985 resultados para As-Sb-Se glasses
Resumo:
Digital Image
Resumo:
New glasses of 16.66SrO–16.66[(1 − x)Bi2O3–xSm2O3]–16.66Nb2O5–50Li2B4O7 (0 ≤ x ≤ 0.5, in molar ratio), i.e., the pseudo-binary Sm2O3-doped SrBi2Nb2O9–Li2B4O7 glass system, giving the crystallization of Sm3+-doped SrBi2Nb2O9 nanocrystals are developed. It is found that the thermal stability of the glasses against the crystallization and the optical band gap energy increases with increasing Sm2O3 content. The formation of fluorite-type Sm3+-doped SrBi2Nb2O9 nanocrystals (diameters: 13–37 nm) with a cubic structure is confirmed in the crystallized (530 °C, 3 h) samples from X-ray powder diffraction analyses, Raman scattering spectrum measurements, and transmission electron microscope observations. The effect of Sm3+-doping on the microstructure, Raman scattering peak positions, and dielectric properties of composites comprising of fluorite-type SrBi2Nb2O9 nanocrystals and the Li2B4O7 glassy phase is clarified. It is found that fluorite-type SrBi2Nb2O9 nanocrystals transform to stable perovskite-type SrBi2Nb2O9 crystals with an orthorhombic structure by heat treatments at around 630 °C.
Resumo:
Transparent glasses in the composition BaO-0.5Li(2)O-4.5B(2)O(3) (BLBO) were fabricated via the conventional melt-quenching technique. X-ray powder diffraction combined with differential scanning calorimetric (DSC) studies carried out on the as-quenched samples confirmed their amorphous and glassy nature, respectively. The crystallization behavior of these glasses has been studied by isothermal and nonisothermal methods using DSC. Crystallization kinetic parameters were evaluated from the Johnson-Mehl-Avrami equation. The value of the Avrami exponent (n) was found to be 3.6 +/- 0.1, suggesting that the process involves three-dimensional bulk crystallization. The average value of activation energy associated with the crystallization of BLBO glasses was 317 +/- 10 kJ/mol. Transparent glass-ceramics were fabricated by controlled heat-treatment of the as-quenched glasses at 845 K/40 min. The dielectric constants for BLBO glasses and glass-ceramics in the 100 Hz-10 MHz frequency range were measured as a function of the temperature (300-925 K). The electrical relaxation and dc conductivity characteristics were rationalized using electric modulus formalism. The imaginary part of the electric modulus spectra was modeled using an approximate solution of the Kohlrausch-Williams-Watts relation. The temperature-dependent behavior of stretched exponent (beta) was discussed for the as-quenched and heat-treated BLBO glasses.
Resumo:
Dielectric constants and loss tangents of As-Se glasses have been measured between 300 K and the respective glass transition temperatures and between 1 kHz and 20 kHz. The variation of dielectric constants has been interpreted in terms of both heteropolarity of bonds and average bond energies employing a chemically ordered network model. Various contributions to total molar polarizations have been estimated. Rapid rise of loss tangent in the vicinity of glass transitions has been interpreted in terms of rapid increase; of d.c. conductivity.
Resumo:
IR absorption spectra of As-Se glasses have been studied over a wide range of compositions. Various two-phonon, multiphonon (combination tones) and impurity absorptions have been identified. Compositional variation of relative band intensities has been explained in terms of the chemically ordered network model.
Resumo:
X-ray absorption edge and X-ray photoelectron spectroscopic studies of As-Se glasses seem to support a chemical ordering model.
Resumo:
The stress-optic coefficient (n3/2)(q11-q12) has been determined for a series of 18 optical glasses of different compositions in the wavelength range 5700-3200 Å. The coefficients are negative for all the glasses except for a high-lead-content glass of density 6·7 and refractive index 1·89. The numerical value of the coefficient decreases as one proceeds to the ultraviolet. This behaviour is just the opposite of what is observed in fused silica. By applying Mueller's theory, the strain polarizability constant and its dispersion have been evaluated.
