964 resultados para Solid phase reaction
Resumo:
Compounds of Sr4Al14O15: Eu were prepared in air atmosphere by high temperature solid state reaction. The reduction of Eu3+--> Eu2+ was firstly observed in the aluminate phosphor of Sr4Al14O25: Eu synthesized in air condition. This made aluminate a new family and Sr4Al14O25 a new member of compounds in which Eu3+ ion could be reduced to Eu2+ form when fired in air atmosphere. The reduction of Eu3+ --> Eu2+ in Sr4Al14O25: Eu was explained by means of a charge compensation model. Experiments based on the model were designed and carried out, and the results supported this model.
Resumo:
In this paper for the first time the compounds Y0.5-xLi1.5VO4:(Dy3+, Eu3+),(YLV:Dy,Eu) (0.01
Resumo:
The VUV-UV spectra of rare earth ions activated calcium borophosphate, CaBPO5:RE (RE = Ce3+, sm(3+), Eu2+, Eu3+, Tb3+ and Dy3+) were determined. The bands at about 155 nm in the VUV excitation spectra are attributed to the host lattice absorptions. The bands at 166 and 190 nm for the sample CaBPO5:Sm have been considered as related to the f-d transition and the charge transfer band (CTB) of Sm3+ ions, and the band at 169 nm for the sample CaBPO5:Dy is assumed to be connected with the f-d transition of the Dy3+ ions in CaBPO5. The partial reduction of Eu3+ CaBPO5:Eu prepared by high temperature solid state reaction in air is confirmed by the VUV-UV spectra.
Resumo:
Sodium dodecyl sulfate(SDS) is a powerful solubilizing detergent which is often used during the separation of highly complex protein mixtures by one- or two-dimensional (2D) gel electrophoresis. Matrix-assisted laser desorption/ionization mass spectrometry (MALDI-MS) is a widely used technique for mass spectrometric analysis of some protein molecules compared to other techniques. But the presence of SDS or some salts usually leads to signal deterioration when using MALDI-MS. A method for using nitrocellulose membrane as the solid-phase carrier combined with n-octyl-beta-D-glucopyranoside in the matrix highly enhances the sensitivity of the molecular mass determination of lysozyme. This technique has the advantage that the signal-to-noise of the molecular weight profile is improved compared with the mass spectrum and the profile is relatively easy to interpret.
Resumo:
The high-resolution luminescent spectrum of divalent samarium excited by 355 nm UV light at 77 K, the VUV excitation spectra, the VUV excited emission spectra and EXAFS at Sm-L-3 edge were reported for samarium doped strontium borophosphate, SrBPO5:Sm prepared by solid state reaction in air at high temperature. The high-resolution luminescent spectrum showed that the divalent samarium ions occupied the C-2upsilon lattice sites. The VUV excitation spectra indicated that the sample exhibited absorption bands with the maxima at 129 and 148 nm, respectively. The performance of EXAFS at Sm-L3 absorption edge suggested that the samarium ions were nine-coordinated and the mean distances of bond Sm-O were 2.38 Angstrom.
Resumo:
In this paper, we report on a solid phase time-resolved fluorescence immunoassay chelate reagent-4,7-bis(chlorosulfophenyl)1, 10-phenanthroline-2,9-dicarboxylic acid (BCPDA), which is suitable as a fluorescent labeling agent. The five step synthesis product of BCPDA was presented for improving the purity of the product based on the three step synthesis product. The approach involves chlorization, hydrolyzing the ester, preparing disodium, carboxylate to diacid, sulfonation. The yield of five step product is 99 %, 45 %, 94 %, 95 %, 80 % respectively. The structure and purity of product was characterized by the melting point, IR,H-1 NMR, UV spectrum, element analysis, and proved to be consistent with the structure predictal.
Resumo:
VUV-UV and Eu-L-3 edge XANES spectra were measured for europium-doped strontium tetraborate prepared by solid state reaction at high temperature in air. The VUV-UV spectra show that the host absorption band of (SrBO7)-O-4 appears below 170 nm. The charge transfer band of Eu3+ doped in SrB4O7 is peaked at 272 nm. The 4f-5d transitions of Eu2+ consist of a band peaked at 310 nm with a shoulder at 280 nm and also include the bands peaked at 238 (weak) and 203 (strong) nm. The result of XANES spectrum at Eu-L3 edge of the synthesized sample indicates that Eu3+ and Eu2+ coexist in SrB4O7:Eu prepared in air, which is consistent with the results of the VUV-UV spectra.
Resumo:
The (Y, Gd) BO3 : Eu phosphor was synthesized by solid-state reaction, The UV spectra showed that in a certain range of Gd3+ concentration, more Gd3+ absorbed energy and transferred it to Eu3+ with its increasing concentration. From the spectra in VUV region, it was observed that both the doping and the concentrations of Gd3+, Eu3+ greatly affected the absorption of the host lattice. The absorbances at 147 nm and 170 nm increased when the Gd3+ was doped which can be explained as that Gd3+ transferred energy to BO4. The optical properties of (Y, Gd)BO3 : Eu were the best when the concentration of Eu3+ was about 0.04.
