863 resultados para Vickers indentation


Relevância:

10.00% 10.00%

Publicador:

Resumo:

Spherical scratch tests were conducted in individual grains of a randomly oriented polycrystalline body-centered-cubic (bcc) Ti-Nb alloy. For each grain, scratch tests were conducted at four different levels of normal load, which resulted in varying amounts of plastic strain during indentation. The results show a dependence of the horizontal load component on the crystallographic orientation and on the amount of plastic strain. The component of the horizontal force that resulted from plastic deformation was found to correlate with the active slip systems for the particular grain orientation. © 2010 Materials Research Society.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

The increasing demand for high capacity data storage requires decreasing the head-to-tape gap and reducing the track width. A problem very often encountered is the development of adhesive debris on the heads at low humidity and high temperatures that can lead to an increase of space between the head and media, and thus a decrease in the playback signal. The influence of stains on the playback signal of reading heads is studied using RAW (Read After Write) tests and their influence on the wear of the heads by using indentation technique. The playback signal has been found to vary and the errors to increase as stains form a patchy pattern and grow in size to form a continuous layer. The indentation technique shows that stains reduce the wear rate of the heads. In addition, the wear tends to be more pronounced at the leading edge of the head compared to the trailing one. Chemical analysis of the stains using ferrite samples in conjunction with MP (metal particulate) tapes shows that stains contain iron particles and polymeric binder transferred from the MP tape. The chemical anchors in the binder used to grip the iron particles now react with the ferrite surface to create strong chemical bonds. At high humidity, a thin layer of iron oxyhydroxide forms on the surface of the ferrite. This soft material increases the wear rate and so reduces the amount of stain present on the heads. The stability of the binder under high humidity and under high temperature as well as the chemical reactions that might occur on the ferrite poles of the heads influences the dynamic behaviour of stains. A model of stain formation taking into account the channels of binder degradation and evolution upon different environmental conditions is proposed.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

      This thesis examines the mechanism of wear occuring to the video head and their effect on signal reproduction. in particular it examines the wear occuring to manganese-zinc ferrite heads in sliding contact with iron oxide media.       A literature survey is presented, which covers magnetic recording technologies, focussing on video recording. Existing work on wear of magnetic heads is also examined, and gaps in the theoretical account of wear mechanisms presented in the literature are identified.       Pilot research was carrried out on the signal degradation and wear associated witha number of commercial video tapes, containing a range of head cleaning agents. From this research, the main body of the research was identified. A number of methods of wear measurement were examined for use in this project. Knoop diamond indentation was chosen because experimentation showed it to be capable of measuring wear occuring in situ. This technique was then used to examine the wear associated with different levels of A12O3 and Cr2O3 head cleaning agents.      The results of the research indicated that, whilst wear of the video head increases linearly with increasing HCA content, signal degradation does not vary significantly. The most significant differences in wear and signal reproduction were observed between the two HCAs. The signal degradation of heads worn with tape samples containing A12O3 HCA was found to be lower than heads worn with tapes containing Cr2O3 HCA.      The results also indicate that the wear to the head is an abrasive process characterised by ploughing of the ferrite surface and chipping of the edges of the head gap. Both phenomena appear to be caused by poor iron oxide and head cleaning particles, which create isolated asperities on the tape surface.   

Relevância:

10.00% 10.00%

Publicador:

Resumo:

