937 resultados para resonant Raman scattering
Resumo:
Raman spectroscopy and FT-IR imaging analyses of cave wall pigment samples from north Queensland (Australia) indicate that some hand stencils were undertaken during a dry environmental phase indicating late Holocene age. Other, earlier painting episodes also took place during dry environmental periods of the terminal Pleistocene and/or early Holocene. These results represent a rare opportunity to attain chronological information for rock art in conditions where insufficient carbon is present for radiocarbon dating.
Resumo:
The interactions of phenyldithioesters with gold nanoparticles (AuNPs) have been studied by monitoring changes in the surface plasmon resonance (SPR), depolarised light scattering, and surface enhanced Raman spectroscopy (SERS). Changes in the SPR indicated that an AuNP-phenyldithioester charge transfer complex forms in equilibrium with free AuNPs and phenyldithioester. Analysis of the Langmuir binding isotherms indicated that the equilibrium adsorption constant, Kads, was 2.3 ± 0.1 × 106 M−1, which corresponded to a free energy of adsorption of 36 ± 1 kJ mol−1. These values are comparable to those reported for interactions of aryl thiols with gold and are of a similar order of magnitude to moderate hydrogen bonding interactions. This has significant implications in the application of phenyldithioesters for the functionalization of AuNPs. The SERS results indicated that the phenyldithioesters interact with AuNPs through the C═S bond, and the molecules do not disassociate upon adsorption to the AuNPs. The SERS spectra are dominated by the portions of the molecule that dominate the charge transfer complex with the AuNPs. The significance of this in relation to the use of phenyldithioesters for molecular barcoding of nanoparticle assemblies is discussed.
Resumo:
Raman spectroscopy has been used to characterise the antimonate mineral bahianite Al5Sb35+O14(OH)2 , a semi-precious gem stone. The mineral is characterised by an intense Raman band at 818 cm-1 assigned to Sb3O1413- stretching vibrations. Other lower intensity bands at 843 and 856 cm-1 are also assigned to this vibration and this concept suggests the non-equivalence of SbO units in the structure. Low intensity Raman bands at 669 and 682 cm-1 are probably assignable to the OSbO antisymmetric stretching vibrations. Raman bands at 1756, 1808 and 1929 cm-1 may be assigned to δ SbOH deformation modes, whilst Raman bands at 3462 and 3495 cm-1 are assigned to AlOH stretching vibrations. Complexity in the low wave number region is attributed to the composition of the mineral.
Resumo:
Raman spectroscopy has been used to study the rare earth mineral churchite-(Y) of formula (Y,REE)(PO4) •2H2O. The mineral contains yttrium and depending on the locality, a range of rare earth metals. The Raman spectra of two churchite-(Y) mineral samples from Jáchymov and Medvědín in the Czech Republic were compared with the Raman spectra of churchite-(Y) downloaded from the RRUFF data base. The Raman spectra of churchite-(Y) are characterized by an intense sharp band at 975 cm-1 assigned to the ν1 (PO4)3- symmetric stretching mode. A lower intensity band observed at around 1065 cm-1 is attributed to the ν3 (PO43-) antisymmetric stretching mode. The (PO43-) bending modes are observed at 497 cm-1 (ν2) and 563 cm-1(ν4). Some small differences in the band positions between the four churchite-(Y) samples from four different localities were found. These differences are possible to explain as different compositions of the churchite-(Y) minerals.
Resumo:
The mineral lewisite, (Ca,Fe,Na)2(Sb,Ti)2O6(O,OH)7 an antimony bearing mineral has been studied by Raman spectroscopy. A comparison is made with the Raman spectra of other minerals including bindheimite, stibiconite and roméite. The mineral lewisite is characterised by an intense sharp band at 517 cm-1 with a shoulder at 507 cm-1 assigned to SbO stretching modes. Raman bands of medium intensity for lewisite are observed at 300, 356 and 400 cm-1. These bands are attributed to OSbO bending vibrations. Raman bands in the OH stretching region are observed at 3200, 3328, 3471 cm-1 with a distinct shoulder at 3542 cm-1. The latter is assigned to the stretching vibration of OH units. The first three bands are attributed to water stretching vibrations. The observation of bands in the 3200 to 3500 cm-1 region suggests that water is involved in the lewisite structure. If this is the case then the formula may be better written as Ca, Fe2+, Na)2(Sb, Ti)2(O,OH)7 •xH2O.
Resumo:
Raman spectra of antimonate mineral brizziite NaSbO3 were studied and related to the structure of the mineral. Two sharp bands at 617 and 660 cm-1 are attributed to the SbO3- symmetric stretching mode. The reason for two symmetric stretching vibrations depends upon the bonding of the SbO3- units. The band at 617 cm-1 is assigned to bonding through the Sb and the 660 cm-1 to bonding through the oxygen. The low intensity band at 508 cm-1 is ascribed to the SbO antisymmetric stretching vibration. Low intensity bands were found at 503, 526 and 578 cm-1. Sharp Raman bands observed at 204, 230, 307 and 315 cm-1are assigned to OSbO bending modes. Raman spectroscopy enables a better understanding of the molecular structure of the mineral brizziite.
