The three crystal structures reported here provide details of the interactions of mannose and the mannosyl-alpha-1,3-mannose component of a pentamannose with banana lectin and evidence for the binding of glucosyl-alpha-1,2-glucose to the lectin. The known structures involving the lectin include a complex with glucosyl-beta-1,3-glucose. Modeling studies on the three disaccharide complexes with the reducing end and the nonreducing end at the primary binding site are also provided here. The results of the Xray and modeling studies show that the disaccharides with an alpha-1,3 linkage prefer to have the nonreducing end at the primary binding site, whereas the reducing end is preferred at the site when the linkage is beta-1,3 in mannose/glucose-specific beta-prism I fold lectins. In the corresponding galactose-specific lectins, however, alpha-1,3-linked disaccharides cannot bind the lectin with the nonreducing end at the primary binding site on account of steric clashes with an aromatic residue that occurs only when the lectin is galactose-specific. Molecular dynamics simulations based on the known structures involving banana lectin enrich the information on lectin-carbohydrate interactions obtained from crystal structures. They demonstrate that conformational selection as well as induced fit operate when carbohydrates bind to banana lectin.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

C17H19ClO, M(r) = 274.7, triclinic, P1BAR, a = 11.154 (3), b = 12.685 (2), c = 12.713 (2) angstrom, alpha = 100.68 (1), beta = 113.58 (1), gamma = 104.50 (2)-degrees, V = 1511.1 (6) angstrom3, Z = 4, D(m) = 1.22, D(x) = 1.215 Mg m-3, Cu K-alpha, lambda = 1.5418 angstrom, mu = 2.16 mm-1, F(000) = 584, T = 293 K, R = 0.057 for 3481 observed reflections. The title compound is photostable in the crystalline state and lattice-energy calculations have been employed to rationalize the photobehaviour. The well-known beta-steering ability of the chloro group is not operative in this system as there are no Cl...Cl interactions in the crystal lattice. All five benzylidene-DL-piperitone structures so far studied are alpha-packed and the molecular topology appears to be a deciding factor even in the presence of steering groups.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The influence of pH on the corrosion behaviour of two aluminium-lithium-copper-magnesium-zirconium (8090 and 2091) alloys was studied and compared with a standard aircraft alloy, 2014 (Al-4.4% Cu) and 99.9% pure Al. In constant exposure and potentiodynamic polarization studies conducted in 3.5% NaCl solution having different pH values, all the alloys exhibited high corrosion rates in acidic and alkaline environments, with a minimum in less hostile environments close to neutral pH. The pitting potentials for aluminium-lithium alloys were slightly lower than those for 2014 and pure Al. The effect of pH on the passive current density was also less for aluminium-lithium alloys.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Zinc oxide ceramic varistors with simplified compositions of ZnO+Bi2O3+Co3O4+M(2)O (M=K or Na) show nonlinearity coefficients (alpha) of 40-75. The electron paramagnetic resonance spectra and optical reflectance spectra show that there is a direct interdependence between the oxidation state of transition metals and the alkali ions. The X-ray photoelectron spectra indicate that the alkali ions preserve a higher oxidation state of cobalt, Co(III), in the grain boundary regions than in the grain interiors having more Co(II). Admittance spectroscopy shows that, while the nature of traps remains unaltered, the trap density increases with the concentration of alkali ions near the interface. The observed defect states are associated with the grain bulk than with the grain boundary interfaces, as indicated by the isothermal capacitance transient signals

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The domain of dynamic recrystallization (DRX) in as-cast 304 stainless steel material occurs at higher temperatures (1250 degrees C) and lower strain rates (0.001 s(-1)) than in wrought 304 stainless steel (1100 degrees C and 0.01 s(-1)). The above result has been explained earlier on the basis of a simple theoretical DRX model involving the rate of nucleation versus rate of grain boundary migration. The present investigation is aimed at examining experimentally the influence of carbide particles on the DRX of ascast 304 using secondary ion mass spectrometric (SIMS) analysis. Isothermal compression tests at a constant true strain rate have been performed on wrought 304 and as-cast 304 materials in the temperature and strain rate ranges of 1000 to 1250 degrees C and 0.001 to 1 s(-1) respectively. The SIMS analysis carried out on the deformed samples revealed that the large carbides present in the as-cast 304 material strongly influence the DRX process. In as-cast 304 material, the presence of large carbide particles in the microstructure shifts the DRX domain to higher temperature and lower strain rate in comparison with wrought 304 material.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Cadmium (Cd) influences lipid peroxidation (LPO) by enhancing peroxidation of membrane lipids and by disturbing the antioxidant system of cells. In isolated rat hepatocytes, LPO was observed in cells incubated with Cd (50-250 mu M) for various time periods up to 90 min. The antioxidant enzymes such as superoxide dismutase (SOD) and catalase (CAT) were inhibited along with depletion of glutathione (GSH) in hepatocytes treated with Cd. The results show that Cd influences LPO in rat hepatocytes due to decrease in antioxidant status.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

KTP crystals have been grown below and above the ferroelectric transition temperature by flux method employing both spontaneous and top-seeded solution growth techniques. A slight morphological difference has been observed in these crystals when grown below and above the T-c. Ferroelectric domains are studied in these crystals by selective domain etching. It is seen that the ferroelectric domains in crystals grown spontaneously below T, show a complicated structure. A systematic investigation of the factors influencing domain structure has been carried out. Stress to some extent has been shown to affect the domain structure. Finally, a convenient way of converting the multidomain crystals into monodomain ones is described.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Soil incorporation of metalaxyl [methyl N-(2-methoxyacetyl)-N-(2,6,xylyl)-DL-alaninate] significantly enhanced root colonization of the vesicular-arbuscular (VA) mycorrhizal fungi Glomus fasciculatum associated with wheat. The stimulatory response of VA mycorrhizal fungi to low concentration of metalaxyl resulted in increased plant biomass production, nutrient uptake and grain yield of wheat. However, higher concentrations of metalaxyl, particularly 2.5 ppm of metalaxyl affected the mycorrhizal infection and seed yield of wheat, Addition of urban compost to an extent ameliorated the toxic effect of fungicide on VA mycorrhizal colonization, plant growth and yield of wheat when compared to unamended soil.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

