997 resultados para alginate nanoparticles
Resumo:
Hemorrhage is the leading cause of preventable death after a traumatic injury. Commercial hemostatic agents exist, but have various disadvantages including high cost, short shelf-lives, or secondary tissue damage. Polymer hydrogels provide a promising platform for the use of both biological and mechanical mechanisms to accelerate natural hemostasis and control hemorrhage. The goal of this work was to develop hydrogel particles composed of chitosan and alginate and loaded with zeolite in order to stop blood loss by targeting multiple hemostatic mechanisms. Several ii particle compositions were synthesized and then characterized through swelling studies, particle sizing, Scanning Electron Microscopy (SEM), and Fourier Transform Infrared Spectroscopy (FTIR). The in vitro interactions of the particles were evaluated through coagulation, degradation, platelet aggregation, and cytotoxicity studies. The results indicate that 4% alginate, 1% chitosan, 4% zeolite-loaded hydrogel beads can significantly reduce time to coagulation and increase platelet aggregation in vitro. Future research can look into the efficacy of these particles in vivo.
Resumo:
Silica nanoparticles (MSNs) with a highly ordered mesoporous structures (103A) with cubic Im3 m have been synthesized using triblock copolymers with high poly(alkylene oxide) (EO) segments in acid media. The produced nanoparticles displayed large specific surface area (approximately 765 cm(2)/g) with an average particles size of 120 nm. The loading efficiency was assessed by incorporating three major antiepileptic active substances via passive loading and it was found to varying from 17 to 25%. The state of the adsorbed active agents was further analyzed using differential scanning calorimetry (DSC) and X-ray powder diffraction (XRPD). Dissolution studies revealed rapid release profiles within the first 3 h. The viability of 3T3 endothelial cells was not affected in the presence of MSNs indicating negligible cytotoxicity. 2009 Elsevier B.V. All rights reserved.
Resumo:
In recent years, the use of swelling polymeric matrices for the encapsulation and controlled release of protein drugs has received significant attention. The purpose of the present study was to investigate the release of albumin, a model protein from alginate/hydroxypropyl-methylcellulose (HPMC) gel beads. A hydrogel system comprised of two natural, hydrophilic polymers; sodium alginate and HPMC was studied as a carrier of bovine serum albumin (BSA) which was used as a model protein. The morphology, bead size and the swelling ratio were studied in different physical states; fully swollen, dried and reswollen using scanning electron microscopy and image analysis. Finally the effect of different alginate/HPMC ratios on the BSA release profile in physiological saline solution was investigated. Swelling experiments revealed that the bead diameter increases with the viscosity of the alginate solution while the addition of HPMC resulted in a significant increase of the swelling ratio. The BSA release patterns showed that the addition of HPMC increased the protein-release rate while the release mechanism fitted the Peppas model. Alginate/HPMC beads prepared using the ionic gelation exhibited high BSA loading efficiency for all formulations. The presence of HPMC increased the swelling ability of the alginate beads while the particle size remained unaffected. Incorporation of HPMC in the alginate gels also resulted in improved BSA release in physiological saline solution. All formulations presented a non-Fickian release mechanism described by the Peppas model. In addition, the implementation of non-parametric tests showed significant differences in the release patterns between the alginate/HPMC and the pure alginate beads, respectively.
Resumo:
Laboratory simulation of cloud processing of three model dust types with distinct Fe-content (Moroccan dust, Libyan dust and Etna ash) and reference goethite and ferrihydrite were conducted in order to gain a better understanding of natural nanomaterial inputs and their environmental fate and bioavailability. The resulting nanoparticles (NPs) were characterised for Fe dissolution kinetics, aggregation/size distribution, micromorphology and colloidal stability of particle suspensions using a multi-method approach. We demonstrated that the: (i) acid-leachable Fe concentration was highest in volcanic ash (1 m Mg(-1) dust) and was followed by Libyan and Moroccan dust with an order of magnitude lower levels; (ii) acid leached Fe concentration in the<20 nm fraction was similar in samples processed in the dark with those under artificial sunlight, but average hydrodynamic diameter of NPs after cloud-processing (pH~6) was larger in the former; iii) NPs formed at pH~6 were smaller and less poly-disperse than those at low pH, whilst unaltered zeta potentials indicated colloidal instability; iv) relative Fe percentage in the finer particles derived from cloud processing does not reflect Fe content of unprocessed dusts (e.g. volcanic ash>Libyan dust). The common occurrence of Fe-rich "natural nanoparticles" in atmospheric dust derived materials may indicate their more ubiquitous presence in the marine environment than previously thought.
