1000 resultados para Different EPM
Resumo:
We have studied the effect of the post-growth rapid thermal annealing on optical and electrical properties of InAs/InAlAs/InP quantum wires with various InAs deposited thickness. Quite different annealing behaviors in photoluminescence and dark resistance are observed, which can be attributed to dislocations in samples. After annealing at 800 degrees C, quantum wires still exist in the sample with two monolayer InAs deposited thickness, but the temperature-dependent PL properties are changed greatly due to the intermixing of In/Al atoms. (c) 2005 Elsevier B.V. All rights reserved.
Resumo:
We present a comparative study of InAs quantum dots grown on Si-doped GaAs (10 0) substrates, Si-doped GaAs (10 0) vicinal substrates, and semi-insulating GaAs (10 0) substrates. The density and size distribution of quantum dots varied greatly with the different substrates used. While dots on exact substrates showed only one dominant size, a clear bimodal size distribution of the InAs quantum dots was observed on GaAs vicinal substrates, which is attributed to the reduced surface diffusion due to the presence of multiatomic steps. The emission wavelength is blueshifted during the growth of GaAs cap layer with a significant narrowing of FWHM. We found that the blueshift is smaller for QDs grown on GaAs (10 0) vicinal substrates than that for dots on exact GaAs (100) substrates. This is attributed to the energy barrier formed at the multiatomic step kinks which prohibits the migration of In adatoms during the early stage of cap layer growth. (c) 2005 Elsevier B.V. All rights reserved.
Resumo:
The PL spectra for the 10, 4. 5, 3. 5, 3, 1 nm sized ZnS:Mn2+ nanoparticles and corresponding bulk material under different pressures were investigated. The orange emission band originated from the T-4(1)-(6)A(1) transition of Mn2+ ions showed obvious red shift with the increasing of pressures. The pressure coefficients of Mn-related emissions measured from bulk, 10, 4. 5, 3.5 and 3 nm samples are -29.4 +/- 0.3, -30.1 +/- 0.3, -33.3 +/- 0.6, -34.6 +/- 0.8 and -39 +/- 1 meV/GPa, respectively. The absolute value of the pressure coefficient increases with the decrease of the size of particles. The size dependence of crystal field strength Dq and Racah parameter B accounts for the size behavior of the Mn-related emission in ZnS:Mn nanoparticles. The pressure behavior of Mn-related emission in the 1 nm sized sample is somewhat different from that of other nanoparticles. It may be due to smaller size of 1 nm sample and the special surface condition since ZnS nanoparticles are formed in the cavities of ziolite-Y for the 1 nm sample.
Resumo:
InGaN/GaN quantum dots were grown on the sapphire (0 0 0 1) substrate in a metalorganic chemical vapor deposition system. The morphologies of QDs deposited on different modified underlayer (GaN) surfaces, including naturally as grown, Ga-mediated, In-mediated, and air-passivated ones, were investigated by atomic force microscopy (AFM). Photo luminescence (PL) method is used to evaluate optical properties. It is shown that InGaN QDs can form directly on the natural GaN layer. However, both the size and distribution show obvious inhomogeneities. Such a heavy fluctuation in size leads to double peaks for QDs with short growth time, and broad peaks for QDs with long growth time in their low-temperature PL spectra. QDs grown on the Ga-mediated GaN underlayer tends to coalesce. Distinct transform takes place from 3D to 2D growth on the In-mediated ones, and thus the formation of QDs is prohibited. Those results clarify Ga and In's surfactant behavior. When the GaN underlayer is passivated in the air, and together with an additional low-temperature-grown seeding layer, however, the island growth mode is enhanced. Subsequently, grown InGaN QDs are characterized by a relatively high density and an improved Gaussian-like distribution in size. Short surface diffusion length at low growth temperature accounts for that result. It is concluded that reduced temperature favors QD's 3D growth and surface passivation can provide another promising way to obtain high-density QDs that especially suits MOCVD system. (c) 2004 Elsevier Ltd. All rights reserved.
