The specific high energy and power capacities of rechargeable lithium metal (Li0) batteries are ideally suited to portable devices and are valuable as storage units for intermittent renewable energy sources. Lithium, the lightest and most electropositive metal, would be the optimal anode material for rechargeable batteries if it were not for the fact that such devices fail unexpectedly by short-circuiting via the dendrites that grow across electrodes upon recharging. This phenomenon poses a major safety issue because it triggers a series of adverse events that start with overheating, potentially followed by the thermal decomposition and ultimately the ignition of the organic solvents used in such devices.

In this thesis, we developed experimental platform for monitoring and quantifying the dendrite populations grown in a Li battery prototype upon charging under various conditions. We explored the effects of pulse charging in the kHz range and temperature on dendrite growth, and also on loss capacity into detached “dead” lithium particles.

Simultaneously, we developed a computational framework for understanding the dynamics of dendrite propagation. The coarse-grained Monte Carlo model assisted us in the interpretation of pulsing experiments, whereas MD calculations provided insights into the mechanism of dendrites thermal relaxation. We also developed a computational framework for measuring the dead lithium crystals from the experimental images.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

In this thesis we study the growth of a Li electrode-electrolyte interface in the presence of an elastic prestress. In particular, we focus our interest on Li-air batteries with a solid electrolyte, LIPON, which is a new type of secondary or rechargeable battery. Theoretical studies and experimental evidence show that during the process of charging the battery the replated lithium adds unevenly to the electrode surface. This phenomenon eventually leads to dendrite formation as the battery is charged and discharged numerous times. In order to suppress or alleviate this deleterious effect of dendrite growth, we put forth a study based on a linear stability analysis. Taking into account all the mechanisms of mass transport and interfacial kinetics, we model the evolution of the interface. We find that, in the absence of stress, the stability of a planar interface depends on interfacial diffusion properties and interfacial energy. Specifically, if Herring-Mullins capillarity-driven interfacial diffusion is accounted for, interfaces are unstable against all perturbations of wavenumber larger than a critical value. We find that the effect of an elastic prestress is always to stabilize planar interfacial growth by increasing the critical wavenumber for instability. A parametric study results in quantifying the extent of the prestress stabilization in a manner that can potentially be used in the design of Li-air batteries. Moreover, employing the theory of finite differences we numerically solve the equation that describes the evolution of the surface profile and present visualization results of the surface evolution by time. Lastly, numerical simulations performed in a commercial finite element software validate the theoretical formulation of the interfacial elastic energy change with respect to the planar interface.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Many researchers and industry observers claim that electric vehicles (EV) and plug-in hybrid electric vehicles (PHEV) could provide vehicle-to-grid (V2G) bulk energy and ancillary services to an electricity network. This work quantified the impact on various battery characteristics whilst providing such services. The sensitivity of the impact of V2G services on battery degradation was assessed for EV and PHEV for different battery capacities, charging regimes, and battery depth of discharge. Battery degradation was found to be most dependent on energy throughput for both the EV and PHEV powertrains, but was most sensitive to charging regime (for EVs) and battery capacity (for PHEVs). When providing ancillary services, battery degradation in both powertrains was most sensitive to individual vehicle battery depth of discharge. Degradation arising from both bulk energy and ancillary services could be minimised by reducing the battery capacity of the vehicle, restricting the number of hours connected and reducing the depth of discharge of each vehicle for ancillary services. Regardless, best case minimum impacts of providing V2G services are severe such as to require multiple battery pack replacements over the vehicle lifetime. © 2013 Elsevier Ltd.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The ever increasing demand for storage of electrical energy in portable electronic devices and electric vehicles is driving technological improvements in rechargeable batteries. Lithium (Li) batteries have many advantages over other rechargeable battery technologies, including high specific energy and energy density, operation over a wide range of temperatures (-40 to 70. °C) and a low self-discharge rate, which translates into a long shelf-life (~10 years) [1]. However, upon release of the first generation of rechargeable Li batteries, explosions related to the shorting of the circuit through Li dendrites bridging the anode and cathode were observed. As a result, Li metal batteries today are generally relegated to non-rechargeable primary battery applications, because the dendritic growth of Li is associated with the charging and discharging process. However, there still remain significant advantages in realizing rechargeable secondary batteries based on Li metal anodes because they possess superior electrical conductivity, higher specific energy and lower heat generation due to lower internal resistance. One of the most practical solutions is to use a solid polymer electrolyte to act as a physical barrier against dendrite growth. This may enable the use of Li metal once again in rechargeable secondary batteries [2]. Here we report a flexible and solid Li battery using a polymer electrolyte with a hierarchical and highly porous nanocarbon electrode comprising aligned multiwalled carbon nanotubes (CNTs) and carbon nanohorns (CNHs). Electrodes with high specific surface area are realized through the combination of CNHs with CNTs and provide a significant performance enhancement to the solid Li battery performance. © 2013 Elsevier Ltd.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Nano-structured silicon anodes are attractive alternatives to graphitic carbons in rechargeable Li-ion batteries, owing to their extremely high capacities. Despite their advantages, numerous issues remain to be addressed, the most basic being to understand the complex kinetics and thermodynamics that control the reactions and structural rearrangements. Elucidating this necessitates real-time in situ metrologies, which are highly challenging, if the whole electrode structure is studied at an atomistic level for multiple cycles under realistic cycling conditions. Here we report that Si nanowires grown on a conducting carbon-fibre support provide a robust model battery system that can be studied by (7)Li in situ NMR spectroscopy. The method allows the (de)alloying reactions of the amorphous silicides to be followed in the 2nd cycle and beyond. In combination with density-functional theory calculations, the results provide insight into the amorphous and amorphous-to-crystalline lithium-silicide transformations, particularly those at low voltages, which are highly relevant to practical cycling strategies.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

