959 resultados para Sol-gels (xerogels)
Resumo:
Silica-poly(oxypropylene) (PPO) nanocomposites containing PPO with weak physical bonds between the organic (PPO) and inorganic (silica) phases were obtained by the sol-gel procedure. Three precursor sols containing silica and PPO with molecular weights of 1000, 2000 and 4000g/mol were prepared. The structure changes during the whole sol-gel process, i.e. sol formation, sol-gel transition and gel aging and drying were investigated in situ by small angle X-ray scattering (SAXS). The experimental SAXS curves corresponding to sols and wet gels containing PPO of molecular weight 1000g/mol indicate that the aggregates formed during the studied process are fractal objects. Close to the sol-gel transition and during gel aging the fractal dimension is D=2.5. A clearly different structure evolution occurs in samples prepared with PPO with molecular weights 2000 and 4000 g/mol. Our SAXS results indicate the presence of two coexisting and well-defined structure levels, one of them corresponding to small silica clusters and the other to large silica aggregates. These two levels remain along the whole transformation. The SAXS curves of all dry samples are similar to those of the corresponding wet gels suggesting that no significant changes at nanoscopic scale occur during the drying process.
Resumo:
Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)
Resumo:
Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)
Resumo:
The aim of the present study was to evaluate the effect of 20% and 35% hydrogen peroxide bleaching gels on the color, opacity, and fluorescence of composite resins. Seven composite resin brands were tested and 30 specimens, 3-mm in diameter and 2-mm thick, of each material were fabricated, for a total of 210 specimens. The specimens of each tested material were divided into three subgroups (n=10) according to the bleaching therapy tested: 20% hydrogen peroxide gel, 35% hydroxide peroxide gel, and the control group. The baseline color, opacity, and fluorescence were assessed by spectrophotometry. Four 30-minute bleaching gel applications, two hours in total, were performed. The control group did not receive bleaching treatment and was stored in deionized water. Final assessments were performed, and data were analyzed by two-way analysis of variance and Tukey tests (p<0.05). Color changes were significant for different tested bleaching therapies (p<0.0001), with the greatest color change observed for 35% hydrogen peroxide gel. No difference in opacity was detected for all analyzed parameters. Fluorescence changes were influenced by composite resin brand (p<0.0001) and bleaching therapy (p=0.0016) used. No significant differences in fluorescence between different bleaching gel concentrations were detected by Tukey test. The greatest fluorescence alteration was detected on the brand Z350. It was concluded that 35% hydrogen peroxide bleaching gel generated the greatest color change among all evaluated materials. No statistical opacity changes were detected for all tested variables, and significant fluorescence changes were dependent on the material and bleaching therapy, regardless of the gel concentration.
Resumo:
Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)
Resumo:
Coordenação de Aperfeiçoamento de Pessoal de Nível Superior (CAPES)
Resumo:
Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)
Resumo:
Coordenação de Aperfeiçoamento de Pessoal de Nível Superior (CAPES)
Resumo:
Conselho Nacional de Desenvolvimento Científico e Tecnológico (CNPq)
Resumo:
Unsupported SnO2 membranes were prepared by sol-gel process and characterized by N2 adsorption-desorption isotherms and X-ray diffraction. Results show that the texture of dried samples does not change appreciably with the concentration of electrolyte. All of the pore size range used in ultrafiltration process was screened using sintering temperature between 300 and 700°C. © 1994 Kluwer Academic Publishers.
Resumo:
The structural evolution during sintering of compacted SnO2 sol-gel powder was investigated using nitrogen adsorption isotherm analysis. Results show that for sintering temperatures up to 400°C the samples have a fractal pore size distribution. As the sintering temperature increases, a structural rearragement occurs, allowing an increase of the efficiency of particle packing and the reduction of fractality. Above 400°C, the pore size growth associated with grain coalescence is the main structural change observed as the sintering temperature increases. © 1995.
