Resumo:
Isothermal melt and cold crystallization kinetics of PEDEKmK linked by meta-phenyl and biphenyl were investigated by differential scanning calorimetry in two temperature regions. Avrami analysis is used to describe the primary stages of the melt and cold crystallization, with exponent n = 2 and n = 4, respectively. The activation energies are -118 kJ/mol and 510 kJ/mol for crystallization from the melt and the glassy states, respectively. The equilibrium melting point T-m(0) is estimated to be 309 degrees C by using the Hoffman-Weeks approach, which compares favorably with determination from the Thomson-Gibbs method. The lateral and end surface free energies derived from the Lauritzen-Hoffman spherulitic growth rate equation are sigma = 8.45 erg/cm(2) and sigma(e) = 45.17 erg/cm(2), respectively. The work of chain folding q is determined as 3.06 kcal/mol. These observed crystallization characteristics of PEDEKmK are compared with those of the other members of poly(aryl ether ketone) family. (C) 1997 John Wiley & Sons, Inc.
Resumo:
The modification of ethylene-propylene copolymer (EPM) has been accomplished by melt grafting of maleic anhydride (MAH) molecules promoted by radical initiators. The resulting EPM-g-MAH and EPM have been used to obtain binary nylon 1010/EPM or nylon 1010/EPM-g-MAH blends by melt mixing. It was found that the EPM-g-MAH copolymer used as the second component has a profound effect upon the properties of the resulting blends. This behavior has been attributed to a series of chemical and physicochemical interactions taking place between the two components. The interactions are due to the presence of the anhydride functionality on the copolymer and do not occur when this functionality is absent. The interaction has been confirmed by Fourier-transform infrared spectroscopy, differential scanning calorimetry, dynamic mechanical analysis, and scanning electron microscopic.
Resumo:
In this paper, unepoxidized ethylene propylene diene rubber (uEPDM) was first epoxidized with formic acid and H2O2, and then the epoxidized ethylene propylene diene rubber (eEPDM) was melt-mixed with PET resin in a Brabender-like apparatus. Toughening of PET matrix was achieved by this method. The dispersion of rubber particles and phase structure of the blends were also observed by SEM. It has been suggested that the epoxy groups in the eEPDM could react with PET end groups to form a graft copolymer which could act as an interfacial compatibilizer between the PBT matrix and eEPDM rubber dispersed phase. This is beneficial to the improvement of the impact performance of PBT. (C) 1997 Elsevier Science Ltd.
Resumo:
The crystallization and unusual crystalline morphologies of compatible mixtures of tetrahydrofuran-methyl methacrylate diblock copolymer with tetrahydrofuran homopolymer were studied. It is shown that the PTHF [poly(tetrahydrofuran)] block of the copolymer cocrystalizes with the PTHF homopolymer in the PTHF microphase of the blend. However, the degree of crystallinity of the PTHF block is always lower than that of the PTHF homopolymer in the PTHF microphase. The crystallizability of the PTHF microphase increases appreciably with increasing PTHF microphase size and PTHF homopolymer weight fraction in the microphase. The morphology study of the blends shows that the crystalline morphology is strongly dependent on blend composition, copolymer composition and PTHF block length, as well as crystallization temperature. When alternating PTHF and PMMA [poly(methyl methacrylate)] lamellae are formed, the macroscopic crystalline morphology could be only observed when the thickness of the PTHF lamellae is large enough (similar to 20 nm). In the blend where PMMA spherical or cylindrical microphases are formed, the crystalline morphology changes dramatically with the change in the PTHF microdomain size and PMMA interdomain distance. Many unusual crystalline morphologies have been observed. A study of the solution-crystallized morphology of the blends at different temperatures shows that the morphology is also strongly dependent on the isothermal crystallization temperature, suggesting that the PMMA microdomains may have different effects on the morphology formation when the blend is crystallized at different rates.
Resumo:
This work deals with the effect of compatibilizer on the morphological, thermal, rheological, and mechanical properties of polypropylene/polycarbonate (PP/ PC) blends. The blends, containing between 0 to 30 vol % of polycarbonate and a compatibilizer, were prepared by means of a twin-screw extruder. The compatibilizer was produced by grafting glycidyl methacrylate (GMA) onto polypropylene in the molten state. Blend morphologies were controlled by adding PP-g-GMA as compatibilizer during melt processing, thus changing dispersion and interfacial adhesion of the polycarbonate phase. With PP-g-GMA, volume fractions increased from 2.5 to 20, and much finer dispersions of discrete polycarbonate phase with average domain sizes decreased from 35 to 3 mu m were obtained. The WAXD spectra showed that the crystal structure of neat PP was different from that in blends. The DSC results suggested that the degree of crystallization of PP in blends decreased as PC content and compatibilizer increased. The mechanical properties significantly changed after addition of PP-g-GMA. (C) 1997 John Wiley & Sons, Inc.
