This thesis presents a novel active mirror technology based on carbon fiber composites and replication manufacturing processes. Multiple additional layers are implemented into the structure in order to provide the reflective layer, actuation capabilities and electrode routing. The mirror is thin, lightweight, and has large actuation capabilities. These features, along with the associated manufacturing processes, represent a significant change in design compared to traditional optics. Structural redundancy in the form of added material or support structures is replaced by thin, unsupported lightweight substrates with large actuation capabilities.
Several studies motivated by the desire to improve as-manufactured figure quality are performed. Firstly, imperfections in thin CFRP laminates and their effect on post-cure shape errors are studied. Numerical models are developed and compared to experimental measurements on flat laminates. Techniques to mitigate figure errors for thicker laminates are also identified. A method of properly integrating the reflective facesheet onto the front surface of the CFRP substrate is also presented. Finally, the effect of bonding multiple initially flat active plates to the backside of a curved CFRP substrate is studied. Figure deformations along with local surface defects are predicted and characterized experimentally. By understanding the mechanics behind these processes, significant improvements to the overall figure quality have been made.
Studies related to the actuation response of the mirror are also performed. The active properties of two materials are characterized and compared. Optimal active layer thicknesses for thin surface-parallel schemes are determined. Finite element simulations are used to make predictions on shape correction capabilities, demonstrating high correctabiliity and stroke over low-order modes. The effect of actuator saturation is studied and shown to significantly degrade shape correction performance.
The initial figure as well as actuation capabilities of a fully-integrated active mirror prototype are characterized experimentally using a Projected Hartmann test. A description of the test apparatus is presented along with two verification measurements. The apparatus is shown to accurately capture both high-amplitude low spatial-frequency figure errors as well as those at lower amplitudes but higher spatial frequencies. A closed-loop figure correction is performed, reducing figure errors by 94%.
Resumo:
O objetivo deste trabalho foi criar uma metodologia de validação e revalidação dos processos de esterilização por calor úmido em autoclaves horizontais, destacando os pontos críticos do processo e concentrando esforços onde são realmente necessários. Foram realizados estudos de distribuição térmica, de penetração de calor e de desafio microbiológico na validação da autoclave STERIS FINNAQUA 6912. Com o objetivo de avaliar o impacto de uma mudança e compreender a relação entre os fatores e suas interações para o processo de esterilização, foi utilizado o planejamento fatorial 23 dos fatores densidade da carga (quantidade de itens), embalagem do produto e localização na câmara interna. Os estudos de distribuição térmica confirmaram a distribuição homogênea de calor na câmara interna durante o tempo de exposição a 121C. As temperaturas variaram entre 120,35C e 120,92C com desvio padrão máximo de 0,12C. Os estudos de penetração de calor confirmaram exposições equivalentes a 121C por 24 minutos em todos os itens da carga (F0 > 24 minutos). Em todos os estudos para cargas secas, os índices de capacidade do processo (Cpk) foram maiores que 1,33. Os ensaios de desafio microbiológico garantiram níveis de esterilidade (S.A.L.) maiores que 12 reduções logarítmicas em relação aos indicadores biológicos Geobacillus stearothermophilus. Não foi detectada a presença de endosporos sobreviventes nos 132 indicadores biológicos utilizados nos quatro ciclos desafiados. Com base no planejamento experimental verificou-se que, para o nível de significância de 95% , as mudanças nos fatores posição, embalagem e quantidade da carga não são significativas para o processo de esterilização, em autoclave com remoção forçada de ar. Já para o nível de significância de 90%, a interação Posição x Embalagem apresentou significância estatística no processo de esterilização com valor P de 0,080
Resumo:
I. THE CRYSTAL STRUCTURE OF A NEW DIMER OF TRIPHENYLFLUOROCYCLOBUTADIENE
The crystal structure of thermal isomer of the “head-to-head” dimer of triphenylfluorocyclobutadiene was determined by the direct method. The Σ2 relationship involving the low angle reflections with the largest E’s were found and solved for the signs by the symbolic method of Zachariasen. The structure was seen in the electron density map and the E-map, and was refined antisotropically by the method of least squares. The residual R was 0.065.
