A method is presented for including path propagation effects into models of radiofrequency resonators for use in magnetic resonance imaging. The method is based on the use of Helmholtz retarded potentials and extends our previous work on current density models of resonators based on novel inverse finite Hilbert transform solutions to the requisite integral equations. Radiofrequency phase retardation effects are most pronounced at high field strengths (frequencies) as are static field perturbations due to the magnetic materials in the resonators themselves. Both of these effects are investigated and a novel resonator structure presented for use in magnetic resonance microscopy.
Resumo:
First of all, we would like to clarify that the passive to active transition was determined not by using Solgasmix [1], but by combining thermodynamic equilibrium and mass balance for the oxidation of SiC under pure CO2 and pure CO. The model used in our paper [2]was an extension ofWagner’s model [3], in a similar way as Balat et al. [4] did for the oxidation of SiC in oxygen.
Resumo:
This article reports on the liquid phase adsorption of flavour esters onto granular activated carbon. Ethyl propionate, ethyl butyrate, and ethyl isovalerate were used as adsorbates, and Filtrasorb 400 activated carbon was chosen as the adsorbent. Sips, Toth, Unilan, and Dubinin-Radushkevich isotherm equations which are generally used for heterogeneous adsorbents were used to fit the data. Although satisfactory in fitting the data, inconsistency in parameter values indicated these models to be inadequate. On the other hand the Dubinin-Radushkevich model gave more consistent and meaningful parameter values and adsorption capacities. By employing the Dubinin-Radushkevich equation, the limiting volume of the adsorbed space, which equals the accessible micropore volume, was determined, and found to correlate with the value from carbon dioxide adsorption.
Resumo:
In order to understand rock bolt Stress Corrosion Cracking (SCC), a series of experiments have been performed in Linearly Increasing Stress Test (LIST) apparatus. One series of experiments determined the threshold stress of various bolt metallurgies (900 MPa for Steel A, and 800 MPa for Steel B and C). The high values of threshold stress suggest that SCC begins in rock bolts when they are sheared by moving rock strata. Typical crack velocity values have been measured to be 2.5 x 10(-8) m s(-1), indicating that there is not much benefit for rock bolt steel of higher fracture toughness. Another series of experiments were performed to understand the environmental conditions causing SCC of steel A and galvanised Steel A rock bolt steel. SCC only occurred for environmental conditions for which produce hydrogen on the sample surface, leading to hydrogen embrittlement and SCC. Fracture surfaces of LIST samples failed by SCC were found to display the same fracture regions as fracture surfaces of rock bolts failed in service by SCC: Tearing Topography Surface (TTS), Corrugated Irregular Surface (CIS), quasi Micro Void Coalescence (qMVC) and Fast Fracture Surface (FFS). Water chemistry analysis were carried out on samples collected from various Australian mines in order to compare laboratory electrolyte conditions to those found in underground mines.
Resumo:
Rock bolt stress corrosion cracking (SCC) has been investigated using the linearly increasing stress test (LIST). One series of experiments determined the threshold stress of various bolt metallurgies (900 MPa for 1355AXRC, and 800 MPa for MAC and MA840B steels). The high values of threshold stress suggest that SCC begins in rock bolts when they are sheared by moving rock strata. SCC only occurred for environmental conditions which produce hydrogen on the sample surface, leading to hydrogen embrittlement and SCC. Different threshold potentials were determined for a range of metallurgies. Cold work was shown to increase the resistance of the steel to SCC. Rock bolt rib geometry does not have a direct impact on the SCC resistance properties of the bolt, although the process by which the ribs are produced can introduce tensile stresses into the bolt which lower its resistance to SCC. (C) 2004 Elsevier Ltd. All rights reserved.
Resumo:
This paper reports an investigation on techniques for determining elastic modulus and intrinsic stress gradient in plasma-enhanced chemical vapor deposition (PECVD) silicon nitride thin films. The elastic property of the silicon nitride thin films was determined using the nanoindentation method on silicon nitride/silicon bilayer systems. A simple empirical formula was developed to deconvolute the film elastic modulus. The intrinsic stress gradient in the films was determined by using micrometric cantilever beams, cross-membrane structures and mechanical simulation. The deflections of the silicon nitride thin film cantilever beams and cross-membranes caused by in-thickness stress gradients were measured using optical interference microscopy. Finite-element beam models were built to compute the deflection induced by the stress gradient. Matching the deflection computed under a given gradient with that measured experimentally on fabricated samples allows the stress gradient of the PECVD silicon nitride thin films introduced from the fabrication process to be evaluated.
Resumo:
The stress corrosion cracking (SCC) behavior and pre-exposure embrittlement of AZ31 magnesium alloy have been studied by slow strain rate tensile (SSRT) tests in this paper. It is showed that AZ31 sheet material is susceptible to SCC in distilled water, ASTM D1.387 solution, 0.01 M NaCl and 0.1 M NaCl solution. The AZ31 magnesium alloy also becomes embrittled if pre-exposed to 0.01 M NaCl solution prior to tensile testing. The degree of embrittlement increased with increasing the pre-exposure time, It is proposed that both the pre-exposure embrittlement and SCC were due to hydrogen which reduces the cohesive strength. i,e,. hydrogen embrittlement, (c) 2005 Elsevier B.V. All rights reserved.