Resumo:
A high voltage pulsed power supply is proposed in this paper based on oscillation between an inductor and a capacitor in an LC circuit. A two-leg resonant circuit, supplied through an inverter with an alternative voltage waveform, can generate output voltage up to four times an input voltage magnitude. Bipolar and unipolar modulations are used in a single phase inverter to analyse their effects on the proposed resonant converter. Simulations have been carried out to evaluate the proposed topology and control.
Resumo:
The arsenite minerals finnemanite Pb5(As3+O3)3Cl been studied by Raman spectroscopy. The most intense Raman band at 871 cm-1 is assigned to the ν1 (AsO3)3- symmetric stretching vibration. Three Raman bands at 898, 908 and 947 cm-1 are assigned to the ν3 (AsO3)3- antisymmetric stretching vibration. The observation of multiple antisymmetric stretching vibrations suggest that the (AsO3)3- units are not equivalent in the molecular structure of finnemanite. Two Raman bands at 383 and 399 cm-1 are assigned to the ν2 (AsO3)3- bending modes. DFT calculations enabled the position of AsO32- symmetric stretching mode at 839 cm-1, the antisymmetric stretching mode at 813 cm-1, and the deformation mode at 449 cm-1 to be calculated. Raman bands are observed at 115, 145, 162, 176, 192, 216 and 234 cm-1 as well. The two most intense bands are observed at 176 and 192 cm-1. These bands are assigned to PbCl stretching vibrations and result from transverse/ longitudinal splitting. The bands at 145 and 162 cm-1 may be assigned to Cl-Pb-Cl bending modes.
Resumo:
The selected arsenite minerals leiteite, reinerite and cafarsite have been studied by Raman spectroscopy. DFT calculations enabled the position of AsO22- symmetric stretching mode at 839 cm-1, the antisymmetric stretching mode at 813 cm-1, and the deformation mode at 449 cm-1 to be calculated. The Raman spectrum of leiteite shows bands at 804 and 763 cm-1 assigned to the As2O42- symmetric and antisymmetric stretching modes. The most intense Raman band of leiteite is the band at 457 cm-1 and is assigned to the ν2 As2O42- bending mode. A comparison of the Raman spectrum of leiteite is made with the arsenite minerals reinerite and cafarsite.
Resumo:
Raman spectra of mineral peretaite Ca(SbO)4(OH)2(SO4)2•2H2O were studied, and related to the structure of the mineral. Raman bands observed at 978 and 980 cm-1 and a series of overlapping bands observed at 1060, 1092, 1115, 1142 and 1152 cm-1 are assigned to the SO42- ν1 symmetric and ν3 antisymmetric stretching modes. Raman bands at 589 and 595 cm-1 are attributed to the SbO symmetric stretching vibrations. The low intensity Raman bands at 650 and 710 cm-1 may be attributed to SbO antisymmetric stretching modes. Raman bands at 610 cm-1 and at 417, 434 and 482 cm-1 are assigned to the SO42- 4 and 2 bending modes, respectively. Raman bands at 337 and 373 cm-1 are assigned to O-Sb-O bending modes. Multiple Raman bands for both SO42- and SbO stretching vibrations support the concept of the non-equivalence of these units in the coquandite structure.
Resumo:
Natural iowaite, magnesium–ferric oxychloride mineral having light green color originating from Australia has been characterized by EPR, optical, IR, and Raman spectroscopy. The optical spectrum exhibits a number of electronic bands due to both Fe(III) and Mn(II) ions in iowaite. From EPR studies, the g values are calculated for Fe(III) and g and A values for Mn(II). EPR and optical absorption studies confirm that Fe(III) and Mn(II) are in distorted octahedral geometry. The bands that appear both in NIR and Raman spectra are due to the overtones and combinations of water and carbonate molecules. Thus EPR, optical, and Raman spectroscopy have proven most useful for the study of the chemistry of natural iowaite and chemical changes in the mineral.
