897 resultados para Chlorobutyl Rubber


Relevância:

20.00% 20.00%

Publicador:

Resumo:

Blends of poly (butylene terephthalate) (PBT) and epoxided ethylene-propylene-diene terpolymer (EEPDM) were prepared. Their mechanical properties and morphology were studied by Izod impact test machine and scanning electronic microscope respectively, It was found that the notched Izod impact strength of blend PBT/EEPDM was as about 23 times as that of pure PET and about 10 times as that of blend PBT/EPDM at room temperature, The dispersed rubber particles were much smaller and the phase boundary was more blurred in blend PBT/EEPDM than in blend PBT/EPDM. The toughness of blend PBT/EEPDM was much more better than that of blend PET and PBT/EPDM, which was in good agreement with the difference between their morphologies.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Raw polymer and compound of hydrogenated acrylonitrile butadiene rubber (HNBR) were subjected to gamma-ray irradiation. Crosslinking was found to be the main chemical reaction induced by irradiation; the ratio of chain scission to crosslinking as well as

Relevância:

20.00% 20.00%

Publicador:

Resumo:

End-linked hydroxyl-terminated polybutadiene containing unattached linear polybutadiene was used to study the effect of reptating species on the fracture mechanics of rubber networks. The concentration of reptating species in the networks ranged from 0 to 100%. The fracture mechanics of the networks was described using the critical strain energy release rate in mode III testing, i.e. the tearing energy. The tearing energy was measured at room temperature using a 'trouser' specimen at a strain rate spanning five logarithmic decades. When the strain rate was as low as 10(-4) s-1, the tearing energy of the networks increased with reduction in reptating species. In this case the reptating species did not contribute to the tearing energy of the networks due to relaxation. Hence, the tearing energy increased with the number of crosslinked chains per unit volume in the networks. At a strain rate ranging from 10(-3) to 10(-1) s-1, the tearing energy of the networks was governed by local viscosity. The tearing energies of the networks containing various amounts of reptating species were superimposed to give a master curve based on the Williams-Landel-Ferry equation.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

A novel poly sulfone/polyethylene oxide/silicone rubber (PSOPEO/SR) multilayer composite membrane was fabricated by double coating polysulfone substrate membrane with polyethylene oxide and silicone rubber. Gas permeation experiments were performed at 30 degrees C for hydrogen and nitrogen. PSf(PEO/SR membrane displayed high and steady performance for H-2/N-2: permeances of H-2 and N-2 of 49.51 and 0.601 GPU, respectively, and H-2/N-2 ideal separation factor of 82.3. It was explained that layer interfaces due to the introduction of PEO layer act as the permselective media and are responsible for the higher H-2/N-2 ideal separation factor which has exceeded the intrinsic permselectivities of the three polymers used in this study. (c) 2005 Elsevier B.V. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Image warping, often referred to as "rubber sheeting" represents the deformation of a domain image space into a range image space. In this paper, a technique is described which extends the definition of a rubber-sheet transformation to allow a polygonal region to be warped into one or more subsets of itself, where the subsets may be multiply connected. To do this, it constructs a set of "slits" in the domain image, which correspond to discontinuities in the range image, using a technique based on generalized Voronoi diagrams. The concept of medial axis is extended to describe inner and outer medial contours of a polygon. Polygonal regions are decomposed into annular subregions, and path homotopies are introduced to describe the annular subregions. These constructions motivate the definition of a ladder, which guides the construction of grid point pairs necessary to effect the warp itself.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The cultivation of rubber trees in Xishuangbanna Prefecture in China’s Yunnan Province has triggered an unprecedented economic development but it is also associated with severe environmental problems. Rubber plantations are encroaching the indigenous rainforests at a large scale and a high speed in Xishuangbanna. Many rare plant and animal species are endangered by this development, the natural water management is disturbed and even the microclimate in this region has changed over the past years. The present study aims at an assessment of the environmental benefits accruing from a reforestation project partly reversing the deforestation that has taken place over the past years. To this end a Contingent Valuation survey has been conducted in Xishuangbanna to elicit local residents’ willingness to pay for this reforestation program that converts existing rubber plantations back into forest. It is shown that local people's awareness of the environmental problems caused by increasing rubber plantation is quite high and that in spite of the economic advantages of rubber plantation there is a positive willingness among the local population to contribute financially to a reduction of existing rubber plantations for the sake of a partial restoration of the local rainforest. These results could be used for the practical implementation of a PES (Payments for Eco-System Services) system for reforestation in Xishuangbanna.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Conservators have long been aware of the problems associated with the preservation of rubber objects due to inherent instability that can be attributed, in part, to the presence of additives. Inorganic additives, such as fillers, accelerators, stabilizers, and special ingredients are necessary in manufacturing to alter the properties of natural rubber. These materials all have different interactions with the rubber, and each other, and differing effects on the ageing process. To date, the most effective and accepted methods to preserve rubber are cold, dark storage of objects, or the use of low oxygen environments. While these methods are effective, they greatly limit access. The application of coatings to the surface of rubber objects can slow deterioration and greatly increase the ability of an institution to handle and display rubber objects. While numerous coatings for preventive and interventive treatment have been tested, none have been so successful to warrant routine use. The first section of this research highlighted the relationship between the inclusion of certain additives in natural rubber objects and the accelerated or slowed down overall degradation. In the second part of this research, the acrylic varnishes Golden Polymer Varnish with UVLS, Lascaux Acrylic Transparent Varnish-UV, Sennelier Matte Lacquer with UV Protection, and Liquitex Soluvar Varnish containing ultraviolet light absorbers or stabilizers were tested as a preventative coating for rubber. Through testing the visual and physical properties of the samples, as well as compound analysis the results of this research suggest that acrylic varnishes do provide protection, each to varying degrees. The results also provided insight into the behavior of rubber and these varnishes with continuing light exposure.