The structure is a gem-difluorohexaphenyldihydropentalene. All of the phenyl groups are planar as it is the cyclopentadiene ring of the dihydropentalene skeleton. Overcrowding at the position of the flourines causes some deviations from the normal bond angles in the cyclopentene ring.
The list of observed and calculated structure factors on pages 32-34 will not be legible on the microfilm. Photographic copies may be obtained from the California Institute of Technology.
II. A LOW TEMPERATURE REFINEMENT OF THE CYANURIC TRIAZIDE STRUCTURE
The structure of cyanuric triazide was refined anisotropically by the method of least squares. Three-dimensional intensity data, which has been collected photographically with MoKα radiation at -110˚C, were used in the refinement. The residual R was reduced to 0.081.
The structure is completely planar, and there is no significant bond alternation in the cyanuric ring. The packing of the molecules causes the azide groups to deviate from linearity by 8 degrees.
Resumo:
Considerable interest has been expressed in the composition of the stream gravels, the movement of bed materials and the relationship of sediment composition, packing and siltation of void space to invertebrate ecology. In the autumn of 1982, freeze-samples of gravel were obtained in Dorset streams. Data were required on the depth of salmonid egg pocke and were part of a broader investigation of regional variation in the independent variables of salmonid fish length, gravel size, current velocity and the resultant dependent variable ~egg burial depth. The Dorset river gravels examined are bimodal. The grain size distribution may be resolved into two near-normal frequency distributions interpreted as representing a primary framework or lattice of gravel particles into which a secondary matrix population of sand particles has penetrated.
Resumo:
A Casa da Moeda do Brasil (CMB) é uma empresa nacional, com mais de 300 anos de experiência na produção de valores e impressos de segurança. A produção de cédulas, realizada pelo Departamento de Cédulas (DECED), consiste de três etapas de impressão, off-set, calografia e tipografia, seguida de acabamento e embalagem semi-automatizado. A impressão calcográfica consome solução de limpeza, composta de soda cáustica e óleo sulfonado, para limpeza do cilindro de impressão, gerando um efluente líquido saturado de tinta. Este efluente apresenta baixa biodegradabilidade, apresentando uma relação DBO / DQO de aproximadamente 1:4. Em termos de tratabilidade, as estações de tratamento de efluentes (ETE) apresentam uma configuração convencional, por via biológica, demonstram pouca eficiência na degradação da matéria orgânica deste efluente. Com compostos recalcitrantes, torna-se necessária a inclusão de uma etapa terciária que permita sua degradação por via química, permitindo o descarte do efluente com características menos danosas ao ambiente. Neste trabalho, aplicou-se a reação de Fenton no efluente do DECED por sua capacidade de converter a matéria orgânica em gás carbônico e água ou, caso seja utilizado em pré-tratamentos, torna-os biodegradáveis. Foram estudadas diferentes condições para medir a influência de diferentes parâmetros na eficiência da reação. A reação de Fenton consiste na geração de radicais hidroxil (HO), por diferentes rotas, em quantidades suficientes para a degradação de matéria orgânica. Esses radicais são gerados a partir de peróxido de hidrogênio (H2O2) em reações com diferentes precursores como ozônio (O3), luz UV (ultravioleta), ultra-som e sais de ferro. No presente trabalho restringiu-se às reações com sais de ferro. Dentre os resultados obtidos, verificou-se o tempo mínimo para reação em 10 minutos. A relação entre íons ferro e peróxido de hidrogênio é menor do que a literatura normalmente sugere, 1:2, contra 1:3. Como a solução de sulfato ferroso é muito instável, passando os íons ferrosos a férricos, utilizou-se a adição direta do sal. Em escala industrial, a solução de sulfato ferroso deve ser preparada em poucas quantidades para que tenha baixo tempo de estocagem, a fim de não ser degradada. A temperatura, na faixa estudada (de 20C à 45C), é um parâmetro que tem pouca influência, pois a redução da eficiência da reação foi pequena (de 99,0% para 94,9%). O ferro utilizado na reação não se demonstrou uma nova fonte de transtornos para o ambiente. Nas condições utilizadas, a concentração de ferro residual esteve próxima ao limite permitido pela legislação no efluente tratado, necessitando apenas de alguns ajustes para a correção do problema
Resumo:
Part I
Potassium bis-(tricyanovinyl) amine, K+N[C(CN)=C(CN)2]2-, crystallizes in the monoclinic system with the space group Cc and lattice constants, a = 13.346 ± 0.003 Å, c = 8.992 ± 0.003 Å, B = 114.42 ± 0.02°, and Z = 4. Three dimensional intensity data were collected by layers perpendicular to b* and c* axes. The crystal structure was refined by the least squares method with anisotropic temperature factor to an R value of 0.064.