Resumo:
The frequency and temperature dependences of the dielectric constant and the electrical conductivity of the transparent glasses in the composition Li2O-3B(2)O(3) were investigated in the 100 Hz-10 MHz frequency range. The dielectric constant and the loss in the low frequency regime were electrode material dependent. Dielectric and electrical relaxations were, respectively, analyzed using the Cole-Cole and electric modulus formalisms. The dielectric relaxation mechanism was discussed in the framework of electrode and charge carrier (hopping of the ions) related polarization using generalized Cole-Cole expression. The frequency dependent electrical conductivity was rationalized using Jonscher's power law. The activation energy associated with the dc conductivity was 0.80 +/- 0.02 eV, which was ascribed to the motion of Li+ ions in the glass matrix. The activation energy associated with dielectric relaxation was almost equal to that of the dc conductivity, indicating that the same species took part in both the processes. Temperature dependent behavior of the frequency exponent (n) suggested that the correlated barrier hopping model was the most apposite to rationalize the electrical transport phenomenon in Li2O-3B(2)O(3) glasses. These glasses on heating at 933 K/10 h resulted in the known nonlinear optical phase LiB3O5.
Resumo:
Arsenic selenide-telluride glasses have been investigated by X-ray absorption and photoelectron spectroscopy. The core electron energy shifts and chemical shifts in K-absorption edge measurements associated with the glass-crystal transitions of pure As2Se3 and As2Te3 have been studied. The effect of composition on the core level energy and valence bands of As2(Se,Te)3 glasses, has been discussed. Mixed-composition glasses are found to be considerably ionic.
Resumo:
The light and heat induced changes in the optical band gap of Sb/As2S3 nanomultilayered chalcogenide film has been studied. Even though the changes in optical bandgap are attributed to the light and heat induced interdiffusion, the diffusional intermixing between the layers is rather different with light and heat. The observed difference in the light and heat induced interdiffusion is due to unequal diffusion coefficients of light and heat predicted by thermal spike model.
Resumo:
We report the in situ optical transmission change in the complete visible region of the electromagnetic spectrum to asses the kinetics of photo induced interdiffusion in Sb/As2S3 nanomultilayered film. The interdiffusion of Sb into As2S3 matrix results in the formation of Sb-As2S3 ternary solid solutions which is explained by the change in optical band gap, absorption coefficients and Tauc parameter (B-1/2) with evolution of time. The wavelength dependence of the time constants provides a better description of photo induced effects. The time evolution of the absorption coefficients and optical band gap are significantly faster in this process. (C) 2009 Elsevier B.V. All rights reserved.
Resumo:
In Ge-As-Te system, the glass forming region determined by normal melt quenching method has two regions (GFR I and GFR II) separated by few compositions gap. With a simple laboratory built twin roller apparatus, we have succeeded in preparing Ge7.5AsxTe92.5-x glasses over extended composition ranges. A distinct change in T-g is observed at x = 40, exactly at which the separation of the glass forming regions occur indicating the changes in the connectivity and the rigidity of the structural network. The maximum observed in glass transition (T-g) at x = 55 corresponding to the average coordination number (Z(av)) = 2.70 is an evidence for the shift of the rigidity percolation threshold (RPT) from Z(av) = 2.40 as predicted by the recent theories. The glass forming tendency (K-gl) and Delta T (=T-c-T-g) is low for the glasses in the GFR I and high for the glasses in the GFR II.
Resumo:
Glaiis transitions of As-Se glasses have been investigated over a wide range of compositions by using differential scanning calorimetry. The variation of Tg with composition has been interpreted on the basis of a bond-lattice model.
Resumo:
Optically clear glasses were fabricated by quenching the melt of CaCO3-Bi2O3-B2O3 (in equimolecular ratio). The amorphous and glassy characteristics of the as-quenched samples were confirmed via the X-ray powder diffraction (XRD) and differential scanning calorimetric (DSC) studies These glasses were found to. have high thermal stability parameter (S). The optical transmission studies carried out in the 200-2500 nm wavelength range confirmed both the as-quenched and heat-treated samples to be transparent between 400 nm and 2500 nm. The glass-plates that were heat-treated just above the glass transition temperature (723 K) for 6 h retained approximate to 60% transparency despite having nano-crystallites (approximate to 50-100 nm) of CaBi2B2O7 (CBBO) as confirmed by both the XRD and transmission electron microscopy (TEM) studies. The dielectric properties and impedance characteristics of the as-quenched and heat-treated (723 K/6 h) samples were studied as a function of frequency at different temperatures. Cole-Cole equation was employed to rationalize the impedance data.