This study demonstrates a novel approach to characterizing hydrated bone's viscoelastic behavior at lamellar length scales using dynamic indentation techniques. We studied the submicron-level viscoelastic response of bone tissue from two different inbred mouse strains, A/J and B6, with known differences in whole bone and tissue-level mechanical properties. Our results show that bone having a higher collagen content or a lower mineral-to-matrix ratio demonstrates a trend towards a larger viscoelastic response. When normalized for anatomical location relative to biological growth patterns in the antero-medial (AM) cortex, bone tissue from B6 femora, known to have a lower mineral-to-matrix ratio, is shown to exhibit a significantly higher viscoelastic response compared to A/J tissue. Newer bone regions with a higher collagen content (closer to the endosteal edge of the AM cortex) showed a trend towards a larger viscoelastic response. Our study demonstrates the feasibility of this technique for analyzing local composition-property relationships in bone. Further, this technique of viscoelastic nanoindentation mapping of the bone surface at these submicron length scales is shown to be highly advantageous in studying subsurface features, such as porosity, of wet hydrated biological specimens, which are difficult to identify using other methods. © 2010 Elsevier Ltd.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Progressive tissue fibrosis is involved in debilitating diseases that affect organs including the lungs, liver, heart, skin, and kidneys. Recent evidence suggests that tissue transglutaminase, an enzyme that crosslinks proteins, may be involved in tissue fibrosis by crosslinking and stabilizing the extracellular matrix or by recruiting and activating the large latent transforming growth factor (TGF)-β1 complex. We treated rats that had undergone 5/6-nephrectomy with two different irreversible inhibitors of transglutaminase and found that both prevented a decline in kidney function and reduced the development of glomerulosclerosis and tubulointerstitial fibrosis by up to 77% and 92%, respectively. Treatment reduced the accumulation of collagen I and collagen III, with the primary mechanism of action being direct interference with the crosslinking of extracellular matrix rather than altered regulation of TGFβ1. We conclude that inhibition of transglutaminase offers a potential therapeutic option for chronic kidney disease and other conditions that result from tissue fibrosis. Copyright © 2007 by the American Society of Nephrology.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

The development of new products in today's marketing environment is generally accepted as a requirement for the continual growth and prosperity of organisations. The literature is consequently rich with information on the development of various aspects of good products. In the case of service industries, it can be argued that new service product development is of as least equal importance as it is to organisations that produce tangible goods products. Unlike the new goods product literature, the literature on service marketing practices, and in particular, new service product development, is relatively sparse. The main purpose of this thesis is to examine a number of aspects of new service product development practice with respect to financial services and specifically, credit card financial services. The empirical investigation utilises both a case study and a survey approach, to examine aspects of new service product development industry practice relating specifically to gaps and deficiencies in the literature with respect to the financial service industry. The findings of the empirical work are subsequently examined in the context in which they provide guidance and support for a new normative new service product development model. The study examines the UK credit card financial service product sector as an industry case study and perspective. The findings of the field work reveal that the new service product development process is still evolving, and that in the case of credit card financial services can be seen as a well-structured and well-documented process. New product development can also be seen as an incremental, complex, interactive and continuous process which has been applied in a variety of ways. A number of inferences are subsequently presented.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

An investigation has been undertaken to determine the major factors influencing the corrosion resistance of duplex-zinc coatings on steel substrates.Premature failure of these systems has been attributed to the presence of defects such as craters and pinholes in the polymer film and debonding of the polymer film from the zinc substrate.Defects found on commercially produced samples have been carefully characterised using metallographic and scanning electron microscopy techniques. The influence of zinc substrate surface roughness, polymer film thickness and degassing of conversion coatings films on the incidence of defects has been determined.Pretreatments of the chromate, chromate-phosphate, non chromate, and alkali-oxide types were applied and the conversion coatings produced characterised with respect to their nature and composition. The effect of degassing on the properties of the films was also investigated. Electrochemical investigations were carried out to determine the effect of the presence of the eta or zeta phase as the outermost layer of the galvanized coating.Flow characteristics of polyester on zinc electroplated hot-dip continuous and batch galvanized and zinc sprayed samples were investigated using hot-stage microscopy. The effects of different pretreatments and degassing after conversion coating formation on flow characteristics were determined.Duplex coatings were subjected to the acetic acid salt spray test. The effect on adhesion was determined using an indentation debonding test and the results compared with those obtained using cross-cut/peel and pull-off tests. The locus of failure was determined using scanning electron microscopy and X-ray photoelectron spectroscopy techniques.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