Resumo:
Laboratory studies were conducted to investigate the interactions of nanoparticles (NPs) formed via simulated cloud processing of mineral dust with seawater under environmentally relevant conditions. The effect of sunlight and the presence of exopolymeric substances (EPS) were assessed on the: (1) colloidal stability of the nanoparticle aggregates (i.e. size distribution, zeta potential, polydispersity); (2) micromorphology and (3) Fe dissolution from particles. We have demonstrated that: (i) synthetic nano-ferrihydrite has distinct aggregation behaviour from NPs formed from mineral dusts in that the average hydrodynamic diameter remained unaltered upon dispersion in seawater (~1500 nm), whilst all dust derived NPs increased about three fold in aggregate size; (ii) relatively stable and monodisperse aggregates of NPs formed during simulated cloud processing of mineral dust become more polydisperse and unstable in contact with seawater; (iii) EPS forms stable aggregates with both the ferrihydrite and the dust derived NPs whose hydrodynamic diameter remains unchanged in seawater over 24h; (iv) dissolved Fe concentration from NPs, measured here as <3 kDa filter-fraction, is consistently >30% higher in seawater in the presence of EPS and the effect is even more pronounced in the absence of light; (v) micromorphology of nanoparticles from mineral dusts closely resemble that of synthetic ferrihydrite in MQ water, but in seawater with EPS they form less compact aggregates, highly variable in size, possibly due to EPS-mediated steric and electrostatic interactions. The larger scale implications on real systems of the EPS solubilising effect on Fe and other metals with the additional enhancement of colloidal stability of the resulting aggregates are discussed.
Resumo:
Laboratory studies were conducted to evaluate the interaction between bare and polymer-coated magnetic nanoparticles (MNPs) with various environmentally relevant carrying solutions including natural oceanic seawater with and without addition of algal exopolymeric substances (EPS). The MNPs were coated with three different stabilising agents, namely gum Arabic (GA-MNP), dextran (D-MNP) and carboxymethyl-dextran (CMD-MNP). The colloidal stability of the suspensions was evaluated over 48 h and we demonstrated that: (i) hydrodynamic diameters increased over time regardless of carrying solution for all MNPs except the GA-coated ones; however, the relative changes were carrying solution- and coat-dependent; (ii) polydispersity indexes of the freshly suspended MNPs are below 0.5 for all coated MNPs, unlike the much higher values obtained for the uncoated MNPs; (iii) freshly prepared MNP suspensions (both coated and uncoated) in Milli-Q (MQ) water show high colloidal stability as indicated by zeta-potential values below -30 mV, which however decrease in absolute value within 48 h for all MNPs regardless of carrying solution; (iv) EPS seems to "stabilise" the GA-coated and the CMD-coated MNPs, but not the uncoated or the D-coated MNPs, which form larger aggregates within 48 h; (v) despite this aggregation, iron (Fe)-leaching from MNPs is sustained over 48 h, but remained within the range of 3-9% of the total iron-content of the initially added MNPs regardless of suspension media and capping agent. The environmental implications of our findings and biotechnological applicability of MNPs are discussed.
Resumo:
It is estimated that approximately 1.1 billion people globally drink unsafe water. We previously reported both a novel copper-alginate bead, which quickly reduces pathogen loading in waste streams and the incorporation of these beads into a novel swirl flow bioreactor (SFB), of low capital and running costs and of simple construction from commercially available plumbing pipes and fittings. The purpose of the present study was to trial this system for pathogen reduction in waste streams from an operating Dewats system in Hinjewadi, Pune, India and in both simulated and real waste streams in Seattle, Washington, USA. The trials in India, showed a complete inactivation of coliforms in the discharged effluent (Mean Log removal Value (MLRV) = 3.51), accompanied by a total inactivation of E. coli with a MLRV of 1.95. The secondary clarifier effluent also showed a 4.38 MLRV in viable coliforms during treatment. However, the system was slightly less effective in reducing E. coli viability, with a MLRV of 1.80. The trials in Seattle also demonstrated the efficacy of the system in the reduction of viable bacteria, with a LRV of 5.67 observed of viable Raoultella terrigena cells (100%).
Resumo:
We show in this study that the combination of a swirl flow reactor and an antimicrobial agent (in this case copper alginate beads) is a promising technique for the remediation of contaminated water in waste streams recalcitrant to UV-C treatment. This is demonstrated by comparing the viability of both common and UV-C resistant organisms in operating conditions where UV-C proves ineffective - notably high levels of solids and compounds which deflect UV-C. The swirl flow reactor is easy to construct from commonly available plumbing parts and may prove a versatile and powerful tool in waste water treatment in developing countries.