Resumo:
Conselho Nacional de Desenvolvimento Científico e Tecnológico (CNPq)
Resumo:
In order to determine structural changes during drying of inorganic gels, the local and long-range order structure of SnO2-x(OH)2x xerogels resulting from drying hydrogels with different concentrations of electrolyte (Cl- and NH+ 4) have been measured by extended X-ray absorption fine structure (EXAFS), X-ray diffraction (XRD) and N2 adsorption techniques. EXAFS measurements performed at the Sn K edge on the hydrogels and xerogels show the existence of microcrystallites with the cassiterite structure. Two drying modes have been used: freeze drying and drying by evaporation at 45°C. It is shown that the microcrystallite size determined by XRD and EXAFS techniques on the drying mode and on the electrolyte concentrations. The microcrystallite size measured on the freeze dried xerogels is similar to that of their parent hydrogels, whatever the concentration of electrolyte; however, during drying by evaporation, a preferential growth of microcrystallites along the c-axis of the cassiterite structure is observed. The size of these crystallites is enhanced with a decrease of the electrolyte concentration. Specific surface areas calculated by the Brunauer-Emmett-Teller method indicate that this preferential growth is related to the improvement of the network connectivity. The comparison of both drying processes indicates that crystallization and polycondensation are independent phenomena. © 1995 Elsevier Science B.V. All rights reserved.
Resumo:
The luminescence spectra and extended x-ray-absorption fine-structure (EXAFS) measurements of a series of Eu3+-based organic/inorganic xerogels were reported and related to the local coordination of the lanthanide cations. The hybrid matrix of these organically modified silicates, classed as U(2000) ureasils, is a siliceous network to which short organic chains containing oxyethylene units are covalently grafted by means of urea bridges. The luminescent centers were incorporated as europium triflate, Eu(CF3SO3)3, and europium bromide, EuBr3, with concentrations 200≥n≥20 and n=80, 40, and 30, respectively - where n is the number of ether oxygens in the polymer chains per Eu3+ cation. EXAFS measurements were carried out in some of the U(2000)nEu(CF3SO3)3 xerogels (n=200, 80, 60, and 40). The obtained coordination numbers N ranging from 12.8, n=200, to 9.7, n=40, whereas the average Eu3+ first neighbors distance R is 2.48-2.49 Å. The emission spectra of these multiwavelength phosphors superpose a broad green-blue band to a series of yellow-red narrow 5D0→7F0-4 Eu3+ lines and to the eye the hybrids appeared to be white, even at room temperature. The ability to tune the emission of the xerogels to colors across the chromaticity diagram is achieved by changing the excitation wavelength and the amount of salt incorporated in the hybrid host. The local environment of Eu3+ is described as a continuous distribution of closely similar low-symmetry network sites. The cations are coordinated by the carbonyl groups of the urea moieties, water molecules, and, for U(2000)nEu(CF3SO3)3, by the SO3 end groups of the triflate anions. No spectral evidences have been found for the coordination by the ether oxygens of the polyether chains. A mean radius for the first coordination shell of Eu3+ is calculated on the basis of the emission energy assignments. The results obtained for U(2000)nEu(CF3SO3)3, 2.4 Å for 90 ≥n≥40 and 2.6 and 2.5 Å for n=30 and 20, respectively, are in good agreement with the values calculated from EXAFS measurements. The energy of the intraconfigurational charge-transfer transitions, the redshift of the 5D0→7F0 line, with respect to the value calculated for gaseous Eu3+, and the hypersensitive ratio between the 5D0→7F2 and 5D0→7F1 transitions, point out a rather low covalency nature of the Eu3+ first coordination shell in these xerogels, comparing to the case of analogous polymer electrolytes modified by europium bromide. ©1999 The American Physical Society.
Evolution of the viscoelastic properties of SnO2 colloidal suspensions during the sol-gel transition
Resumo:
This paper describes the effect of the concentration of electrolyte and pH on the kinetics of aggregation and gelation processes of SnO2 colloidal suspensions. Creep, creep-recovery, and oscillatory rheological experiments have been done in situ during aggregation and gelation. A phenomenological description of the structure of the colloidal system is given from the time evolution of rheological parameters. The dependence of the equilibrium steady-state shear compliance on the terminal region of clusters or aggregates seems to be a way to determine the beginning of interconnection of aggregates and the gel point. We propose that at this point the equilibrium steady-state compliance is a minimum. The steady-state viscosity determined from creep experiment can be fit with a power law with the extent of the transformation, giving critical exponent s = 0.7 ± 0.1. The value of the critical exponent Δ = 0.78 ± 0.05 was determined from oscillatory experiment. These results indicate that gelation of SnO2 colloidal suspension exhibits the typical scale expected from the scalar percolation theory. © 2000 Elsevier Science B.V. All rights reserved.