LiAlO2 single crystals doped with Ti at concentration 0.2 at.% are grown by the Czochralskl technique with dimensions Phi 42 x 55 mm. Ti ions in the crystal are quadrivalence proven by comparing the absorption and fluorescence spectra of pure LiAlO2 and Ti: LiAlO2. After air and Li-rich atmosphere annealing, the absorption peaks in the range of 600-800nm disappear. We conclude that 682 and 756nm absorption peaks are attributed to the V-Li and V-O absorptions, respectively. The peaks at 716nm and 798nm may stem from the V-Li(+) and F+ absorptions. The colour-centre model can be applied to explain the experimental phenomena. Ti4+-doping produces more lithium vacancies in the LiAlO2 crystal. The intensities of [LiO4] and the associated bonds remain unchanged, which improves the anti-hydrolyzation and thermal stability of LiAlO2 crystals.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The structure of the titanate glass is destroyed during irradiation by the femtosecond laser pulses, and (TiO6)(8-) and (TiO4)(4-) anion units are exsolved from the network of the titanate glass. These anion units are rearranged to form some crystals such as anatase and Ba2TiO4 crystals. By Raman spectroscopy, it is found that these crystals have a strong dependence on the intensity of the femtosecond laser pulses. The relation between the generation of these crystals and space distribution of the femtosecond laser power intensity is qualitatively explained. (c) 2005 Elsevier B.V. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

By using an Ar+ ion laser, a tunable Rh 6G dye laser(Linewidth : 0.5 cm(-1)) and a Coherent 899-21 dye laser as light sources and using a monochromator and a phase-locking amplifier, the optical properties of Eu3+ : Y2SiO5 crystal were detected. Persistent spectral hole burning (PSHB) were also observed in (5)Do-(7)Fo transition in the crystal at the temperature of 16 K. For 15 mW dye laser (Wavelength : 579.62 nm) burning the crystal for 0.1 s a spectral hole with about 80 MHz hole width were detected and the hole can been keep for longer than 10 h.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

A finite-element model is employed to analysis the thermal environments in Temperature Gradient Technique (TGT) furnace during the growth of large-sized Nd:YAG crystal. The obtained results show that when the crucible is located at the lower position inside of the heater, a flatter solid-liquid interface is established, which makes it easier to obtain the core-free Nd:YAG crystal. Meanwhile, the lower crucible position can induce higher axial temperature gradient, which is beneficial to the release of latent heat. (c) 2007 WILEY-VCH Verlag GmbH & Co. KGaA, Weinheim.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Absorption and emission spectral properties of GdVO4 single crystal doped with Ho3+ ions were investigated at room temperature. Polarized absorption cross section is calculated in the range of 400-2200nm. Results were analyzed and parameters were calculated based on Judd-Ofelt theory, the emission spectrum shows that the emission intensity around the wavelength of 546 nm associated with transition S-5(2) -> I-5(8) is much stronger than other bands in the observed range and potentially enable the green light output around this emission band in this crystal. (c) 2006 Elsevier B.V. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Transparent polycrystalline Nd:YAG ceramics were fabricated by solid-state reactive sintering a mixture of commercial Al2O3,Y2O3, and Nd2O3 powders. The powders were mixed in ethanol and doped with 0.5 wt% tetraethoxysilane, dried, and pressed. Pressed samples were sintered at 1750 degrees C in vacuum. Transparent fully dense samples with average grain sizes of 10 mu m were obtained. The 1 at.% Nd:YAG ceramic was used to research passively Q-switched laser output with a Cr4+:YAG crystal as a saturable absorber. An average output power of 94 mW with a pulse width of 50 ns was obtained when the incident pump power was 750 mW. The slope efficiency was 13%. The pulse energy is 5 mu J, and the peak power is about 100 W.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