Resumo:
The photocurrent curves of reflection-mode GaAs photocathodes as a function of time, when were illuminated by white light with an intensity of 0, 33 and 100 Ix, respectively, were measured using a multi-information measurement system. The calculated lifetimes of cathodes are 320, 160 and 75 min, respectively, showing that the stability of cathodes degraded with the increase of light intensity. The lifetime of cathode, illuminated by white light with an intensity of 100 Ix, while no photocurrent was being drawn during the illumination, was 100 min. Through comparison, we found that the influence of illumination on cathodes stability is greater than that of photocurrent. The quantum-yield curves of cathodes as a functions of time, when illuminated by white light with an intensity of 33 Ix, were measured also. The measured results show that the shape of the yield curves changes with increasing illumination time due to the faster quantum-yield degradation rate of low energy photons. Based on the revised quantum-efficiency equations for the reflection-mode cathodes, the variation of yield curves are analyzed to be due to the intervalley diffusion of photoelectrons and the evolution of the surface potential barrier profile of the photocathodes during degradation process.
Resumo:
Magnetotransport properties of In-0.53 GaAs/In-0.52 AlAs high electron mobility transistor (HEMT) structures with different channel thickness of 10-35 nm have been investigated in magnetic fields up to 13 T at 1.4 K. Fast Fourier transform has been employed to obtain the subband density and mobility of the two-dimensional electron gas in these HEMT structures. We found that the thickness of channel does not significantly enhance the electron density of the two-dimensional electron gas, however, it has strong effect on the proportion of electrons inhabited in different subbands. When the size of channel is 20 nm, the number of electrons occupying the excited subband, which have higher mobility, reaches the maximum. The experimental values obtained in this work are useful for the design and optimization of InGaAs/InAlAs HEMT devices.
Resumo:
Straight single-line defect optical waveguides in photonic crystal slabs are designed by the plane wave expansion method and fabricated into silicon-on-insulator (SOI) wafer by 248-nm deep UV lithography. We present an efficient way to measure the light transmission spectrum of the photonic crystal waveguide (PhC WG) at given polarization states. By employing the Mueller/Stokes method, we measure and analyse the light propagation properties of the PhC WG at different polarized states. It is shown that experimental results are in agreement with the simulation results of the three-dimensional finite-difference-time-domain method.
Resumo:
We have performed a narrow stripe selective growth of oxide-free A1GaInAs waveguides on InP substrates patterned with pairs of SiO2 mask stripes under optimized growth conditions. The mask stripe width varied from 0 to 40 mu m, while the window region width between a pair of mask stripes was fixed at 1.5, 2.5 or 3.5 mu m. Flat and smooth A1GaInAs waveguides covered by specific InP layers are successfully grown on substrates patterned with different mask designs. The thickness enhancement ratio and the photoluminescence (PL) spectrum of the A1GaInAs narrow stripe waveguides are strongly dependent on the mask stripe width and the window region width. In particular, a large PL wavelength shift of 79 nm and a PL FWHM of less than 64 meV are obtained simultaneously with a small mask stripe width varying from 0 to 40 mu m when the window region width is 1.5 mu m. We present some possible interpretations of the experimental observations in considering both the migration effect from a masked region and the lateral vapour diffusion effect.
Resumo:
The band structures of wurtzite ZnO are calculated using the empirical pseudopotential method (EPM). The 8 parameters of the Zn and O atom pesudopotential form factors with Schluter's formula are obtained. The effective mass parameters are extracted by using k.p Hamiltonian to fit the EPM results. The calculated band edge energies (E-g, E-A, E-B, and E-C) at Gamma point are in good agreement with experimental results. The ordering of ZnO at the top of valence band is found to be A(Gamma(7))-B(Gamma(9))-C(Gamma(7)) due to a negative spin-orbit (SO) splitting. Based on the band parameters obtained, the valence hole subbands of wurzite ZnO/MgxZn1-xO tensile-strained quantum wells (QWs) with different well widths and Mg compositions are calculated using 6-band k.p method. (c) 2005 Elsevier B.V. All rights reserved.
