930 resultados para Cement composites. Waste tire rubber. Limestone gravel. Deformation
Resumo:
The management of municipal solid waste has become an acute problem due to enhanced economic activities and rapid urbanisation. Increased attention has been given by the government in recent years to handle this problem in a safe and hygienic manner. In this regard, Municipal Solid Waste Management (MSWM) environmental audit has been carried out for Bangalore city through the collection of secondary data from government agencies, and interviews with stakeholders and field surveys. Field surveys were carried out in seven wards (representative samples of the city) to understand the practice and identify the lacunae. The MSWM audit that was carried out functional-element-wise in selected wards to understand the efficacy and shortfalls, if any, is discussed in this paper.
Resumo:
The Indian Ocean earthquake of 26 December 2004 led to significant ground deformation in the Andaman and Nicobar region, accounting for ~800 km of the rupture. Part of this article deals with coseismic changes along these islands, observable from coastal morphology, biological indicators, and Global Positioning System (GPS) data. Our studies indicate that the islands south of 10° N latitude coseismically subsided by 1–1.5 m, both on their eastern and western margins, whereas those to the north showed a mixed response. The western margin of the Middle Andaman emerged by >1 m, and the eastern margin submerged by the same amount. In the North Andaman, both western and eastern margins emerged by >1 m. We also assess the pattern of long-term deformation (uplift/subsidence) and attempt to reconstruct earthquake/tsunami history, with the available data. Geological evidence for past submergence includes dead mangrove vegetation dating to 740 ± 100 yr B.P., near Port Blair and peat layers at 2–4 m and 10–15 m depths observed in core samples from nearby locations. Preliminary paleoseismological/tsunami evidence from the Andaman and Nicobar region and from the east coast of India, suggest at least one predecessor for the 2004 earthquake 900–1000 years ago. The history of earthquakes, although incomplete at this stage, seems to imply that the 2004-type earthquakes are infrequent and follow variable intervals
Resumo:
The role of homogeneity in ex situ grown conductive coatings and dimensionality in the lithium storage properties of TiO(2) is discussed here. TiO(2) nanotube and nanosheet comprising of mixed crystallographic phases of anatase and TiO(2) (B) have been synthesized by an optimized hydrothermal method. Surface modifications of TiO(2) nanotube are realized via coating the nanotube with Ag nanoparticles and amorphous carbon. The first discharge cycle capacity (at current rate = 10 mA g(-1)) for TiO(2) nanotube and nanosheet were 355 mAh g(-1) and 225 mAhg(-1), respectively. The conductive surface coating stabilized the titania crystallographic structure during lithium insertion-deinsertion processes via reduction in the accessibility of lithium ions to the trapping sites. The irreversible capacity is beneficially minimized from 110 mAh g(-1) for TiO(2) nanotubes to 96 mAh g(-1) and 57 mAhg(-1) respectively for Ag and carbon modified TiO(2) nanotubes. The homogeneously coated amorphous carbon over TiO(2) renders better lithium battery performance than randomly distributed Ag nanoparticles coated TiO(2) due to efficient hopping of electrons. (C) 2011 Elsevier B.V. All rights reserved.
Resumo:
The properties of widely used Ni-Ti-based shape memory alloys (SMAs) are highly sensitive to the underlying microstructure. Hence, controlling the evolution of microstructure during high-temperature deformation becomes important. In this article, the ``processing maps'' approach is utilized to identify the combination of temperature and strain rate for thermomechanical processing of a Ni(42)Ti(50)Cu(8) SMA. Uniaxial compression experiments were conducted in the temperature range of 800-1050 degrees C and at strain rate range of 10(-3) and 10(2) s(-1). Two-dimensional power dissipation efficiency and instability maps have been generated and various deformation mechanisms, which operate in different temperature and strain rate regimes, were identified with the aid of the maps and complementary microstructural analysis of the deformed specimens. Results show that the safe window for industrial processing of this alloy is in the range of 800-850 degrees C and at 0.1 s(-1), which leads to grain refinement and strain-free grains. Regions of the instability were identified, which result in strained microstructure, which in turn can affect the performance of the SMA.