The average carbon-carbon and carbon-nitrogen bond distances in –C-CΞN are 1.441 ± 0.016 Å and 1.146 ± 0.014 Å respectively. The bis-(tricyanovinyl) amine anion is approximately planar. The coordination number of the potassium ion is eight with bond distances from 2.890 Å to 3.408 Å. The bond angle C-N-C of the amine nitrogen is 132.4 ± 1.9°. Among six cyano groups in the molecule, two of them are bent by what appear to be significant amounts (5.0° and 7.2°). The remaining four are linear within the experimental error. The bending can probably be explained by molecular packing forces in the crystals.
Part II
The nuclear magnetic resonance of 81Br and 127I in aqueous solutions were studied. The cation-halide ion interactions were studied by studying the effect of the Li+, Na+, K+, Mg++, Cs+ upon the line width of the halide ions. The solvent-halide ion interactions were studied by studying the effects of methanol, acetonitrile, and acetone upon the line width of 81Br and 127I in the aqueous solutions. It was found that the viscosity plays a very important role upon the halide ions line width. There is no specific cation-halide ion interaction for those ions such as Mg++, Di+, Na+, and K+, whereas the Cs+ - halide ion interaction is strong. The effect of organic solvents upon the halide ion line width in aqueous solutions is in the order acetone ˃ acetonitrile ˃ methanol. It is suggested that halide ions do form some stable complex with the solvent molecules and the reason Cs+ can replace one of the ligands in the solvent-halide ion complex.
Part III
An unusually large isotope effect on the bridge hydrogen chemical shift of the enol form of pentanedione-2, 4(acetylacetone) and 3-methylpentanedione-2, 4 has been observed. An attempt has been made to interpret this effect. It is suggested from the deuterium isotope effect studies, temperature dependence of the bridge hydrogen chemical shift studies, IR studies in the OH, OD, and C=O stretch regions, and the HMO calculations, that there may probably be two structures for the enol form of acetylacetone. The difference between these two structures arises mainly from the electronic structure of the π-system. The relative population of these two structures at various temperatures for normal acetylacetone and at room temperature for the deuterated acetylacetone were calculated.
Resumo:
报道了基于双面反射镜的N×N光开关器件。介绍了使用双面反射镜的2×2, 4×4光开关的集成光路设计和工作原理; 采用Benes网络, 以2×2和4×4光开关为基本单元的N×N光开关器件的整体结构, 并根据“一笔画”原理, 分析了4×4, 8×8和16×16光开关矩阵的可重排无阻塞特性和光开关矩阵的光路选择算法。最后, 基于2×2, 4×4光开关技术制备了16×16光开关矩阵。测试表明, 该器件具有良好的插入损耗、回波损耗、串扰和开关时间等性能, 从而验证了设计思想和工艺的可行性。在基于双面反射镜的光开关矩
Resumo:
Part I
The physical phenomena which will ultimately limit the packing density of planar bipolar and MOS integrated circuits are examined. The maximum packing density is obtained by minimizing the supply voltage and the size of the devices. The minimum size of a bipolar transistor is determined by junction breakdown, punch-through and doping fluctuations. The minimum size of a MOS transistor is determined by gate oxide breakdown and drain-source punch-through. The packing density of fully active bipolar or static non-complementary MOS circuits becomes limited by power dissipation. The packing density of circuits which are not fully active such as read-only memories, becomes limited by the area occupied by the devices, and the frequency is limited by the circuit time constants and by metal migration. The packing density of fully active dynamic or complementary MOS circuits is limited by the area occupied by the devices, and the frequency is limited by power dissipation and metal migration. It is concluded that read-only memories will reach approximately the same performance and packing density with MOS and bipolar technologies, while fully active circuits will reach the highest levels of integration with dynamic MOS or complementary MOS technologies.