Resumo:
The microphase transition in a styrene-butadiene-styrene triblock copolymer was studied by rheometric mechanical spectroscopy. A high-temperature-melt rheological transition from the highly elastic, nonlinear viscous behavior typical of a multiphase structure to linear viscous behavior with insignificant elasticity typical of a single-phase structure was observed. The transition temperature is determined according to the discontinuity of the rheological properties across the transition region, which agrees well with the results obtained from the small angle X-ray scattering data and the expectation of the random phase approximation theory. Maybe for the first time, microphase dissolution was investigated theologically. The storage modulus (G') and the loss modulus (G '') increase with time during the process. An entanglement fluctuation model based on the segmental density fluctuations is presented to explain the rheological behavior in this dissolution process. (C) 1997 John Wiley & Sons.
Resumo:
Interpenetrating polymer networks (IPNs) have been synthesized from prepolymers that form miscible blends. All IPNs made from polyacrylate ((polyethylene glycol diacrylate), PEGDA) and epoxy (diglycidyl ether of bisphenol A, DGEBA) can be made in phase separated states by incorporating crosslinks. However, blends of these prepolymers, having a negative Flory-Huggins interaction parameter, are highly miscible. This indicates that formation of IPNs favours phase separation relative to blends. The microphase separation characteristics in the PEGDA/DGEBA IPNs were determined using smalt-angle X-ray scattering (SAXS). The Debye-Bueche and Guinier methods were used to calculate the correlation lengths of the segregated phases existing in the PEGDA/DGEBA IPNs. The results from SAXS showed that the size of the phase segregation zones changed with composition from about 50 to 100 Angstrom.
Resumo:
Bright blue polymer light-emitting diodes have been fabricated by using the poly(p-phenylenevinylene)-based copolymers with 10 C long aliphatic chains as the electroluminescent layers, PBD in PMMA and Alq(3) as the electron-transporting layers, and aluminum as the cathode. The multilayer structure devices show 190 cd/m(2) light-emitting brightness at 460 nm, 15 V turn-on vol- tage. It is found that the intensities of photoluminescence and electroluminescence (EL) increase with increasing aliphatic chain length, the EL intensity and operation stability of these polymer light-emitting diodes can be improved by reasonable design of the structure.
Resumo:
The structural parameters of the aggregated state of polyamide (PA)-1010 annealed at various temperatures were computed by means of the desmearing intensity from Smalt Angle X-ray Scattering (SAXS) measurements and by using the concept of the distance distribution function. The results indicated that the structural parameters of the aggregated state were strongly dependent upon heat treatment conditions and the maximum values of the structural parameters were obtained for the samples annealed at T = 175 degrees C. The particle size Z annealed at different temperature was ranged between 8.1-12.8nm, and the values of the distance distribution function P-max(Z) were obtained when Z = 4.0-6.8 nm. Using one dimension electron density correlation function (1D EDCF) method long period (L) and thickness of the lamellar (d(0)) were estimated and were found to increase with the increase of the degree of crystallinity.
Resumo:
Blends of poly (butylene terephthalate) (PBT) and epoxided ethylene-propylene-diene terpolymer (EEPDM) were prepared. Their mechanical properties and morphology were studied by Izod impact test machine and scanning electronic microscope respectively, It was found that the notched Izod impact strength of blend PBT/EEPDM was as about 23 times as that of pure PET and about 10 times as that of blend PBT/EPDM at room temperature, The dispersed rubber particles were much smaller and the phase boundary was more blurred in blend PBT/EEPDM than in blend PBT/EPDM. The toughness of blend PBT/EEPDM was much more better than that of blend PET and PBT/EPDM, which was in good agreement with the difference between their morphologies.
Resumo:
The thermal properties of ethylene-propylene copolymer grafted with glycidyl methacrylate (EP-g-GMA) were investigated by using differential scanning calorimetry (DSC). Compared to the plain ethylene-propylene copolymer (EP), peak values of melting temperature (T-m) of the propylene sequences in the grafted EP changed a little, crystallization temperature (T-c) increased about 8-12 degrees C, and melting enthalpy (Delta H-m) increased about 4-6 J/g. The isothermal and nonisothermal crystallization kinetics of grafted and ungrafted samples was carried out by DSC. Within the scope of the researched crystallization temperature, the Avrami exponent (n) of ungrafted sample is 1.6-1.8, and those of grafted samples are all above 2. The crystallization rates of propylene sequence in EP-g-GMA were faster than that in the plain EP and increased with increasing of grafted monomer content. It might be attributed to the results of rapid nucleation rate. (C) 1996 John Wiley & Sons, Inc.