The structure and thermal properties of yttrium alumino-phosphate glasses, of nominal composition (Y2O3)(0.31-z)(Al2O3)(z)(P2O5)(0.69) with 0 less than or similar to z less than or similar to 0.31, were studied by using a combination of neutron diffraction, Al-27 and P-31 magic angle spinning nuclear magnetic resonance, differential scanning calorimetry and thermal gravimetric analysis methods. The Vickers hardness of the glasses was also measured. The data are compared to those obtained for pseudo-binary Al2O3-P2O5 glasses and the structure of all these materials is rationalized in terms of a generic model for vitreous phosphate materials in which Y3+ and Al3+ act as modifying cations that bind only to the terminal (non-bridging) oxygen atoms of PO4 tetrahedra. The results are used to help elucidate the phenomenon of rare-earth clustering in phosphate glasses which can be reduced by substituting Al3+ ions for rare-earth R3+ ions at fixed modifier content.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

The principle theme of this thesis is the advancement and expansion of ophthalmic research via the collaboration between professional Engineers and professional Optometrists. The aim has been to develop new and novel approaches and solutions to contemporary problems in the field. The work is sub divided into three areas of investigation; 1) High technology systems, 2) Modification of current systems to increase functionality, and 3) Development of smaller more portable and cost effective systems. High Technology Systems: A novel high speed Optical Coherence Tomography (OCT) system with integrated simultaneous high speed photography was developed achieving better operational speed than is currently available commercially. The mechanical design of the system featured a novel 8 axis alignment system. A full set of capture, analysis, and post processing software was developed providing custom analysis systems for ophthalmic OCT imaging, expanding the current capabilities of the technology. A large clinical trial was undertaken to test the dynamics of contact lens edge interaction with the cornea in-vivo. The interaction between lens edge design, lens base curvature, post insertion times and edge positions was investigated. A novel method for correction of optical distortion when assessing lens indentation was also demonstrated. Modification of Current Systems: A commercial autorefractor, the WAM-5500, was modified with the addition of extra hardware and a custom software and firmware solution to produce a system that was capable of measuring dynamic accommodative response to various stimuli in real time. A novel software package to control the data capture process was developed allowing real time monitoring of data by the practitioner, adding considerable functionality of the instrument further to the standard system. The device was used to assess the accommodative response differences between subjects who had worn UV blocking contact lens for 5 years, verses a control group that had not worn UV blocking lenses. While the standard static measurement of accommodation showed no differences between the two groups, it was determined that the UV blocking group did show better accommodative rise and fall times (faster), thus demonstrating the benefits of the modification of this commercially available instrumentation. Portable and Cost effective Systems: A new instrument was developed to expand the capability of the now defunct Keeler Tearscope. A device was developed that provided a similar capability in allowing observation of the reflected mires from the tear film surface, but with the added advantage of being able to record the observations. The device was tested comparatively with the tearscope and other tear film break-up techniques, demonstrating its potential. In Conclusion: This work has successfully demonstrated the advantages of interdisciplinary research between engineering and ophthalmic research has provided new and novel instrumented solutions as well as having added to the sum of scientific understanding in the ophthalmic field.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

We conducted nanoindentation to explore the hardness and elastic properties of silica stishovite, synthesized at high pressure and quenched to ambient conditions. A total of 10 crystallographic orientations were examined on selected grains with a maximum load of 4 or 20 mN. We observed discontinuity in the load-displacement curve (pop-in) for the [2 5 over(1, -)] and [6 2 over(1, -)] grains subjected to a maximum load of 20 mN. The single-crystal hardness at high plastic deformation is quasi-isotropic with an average of 32 ± 1 GPa, similar to the polycrystalline hardness reported earlier; the theoretical hardness determined from the experiments is about 54 ± 3 GPa. These two hardnesses suggest that stishovite is one of the hardest oxides. The measured indentation moduli are close to the predictions at low load (minor plasticity) but are considerably lower at high load (high plasticity). Both indentation hardness and modulus decrease with increasing plasticity. Our results underscore the necessity of considering the degree of plastic deformation when interpreting hardness and elastic moduli from indentation experiments. © 2007 Elsevier B.V. All rights reserved.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