Resumo:
CaY1-xBO4: xEu was synthesied by solid state reaction method, and the displacement and luminescence of the Eu3+ in CaYBO4 host were studied. Two luminescent centers could be observed at certain Eu3+-concentration, indicating that the Eu3+ occupies two different crystallographic sites. This result shows that the Eu3+ occupies two different Y3+ sites in CaYBO4. The investigation on Eu-O charge transfer bands indicates that the larger distortion or the lower symmetry of Eu3+ site is,the shorter wavelength of the Eu-O charge transfer band is. When the Eu3+-concentration is high (x > 0.10), Eu3+ occupies the sites of Ca2+ and is reduced to Eu2+.
Resumo:
This paper described a laser-excited time-resolved fluoroimmunoassay set. It made lanthanide ion to couple the anhydrde of diethylenetriaminepentaacetic acid (DTPAA) for labeling antibodies. The experiment used polystyrene tap coated with HCV antigen as the solid phase and a chelate of the rare earth metal europium as fluorescent label. A nitrogen laser beam was used to excite the Eu3+ chelates and after 60 ys delay time,the emission fluorescence was measured. Background fluorescence of short lifetimes caused by serum components and Raman scattering can be eliminated by set the delay rime. In the system condition, fluorescent spectra and fluorescent lifetimes of Eu3+ beta-naphthoyltrifluroacetone (NTA) chelates were measured. The fluorescent lifetime value is 650 mu s. The maximum emssion wavelength is 613 nm. The linear range of europium ion concentration is 1 x 10(-7)- 1 x 10(-11) g.mL(-1) and the detection limit is 1 x 10(-13) g.mL(-1). The relative standard deviation of determination ( n = 12) for samples at 0.01 ng.mL(-1) magnitude is 6.4%. Laser-TRFIA was also found to be suitable for diagnosis of HCV. The sensitvity and specificity were comparable to enzyme immunoassay. The result was obtained with laser-TRFIA for 29 human correlated well with enzyme immunoassay.
Resumo:
The excitation and emission spectra of the BaLiF3:Ce3+ phosphors synthesized through solid state reaction have been measured. By investigating the properties of the excitation spectra we point out that the variation in the excitation spectra with the amount of CeF3 dopant results from the different patterns of charge compensation in the matrices. The vacancies of Li+ ions are the favorable charge compensation pattern at low concentration of CeF3 doped, but interstitial F- ions are the major charge compensation pattern when the concentration of CeF3 doped goes beyond a certain value. (C) 2000 Academic Press
Resumo:
KMgF3 doped with Eu was synthesized by mild hydrothermal method at 240 degreesC for the first time. The excitation and emission spectra of the KMgF3 : Eu2+ phosphor were measured. Comparing with the sample synthesized through solid state reaction, the variation in the excitation spectra at 360 nm resulted from the existences of V-K color centers; the low emission intensity was due to Eu2+ having transferred part energy to V-K color centers.
Resumo:
The reduction of RE3+ to RE2+ (RE=Eu, Sm and Tm) in SrB6O10 prepared in air by high-temperature solid state reaction was observed. The luminescent properties of Eu2+ and Tm2+ show f-d transition and Sm2+ shows f-f transition at room temperature. Three crystallographic sites for Sm2+ in matrix are available. Vibronic transition of D-5(0)-F-7(0) of Sm2+ was studied. The coupled phonon energy about 108 cm(-1), was determined: from the vibronic transition. Due to the thermal population from D-5(0) level, (D1-FJ)-D-5-F-7 (J=0, 1, 2) transitions of Sm2+ were observed at room temperature. A charge compensation mechanism is proposed as a possible explanation.
Resumo:
(Y1-xEux)(3)Al5O12 and (Y1-x-yEuxBiy)(3)Al5O12 were prepared by so-gel method. Their structures of the luminophor are similar to that of YAG, which is recorded on the ASTM card and belongs to a cubic system. The luminescent properties show that the reaction temperature of the current sol-gel method is in the range of 400-500 degrees C, which is lower than that of the conventional solid state reaction. The luminophors have the strongest emission intensity when the values of x and y are 0.06 and 0.013, respectively.
Resumo:
The reduction of Eu3+ to Eu2+ in SrB6O10 prepared in air by a high-temperature solid state reaction was studied. The luminescent properties of Eu2+ in this matrix show f-d broad band emission peaking at about 386 and 432 nm at room temperature. A charge compensation mechanism is proposed as a possible explanation. The luminescence of Eu3+ with f-f transitions was studied in this sample and reflected that the Eu3+ ion occupied a site with non-centro-symmetry. The ESR spectrum was used to detect the existence of Eu2+ in the samples. (C) 1998 Elsevier Science S.A.