979 resultados para structural and optical characteristics
Resumo:
The functional polystyrene, (Cl-PS)(2)-CHCOOCH2CH2OH ( designated as XPSt and coded P2) was prepared by ATRP at 130(0)C using CuCl and bipyridine as catalysts, 2,2-dichloro acetate-ethylene glycol (DCAG) as multifunctional initiator and THF as solvent. 4-Nitoroaniline azomethine-4' phenol (P1) as chromophores were covalently linked to the functional end groups of the polymer by using simple displacement reaction. The functional polystyrenes, namely XPSt (P2) and (PS)(2)-CHCOOCH2CH2OH, designated as X-PSt and coded P3 and their post-derivatives, namely, DXPSt (P4) and DX-PSt (P5) respectively were characterized by IR, NMR and UV spectroscopies, gel permeation chromatography (GPC) and thermogravimetric analysis (TGA) and differential scanning calorimetry (DSC), polarising optical microscopy (POM) and XRD studies. DSC showed that incorporation of chromophores in the side chains of polymers towards the polystyrene moiety increases the rigidity of the polymer and subsequently, its glass transition temperature; however the incorporation of side chain towards the alcoholic functional group decreases the glass transition temperature. The post derivatives do not play any significant role to increase the thermal stability ( TGA).
Resumo:
The structures and the electrochemical characteristics of La0.7-xCexMg0.3Ni2.8Co0.5 (x = 0.1-0.5) alloy, Ti0.25-xZrxV0.35Cr0.1Ni0.3 (x = 0.05-0.15) alloy and AB(3
Resumo:
Rhodamine B (RB)-doped organic-inorganic silica films and their patterning were fabricated by a sol-gel process combined with a soft lithography. The resulted film samples were characterized by atomic force microscope (AFM), optical microscope and UV/Vis absorption and photoluminescence excitation and emission spectra. The effects of the concentration of the RB dye and heat treatment temperature on the optical properties of the hybrid silica films have been studied. Four kinds of patterning structures with film line widths of 5, 10, 20 and 50 mum have been obtained by micromolding in capillaries by a soft lithography technique. The RB-doped hybrid silica films present a red color, with an excitation and emission bands around 564 and 585 mum, respectively. With increasing the RB concentration, the emission intensity of the RB-doped hybrid silica films increases and the emission maximum presents a red shift. The emission intensity of the films decreases with increasing the heat treatment temperatures.
Resumo:
The complex fluoride LiBaF3 and LiBaF3:M(M = Eu, Ce) is solvothermally synthesized at 180 degreesC and characterized by means of X-ray powder diffraction, scanning electron microscopy, thermogravimetric analysis and infrared spectroscopy. In the solvothermal process, the solvents, molar ratios of initial mixtures and reaction temperature play important roles in the formation of products. The excitation and emission spectra of the LiBaF3:M(M= Eu,Ce) have been measured by fluorescence spectrophotometer. In the LiBaF3: Eu emission spectra, there is one sharp line emission located at 360 nm arising from f --> f transition of Eu2+ in the host lattice, and typical doublet 5d-4f emission of Ce3+ in LiBaF3 powder is shown.
Resumo:
Nanocrystalline YVO4:A (A = Eu3+, Dy3+, Sm3+, Er3+) phosphor films and their patterning were fabricated by a Pechini sol-gel process combined with soft lithography. X-ray diffraction (XRD), Fourier transform infrared spectroscopy (FT-IR), thermogravimetric and differential thermal analysis (TG-DTA), atomic force microscopy (AFM) and optical microscopy, UV/vis transmission and absorption spectra, photoluminescence (PL) spectra, and lifetimes were used to characterize the resulting films. The results of XRD indicated that the films began to crystallize at 400 degreesC and the crystallinity increased with the increase of annealing temperatures. Transparent nonpatterned phosphor films were uniform and crack-free, which mainly consisted of grains with an average size of 90 nm. Patterned gel and crystalline phosphor film bands with different widths (5-60 mum) were obtained. Significant shrinkage and a few defects were observed in the patterned films during the heat treatment process. The doped rare earth ions (A) showed their characteristic emission in crystalline YVO4 phosphor films because of an efficient energy transfer from vanadate groups to them. The Sm3+ and Er3+ ions also showed upconversion luminescence in a YVO4 film host. Both the lifetimes and PL intensity of the rare earth ions increased with increasing annealing temperature from 400 to 800 degreesC, and the optimum concentration for Eu3+ was determined to be 7 mol % and those for Dy3+, Sm3-, and Er3+ were 2 Mol % of Y3- in YVO4 films, respectively.
Resumo:
Four lanthanide complexes with 2-nitro-5,10,15,20-tetraphenylporphyrin and acetylacetonate were prepared and characterized by elemental analyses, LR, UV-Visible,H-1 NMR, XPS and molar conductance. The redox properties of the lutetium complex with 2-nitro-5,10,15,20-tetraphenylporphyrin and acetylacetonate in dichloromethane were studied by cyclic voltammetry.
Resumo:
KMgF3 doped with Eu was synthesized by mild hydrothermal method at 240 degreesC for the first time. The excitation and emission spectra of the KMgF3 : Eu2+ phosphor were measured. Comparing with the sample synthesized through solid state reaction, the variation in the excitation spectra at 360 nm resulted from the existences of V-K color centers; the low emission intensity was due to Eu2+ having transferred part energy to V-K color centers.