A novel ultra-lightweight three-dimensional (3-D) cathode system for lithium sulphur (Li-S) batteries has been synthesised by loading sulphur on to an interconnected 3-D network of few-layered graphene (FLG) via a sulphur solution infiltration method. A free-standing FLG monolithic network foam was formed as a negative of a Ni metallic foam template by CVD followed by etching away of Ni. The FLG foam offers excellent electrical conductivity, an appropriate hierarchical pore structure for containing the electro-active sulphur and facilitates rapid electron/ion transport. This cathode system does not require any additional binding agents, conductive additives or a separate metallic current collector thus decreasing the weight of the cathode by typically ∼20-30 wt%. A Li-S battery with the sulphur-FLG foam cathode shows good electrochemical stability and high rate discharge capacity retention for up to 400 discharge/charge cycles at a high current density of 3200 mA g(-1). Even after 400 cycles the capacity decay is only ∼0.064% per cycle relative to the early (e.g. the 5th cycle) discharge capacity, while yielding an average columbic efficiency of ∼96.2%. Our results indicate the potential suitability of graphene foam for efficient, ultra-light and high-performance batteries.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

This paper presents results concerning structure and electrochemical characteristics of the La0.67Mg0.33 (Ni0.8Co0.1Mn0.1) (x) (x=2.5-5.0) alloy. It can be found from the result of the Rietveld analyses that the structures of the alloys change obviously with increasing x from 2.5 to 5.0. The main phase of the alloys with x=2.5-3.5 is LaMg2Ni9 phase with a PuNi3-type rhombohedral structure, but the main phase of the alloys with x=4.0-5.0 is LaNi(5)phase with a CaCu5-type hexagonal structure. Furthermore, the phase ratio, lattice parameter and cell volume of the LaMg2Ni9 phase and the LaNi5 phase change with increasing x. The electrochemical studies show that the maximum discharge capacity increases from 214.7 mAh/g (x=2.5) to 391.1 mAh/g (x=3.5) and then decreases to 238.5 mAh/g (x=5.0). As the discharge current density is 1,200 mA/g, the high rate dischargeability (HRD) increases from 51.1% (x=2.5) to 83.7% (x=3.5) and then decreases to 71.6% (x=5.0). Moreover, the exchange current density (I-0) of the alloy electrodes first increases and then decrease with increasing x from 2.5 to 5.0, which is consistent with the variation of the HRD. The cell volume reduces with increasing x in the alloys, which is detrimental to hydrogen diffusion and accordingly decreases the low-temperature dischargeability of the alloy electrodes.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The irreversible capacity loss of the carbon electrode in lithium-ion batteries at the first cycle is caused mostly by surface film growth. We inspected an unknown irreversible capacity loss (UICL) of the natural graphite electrodes. The charge/discharge behavior of graphite and meso-phase carbon microbeads heat-treated at 2800 degrees C (MCMB28) as the materials of the carbon anode in the lithium-ion battery were compared. It was found that the capacity loss of the natural graphite electrode in the first cycle is caused not only by surface film growth, but also by irreversible lithium-ion intercalation on the new formed surface at the potential range of lithium intercalation, while the capacity loss of the MCMB28 electrode is mainly originated from surface film growth. The reason for the difference of their irreversible capacity losses of these two kinds of carbon material was explained in relation to their structural characteristics. (C) 1997 Published by Elsevier Science S.A.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

A variety of cokes pretreated at different temperatures are used as anodic materials and their electrochemical characteristics are examined by cyclic voltammetry. It is found that for some cokes such as petroleum coke (preheated at 1300 degrees C), pitch coke (1300 degrees C), needle coke (1900 degrees C), metallurgical coke (1900 degrees C), high capacity and cyclic efficiency are achieved. Needle coke (1900 degrees C) and metallurgical coke (1900 degrees C) in particular give a capacity of over 200 mAh/g and a cyclic efficiency of nearly 100%, whereas poor performance is exhibited by those pretreated at higher or lower temperatures, e.g., petroleum cokes (500 degrees C, 2800 degrees C), pitch coke (500 degrees C) and needle coke (2800 degrees C). The cyclic voltammograms show two electrochemical processes, one at about 0.1 V vs. Li+/Li which is electrochemically reversible, and may be attributed to the intercalation/deintercalation of lithium ions while the other, at about 0.6 V vs. Li+/Li, is electrochemically irreversible and may be assigned to the decomposition of the electrolyte solvent, which leads to formation of the passive film on the anode surface. The experimental results strongly suggest that the pretreatment temperature of cokes and of the solvent are determining factors for the growth, structure and properties of the passive film.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The preliminary work indicated that passive film is the most important factor influencing cell performance of carbon anode, and the carbon and solvent used govern cell performance by forming the passive film of different properties. A in situ XRD result is also presented.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The cylindrical 'D'-size batteries were fabricated by polyaniline paste cathode and lithium foil anode sandwiched with microporous polypropylene separator. The electrolyte used was LiClO4 dissolved in a mixed solvent of propylene carbonate and dimethoxyethane. The results of charge/discharge curves, charge/discharge cycles, the short-circuit current, the open-circuit voltage storage and the change of discharge capacity with temperature, discharge current are reported.