966 resultados para energy transfer efficiency
Resumo:
The different ions doped KMgF3 single crystals are prepared by the vertical Bridgman method. The near-infrared absorption spectra for different parts of all as-growth crystals indicate that there is the best transparency in middle part. The correlation between the vibronic frequencies of Eu2+ and the site displacement of Cu+ co-doped ions is firstly studied, which indicates that Cu+ ions replace the site of the Mg2+ ions. The co-doped Eu2+ counteracts the charge misfit causing by the replacement of Mg2+ with Cu+. The overlapping of the emission spectra of the Eu2+ and the excitation spectra of the Cu+ results in the energy transfer from Eu2+ to Cu+.
Resumo:
Luminescent hybrid thin films consisting of terbium complex covalently bonded to a silica-based network have been obtained in situ via a sol-gel approach. A new monomer, N-(4-benzoic acid-yl), N'-(propylthiethoxysilyl)urea (PABI), has been synthesized by grafting isocyanatopropyltriethoxysilane (ICPTES) to p-aminobenzoic acid and characterized by H-1 NMR IR and MS, The monomer acts as a ligand for Tb3+ ion and as a sol-gel precursor. Band emission front Tb3+ ion due to an efficient ligand-to-metal energy transfer was observed by UV excitation. The decay curves of Tb3+ in the hybrid films were measured. The energy difference between the triplet state energy of PABI and the D-5(4) level of Tb3+ ion falls in the exciting range to sensitize Tb3+ ion fluorescence.
Resumo:
The rare earth (Eu3+, Dy3+)-polyoxometalate thin films were fabricated on quartz plate by the sol-gel method. The thin films were demonstrated by the luminescence spectra. The thin films exhibit the characteristic emission bands of the rare-earth ions. It is noticed that the yellow to blue intensity ratio (Y:B) of Dy3+ and the red to orange ratio (R:O) of Eu3+ in the films are different from that of the corresponding solids. Furthermore, the thin films present shorter fluorescence lifetime than the pure complexes. The reasons that were responsible for these results were also discussed.
Resumo:
Rare-earth (Eu3+, Tb3+)-doped Ca2Y8(SiO4)(6)O-2 luminescent thin films were dip-coated on silicon and quartz glass substrates through a sol-gel route. X-ray diffraction (XRD), scanning electron microscopy (SEM) and luminescence excitation and emission spectra as well as luminescence decays were used to characterize the resultant films. The results of XRD reveal that these films remain amorphous below 700 degreesC, begin to crystallize at 800 degreesC, and crystallize completely around 1000 degreesC with an oxyapatite structure. The grain structure of the film can be seen clearly from SEM micrographs, where particles with various shape and average size of 250 nm can be resolved. The Eu3+ and Tb3+ ions show their characteristic red (D-5(0)-F-7(2)) and green (D-5(4)-F-7(5)) emission in the films with a quenching concentration of 10 and 6 mol% (of Y3+), respectively. The lifetime of Eu-3divided by increases with the heat treatment temperature front 700 to 1100 degreesC.
Resumo:
Novel hybrid thin films covalently doped with Eu3+ (Tb3+) have been prepared via direct routes involving co-condensation of tetraethoxysilane and phen-Si in the presence of Eu3+ (Tb3+) by spin-casting and their luminescence properties have been investigated in detail. Lanthanide ions can be sensitized by anchored phenanthroline in hybrid thin films. Excitation at the ligand absorption wavelength (272 nm) resulted in the strong emission of the lanthanide ions i.e. Eu3+ D-5(0)-F-7(J) (J=0, 1, 2, 3, 4) emission lines and Tb3+ D-5(4)-F-7(J) (J = 6, 5, 4, 3) due to the energy transfer from the ligands to the lanthanide ions.
Resumo:
Luminescent thin films of heteropolytungstate complexes containing lanthanide (europium or samarium) were successfully fabricated by the Langmuir-Blodgett (LB) technique. The pressure-area isotherm of the monolayer of dimethyldioctadecylammonium. bromide (DODA) is modified rather markedly when the subphase contains the complex of Na9EuW10O36 or Na9SmW10O36. The above results indicate that the monolayer of DODA has a strong interaction with the polyanions of EuW10O369-. (or SmW10O369-). X-ray photoelectron spectra and fluorescent spectra verify that europium and tungsten atoms are 36 36 incorporated into the LB films. Ultraviolet (UV), fluorescent spectra and low-angle X-ray diffraction experiments demonstrate that these LB films have a well-defined lamellar structure. The LB film containing EuW10O369- can give off strong fluorescence 16 on UV irradiation. The characteristic emission behaviors of europium ions in LB films and in the powder of Na9EuW10O369- are discussed. It is found that the intensity ratio of the D-5(0)-F-7(2) transition to the D-5(0)-->F-7(1) transition in LB film is quite different from that in the powder of Na9EuW10O36. The difference of the ratio indicates that the site symmetry of europiurn is distorted in LB film, which is probably due to the strong electrostatic interactions between DODA and polyanions.
