The rheological characteristics of short Nylon-6 fiber reinforced styrene butadiene rubber (SBR) were studied using a capillary rheometer. The study was done with respect to the effect of shear rate, fiber concentration, and temperature on shear viscosity and die swell. All the melts showed pseudoplastic nature, which decreased with increasing temperature. Shear viscosity increased in the presence of fibers. Introduction of fiber reduces the temperature sensitivity of the rubber matrix. A reduction in die swell was found in presence of fibers.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The thermal properties of short Nylon-6 fiber-reinforced Styrene butadiene rubber (SBR) composites were studied by Thermogravimetric Analysis (TGA). The effect of epoxy-based bonding agent on thermal degradation of the gum and the composites was also studied. The thermal stability of the SBR was enhanced in the presence of Nylon-6 fibers and the stability of the composites increased in the presence of bonding agent. The epoxy resin did not significantly change the thermal stability of SBR gum vulcanizate. Results of kinetic studies showed that the degradation of SBR and the short nylon fiber-reinforced composites with and without bonding agents followed first-order kinetics.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The effect of diphenylmethane diisocyanate (MDI) -polyethyleneglycol (PEG) resin on the cure characteristics and mechanical properties of nitrile rubber/whole tyre eclaim-short nylon fiber composite-was studied. At a constant loading of 5 phr, the resin composition was varied. The minimum torque .,id (maximum - minimum) torque increased with isocyanate concentration. Scorch time and cure time showed a reduction on introduction of bonding agent. Properties like tensile strength, tear strength, and abrasion resistance increased with increase in MDI/PEG ratio, and these properties are higher in the longitudinal direction of fiber orientation. Compression set increased with isocyanate concentration and the resilience remain unchanged.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Cure characteristics and mechanical properties of short nylon fiber reinforced acrylonitrile butadiene rubber-reclaimed rubber composites were studied. Minimum torque, (maximum-minimum) torque and cure rate increased with fiber concentration. Scorch time and cure time decreased by the addition of fibers. Properties like tensile strength, tear strength, elongation at break, abrasion loss and heat build up were studied in both orientations of fibers. Tensile and tear properties were enhanced by the addition of fibers and were higher in the longitudinal direction. Heat build up increased with fiber concentration and were higher in the longitudinal direction. Abrasion resistance was improved in presence of short fibers and was higher in the longitudinal direction. Resilience increased on the introduction of fibers. Compression set was higher for blends.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The cure characteristics and mechanical properties of short nylon fiber- styrene /whole tyre reclaim (SBR/WTR) composites with and without an interfacial bonding agent based on 4,4 diphenyl methane diisocyanate and polyethylene glycol (MDI/PEG) have been studied. An 80:40 blend of SBR/ WTR reinforced with 20 phr of short nylon fiber has been selected and the MDI/ PEG ratio has been changed from 0.67:1 to 2:1. The minimum and maximum torques increased with isocyanate concentration. The scorch time and cure time showed an initial reduction. The cure rate showed an initial improvement. Tensile strength, tear strength and abrasion resistance increased with MDI/PEG ratio, these values were higher in longitudinal direction. Resilience and compression set increased with isocyanate concentration.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Acrylonitrile butadiene rubber (NBR) matrix was reinforced with different levels of short nylon fiber loading. Cure characteristics and mechanical properties of composites in longitudinal and transverse directions have been studied. Cure time was reduced while processability, as indicated by the minimum torque, was marginally reduced with increase in fiber loading. Tensile and tear properties improved with fiber concentration and the values were higher in longitudinal direction of fiber orientation. Abrasion resistance, resilience and compression set were increased in presence of fibers. Elongation at break values showed a drastic drop on introduction of fibers. Heat build up was higher for composites.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Cure characteristics of short polyester fiber-polyurethane composites with respect to different bonding agents (MD resins) based on 4, 4' diphenylmethanediisocyanate (MDI) and various diols like propyleneglycol (PG), polypropyleneglycol (PPG) and glycerol (GL) were studied. Tmax. - Tmin. of composites having MD resin were found to be higher than the composite without MD resin. Minimum torque and Tmax. - Tmin., scorch time and optimum cure time were increased with the increase of MDI equivalence. Optimum ratio of MDI / -of in the resin was found to be within the range of 1-1.5. It was observed from the cure characteristics that for getting better adhesion between short polyester fiber and the polyurethane matrix the best choice of MD resin was one based on MDI and 1:1 equivalent mixture of polypropyleneglycol and glycerol.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The rheological behavior of a short-polyester-fiber-filled polyurethane elastomer composite containing different bonding agents has been studied in the temperature range 120-160°C and in the shear rate range 63-608 s-'. The composite with and without bonding agents showed a pseudoplastic behavior which decreased with the increase of temperature. Composites containing bonding agents based on polypropyleneglycol and 4,4'-diphenylmethanediisocyanate showed the lowest viscosity values at a particular shear rate, whereas composites containing a glycerol- (GL) based bonding agent showed the highest viscosity. The viscosity of the composite decreased sharply after a particular temperature (140°C) and the fall was less drastic in the composite containing a GL-based bonding agent.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The stress relaxation behavior of polyurethane elastomer and short polyester fiber filled elastomer composites with and without bonding agents at different strain levels and strain rates was studied. It was found that these compounds exhibit a multistage relaxation mechanism and that the rate of relaxation and cross-over time depend on the strain level and strain rate. The incorporation of fibers reduced the stage-I relaxation rate and increased the cross-over time of the gum vulcanisate. A higher rate of relaxation (first stage) was shown by the composites with longitudinal fiber orientation and composites with bonding agents.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The cure characteristics of short fiber-polyurethane elastomer were studied with respect to different fiber-matrix bonding agents. A hexamethylenetetramine- resorcinol -hydrated silica based bonding agent was found to affect the stability of the composite. A new bonding agent, TP resin, based on polymeric toluenediisocyanate and polypropylene glycol has been developed. Cure characteristics of the composite with and without TP resin at different fiber loadings were also compared. Minimum torque, scorch time and optimum cure time increased with fiber content. Maximum torque was consistently higher with TP resin at all fiber loadings.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The thermal degradation of short polyester fiber reinforced polyurethane composites with and without different bonding agents has been studied by thermogravimetric analysis . It was found that degradation of the polyurethane takes place in two steps and that of the composites takes place in three steps. With the incorporation of 30 phr of fiber in the matrix , the onset of degradation was shifted from 230 to 238 ° C. The presence of bonding agents in the virgin elastomer and the composite gave an improved thermal stability . Results of kinetic studies showed that the degradation of polyurethane and the reinforced composites with and without bonding agents follows first -order reaction kinetics

