nanciparticles are being increasingly used in bio-sensing applications owing to excellent optoelectronic properties. Among the serum albumins, the most abundant proteins in plasma, a wide range of physiological functions of Bovine Serum Albumin (BSA) has made it a model system for biofunctionalization. In absence of adequate prior reports, this study aims to investigate the interaction between silver nanoparticles and BSA. The interaction of BSA [0.05-0.85% concentrations] with Ag nanoparticles [50 ppm concentration] in aqueous dispersion was Studied through UV-vis spectral changes, morphological and surface structural changes. At pH 7, which is More than the isoelectric point of BSA, a decrease in absorbance at plasmon peak of uninteracted nanciparticles (425 mn) was noted till 0.45% BSA, beyond that a blue shift towards 410 urn was observed. The blue shift may be attributed to enhanced electron density on the particle surfaces. Increasing pH to 12 enhanced the blue shift further to 400 rim. The conformational changes in BSA at alkaline pH ranges and consequent hydrophobic interactions also played an important role. The equilibrium adsorption data fitted better to Freundlich isotherm compared to Langmuir Curve. The X-ray diffraction study revealed complete coverage of Ag nanoparticles by BSA. The scanning electron microscopic study of the interacted nanoparticles was also carried Out to decipher morphological changes. This study established that tailoring the concentration of BSA and pH of the interaction it was possible to reduce aggregation of nanoparticles. Biofunctionalized Ag nanoparticles with reduced aggregation will be more amenable towards bio-sensing applications. (C) 2009 Elsevier B.V. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Crystallization kinetics of MSI and MSII stages in Metglas 2826A has been investigated by quantitative transmission electron microscopy. The volume fraction of crystallization against time curve has been found to show a plateau in the lower temperature region of annealing. It has been found that the glass transition temperature, T g, has no effect on the sequence reversal of the crystallization reaction. It has been shown that the sequence reversal of transformation stages occurs due to the large difference in the activation energy of crystallization of MSI and MSII. In addition, the change in the morphology of the crystals obtained by annealing the amorphous alloy below and above the glass transition temperature, T g, is reported.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Composite ZrO2-SiO2 powders were prepared using a gel route. Morphological and crystallographic features of ZrO2 particles formed during the heat treatment, and the particle sizes of the composites have been investigated. The following polymorphic changes have been observed during the heat treatment: amorphous -> metastable-cubic/tetragonal ZrO2 -> tetragonal ZrO2 -> monoclinic ZrO2. SiO2 crystallizes above 1273 K. The martensitic transformation of ZrO2 (t -> m) was observant in situ, when exposed to a high-energy electron beam. These results are important in the production of ZrO2-toughened ceramics of controlled microstructure.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

A detailed evaluation of size, shape and microstrains of BaTiO3 crystallites produced by hydrothermal crystallization at 90 – 180 °C and 0.1 – 1.2 MPa, from amorphous TiO2· xH2O (3 < × < 8) gel and aqueous Ba(OH)2 is presented, using X-ray line-broadening and TEM studies. Whereas the concentration of Ba(OH)2 and the acceptor impurities affect the crystallite shape, the stoichimetry with respect to Ba/Ti, donor as well as acceptor impurities, and the temperature of crystallization influence the microstrains. It is shown that strains in the crystallites are related to the point defects in the lattice. Compensation of the residually present hydroxyl ions in the oxygen sublattice by cation vacancies results in strains leading to metastable presence of the cubic phase at room temperature. Studies on the diffuse phase transition behaviour of these submicron powders show that the stable tetragonal phase is produced only on annealing at high temperatures where the mobility of cations vacancies are larger. Heat-treatment reduces anisotropy and strain in undoped samples, whereas annealing is less effective in doped materials. Comparison of the crystillite size by TEM showed better agreement with the Warren—Averbach method.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

On hydrogenation of the Laves phase SmFe2, an amorphous SmFe2H3.6 (a-SmFe2H3.6) alloy was formed between 400 K and 500 K. The amorphous nature of the alloy was confirmed by X-ray diffraction, transmission electron microscopy and thermal analysis. However, SmFe2 absorbed hydrogen in the crystal state below 350 K and decomposed into SmH2 and α-Fe above 550 K. The crystallization behaviour of a-SmFe2H3.6 was investigated by differential scanning calorimetry in combination with electron microscopy. Even after considerable hydrogen desorption (Image ) by an endothermic reaction on heating, the amorphous state was retained. Crystallization of a-SmFe2H3.6 took place in two stages. The first stage involved the precipitation of α-Fe in the amorphous matrix. The second stage involved the decomposition of the remaining amorphous phase into the equilibrium phases SmH2 and SmFe2.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The galactose-specific lectin from the seeds of Dolichos lablab has been crystallized using the hanging-drop vapour-diffusion technique. The crystals belong to space group P1, with unit-cell parameters a = 73.99, b = 84.13, c = 93.15 angstrom, alpha = 89.92, beta = 76.01, gamma = 76.99 degrees. X-ray diffraction data to a resolution of 3.0 angstrom have been collected under cryoconditions ( 100 K) using a MAR imaging-plate detector system mounted on a rotating-anode X-ray generator. Molecular-replacement calculations carried out using the available structures of legume lectins as search models revealed that the galactose-specific lectin from D. lablab forms a tetramer similar to soybean agglutinin; two such tetramers are present in the asymmetric unit.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

A nonequilibrium generalization of the density-functional theory of freezing is proposed to investigate the shear-induced first-order phase transition in colloidal suspensions. It is assumed that the main effect of a steady shear is to break the symmetry of the structure factor of the liquid and that for small shear rate, the phenomenon of a shear-induced order-disorder transition may be viewed as an equilibrium phase transition. The theory predicts that the effective density at which freezing takes place increases with shear rate. The solid (which is assumed to be a bcc lattice) formed upon freezing is distorted and specifically there is less order in one plane compared with the order in the other two perpendicular planes. It is shown that there exists a critical shear rate above which the colloidal liquid does not undergo a transition to an ordered (or partially ordered) state no matter how large the density is. Conversely, above the critical shear rate an initially formed bcc solid always melts into an amorphous or liquidlike state. Several of these predictions are in qualitative agreement with the light-scattering experiments of Ackerson and Clark. The limitations as well as possible extensions of the theory are also discussed.