Resumo:
Organo-functionalized MCM-41 containing non-covalently linked 1,10-phenanthroline (denoted as Phen-MCM-41) was synthesized by template-directed co-condensation of tetraethoxysilane and the modified phenanthroline (denoted as Phen-Si). XRD, FTIR, UV/VIS spectroscopy as well as luminescence spectroscopy were employed to characterize Phen-MCM-41. No disintegration or loss of the Phen-Si during the solvent extraction procedure could be observed. When monitored by the ligand absorption wavelength (272 nm), the undoped MCM-41 produces a broad band emission centered at 450 run, whereas europium (III) doped Phen-MCM-41 displays the emission of the Eu3+, i.e., D-5(0) --> F-7(J) (J = 0, 1, 2, 3, 4) transition lines due to the energy transfer from the ligands to Eu3+ as well as a broad band emission centered at 442 nm.
Resumo:
A new kind of luminescent organic-inorganic hybrid material (denoted Hybrid I) consisting of europium 1,10-phenanthroline complexes covalently attached to a silica-based network was prepared by a sol-gel process. 1,10-Phenanthroline grafted to 3-(triethoxysilyl)propyl isocyanate was used as one of the precursors for the preparation of an organic-inorganic hybrid materials. For comparison purposes, the hybrid material (denoted Hybrid II) in which phenanthroline was not grafted onto the silica backbone of the frameworks was also prepared. Elemental analysis; NMR, FT-IR, UV/vis absorption, and luminescence spectroscopies, and luminescence decay analysis were used to characterize the obtained hybrid materials. It is shown that the homogeneity of Hybrid I is superior to that of Hybrid II, and a higher concentration europium can be incorporated into Hybrid I than Hybrid II. Excitation at the ligand absorption wavelength (283 nm) resulted in the strong emission of the Eu3+ D-5(0)-F-7(J) (J = 0-4) transition lines as a result of the efficient energy transfer from the ligands to the EU3+ in Hybrid I. The number of water molecules coordinated to the europium ion was estimated, and the structure of the as-synthesized Hybrid I was predicted on the basis of the experimental results.
Resumo:
Nanocrystalline YVO4:A (A = Eu3+, Dy3+, Sm3+, Er3+) phosphor films and their patterning were fabricated by a Pechini sol-gel process combined with soft lithography. X-ray diffraction (XRD), Fourier transform infrared spectroscopy (FT-IR), thermogravimetric and differential thermal analysis (TG-DTA), atomic force microscopy (AFM) and optical microscopy, UV/vis transmission and absorption spectra, photoluminescence (PL) spectra, and lifetimes were used to characterize the resulting films. The results of XRD indicated that the films began to crystallize at 400 degreesC and the crystallinity increased with the increase of annealing temperatures. Transparent nonpatterned phosphor films were uniform and crack-free, which mainly consisted of grains with an average size of 90 nm. Patterned gel and crystalline phosphor film bands with different widths (5-60 mum) were obtained. Significant shrinkage and a few defects were observed in the patterned films during the heat treatment process. The doped rare earth ions (A) showed their characteristic emission in crystalline YVO4 phosphor films because of an efficient energy transfer from vanadate groups to them. The Sm3+ and Er3+ ions also showed upconversion luminescence in a YVO4 film host. Both the lifetimes and PL intensity of the rare earth ions increased with increasing annealing temperature from 400 to 800 degreesC, and the optimum concentration for Eu3+ was determined to be 7 mol % and those for Dy3+, Sm3-, and Er3+ were 2 Mol % of Y3- in YVO4 films, respectively.
Resumo:
Five rare earth complexes (Gd(acae)(3), Gd(TFacaC)(3), Eu(acaC)(3), Eu(TFacaC)(3) and Eu(TFacaC)(3)bipy; acac, acetylacetone; TFacac, 1,1,1-trifluoroacetylacetone; bipy, 2,2'-bipyridyl) were synthesized. By comparing the phosphorescence spectra of Gd(acac)(3) and Gd(TFacac)(3) the effect of the replacement of hydrogen by fluorine was examined. Organic light-emitting devices (OLEDs) based on the corresponding europium complexes as emissive layers were also fabricated by the spin-coating method. The triple-layer-type device with the structure glass substrate/ITO (indium-tin oxide)/PVK [poly(N-vinylcarbazole)]/(PVKEu)-Eu-.(TFacac)(3)bipy:PBD[2-(4-bibipyyl)-5-(4-t-butylbipyl-1,3,4-oxadiazole)]/PBD/Al (aluminum) exhibits a brighter red luminescence than those devices with Eu(acac)(3) and Eu(TFacac)(3) complexes as emissive centers upon applying a d.c. voltage.
