998 resultados para Coal particle


Relevância:

20.00% 20.00%

Publicador:

Resumo:

To find the pathologic cause of the children's dental fluorosis in southwestern China, diet structure before the age of 6 and prevalence rate of dental fluorosis (DF) of 405 children were investigated, and the fluorine and arsenic content of several materials were determined. The prevalence rate of DF of children living on roasted corn before the age of 6 is 100% with nearly 95% having the mild to severe DF; while that of children living on non-roasted corn or rice is less than 5% with all having very mild DF. The average fluorine and arsenic concentration are 20.26 mg/kg and 0.249 mg/kg in roasted corn, which are about 16 times and 35 times more than in non-roasted corn, respectively. The average fluorine concentration is 78 mg/kg in coal, 1116 mg/kg in binder clay and 313 mg/kg in briquette (coal mixed with clay). The average arsenic concentration of coal is 5.83 mg/kg, the binder clay is 20.94 mg/kg, with 8.52 mg/kg in the briquette. Living on roasted corn and chili is the main pathologic cause of endemic fluorosis in southwestern China. The main source of fluorine and arsenic pollution of roasted corn and chill is the briquette of coal and binder clay. (C) 2010 Elsevier B.V. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Thermal properties and crystallization-behavior of ultrafine fully-vulcanized powdered rubber (UFPR) toughened poly propylene (PP) were studied by Differential scanning calorimetry (DSC) and Wide angle X-ray diffraction (WAXD) measurements. It was found that the fraction of beta-form in the PP crystal increased at first, then sharply deceased up to zero with increasing UFPR content

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Hydrogenation of maleic anhydride (MAH) with Pd/C catalysts in supercritical carbon dioxide (scCO(2)) was investigated. The selectivity for gamma-butyrolactone (GBL) reached 97.3% in scCO(2) at 100% conversion of MAH, which was notably higher than that of 77.4% obtained in organic solvent of ethylene glycol dimethyl ether (EGDME). The particle size of Pd exhibited large influence on the reaction rate and selectivity of GBL. Higher selectivity of GBL was obtained with Pd/C catalyst of smaller Pd particle size, and the rate of GBL selectivity increase as a function of CO2 pressure was found to be significantly correlated with Pd particle size.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

A series of Pr0.55Ca0.45MnO3 compounds with average particle size ranging from 2000 to 30 nm have been synthesized by the sol-gel method and their charge ordering (CO) and magnetic properties are investigated. It is observed that with particle size decreasing, the CO transition is gradually suppressed and finally disappears upon particle size down to 35 nm, while the ferromagnetism (FM) emerges and exhibits a nonmonotonous variation with a maximum at 45 nm samples. The FM components in all samples never reach long-range ordering but rather only show short-range clusters. A new explanation considering the coupling between lattice, charge, and spin in the system is raised to understand the suppression of the CO state, Both the competition between the CO/AFM and FM states and the core-shell model are employed to explain the variation of the FM phase. These results may provide a deeper insight into the physics of particle size effect on the charge ordering manganite.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

It was theoretically pointed out that the product of the yield stress and yield strain of matrix polymer that determined the brittle-ductile transition (BDT) of particle toughened polymers. For given particle and test condition, the higher the product of the yield stress and the yield strain of the matrix polymer, the smaller the critical interparticle distance (IDc) of the blends was. This was why the IDc (0.15 mum) of the polypropylene (PP)/rubber blends was smaller than that (0.30 mum) of the nylon 66/rubber blends, and the IDc of the nylon 66/rubber blends was smaller than that (0.60 mum) of the high density polyethylene (HDPE)/rubber blends.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

A series of acrylic impact modifiers (AIMS) with different particle sizes ranging from 55.2 to 927.0 nm were synthesized by seeded emulsion polymerization, and the effect of the particle size on the brittle-ductile transition of impact-modified poly(vinyl chloride) (PVC) was investigated. For each AIM, a series of PVC/AIM blends with compositions of 6, 8, 10, 12, and 15 phr AIM in 100 phr PVC were prepared, and the Izod impact strengths of these blends were tested at 23 degrees C. For AIMs with particle sizes of 55.2, 59.8, 125.2, 243.2, and 341.1 nm, the blends fractured in the brittle mode when the concentration of AIM was lower than 10 phr, whereas the blends showed ductile fracture when the AIM concentration reached 10 phr. It was concluded that the brittle-ductile transition of the PVC/AIM blends was independent of the particle size in the range of 55.2-341.1 nm. When the particle size was greater than 341.1 nm, however, the brittle-ductile transition shifted to a higher AIM concentration with an increase in the particle size. Furthermore, the critical interparticle distance was found not to be the criterion of the brittle-ductile transition for the PVC/AIM blends.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

A two-armed polymer with a crown ether core self-assembles to produce macroporous films with pores perpendicularly reaching through the film down to the substrate. A possible assembling mechanism is discussed. The pore size can be conveniently adjusted by changing the solution concentration. These through-hole macroporous films provide a template for fabricating an array of Cu nanoparticle aggregates.