929 resultados para Glass painting and staining
Resumo:
This paper outlines a study of the microstructure of thin sheets of ivory used as a painting support for portrait miniatures. Warping of the ivory support is one of the main problems commonly found in portrait miniatures from the late eighteenth century and early nineteenth century. Portrait miniatures from this period are painted on very thin sheets of ivory that are often only 0.2 mm in thickness. Warping can lead to cracking of the ivory and can also accentuate flaking of the paint layer. The problem of warping in ivory has thus been of long-term interest to conservators who deal with portrait miniatures, including those at the Victoria and Albert (V&A) Museum. The causes of warping are complex. However, it should be noted that artists normally stuck the thin ivory sheets onto paper or card before commencing the painting. The possible causes of warping therefore are thought to relate to the differential reactions of the ivory/adhesive/paper or card layers to changes in relative humidity (RH). It is well known that ivory is hygroscopic and anisotropic.1 However, only a few scientific studies have been carried out related to this subject and systematic analyses of the morphological and microstructural changes due to changes in RH or moisture in such thin sheets of ivory have yet to be investigated.
Resumo:
Modified fluorcanasite glasses were fabricated by either altering the molar ratios of Na(2)O and CaO or by adding P(2)O(5) to the parent stoichiometric glass compositions. Glasses were converted to glass-ceramics by a controlled two-stage heat treatment process. Rods (2 mm x 4 mm) were produced using the conventional lost-wax casting technique. Osteoconductive 45S5 bioglass was used as a reference material. Biocompatibility and osteoconductivity were investigated by implantation into healing defects (2 mm) in the midshaft of rabbit femora. Tissue response was investigated using conventional histology and scanning electron microscopy. Histological and histomorphometric evaluation of specimens after 12 weeks implantation showed significantly more bone contact with the surface of 45S5 bioglass implants when compared with other test materials. When the bone contact for each material was compared between experimental time points, the Glass-Ceramic 2 (CaO rich) group showed significant difference (p = 0.027) at 4 weeks, but no direct contact at 12 weeks. Histology and backscattered electron photomicrographs showed that modified fluorcanasite glass-ceramic implants had greater osteoconductivity than the parent stoichiometric composition. Of the new materials, fluorcanasite glass-ceramic implants modified by the addition of P(2)O(5) showed the greatest stimulation of new mineralized bone tissue formation adjacent to the implants after 4 and 12 weeks implantation. (C) 2010 Wiley Periodicals, Inc. J Biomed Mater Res Part A: 94A: 760-768, 2010
Resumo:
Kayotypes of four neotropical teiid lizard species (Tupinambinae) were herein studied after conventional as well as silver staining and CBG-banding: Crocodilurus amazonicus (2n = 34), Tupinambis teguixin (2n = 36), Tupinambis merianae and Tupinambis quadrilineatus (2n = 38). The karyological data for T. quadrilineatus as well as those obtained using differential staining for all species were unknown until now. The karyotypes of all species presented 12 macrochromosomes identical in morphology, but differed in the number of microchromosomes: 22 in C. amazonicus, 24 in T. teguixin and 26 in T. quadrilineatus and T. merianae. The Ag-NOR located at the secondary constriction at the distal end of pair 2 is shared by all species, contrasting with the variability observed for this character in species of the related Teiinae. CBG-banding revealed a species-specific pattern in T. quadrilineatus with conspicuous interstitial C-blocks at the proximal region of the long arm of pair 4 and the whole heterochromatic short arm of pair 6. The karyological data reported here corroborates the relationship hypothesis obtained for Tupinambis based on molecular characters. T. teguixin presents the putative ancestral karyotype for the genus with 2n = 36 whereas T. merianae and T. quadrilineatus exhibit 2n = 38, due to an additional pair of microchromosomes.
Resumo:
The mechanisms of nucleation and growth and the solid-to-liquid transition of metallic nanoclusters embedded in sodium borate glass were recently studied in situ via small-angle X-ray scattering (SAXS) and wide-an-le X-ray scattering (WAXS). SAXS results indicate that, under isothermal annealing conditions, the formation and growth of Bi or Ag nanoclusters embedded in sodium borate glass occurs through two successive stages after a short incubation period. The first stage is characterized by the nucleation and growth of spherical metal clusters promoted by the diffusion of Bi or Ag atoms through the initially supersaturated glass phase. The second stage is named the coarsening stage and occurs when the (Bi- or Ag-) doping level of the vitreous matrix is close to the equilibrium value. The experimental results demonstrated that, at advanced stages of the growth process, the time dependence of the average radius and density number of the clusters is in agreement with the classical Lifshitz-Slyozov-Waoner (LSW) theory. However, the radius distribution function is better described by a lognormal function than by the function derived from the theoretical LSW model. From the results of SAXS measurements at different temperatures, the activation energies for the diffusion of Ag and Bi through sodium borate glass were determined. In addition, via combination of the results of simultaneous WAXS and SAXS measurements at different temperatures, the crystallographic structure and the dependence of melting temperature T(m) on crystal radius R of Bi nanocrystals were established. The experimental results indicate that T(m) is a linear and decreasing function of nanocrystal reciprocal radius 1/R, in agreement with the Couchman and Jesser theoretical model. Finally, a weak contraction in the lattice parameters of Bi nanocrystals with respect to bulk crystals was established.