Resumo:
Raman spectroscopy of the mineral partzite Cu2Sb2(O,OH)7 complimented with infrared spectroscopy were studied and related to the structure of the mineral. The Raman spectrum shows some considerable complexity with a number of overlapping bands observed at 479, 520, 594, 607 and 620 cm-1 with additional low intensity bands found at 675, 730, 777 and 837 cm-1. Raman bands of partzite in the spectral region 590 to 675 cm-1 are attributable the ν1 symmetric stretching modes. The Raman bands at 479 and 520 cm-1 are assigned to the ν3 antisymmetric stretching modes. Raman bands at 1396 and 1455 cm-1 are attributed to SbOH deformation modes. A complex pattern resulting from the overlapping band of the water and OH units is found. Raman bands are observed at 3266, 3376, 3407, 3563, 3586 and 3622 cm-1. The first three bands are assigned to water stretching vibrations. The three higher wavenumber bands are assigned to the stretching vibrations of the OH units. It is proposed that based upon observation of the Raman spectra that water is involved in the structure of partzite. Thus the formula Cu2Sb2(O,OH)7 may be better written as Cu2Sb2(O,OH)7 •xH2O
Resumo:
The investigation into the encapsulation of gold nanoparticles (AuNPs) by poly(methyl methacrylate) (PMMA) was undertaken. This was performed by three polymerisation techniques including: grafting PMMA synthesised by reversible addition-fragmentation chain transfer (RAFT) polymerisation to AuNPs, grafting PMMA synthesised by atom transfer radical polymerisation (ATRP) from the surface of functionalised AuNPs and by encapsulation of AuNPs within PMMA latexes produced through photo-initiated oil-in-water (o/w) miniemulsion polymerisation. The grafting of RAFT PMMA to AuNPs was performed by the addition of the RAFT functionalised PMMA to citrate stabilised AuNPs. This was conducted with a range of PMMA of varying molecular weight distribution (MWD) as either the dithioester or thiol end-group functionalities. The RAFT PMMA polymers were characterised by gel permeation chromatography (GPC), ultraviolet-visible (UV-vis), Fourier transform infrared-attenuated total reflectance (FTIR-ATR), Fourier transform Raman (FT-Raman) and proton nuclear magnetic resonance (1H NMR) spectroscopies. The attachment of PMMA to AuNPs showed a tendency for AuNPs to associate with the PMMA structures formed, though significant aggregation occurred. Interestingly, thiol functionalised end-group PMMA showed very little aggregation of AuNPs. The spherical polymer-AuNP structures did not vary in size with variations in PMMA MWD. The PMMA-AuNP structures were characterised using scanning electron microscopy (SEM), transition electron microscopy (TEM), energy dispersive X-ray analysis (EDAX) and UV-vis spectroscopy. The surface confined ATRP grafting of PMMA from initiator functionalised AuNPs was polymerised in both homogeneous and heterogeneous media. 11,11’- dithiobis[1-(2-bromo-2-methylpropionyloxy)undecane] (DSBr) was used as the surface-confined initiator and was synthesised in a three step procedure from mercaptoundecanol (MUD). All compounds were characterised by 1H NMR, FTIR-ATR and Raman spectroscopies. The grafting in homogeneous media resulted in amorphous PMMA with significant AuNP aggregation. Individually grafted AuNPs were difficult to separate and characterise, though SEM, TEM, EDAX and UV-vis spectroscopy was used. The heterogeneous polymerisation did not produce grafted AuNPs as characterised by SEM and EDAX. The encapsulation of AuNPs within PMMA latexes through the process of photoinitiated miniemulsion polymerisation was successfully achieved. Initially, photoinitiated miniemulsion polymerisation was conducted as a viable low temperature method of miniemulsion initiation. This proved successful producing a stable PMMA with good conversion efficiency and narrow particle size distribution (PSD). This is the first report of such a system. The photo-initiated technique was further optimised and AuNPs were included into the miniemulsion. AuNP encapsulation was very effective, producing reproducible AuNP encapsulated PMMA latexes. Again, this is the first reported case of this. The latexes were characterised by TEM, SEM, GPC, gravimetric analysis and dynamic light scattering (DLS).
Resumo:
The mixed anion mineral dixenite has been studied by Raman spectroscopy, complimented with infrared spectroscopy. The Raman spectrum of dixenite shows bands at 839 and 813 cm-1 assigned to the (AsO3)3- symmetric and antisymmetric stretching modes. The most intense Raman band of dixenite is the band at 526 cm-1 and is assigned to the ν2 AsO33- bending mode. DFT calculations enabled the position of AsO22- symmetric stretching mode at 839 cm-1, the antisymmetric stretching mode at 813 cm-1, and the deformation mode at 449 cm-1 to be calculated. Raman bands at 1026 and 1057 cm-1 are assigned to the SiO42- symmetric stretching vibrations and at 1349 and 1386 cm-1 to the SiO42- antisymmetric stretching vibrations. Both Raman and infrared spectra indicate the presence of water in the structure of dixenite. This brings into question the commonly accepted formula of dixenite as CuMn2+14Fe3+(AsO3)5(SiO4)2(AsO4)(OH)6. The formula may be better written as CuMn2+14Fe3+(AsO3)5(SiO4)2(AsO4)(OH)6•xH2O.
Resumo:
Raman and infrared spectroscopies were used to characterise two samples of triclinic ejkaite Na4[UO2(CO3)3] and its synthetic trigonal analogue. The v3 (UO2)2+ mode is not Raman active, whereas both the v3 and v1 (UO2)2+ modes are infrared active. U--O bond lengths in uranyls were calculated from the spectra obtained and compared with bond lengths derived from crystal structure analyses. From the higher number of bands related to the uranyl and carbonate vibrations, the presence of symmetrically distinct (UO2)2+ and (CO3)2- units in both structures is proposed.