A three-dimensional finite element analysis (FEA) model with elastic-plastic anisotropy was built to investigate the effects of anisotropy on nanoindentation measurements for cortical bone. The FEA model has demonstrated a capability to capture the cortical bone material response under the indentation process. By comparison with the contact area obtained from monitoring the contact profile in FEA simulations, the Oliver-Pharr method was found to underpredict or overpredict the contact area due to the effects of anisotropy. The amount of error (less than 10% for cortical bone) depended on the indentation orientation. The indentation modulus results obtained from FEA simulations at different surface orientations showed a trend similar to experimental results and were also similar to moduli calculated from a mathematical model. The Oliver-Pharr method has been shown to be useful for providing first-order approximations in the analysis of anisotropic mechanical properties of cortical bone, although the indentation modulus is influenced by anisotropy.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Mechanistic models based on geometrically necessary dislocations are re-examined in light of recent experiments exhibiting the indentation size effect. A simple method is developed to combine work hardening, solid solution hardening, radiation hardening and size effects. The model is verified by experiments in ionic salt crystals. © 2002 Acta Materialia Inc. Published by Elsevier Science Ltd. All rights reserved.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

The purpose of this study was to investigate the effects of elastic anisotropy on nanoindentation measurements in human tibial cortical bone. Nanoindentation was conducted in 12 different directions in three principal planes for both osteonic and interstitial lamellae. The experimental indentation modulus was found to vary with indentation direction and showed obvious anisotropy (oneway analysis of variance test, P < 0.0001). Because experimental indentation modulus in a specific direction is determined by all of the elastic constants of cortical bone, a complex theoretical model is required to analyze the experimental results. A recently developed analysis of indentation for the properties of anisotropic materials was used to quantitatively predict indentation modulus by using the stiffness matrix of human tibial cortical bone, which was obtained from previous ultrasound studies. After allowing for the effects of specimen preparation (dehydrated specimens in nanoindentation tests vs. moist specimens in ultrasound tests) and the structural properties of bone (different microcomponents with different mechanical properties), there were no statistically significant differences between the corrected experimental indentation modulus (Mexp) values and corresponding predicted indentation modulus (Mpre) values (two-tailed unpaired t-test, P < 0.5). The variation of Mpre values was found to exhibit the same trends as the corrected Mexp data. These results show that the effects of anisotropy on nanoindentation measurements can be quantitatively evaluated. © 2002 Orthopaedic Research Society. Published by Elsevier Science Ltd. All rights reserved.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Many biological materials are known to be anisotropic. In particular, microstructural components of biological materials may grow in a preferred direction, giving rise to anisotropy in the microstructure. Nanoindentation has been shown to be an effective technique for determining the mechanical properties of microstructures as small as a few microns. However, the effects of anisotropy on the properties measured by nanoindentation have not been fully addressed. This study presents a method to account for the effects of anisotropy on elastic properties measured by nanoindentation. This method is used to correlate elastic properties determined from earlier nanoindentation experiments and from earlier ultrasonic velocity measurements in human tibial cortical bone. Also presented is a procedure to determine anisotropic elastic moduli from indentation measurements in multiple directions. © 2001 John Wiley & Sons, Inc. J Biomed Mater Res.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Single crystal Mo3Si specimens were grown and tested at room temperature using established nanoindentation techniques at various crystallographic orientations. The indentation modulus and hardness were obtained for loads that were large enough to determine bulk properties, yet small enough to avoid cracking in the specimens. From the indentation modulus results, anisotropic elastic constants were determined. As load was initially increased to approximately 1.5 mN, the hardness exhibited a sudden drop that corresponded to a jump in displacement. The resolved shear stress that was determined from initial yielding was 10-15% of the shear modulus, but 3 to 4 times the value obtained from the bulk hardness. Non-contact atomic force microscopy images in the vicinity of indents revealed features consistent with {100}(010) slip.