Resumo:
We report on the photoluminescence (PL) properties of InAs/InAlAs/InP quantum wires (QWRs) with various InAs deposited thickness. The PL linewidth of the QWRs decreases with increasing InAs deposited thickness due to the different thicknesses of the QWRs and defects in the samples. The defects and lateral composition modulation of the InAlAs layers play an important role in the temperature-dependent PL properties of the samples. (c) 2005 Elsevier B.V. All rights reserved.
Resumo:
InAs quantum dots have been grown by solid source molecular beam epitaxy on different matrix to investigate the effect on the structure and optical properties. High density of 1.02 x 10(11) cm(-2) of InAs islands on In0.15Ga0.85As and In0.15Al0.85As underlying layer has been achieved. Atomic force microscopy and photoluminescence spectra show the size evolution of InAs islands on In0.15Ga0.85As underlying layer. A strong 1.3 mum photoluminescence from InAs islands on In0.15Ga0.85As underlying layer and with InGaAs strain-reduced layer has been obtained. Single-mirror light emitting diode structures with InAs quantum dots capped by InGaAs grown on InGaAs layer as active layer were fabricated and the corresponding radiative efficiency was deduced to be as high as 20.5%. Our results provide important information for optimizing the epitaxial structures of 1.3 mum wavelength quantum dots devices. (C) 2003 Elsevier B.V. All rights reserved.
Resumo:
Based on the band-anticrossing model, the effect of the strain-compensated layer and the strain-mediated layer on the band structure, the gain, and the differential gain of GaInNAs-GaAs quantum well lasers have been investigated. Different band-filling mechanisms have been illustrated. Compared to the GaInNAs-GaAs single quantum well with the same wavelength,, the introduction. (if the strain-compensated layer and the strain-mediated layer increases the transparency carrier density. However, these multilayer structures help to suppress the degradation of the differential gain.
Resumo:
We have investigated the effect of different cap layers on the photoluminescence (PL) of self-assembled InAs/GaAs quantum dots (QDs). Based upon different cap layers, the wavelength of InAs QDs can be tuned to the range from 1.3 to 1.5 mum. An InAlAs and InGaAs combination layer can enlarge the energy separation between the ground and first excited radiative transition. GaAs/InAs short period superlattices (SLs) make the emission wavelength shift to 1.53 mum. The PL intensity of InAs QDs capped with GaAs/InAs SLs shows an anomalous increase with increasing temperature. We attribute this to the transfer of carriers between different QDs.
Resumo:
Based on the band anticrossing model, the effects of the strain-compensated layer and the strain-mediated layer on the band structure, gain and differential gain of GaInNAs/GaAs quantum well lasers have been investigated. The results show that the GaNAs barrier has a disadvantage in increasing the density of states in the conduction band. Meanwhile, the multilayer quantum wells need higher transparency carrier density than the GaInNAs/GaAs single quantum well with the same wavelength. However, they help to suppress the degradation of the differential gain. The calculation also shows that from the viewpoint of band structure, the strain-compensated structure and the strain-mediated structure have similar features.
Resumo:
The structure and optical properties of In(Ga)As grown with the introduction of InGaAlAs or InAlAs seed dots layers are investigated. The area density and size homogeneity of the upper InGaAs dots are efficiently improved with the introduction of a layer of high-density buried dots. When the GaAs spacer layer is too thin to cover the seed dots, the upper dots exhibit the characterization of a quantum well. By analyzing the growth dynamics, we refer to it as an empty-core structure dot. (C) 2002 Elsevier Science B.V. All rights reserved.