Part II
Because the Schottky diode is a one-carrier device, it has both advantages and disadvantages with respect to the junction diode which is a two-carrier device. The advantage is that there are practically no excess minority carriers which must be swept out before the diode blocks current in the reverse direction, i.e. a much faster recovery time. The disadvantage of the Schottky diode is that for a high voltage device it is not possible to use conductivity modulation as in the p i n diode; since charge carriers are of one sign, no charge cancellation can occur and current becomes space charge limited. The Schottky diode design is developed in Section 2 and the characteristics of an optimally designed silicon Schottky diode are summarized in Fig. 9. Design criteria and quantitative comparison of junction and Schottky diodes is given in Table 1 and Fig. 10. Although somewhat approximate, the treatment allows a systematic quantitative comparison of the devices for any given application.
Part III
We interpret measurements of permittivity of perovskite strontium titanate as a function of orientation, temperature, electric field and frequency performed by Dr. Richard Neville. The free energy of the crystal is calculated as a function of polarization. The Curie-Weiss law and the LST relation are verified. A generalized LST relation is used to calculate the permittivity of strontium titanate from zero to optic frequencies. Two active optic modes are important. The lower frequency mode is attributed mainly to motion of the strontium ions with respect to the rest of the lattice, while the higher frequency active mode is attributed to motion of the titanium ions with respect to the oxygen lattice. An anomalous resonance which multi-domain strontium titanate crystals exhibit below 65°K is described and a plausible mechanism which explains the phenomenon is presented.
Resumo:
Barneko ikerkuntza-txostena
Resumo:
Background: In recent years Galaxy has become a popular workflow management system in bioinformatics, due to its ease of installation, use and extension. The availability of Semantic Web-oriented tools in Galaxy, however, is limited. This is also the case for Semantic Web Services such as those provided by the SADI project, i.e. services that consume and produce RDF. Here we present SADI-Galaxy, a tool generator that deploys selected SADI Services as typical Galaxy tools. Results: SADI-Galaxy is a Galaxy tool generator: through SADI-Galaxy, any SADI-compliant service becomes a Galaxy tool that can participate in other out-standing features of Galaxy such as data storage, history, workflow creation, and publication. Galaxy can also be used to execute and combine SADI services as it does with other Galaxy tools. Finally, we have semi-automated the packing and unpacking of data into RDF such that other Galaxy tools can easily be combined with SADI services, plugging the rich SADI Semantic Web Service environment into the popular Galaxy ecosystem. Conclusions: SADI-Galaxy bridges the gap between Galaxy, an easy to use but "static" workflow system with a wide user-base, and SADI, a sophisticated, semantic, discovery-based framework for Web Services, thus benefiting both user communities.