Relevância:

20.00% 20.00%

Publicador:

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The possible use of wood ash as an adsorbent of nickel sulphate from dilute solutions and the effect of operating parameters were investigated in this study. The rate constants of adsorption were determined at different concentrations and temperatures. The applicability of the first-order reversible equation and an empirical kinetic model were tested to understand the kinetics of nickel sulphate removal at different concentrations. Pore diffusion was found as the rate-controlling step. The Langmuir and Freundlich isotherms were applied to find out the adsorption parameters. The activation energy of adsorption was -11.54 kJ mol-1. The value of the enthalpy change was ?H=-10.35 kcal mol-1.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Background: In this study, the efficiency of Guar gum as a biopolymer has been compared with two other widely used inorganic coagulants, ferric chloride (FeCl3) and aluminum chloride (AlCl3), for the treatment of effluent collected from the rubber-washing tanks of a rubber concentrate factory. Settling velocity distribution curves were plotted to demonstrate the flocculating effect of FeCl3, AlCl3 and Guar gum. FeCl3 and AlCl3 displayed better turbidity removal than Guar gum at all settling velocities.

Result: FeCl3, AlCl3 and Guar gum removed 92.8%, 88.2% and 88.1% turbidity, respectively, of raw wastewater at a settling velocity of 0.1 cm min-1, respectively. Scanning electron microscopic (SEM) study conducted on the flocs revealed that Guar gum and FeCl3produced strong intercoiled honeycomb patterned floc structure capable of entrapping suspended particulate matter. Statistical experimental design Response Surface Methodology (RSM) was used to design all experiments, where the type and dosage of flocculant, pH and mixing speed were taken as control factors and, an optimum operational setting was proposed.

Conclusion: Due to biodegradability issues, the use of Guar gum as a flocculating agent for wastewater treatment in industry is highly recommended.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Hydrogenated nitrile butadiene rubber (HNBR) nanocomposites were prepared using commercially available organoclays (Cloisite 15A). The main focus of the current investigation is to study the influence of the organoclay reinforced in HNBR after subjecting it to long-term oxidative ageing and immersion studies. All the different nanoclay nanocomposites were air aged for a period of 168 h and at 150°C. The changes in the mechanical properties such as tensile strength and elongation at break have been compared with respect to the control sample. For immersion tests, three different liquid mediums were considered for this current investigation. All the samples were immersed in different mediums for a period of 168 h at 150°C. The changes in the swelling index and the mechanical properties have been reported with respect to the control sample. After reinforcing nanoclays into HNBR there was good resistance to swelling in all the three different liquid mediums in comparison to control sample. Tensile testing was performed on the immersed nanocomposites to evaluate the mechanical behaviour after immersion studies. A probable mechanism behind the improved performance has been suggested. © The Author(s) 2012.