Resumo:
The triplet energy state of the HTH [HTH: 4,4,5,5,6,6,6-heptafluoro-1-(2-thienyl) hexane-1,3-dione] ligand was measured to be 20 400 cm(-1), which indicated that Sm(HTH)(3) phen (phen: 1,10-phenanthroline) is a good complex to produce strong PL intensity and high fluorescence yield. Electroluminescent (EL) devices using the Sm( HTH) 3 phen complex as the emissive center were fabricated by vapor deposition and spin-coating methods. The relative intensity of the EL spectra changed compared to the photoluminescence (PL) spectrum, which suggested that the luminescence mechanisms of PL and EL have differences. A luminance of 9 cd m(-2) and a higher brightness of 21 cd m(-2) were obtained from the devices ITO/TPD (40 nm)/ Sm( HTH)(3) phen (50 nm)/ PBD (30 nm)/ Al (200 nm) and ITO/PVK (40 nm)/ PVK : Sm( HTH)(3) phen (2.5 wt%, 50 nm)/ PBD (30 nm)/ Al (200 nm), respectively.
Resumo:
The first heteropoly acid-dipeptide complex, (HGly-Gly)(3)PMo12O40.4H(2)O, was synthesized and characterized by elemental analysis, IR, UV, H-1 NMR and single crystal X-ray diffraction. The X-ray crystallographic study showed that the crystal structure was constructed from N-H...O and O-H...O hydrogen bonds among the (HGly-Gly)(+), H2O and PMo12O403- units. This structure represents a model interaction between polyoxometalates and proteins. The complex has photosensitivity under irradiation by sunlight. The fluorescent activity of this compound is also reported.
Resumo:
The vesicle of didodecyldhnethylammonimn bromide (DDAB) which contained tetrathiafulvalene (TTF) was mixed with xanthine oxidase, and the mixture was cast on the pyrolytic graphite electrode. The lipid films were used to supply a biological environment resembling biomembrane on the surface of the electrode. TTF was used as a mediator because of its high electron-transfer efficiency. A novel xanthine biosensor based on cast DDAB film was developed. The effects of pH and operating potential were explored for optimum analytical performance by using the amperometric method. The response time of the biosensor was less than 10 s. The detection limit of the biosensor was 3.2 x 10(-7) mol/L and the liner range was from 4 x 10(-7) mol/L to 2.4 x 10(-6) mol/L.
Resumo:
Using the Bridgeman-Stockbarger method, the KMgF3:EU2+ single crystal was grown. The color centers in unirradiated KMgF3:Eu crystal were studied. By thermal annealing, we confirmed the 422-nm emission resulted from color centers and oxygen centers, and we proved the energy transfer from EU2+ to color centers. From spectra, the relative oxygen content in crystal was calculated, and the relationships of oxygen displacing fluorine were studied.
Resumo:
Rare-earth and lead ions (Eu3+, Tb3+, Dy3+, Pb2+) doped Ca2Y8 (SiO4)(6)O-2 and Ca2Gd8(SiO4)(6)O-2 thin films have been dip- coated on silicon and quartz glass substrates through the sol- gel route. X- Ray diffraction (XRD), TG- DTA, scanning electron microscopy (SEM), atomic force microscopy (AFM), FT- IR and luminescence excitation and emission spectra as well as luminescence decays were used to characterize the resulting films. The results of XRD reveal that these films remain amorphous below 700 degreesC, begin to crystallize at 800 degreesC and crystallize completely around 1000 degreesC with an oxyapatite structure. The grain structure of the film can be seen clearly from SEM and AFM micrographs, where particles with various shapes and average size of 250 nm can be resolved. Eu3+ and Tb3+ show their characteristic red (D-5(0)-F-7(2)) and green (D-5(4) - F-7(5)) emission in the films with a quenching concentration of 10 and 6 mol% (of Y3+), respectively. The lifetime and emission intensity of Eu3+ increase with the temperature treatment from 700 to 1100 degreesC, while those of Tb3+ show a maximum at 800 degreesC. Energy transfer phenomena have been observed by activating the oxyapatite film host- lattice Ca2Gd8(SiO4)(6)O-2 with Tb3+ (Dy3+). In addition, Pb2+ can sensitize the Gd3+ sublattice in Ca2Gd8(SiO4)(6)O-2.