Resumo:
[ES]En la problemática medioambiental generada por la contaminación atmosférica hay tres aspectos que marcan las directrices de actuación institucional: la presión social, la legislación vigente y la tecnología disponible. En cuanto a este último aspecto, la biofiltración es una tecnología eficaz, asequible y sostenible basada en la actividad biodegradadora de microorganismos específicos adheridos a la superficie de un material soporte que constituye el lecho del biofiltro. La elección de un material soporte adecuado es de especial importancia para asegurar el correcto funcionamiento de los biofiltros. Esta decisión está basada en las propiedades intrínsecas del material que deben ser analizadas previamente a su uso. En este proyecto se ha seleccionado cuales son estas propiedades básicas a partir de una revisión bibliográfica, destacando la capacidad de retención de humedad, superficie específica, porosidad, y estabilidad física y química del material. En este trabajo, también se han fijado los parámetros de control que deben ser medidos de forma rutinaria en un biofiltro para asegurar la eficacia del tratamiento de descontaminación. En base a la información bibliográfica recopilada, se ha concluido que los parámetros básicos son pH, temperatura, contenido de humedad del lecho y pérdidas de carga. A nivel experimental, se han medido las pérdidas de carga generadas en biofiltros empacados con tres materiales soportes que son de especial interés para una investigación posterior a desarrollar por el grupo Biofiltración de la Universidad del País Vasco (UPV/EHU). Durante el período de arranque inicial de los tres biofiltros, las pérdidas de carga medidas fueron muy bajas en los tres casos, aunque algo superiores cuando la alimentación era en sentido ascendente frente al flujo descendente. Sin embargo, cuando se midieron las pérdidas de carga bajo condiciones de encharcamiento del lecho, que es una de las situaciones más problemáticas en un biofiltro, todos los soportes presentaron un aumento puntual de la pérdida de carga aunque la tendencia en los días posteriores fue claramente descendente, recuperando valores de operación habituales. La comparativa del comportamiento frente a las pérdidas de carga permitió seleccionar el soporte más idóneo de los tres analizados, aunque los otros dos podrían ser alternativas viables en caso de sustitución.
Resumo:
[EN]Due to the limitations associated with fossil fuels it is necessary to promote energy sources that are renewable as well as eco-friendly, such as biogas generated in anaerobic digesters. The biogas, composed principally of methane and CO2, is the result of the biodegradation of organic matter under anaerobic conditions. Its use as fuel is limited by the presence of minority compounds such as hydrogen sulphide (H2S); therefore, its pre-treatment is necessary. Currently there are various technologies for the removal of H2S from a gas stream, but most of them are based on physic-chemical treatments which have a number of drawbacks as reactive consumption, generation of secondary flows, etc. Biofiltration has been used as an efficient and low cost alternative to conventional purification processes, and excellent results for the degradation of H2S have been obtained. However process can be limited due to the progressive ageing of the support material, along with the loss of nutrients and other specific characteristics necessary for the good development of biomass. The purpose of this project is to develop a mixed support consisting of a mixture of an organic material and an inorganic support for its application in the removal of the H2S from biogas. This support material helps to optimize the characteristics of the bed and extend its lifespan. The development of such material will contribute to the implementation of biofiltration for treating biogas from anaerobic digesters for its use as biofuel. The inorganic material used is electric arc furnace (EAF) black slag, a by-product generated in large quantities in the production of steel in the Basque Country. Although traditionally the slag has been used in civil engineering, its physicochemical characteristics make it suitable for reuse as a filter medium in biofiltration. The main conclusion drawn from the experimental results is that EAF black slag is a suitable co-packing material in organic biofilters treating H2S-polluted gaseous streams. High pollutant removal rates have been achieved during the whole experimental period. The removal capacity recorded in biofilters with less inorganic material was higher than in those with higher slag portion. Nevertheless, all the biofilters have shown a satisfactory response even at high inlet loads (48 g·m-3·h-1), where the RE has not decreased over 82%.