Resumo:
Binary and ternary europium complexes with dibenzplymethane (DBM) and 1,10-phenanthroline (phen) were synthesized and doped into a sol-gel luminescence thin film and polyvinylbutyral (PVB) film. The luminescent spectra and lifetime of the films were measured. The final results showed that Eu(III) characteristic emission bands were observed in the spectra of all the doped films. Longer lifetimes and a higher photo-stability were observed in SiO2:Eu(III) complex luminescent thin films than in PVB:Eu(III) complex films that contained a corresponding amount of pure complexes. Heat-stability tests showed that SiO2:Eu(III) complex thin films still showed certain fluorescence after heat-treatment at a temperature of 130 degreesC, while little fluorescence could be observed in PVB:Eu(III) complex films under a UV lamp. (C) 2001 Elsevier Science B.V. All rights reserved.
Resumo:
Crystallographic and magnetic properties of intermetallic compounds (PrxSm1-x) Mn2Si2 (x = 0 similar to 0.80) have been investigated by X-ray powder diffraction, XPS and magnetic measurements. All the compounds crystallize in ThCr2Si2-type structure. Substitution of Pr for Sm leads to the increase of the lattice constants and the transition from antiferromagnetism (AFM) to ferromagnetism (FM). The valence-fluctuation in the compounds was observed and the relation between the change of electron binding energy and magnetic properties was also discussed preliminarily.
Resumo:
Circular dichroism (CD), fourier transform infrared (FTIR), and fluorescence spectroscopy were used to explore the effect of dimethyl sulfoxide (DMSO) on the structure and function of hemoglobin (Hb). The native tertiary structure was disrupted completely when the concentration of DMSO reached 50% (v/v), which was determined by loss of the characteristic Soret CD spectrum. Loss of the native tertiary structure could be mainly caused by breaking the hydrogen bonds, between the heme propionate groups and nearby surface amino acid residues, and by disorganizing the hydrophobic interior of this protein. Upon exposure of Hb to 52% DMSO for ca. 12 h in a D2O medium no significant change in 1652 cm(-1) band of the FTIR spectrum was produced, which demonstrated that alpha-helical structure predominated. When the concentration of DMSO increased to 57%: (1) the band at 1652 cm(-1) disappeared with the appearance of two new bands located at 1661 and 1648 cm(-1); (2) another new band at 1623 cm(-1) was attributed to the formation of intermolecular beta-sheet or aggregation, which was the direct consequence of breaking of the polypeptide chain by the competition of S=O groups in DMSO with C=O groups in amide bonds. Further increasing the DMSO concentration to 80%, the intensity at 1623 cm(-1) increased, and the bands at 1684, 1661 and 1648 cm(-1) shifted to 1688, 1664 and 1644 cm(-1), respectively. These changes showed that the native secondary structure of Hb was last and led to further aggregation and increase of the content of 'free' amide C=O groups. In pure DMSO solvent, the major band at 1664 cm(-1) indicated that almost all of both the intermolecular beta-sheet and any residual secondary structure were completely disrupted. The red shift of the fluorescence emission maxima showed that the tryptophan residues were exposed to a greater hydrophilic environment as the DMSO content increased. GO-binding experiment suggested that the biological function of Hb was disrupted seriously even if the content of DMSO was 20%. (C) 1998 Elsevier Science B.V. All rights reserved.
Resumo:
An organo-soluble polyimide was successfully synthesized by two step polycondensation accompanied with chemical imidization. Optical anisotropy of thin films was detected by a prism-coupler technique. The results showed that the optical anisotropic properties of thin films prepared from solutions in different solvents depend on the solution properties. It is concluded that the more expanded the chain conformation in solution, the larger the negative birefringence of thin films. (C) 1997 Elsevier Science Ltd.
Resumo:
By solid state reaction, LiMgAlF6 and LiMgAlF6:Ln(3+) are synthetized with the ratio 120/100/110 of LiF/MgF2/AlF3, at 1008 K, in high-purity Ar stream. Their crystal structure which belongs to hexagonal system are determined by X-Ray-Diffraction (XRD). Luminescence characteristics of Ce3+, Eu3+, Tb3+ and sensitization of Ce3+ to Tb3+ in LiMgAlF6 are studied. It is shown that the sensitization of Ce3+ to Tb3+ is efficient and a bright green emission is observed.
Resumo:
A simple technique for preparation of powder binary fluorides activated with divalent samarium ions is described. The samarium impurity is introduced as samarium trifluoride SmF3 and hydrogen acts as the reducing agent to transform Sm3+ into Sm2+. Using this method, samarium has been stabilized in the divalent state in some fluorides: KMgF3, LiBaF3, BaBeF4, SrMgF4 and BaMgF4. Moreover, BaBeF4, SrMgF4 and BaMgF4 have never been activated with Sm2+ ions up to now. We also find that under the same synthetic conditions samarium can not be stabilized in the divalent state in some fluorides: KCaF3, CaBeF4 and CaMgF4, but the characteristic luminescence of trivalent samarium Sm3+ appears in these matrices. The emission and excitation spectra of samarium (Sm2+ and Sm3+) in these binary fluorides are presented and briefly discussed. The relationship between the oxidation state of samarium and the composition, the structure of matrices is also analyzed.
Resumo:
In most cases the luminescence of Eu~(2+) consists of a d-f broad-band emission, in some particular hosts, however, Eu~(2+) can also give out f-f narrow-line emission. There are two factors of importance here: the first is the strength of the crystal-field