Resumo:
The evidence of successful growth of Mn-doped PbS (Pb(1-x)Mn(x)S) nanocrystals (NCs) in SiO(2)-Na(2)CO(3)-Al(2)O(3)-PbO(2)-B(2)O(3) template, using the fusion method, is reported on in this study. The as-grown Pb(1-x)Mn(x)S NC is characterized using optical absorption, electron paramagnetic resonance, and atomic force microscopy. The data are discussed in terms of two distinct scenarios, namely a core-doped and a shell-doped nanostructure. (C) 2008 Elsevier B.V. All rights reserved.
Resumo:
A Li(2)O-B(2)O(3)-Al(2)O(3) glass system, un-doped and doped with LiF, and/or TiO(2) was synthesized by the fusion method and its physical properties were investigated by thermoluminescence (TL), X-ray diffraction (XRD), electron paramagnetic resonance (EPR), atomic force microscopy (AFM) and differential thermal analysis (DTA). The samples were subjected to gamma-rays from a colbalt-60 ((60)Co) source. These techniques provided evidence of LiF and LiF doped with Ti crystal formation in the glass system. A TL glow peak at about 433 K was sensitive to (60)Co gamma-rays and showed good linearity with doses and consequently could be used to quantify radiation doses. Crown Copyright (C) 2011 Published by Elsevier B.V. All rights reserved.
Resumo:
This paper reports on the effect of glass ceramic silica matrix on [CrO4](4-) and Cr2O3 NIR and visible luminescence. Chromium-containing silica was obtained by precipitation from water-glass and chromium nitrate acid solution with thermal treatment at 1000 degrees C. From XRD results silica and silica-chromium samples are crystalline. The chromium emission spectrum presents two main broad bands: one in the NIR region (1.1-1.7 mu m) and other in the visible region (0.6-0.7 mu m) assigned to Cr4+ and to Cr3+, respectively. This thermal treated glass ceramic silica-chromium sample stabilizes the [CrO4](4-) where Cr4+ substitutes for Si4+ and also hexacoordinated Cr3+ group probably as segregated phase in the system. It can be pointed out that luminescence spectroscopy is a powerful toot for detecting the two chromium optical centers in the glass ceramic silica. (C) 2008 Elsevier B.V. All rights reserved.
Resumo:
The local structure of an ion-conducting glass with nominal composition 50B(2)O(3)-10PbO-40LiF has been investigated by complementary (7)Li, (11)B, (19)F, and (207)Pb single- and double-resonance experiments. The results give insight into the structural role of the lithium fluoride additive in borate glasses: (1) LiF is seen to actively participate in the network transformation process contributing to the conversion of three- into four-coordinate boron units, as shown by (11)B single-resonance as well as by (11)B{(19)F} and (19)F{(11)B} double-resonance experiments. (2) (19)F signal quantification experiments suggest substantial fluoride loss, presumably caused by formation of volatile BF(3). A part of the fluoride remains in the dopant role, possibly in the form of small LiF-like cluster domains, which serve as a mobile ion supply. (3) The extent of lithium-fluorine and lead-fluorine interactions has been characterized by (7)Li{(19)F} and (207)Pb{(19)F} REDOR and SEDOR experiments. On the basis of these results, a quantitative structural description of this system has been developed.
Resumo:
In this report, we describe a rapid and reliable process to bond channels fabricated in glass substrates. Glass channels were fabricated by photolithography and wet chemical etching. The resulting channels were bonded against another glass plate containing a 50-mu m thick PDMS layer. This same PDMS layer was also used to provide the electrical insulation of planar electrodes to carry out capacitively coupled contactless conductivity detection. The analytical performance of the proposed device was shown by using both LIF and capacitively coupled contactless conductivity detection systems. Efficiency around 47 000 plates/m was achieved with good chip-to-chip repeatability and satisfactory long-term stability of EOF. The RSD for the EOF measured in three different devices was ca. 7%. For a chip-to-chip comparison, the RSD values for migration time, electrophoretic current and peak area were below 10%. With the proposed approach, a single chip can be fabricated in less than 30 min including patterning, etching and sealing steps. This fabrication process is faster and easier than the thermal bonding process. Besides, the proposed method does not require high temperatures and provides excellent day-to-day and device-to-device repeatability.
Resumo:
This paper compares the analytical performance of microchannels fabricated in PDMS, glass, and polyester-toner for electrophoretic separations. Glass and PDMS chips were fabricated using well-established photolithographic and replica-molding procedures, respectively. PDMS channels were sealed against three different types of materials: native PDMS, plasma-oxidized PDMS, and glass. Polyester-toner chips were micromachined by a direct-printing process using an office laser printer. All microchannels were fabricated with similar dimensions according to the limitations of the direct-printing process (width/depth 150 mu m/12 mu m). LIF was employed for detection to rule out any losses in separation efficiency due to the detector configuration. Two fluorescent dyes, coumarin and fluorescein, were used as model analytes. Devices were evaluated for the following parameters related to electrophoretic separations: EOF, heat dissipation, injection reproducibility, separation efficiency, and adsorption to channel wall.