Resumo:
Infrared (1.2-1.6 mu m) luminescence in a ytterbium aluminium garnet (YbAG) crystal, doped with Cr (0.05 at.%) ions, was investigated under CW laser diode pumping (lambda = 940 nm). The Cr4+ emission band was observed with its peak at 1.34 mu m and measured to be about 1.3 times with respect to Yb3+ IR luminescence (lambda = 1.03 mu m). We demonstrate that for the excitation wavelength of 940 nm Yb3+ ions act as sensitizers of the B-3(2)(T-3(2))-B-3(1)((3)A(2)) emission of Cr4+ ions. This crystal is promising as a high-efficient system for tunable laser (1.2-1.6 mu m) output. (c) 2004 Elsevier B.V. All rights reserved.
Resumo:
Visible upconversion luminescence was observed in Cr3+: Al2O3 crystal under focused femtosecond laser irradiation. The luminescence spectra show that the upconversion luminescence originates from the E-2-(4)A(2) transition of Cr3+. The dependence of the fluorescence intensity of Cr3+ on the pump power reveals that a two-photon absorption process dominates in the conversion of infrared radiation to the visible emission. It is suggested that the simultaneous absorption of two infrared photons produces the population of upper excited states, which leads to the characteristic visible emission from E-2 state of Cr3+.
Resumo:
Writing computer-generated holograms has been achieved by using near infrared femtosecond laser selective ablation of metal film deposited on glass substrate. The diffraction features with data reconstruction of fabricated computer-generated holograms were evaluated. Both transmission and reflection holograms can be fabricated in a single process. The process required no mask, no pre- or post-treatment of the substrate. (C) 2005 Optical Society of America.
Resumo:
Broadband infrared luminescence covering the optical telecommunication wavelength region of 0, E and S bands was observed in GeO2: Bi, M (M = Ga, B) glasses prepared by conventional melting-quenching technique. The luminescence with a maximum at around 1320 nm possesses a full width at half maximum larger than 300 nm and mean fluorescent lifetime longer than 500 mus when excited by an 808 nm-laser. These glasses may have potential applications in widely tunable laser and super-broadband optical amplifier for the optical communications. (C) 2005 Elsevier B.V. All rights reserved.
Resumo:
Near-infrared broadband emission from bismuth-tantalum-codoped germanium oxide glasses was observed at room temperature when the glasses were pumped by an 808 nm laser diode. The emission band covered the 0, E, S, C, and L bands (1260-1625 nm), with a maximum peak at similar to 1310 nm, a FWHM broader than 400 nm, and a lifetime longer than 200 lis. The observed broadband luminescence was attributed to bismuth clusters in the glasses. Bismuth-tantalum-codoped germanium oxide glass might be promising as amplification media for broadly tunable lasers and wideband amplifiers in optical communications. (c) 2005 Optical Society of America.
Resumo:
Blue frequency-upconversion fluorescence emission has been observed in Ce3+-doped Gd2SiO5 single crystals, pumped with 120-fs 800 nm IR laser pulses. The observed fluorescence emission peaks at about 440nm is due to 5d -> 4f transition of Ce3+ ions. The intensity dependence of the blue fluorescence emission on the IR excitation laser power obeys the cubic law, demonstrating three-photon absorption process. Analysis suggested that three-photon simultaneous absorption induced population inversion should be the predominant frequency upconversion mechanism. (c) 2006 Optical Society of America.
Resumo:
Broadband neat-infrared emission from transparent Ni2+-doped sodium aluminosilicate glass-cermaics is observed. The broad emission is centered at 1290 nm and covers the whole telecommunication wavelength region (1100-1700 nm) with full width at half maximum of about 340 nm. The observed infrared emission could be attributed to the T-3(2)(F) -> (3)A(2)(F) transition of octahedral Ni2+ ions that occupy high-field sites in nanocrystals. The product of the lifetime and the stimulated emission cross section is 2.15 x 10(-24) cm(2)s. It is suggested that Ni2+-doped sodium aluminosilicate glass ceramics have potential applications in tunable broadband light sources and broadband amplifiers.
Resumo:
在分析激光晶体的研究现状的基础上,指出其未来应用及主要发展趋势:面向先进制造技术、激光武器等应用的(1μm波段)高功率、大能量激光晶体;面向人眼安全、遥感、光通讯、医疗等应用的红外激光晶体;面向全色显示、光刻等应用的蓝绿紫和可见光激光晶体;LD泵浦超快激光增益和放大介质材料.
Resumo:
Absorption spectrum from 400 to 2000 run and upconversion fluorescence spectra under 940 nm pumping of YAG single crystal codoped with 5 at.% Yb3+ and 4 at.% Tm3+ were studied at room temperature. The blue upconversion emission centered at 483 nm corresponds to the transition (1)G(4) -> H-3(6), the emission band around 646 nm corresponds to the transition (1)G(4) -> F-3(4) of Tm3+. Energy transfer from Yb3+ to Tm3+ is mainly nonradiative and the transfer efficiency was experimentally assessed. The line strengths, transition probabilities and radiative lifetimes of (1)G(4) level were calculated by using Judd-Ofelt theory. Gain coefficient calculated from spectra shows that the upconversion corresponding with transitions (1)G(4) -> H-3(6) in YAG doped with Yb3+ and Tm3+ is potentially useful for blue light Output. (c) 2006 Elsevier B.V. All rights reserved.
Resumo:
We report both continuous-wave and passively mode-locked laser actions in a Yb3+-doped gadolinium yttrium oxyorthosilicate Yb:GdySiO(5) (Yb:GYSO) crystal. Continuous-wave (CW) laser operations were compared under different pump conditions with high-power diodes of different wavelengths and fiber cores. CW mode-locking was obtained with a semiconductor saturable absorber mirror.
Resumo:
An Ho3+-doped YAlO3 (Ho : YAP) single crystal has been grown by the Czochralski technique. The polarized absorption spectra, polarized fluorescence spectra and fluorescence decay curve of the crystal are measured at room temperature. The spectroscopic parameters are calculated based on Judd-Ofelt theory, and the effective phenomenological intensity parameters Omega(2,eff), Omega(4,eff) and Omega(6,eff) are obtained to be 2.89 x 10(-20), 2.92 x 10(-20) and 1.32 x 10(-20) cm(2), respectively. The room-temperature fluorescence lifetime of the Ho3+ 5I(7) -> I-5(8) transition is measured to be 8.1 ms. Values of the absorption and emission cross-sections with different polarizations are presented for the I-5(7) manifold, and the polarized gain cross-section curves are also provided and discussed.