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Optical fiber based laser induced fluorescence (LIF) measurements were carried out using Rhodamine B to analyze two different species of bacteria , a Gram-positive bacteria namely Bacillus .cmithii , and fibrin alginolvticus, a Gram-' negative bacteria . The fiber sensor was clearly able to distinguish between the two species of bacteria . Quenching effect of the dye Rhodamine B by Bacillus smitltii was observed . The effect of dye on the samples was also studied in detail.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The transient characteristics of an erbium-doped fiber (F.DF) laser, which can switch between wavelengths. are investigated. 77te laser has a set of coupled linear cavities. The slow gain dynamics of EDFs and the cross-gain saturation in the coupled cavities give rise to delayed switching responses and relocation oscillations, which are respertively measured to be l ins and 3.5 ms for the worst rase, and which mar be decreased by increasing the pump power. Thus, the switching speed of the laser may be higher than 100 Hz

Relevância:

20.00% 20.00%

Publicador:

Resumo:

In this paper, the generation of a multiwavelength laser source from a Brillouin -Erbium fiber laser in the long wavelength band (L-band) region is experimentally demonstrated. The proposed laser system utilizes a Fabrv-Perot cavity formed by fiber-loop mirrors. Twenty-four lines of Brillouin-Stokes with line spacings of 10 GHz are obtained in the L-band region

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Nanoscale silica was synthesized by precipitation method using sodium silicate and dilute hydrochloric acid under controlled conditions. The synthesized silica was characterized by Scanning Electron Microscopy (SEM), Transmission Electron Microscopy (TEM), BET adsorption and X-Ray Diffraction (XRD). The particle size of silica was calculated to be 13 nm from the XRD results and the surface area was found to be 295 m2/g by BET method. The performance of this synthesized nanosilica as a reinforcing filler in natural rubber (NR) compound was investigated. The commercial silica was used as the reference material. Nanosilica was found to be effective reinforcing filler in natural rubber compound. Filler-matrix interaction was better for nanosilica than the commercial silica. The synthesized nanosilica was used in place of conventional silica in HRH (hexamethylene tetramine, resorcinol and silica) bonding system for natural rubber and styrene butadiene rubber / Nylon 6 short fiber composites. The efficiency of HRH bonding system based on nanosilica was better. Nanosilica was also used as reinforcing filler in rubber / Nylon 6 short fiber hybrid composite. The cure, mechanical, ageing, thermal and dynamic mechanical properties of nanosilica / Nylon 6 short fiber / elastomeric hybrid composites were studied in detail. The matrices used were natural rubber (NR), nitrile rubber (NBR), styrene butadiene rubber (SBR) and chloroprene rubber (CR). Fiber loading was varied from 0 to 30 parts per hundred rubber (phr) and silica loading was varied from 0 to 9 phr. Hexa:Resorcinol:Silica (HRH) ratio was maintained as 2:2:1. HRH loading was adjusted to 16% of the fiber loading. Minimum torque, maximum torque and cure time increased with silica loading. Cure rate increased with fiber loading and decreased with silica content. The hybrid composites showed improved mechanical properties in the presence of nanosilica. Tensile strength showed a dip at 10 phr fiber loading in the case of NR and CR while it continuously increased with fiber loading in the case of NBR and SBR. The nanosilica improved the tensile strength, modulus and tear strength better than the conventional silica. Abrasion resistance and hardness were also better for the nanosilica composites. Resilience and compression set were adversely affected. Hybrid composites showed anisotropy in mechanical properties. Retention in ageing improved with fiber loading and was better for nanosilica-filled hybrid composites. The nanosilica also improved the thermal stability of the hybrid composite better than the commercial silica. All the composites underwent two-step thermal degradation. Kinetic studies showed that the degradation of all the elastomeric composites followed a first-order reaction. Dynamic mechanical analysis revealed that storage modulus (E’) and loss modulus (E”) increased with nanosiica content, fiber loading and frequency for all the composites, independent of the matrix. The highest rate of increase was registered for NBR rubber.