Resumo:
O câncer de colo de útero é o terceiro tipo de neoplasia mais comum em mulheres no estado do Rio de Janeiro, perdendo apenas para câncer de mama e pulmão. Não há informação disponível sobre a qualidade dos exames utilizados para prevenção do câncer do colo do útero nos municípios fluminenses. O trabalho teve como objetivo avaliar a distribuição geográfica das unidades laboratoriais e a cobertura de exames e a performance da rede de laboratórios de citopatologia do estado do Rio de Janeiro, segundo regiões mesopolitanas e municípios, no que diz respeito aos exames citopatológicos realizados no âmbito do SUS, considerando a qualidade, a normalização dos procedimentos e a gestão do laboratório e propor melhorias. A pesquisa usa um desenho de estudo do tipo transversal incluindo dados relativos ao funcionamento dos laboratórios que fazem exame papanicolaou no âmbito do SUS no estado do Rio de Janeiro. Trata-se de um estudo com dados secundários, já coletados para atender a ação de avaliação dos laboratórios de citopatologia no âmbito do SUS, nesse trabalho também é usada a abordagem ecológica para estimar a cobertura dos exames em relação à população-alvo do programa de rastreamento de câncer de colo de útero. A rede de laboratórios de citopatologia do estado do Rio de Janeiro não teve desempenho satisfatório. As regiões que tiveram laboratórios com melhor desempenho foram Baia da Ilha Grande e Baixada Litorânea e aquelas com laboratórios de pior desempenho foram Médio Paraíba e Noroeste. Os critérios avaliados com melhor desempenho foram da dimensão qualidade e o mais fraco desempenho foi observado para os critérios da dimensão normalização. A dimensão de gestão de laboratórios teve desempenho regular. Um relevante achado desse estudo foi a insuficiente qualidade da leitura de lâminas, inclusive procedimentos de releitura, que pode ser explicado pela suposta falta de capacitação dos profissionais em todo o processo exigido desde a identificação, fixação, e formas de encaminhamento do material até a chegada aos laboratórios. Com relação à cobertura, alguns municípios se aproximam do parâmetro (0,30) porém, embora este dado revele a capacidade da rede estadual do rio de Janeiro de ofertar exames, é preciso que ele seja analisado em conjunto com as situações de citologia anterior e tempo da citologia anterior para verificação da periodicidade da oferta e o melhor dimensionamento do alcance da população alvo assim como a abrangência da rede laboratorial de cada município. Conclusão: Os dados mostram repetição desnecessária de exames citopatológicos, o que implica custos injustificados e uma situação ainda mais deficitária de alcance das ações do que tem revelado o indicador razão. Ocorrendo principalmente em regiões com predominância de laboratórios privados. A expansão da cobertura com base na periodicidade recomendada do exame é relevante no quadro estadual encontrado e deve vir associada a iniciativas que garantam a qualidade no processo de coleta e análise do material, bem como a adequada capacitação dos profissionais para adoção de condutas recomendadas para as lesões identificadas.
Resumo:
[EU]Proiektu honen helburua sare ezberdinetan algoritmo metaheuristikoen erabileraren bitartez bideratze arazoak ebaztea eta aztertzea da. Helburu honetarako erabiliko diren algoritmoak Coral Reefs Optimization eta Firefly Algorithm dira. Bi algoritmoak Python erabiliz inplementatuko dira, baita sareak simulatzen dituen programa ere. Modu honetan, algoritmo bakoitzaren gaitasuna aztertuko da sareko bi punturen arteko bide bideragarri bat, zeinek ezarritako murrizketak betetzen dituen, aurkitzeko; prozesu hau ausaz sortutako simulatutako sare batean oinarrituz garatuko da. Honen bitartez, arazo honen ebazpenerako algoritmo bakoitza egokia den eta bietariko zein den egokiena ondorioztatu ahalko da.
Resumo:
ZrO2, films were deposited by electron-beam evaporation with the oxygen partial pressure varying from 3 X 10(-3) Pa to I I X 10(-3) Pa. The phase structure of the samples was characterized by x-ray diffraction (XRD). The thermal absorption of the films was measured by the surface thermal lensing technique. A spectrophotometer was employed to measure the refractive indices of the samples. The laser-induced damage threshold (LIDT) was assessed using a 1064, nm Nd: yttritium-aluminium-garnet pulsed laser at pulse width of 12 ns. The influence of oxygen partial pressure on the microstructure and LIDT of ZrO2 films was investigated. XRD data revealed that the films changed from polycrystalline to amorphous as the oxygen partial pressure increased. The variation of refractive index at 550 nm wavelength indicated that the packing density of the films decreased gradually with increasing oxygen partial pressure. The absorptance of the samples decreased monotonically from 125.2 to 84.5 ppm with increasing oxygen partial pressure. The damage threshold, values increased from 18.5 to 26.7 J/cm(2) for oxygen partial pressures varying from 3 X 10(-3) Pa to 9 X 10(-3) Pa, but decreased to 17.3 J/cm(2) in the case of I I X 10(-3) Pa. (C) 2005 American Vacuum Society.