Resumo:
The crystallization and melting behaviours of a multiblock copolymer comprising poly(ether ether ketone) (PEEK) and poly(ether sulfone) (PES) blocks whose number average molecular weights <((M)over bar (n)'s)> were 10 000 and 2900, respectively, were studied. The effect of thermal history on crystallization was investigated by wide-angle X-ray diffraction measurement. A differential scanning calorimeter was used to detect the thermal transitions and to monitor the energy evolved during the isothermal crystallization process from the melt. The results suggest that the crystallization of the copolymer becomes more difficult as compared with that of pure PEEK. The equilibrium melting point of the copolymer was found to be 357 degrees C, about 30 degrees C lower than that of pure PEEK. During the isothermal crystallization, relative crystallinity increased with crystallization time, following an Avrami equation with exponent n approximate to 2. The fold surface free energy for the copolymer crystallized from the melt was calculated to be 73 erg cm(-2), about 24 erg cm(-2) higher than that of pure PEEK. Copyright (C) 1996 Elsevier Science Ltd.
Resumo:
A new class of liquid crystalline poly(ester-imide)s was synthesized by melt polycondensation. The basic physical properties of the resulting polymers were investigated by differential scanning calorimetry (d.s.c.), wide-angle X-ray diffraction (WAXD), polarized light microscopy, scanning electron microscopy (SEM), thermogravimetric analysis (t.g.a.), and rheological and mechanical testing. All of these poly(ester-imide)s were amorphous, as reflected by the results obtained from the WAXD and d.s.c. studies. Characterization and comparison of these poly(ester-imide)s with the corresponding polyesters suggested that the introduction of imide groups into the polyester chain is favourable for the formation of liquid crystalline phases. These results, together with the rheological studies, suggested that there existed a form of strong inter- or intramolecular electron donor-acceptor interaction which played a significant role in the liquid crystalline properties of the poly(ester-imide)s. The polymer products thus obtained exhibited good mechanical properties, with flexural strengths and moduli as high as 174 MPa and 6.9 GPa, respectively. The morphology of the fracture surfaces of extruded rod samples showed a sheet-like structure which consisted of ribbons and fibres oriented along the flow direction. The glass transition temperatures and thermal stabilities of the polymers were improved by the incorporation of imide groups. Copyright (C) 1996 Elsevier Science Ltd.
Resumo:
Ethylene-propylene copolymer (EP) was functionalized with glycidyl methacrylate (GMA) by means of a radical-initiated melt grafting reaction. FTIR and ESCA were used to characterize the formation of EP-g-GMA copolymers. The content of GMA in EP-g-GMA was determined by using hydrochloric acid/xylene titration. Effects of concentrations of GMA and dicumyl peroxide on grafting rate were studied. It was found that contact angles of the water on surfaces of EP-g-GMA samples increased with increasing content of GMA in EP-g-GMA. The influence of the content of GMA on the crystallization structure of EP-g-GMA was investigated by DSC and WAXD. Compared with the plain EP, the crystallization temperature of propylene blocks of EP-g-GMA increased over 10 K, and the melting temperature and crystallinity decreased somewhat. Functionalization of EP led to the change of the crystal form of propylene blocks from the mixed form of alpha and beta into the alpha form. (C) 1996 John Wiley & Sons, Inc.
Resumo:
The microphase separation, glass transition and crystallization of two series of tetrahydrofuran-methyl methacrylate diblock copolymers (PTHF-b-PMMA), one with a given PTHF block of M(n) = 5100 and the other with a given PTHF block of (M) over bar(n) = 7000, were studied in this present work. In the case of solution-cast materials, the microphase separation of the copolymer takes place first, with crystallization then gradually starting in the formed PTHF microphase. The T-g of the PMMA microphase shows a strong dependence on the molecular weight of the PMMA block, while the T-g of the PTHF microphase shows a strong dependence on the copolymer composition. The non-isothermal crystallization temperature (T-c) of the diblock copolymer decreases rapidly and continuously with the increase in the amorphous PMMA weight fraction; the lowest T-c of the copolymer is ca. 35 K lower than the T-c of the PTHF homopolymer. There also exists a T-c dependence on the molecular weight of the PTHF block. In addition, when the major component of the copolymer is PMMA, a strong dependence of the crystallizability of the copolymer on the molecular weight of the PTHF block is observed; the higher the molecular weight, then the stronger its crystallizability. The melting temperature of the block copolymer is dependent on the copolymer composition and the molecular weight of its crystallizable block. Copyright (C) 1996 Elsevier Science Ltd.