We investigate the influence of the ferromagnetic layer on the magnetic and transport properties of YBa2Cu3O7-delta in YBa2Cu3O7-delta (YBCO)/La0.7Sr0.3MnO3 (LSMO) bilayers. The temperature dependent dc magnetization study reveals the presence of magnetic anisotropy in YBCO/LSMO bilayer as compared to the pure YBCO layer. The ac susceptibility study on YBCO/LSMO bilayers reveals stronger pinning and the temperature dependent critical current is found to be less prone to temperature. Besides, the current (I) dependent electrical transport studies on YBCO/LSMO exhibit a significant reduction in the superconducting T-c with increase in I and it follows I-2/3 dependence in accord with the pair breaking effect. The higher reduction of superconducting T-c in YBCO/LSMO is believed to be due to the enhanced pair-breaking induced by the spin polarized carriers being injected into the superconductor. (C) 2011 American Institute of Physics. doi: 10.1063/1.3560029]

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The effect on the macroscopic compressive failure features of introduction of two flexible foam layers, either together at mid-region or separately at two locations that are away from the midregion, into a glass-epoxy (G-E) system is studied in this work. In this experimental approach an attempt to look at the possible influence the foam/G-E interface region has on the way the materials respond to compressive loading is made by involving an analyses of macrofractographic features. While foam-free samples fail by extensive ear formation and separation nearer to the mid-region, the foam bearing ones display pronounced interface separation. The positioning of the foam sheet(s) has a bearing on the failure features.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Radially homogeneous bulk alloys of GaxIn1-xSb in the range 0.7 < x < 0.8, have been grown by vertical Bridgman technique. The factors affecting the interface shape during the growth were optimised to achieve zero convexity. From a series of experiments, a critical ratio of the temperature gradient (G) of the furnace at the melting point of the melt composition to the ampoule lowering speed (v) was deduced for attaining the planarity of the melt-solid interface. The studies carried out on directional solidification of Ga0.77In0.23Sb mixed crystals employing planar melt-solid interface exhibited superior quality than those with nonplanar interfaces. The solutions to certain problems encountered during the synthesis and growth of the compound were discussed. (C) 1999 Elsevier Science B.V. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Hardened concrete is a three-phase composite consisting of cement paste, aggregate and interface between cement paste and aggregate. The interface in concrete plays a key role on the overall performance of concrete. The interface properties such as deformation, strength, fracture energy, stress intensity and its influence on stiffness and ductility of concrete have been investigated. The effect of composition of cement, surface characteristics of aggregate and type of loading have been studied. The load-deflection response is linear showing that the linear elastic fracture mechanics (LEFM) is applicable to characterize interface. The crack deformation increases with large rough aggregate surfaces. The strength of interface increases with the richness of concrete mix. The interface fracture energy increases as the roughness of the aggregate surface increases. The interface energy under mode II loading increases with the orientation of aggregate surface with the direction of loading. The chemical reaction between smooth aggregate surface and the cement paste seems to improve the interface energy. The ductility of concrete decreases as the surface area of the strong interface increases. The fracture toughness (stress intensity factor) of the interface seems to be very low, compared with hardened cement paste, mortar and concrete.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The kinetics of thermal degradation of poly(vinyl chloride) (PVC) in solution was investigated at various temperatures (210-250degreesC). The degradation rate coefficients were determined from the time evolution of the molecular weight distribution (MWD). The energy of activation, determined from the temperature dependence of the rate coefficient, was 26.6 kcal/mol. The degradation of PVC was also studied in the presence of a catalyst (HZSM-5 zeolite). The results indicated that increase of the degradation rate of PVC is first order with the HZSM-5 concentration up to 50 g/L and zero order at higher concentrations. The thermal degradation kinetics of PVC in the presence of 50 g/L of the catalyst was studied at various temperatures. The temperature dependency of the rate coefficient was used to calculate the activation energy (21.5 kcal/mol). This is consistent with the observation that the presence of a catalyst generally decreases the activation energy and promotes degradation. (C) 2002 John Wiley Sons, Inc.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

An experimental investigation on the bond strength of the interface between mortar and aggregate is reported. Composite compact specimens were used for applying Mode I and Mode 11 loading effects. The influence of the type of mortar and type of aggregate and its roughness on the bond strength of the interface has been studied. It has been observed that the bond strength of the interface in tension is significantly low, though the mortars exhibited higher strength. The highest tensile bond strength values have been observed with rough concrete surface with M-13 mortar. The bond strength of the interface in Mode I load depends on the type of aggregate surface and its roughness, and the type of mortar, The bond strength of the interface between mortar M-13 cast against rough concrete in direct tension seems to be about one third of the strength of the mortar. However, it is about 1/20th to 1/10th with the mortar M-12 in sandwiched composite specimens. The bond strength of the interface in shear (Mode IT) significantly increases as the roughness and the phase angle of the aggregate surface increase. The strength of mortar on the interface bond strength has been very significant. The sandwiched composite specimens show relatively low bond strength in Mode I loading. The behavior of the interface in both Mode I and Mode 11 loading effects has been brittle, indicating catastrophic failure. (C) 2002 Elsevier Science Ltd. All rights reserved.