For the first time, a high optical quality Yb3+-doped lutetium pyrosilicate laser crystal Lu2Si2O7 (LPS) was grown by the Czochralski (Cz) method. The segregation coefficient of ytterbium ion in Yb:LPS crystal detected by the inductively coupled plasma atomic emission spectrometer (TCP-AES) method is equal to 0.847. X-ray powder diffraction result confirms the C2/m phase monoclinic space group of the grown crystal and the peaks corresponding to different phases were indexed. The absorption and fluorescence spectra, as well as fluorescence decay lifetime of Yb3+ ion in LPS have been investigated. The absorption and fluorescence cross-sections of the transitions F-2(7/2) <-> F-2(5/2) of Yb3+ ion in LPS crystal have been determined. The advantages of the Yb:LPS crystal including high crystal quality, quasi-four-level laser operating scheme, high absorption cross-sections (1.33 x 10(-2) cm(2)) and particularly broad emission bandwidth (similar to 62 nm) indicated that the Yb:LPS crystal seemed to be a promising candidate used as compact, efficient thin chip lasers when LD is pumped at 940 and 980 nm due to its low-symmetry monoclinic structure and single crystallographic site. (c) 2007 Elsevier B.V. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Spectroscopic properties of Ce-doped yttrium orthoaluminate (Ce:YAlO3 or Ce:YAP) crystals grown by temperature gradient technique (TGT) were investigated, and the effects of the growth conditions on the properties were analyzed.. Methods of optical absorption (OA), photoluminescence (PL), photoluminescence decay (PLD), X-ray excited luminescence (XL) and cathodeluminescence (CL) were used in these investigations. The results showed that the absorption band peak at 202, 394 and 532 nm originated from F and F+ color center induced by the weak reducing growth atmosphere, green emission band near 500 ran derived from Ce3+ -Ce3+ pairs and band at 650 similar to 850 run from some unintentional impurity in crystals.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Absorption spectrum from 400 to 2000 run and upconversion fluorescence spectra under 940 nm pumping of YAG single crystal codoped with 5 at.% Yb3+ and 4 at.% Tm3+ were studied at room temperature. The blue upconversion emission centered at 483 nm corresponds to the transition (1)G(4) -> H-3(6), the emission band around 646 nm corresponds to the transition (1)G(4) -> F-3(4) of Tm3+. Energy transfer from Yb3+ to Tm3+ is mainly nonradiative and the transfer efficiency was experimentally assessed. The line strengths, transition probabilities and radiative lifetimes of (1)G(4) level were calculated by using Judd-Ofelt theory. Gain coefficient calculated from spectra shows that the upconversion corresponding with transitions (1)G(4) -> H-3(6) in YAG doped with Yb3+ and Tm3+ is potentially useful for blue light Output. (c) 2006 Elsevier B.V. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Passive Q-switching of a diode-pumped Yb:LYSO laser at 1060 nm with a Yb3+ ions-doped CaF2 crystal without the excited-state absorption (ESA) was demonstrated. An average output power of 174 mW with pulse duration of 5.6 mu s and repetition rate of 27 kHz have been obtained under the unoptimized conditions. And the Q-switching conversion efficiency was as high as 51.7%. (c) 2007 Optical Society of America.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

We report the measured group delay dispersion (GDD) of new crystals Yb:Gd2SiO5 (Yb:GSO), Yb:GdYSiO5 (Yb:GYSO) and Yb:LuYSiO5 (Yb:LYSO) over wavelengths from 1000nm to 1200nm, with a white-light interferometer. Those GDD data should be useful for the dispersion compensation for femtosecond pulse generation in the lasers with these new crystals as the gain media. (C) 2007 Optical Society of America

Relevância:

20.00% 20.00%

Publicador:

Resumo:

In this paper, single crystal of ytterbium (Yb) doped Ca-5(PO4)(3)F (FAP) has been grown along the c-axis by using the Czochralski method. The segregation coefficients of Yb3+ in the Yb:FAP crystal has been determined by ICP-AES method. The absorption spectrum, fluorescence spectrum and fluorescence lifetime of the Yb:FAP crystal has been also measured at room temperature. In the absorption spectra, there are two absorption bands at 904 and 982 nm, respectively, which are suitable for InGaAs diode laser pumping. The absorption cross-section (sigma(abs)) is 5.117 x 10(-20) cm(2) with an FWHM of 4 nm at 982 nm. The emission cross-section is (sigma(em)) 3.678 x 10(-20) cm(2) at 1042 nm. Favorable values of the absorption cross-section at about 982 nm are promising candidates for laser diode (LD) pumping. (c) 2005 Elsevier B.V. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

For the first time, a quaternary doping system of Er3+, Yb3+, Ce3+, Na+:CaF2 single crystal was demonstrated to have high fluorescence yield in the eye-safe 1.5 mu m region under 980 nm laser diode pumping, with relatively broad and flat gain curves. A simplified model was established to illustrate the effect of Ce3+ on the branching ratio for the Er3+4I11/2 -> I-4(13/2) transition. With 0.2-at.% Er3+ and 2.0-at.% Ce3+ in the quaternary-doped CaF2 crystal, the branching ratio was estimated to be improved more than 40 times by the deactivating effect of Ce3+ on the Er3+ 4I11/2 level. The quaternary-doped CaF2, system shows great potential to achieve high laser performance in the 1.5 mu m region. (c) 2006 Elsevier B.V. All rights reserved.