983 resultados para JPEG-LS


Relevância:

10.00% 10.00%

Publicador:

Resumo:

Luminescent hybrid Langmuir-Blodgett (LB) films of polyoxometaloeuropate (Na9EuW10O36) were successfully prepared. Low-angle X-ray diffraction data demonstrate that the LB films have a well-defined lamellar structure. The hybrid LB films can exhibit strong luminescence under UV irradiation, which can be observed by the human eye. The effect of the lipid ocradecylamine, on the luminescence of polyoxometaloeuropate was discussed and compared with that of the lipid dimethyldioctadecylammonium bromide. It is found that the intensity ratio for the D-5(0) --> F-7(2) transition to the D-5(0) --> F-7(1) transition of europium in two kinds of LB films is quite different. The X-ray photoelectron spectra data verify that there exist different interactions between two lipids and the inorganic polyanions. The different interactions between two lipids and the polyanions may result in the distortion of the site symmetry for europium to a different extent, which may account for the difference in luminescent behavior between the two kinds of LB films.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Viscosities of aqueous solutions of five polyethylene oxide (PEO) samples with molar masses from 1.5 x 10(5) to 1.0 x 10(6) were carefully measured in a polytetrafluoroethylene (PTFE) capillary Ubbelohde viscometer in the concentration range from dilute down to extremely dilute concentration regions and compared with those of the same sample obtained from a glass capillary viscometer. At the same time, viscosities of aqueous solutions of three PEG samples in glass and paraffin-coated capillary viscosity were measured. The wall effects occurred in viscosity measurements for PEO and PEG aqueous solutions in different capillary viscometers were theoretically analyzed and discussed. It was found that different interfacial behaviors occurred in both hydrophobic and hydrophilic capillary viscometers respectively and the interfacial behaviors also exhibit molar mass dependence.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

The near-infrared (NIR) luminescent lanthanide ions, such as Er(III), Nd(III), and Yb(III), have been paid much attention for the potential use in the optical communications or laser systems. For the first time, the NIR-luminescent Ln(dbm)(3)phen complexes have been covalently bonded to the ordered mesoporous materials MCM-41 and SBA-15 via a functionalized phen group phen-Si (phen-Si = 5-(N,N-bis-3-(triethoxysilyl)propyl)ureyl-1,10-phenanthroline; dbm = dibenzoylmethanate; Ln = Er, Nd, Yb). The synthesis parameters X = 12 and Y = 6 h (X denotes Ln(dbM)(3)(H2O)(2)/phen-MCM-41 molar ratio or Ln(dbM)(3)(H2O)(2)/phenSBA-15 molar ratio and Y is the reaction time for the ligand exchange reaction; phen-MCM-41 and phenSBA-15 are phen-functionalized MCM-41 and SBA-15 mesoporous materials, respectively) were selected through a systematic and comparative study. The derivative materials, denoted as Ln(dbM)(3)phen-MCM-41 and Ln(dbm)(3)phen-SBA-15 (Ln = Er, Nd, Yb), were characterized by powder X-ray diffraction, nitrogen adsorption/desorption, Fourier transform infrared (FT-IR), elemental analysis, and fluorescence spectra. Upon excitation of the ligands absorption bands, all these materials show the characteristic NIR luminescence of the corresponding lanthanide ions through the intramolecular energy transfer from the ligands to the lanthanide ions.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Bisphenol A solid epoxy serves as an effective reaction compatibilizer to the bisphenol A polycarbonate (PC)/PMMA bilayer systems. Addition of epoxy to the bottom PMMA layer can retard or even prevent the dewetting of PC films by introducing crosslinking between both components at the interface. This is the first investigation of polymer bilayers stabilized by chemical reactions.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

The ligand Hhfth [4,4,5,5,6,6,6-heptafluoro-1-(2-thienyl)hexane-1,3-dione], which contains a heptafluoropropyl group, has been used to synthesize several new ternary lanthanide complexes (Ln = Er, Ho, Yb, Nd) in which the synergistic ligand is 1,10-phenanthroline (phen) or 2,2'-bipyridine (bipy). The two series of complexes are [Ln(hfth)(3)phen] [abbreviated as (Ln)1, where Ln = Er, Ho, Yb] and [Ln(hfth)(3)bipy] [abbreviated as (Ln)2, where Ln = Er, Ho, Yb, Nd]. Members of the two series have been structurally characterized. The growth morphology, diffuse reflectance (DR) spectra, thermogravimetric analyses, and photophysical studies of these complexes are described in detail. After ligand-mediated excitation of the complexes, they all show the characteristic near-infrared (NIR) luminescence of the corresponding Ln(3+) ions (Ln = Er, Ho, Yb, Nd). This is attributed to efficient energy transfer from the ligands to the central Ln(3+) ions, i.e. an antenna effect. The heptafluorinated substituent in the main hfth sensitizer serves to reduce the degree of vibrational quenching. With these NIR-luminescent lanthanide complexes, the luminescent spectral region from 1300 to 1600 nm, which is of particular interest for telecommunication applications, can be covered completely.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Intermolecular hydrogen bonds, miscibility, crystallization and thermal stability of the blends of biodegradable poly(3-hydroxybutyrate) (PHB), poly(3-hydroxybutyrate-co-3-hydroxyhexanoate) [P(3HB-3HHx)] with 4,4-dihydroxydiphenylpropane (DOH2) were investigated by FTIR, C-13 Solid state NMR, DSC, WAXD and TGA. Intermolecular hydrogen bonds were found in both blend systems, which resulted from the carbonyl groups in the amorphous phase of both polyesters and the hydroxyl groups of DOH2. The intermolecular interaction between P(3HB-3HHx) and DOH2 is weaker than that between PHB and DOH2 owing to the steric hindrance of longer 3HHx side chains. Because of the effect of the hydrogen bonds, the chain mobility of both PHB and P(3HB-3HHx) components was limited after blending with DOH2 molecules. Single glass transition temperature depending on the composition was observed in all blends, indicating that those blends were miscible in the melt. The addition of DOH2 suppressed the crystallization of PHB and P(3HB-3HHx) components. Moreover, the crystallinity of PHB and P(3HB-3HHx) components also decreased with increasing DOH2 content in the blends.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

The surface and interface morphologies of polystyrene (PS)/poly(methyl methacrylate) (PMMA) thin-film blends and bilayers were investigated by means of atomic force microscopy (AFM) and X-ray photoelectron spectroscopy. Spin-coating a drop of a PS solution directly onto a PMMA bottom layer from a common solvent for both polymers yielded lateral domains that exhibited a well-defined topographical structure. Two common solvents were used in this study. The structure of the films changed progressively as the concentration of the PS solution was varied. The formation of the blend morphology could be explained by the difference in the solubility of the two polymers in the solvent and the dewetting of PS-rich domains from the PMMA-rich phase. Films of the PS/PMMA blend and bilayer were annealed at temperatures above their glass-transition temperatures for up to 70 h. All samples investigated with AFM were covered with PS droplets of various size distributions. Moreover, we investigated the evolution of the annealed PS/PMMA thin-film blend and bilayer and gave a proper explanation for the formation of a relatively complicated interface inside a larger PS droplet.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

The electrochemical polymerization of 0.01 M aniline in 1 M H2SO4 aqueous solution on roughened Au surface modified with a self-assembled monolayer (SAM) of 4-aminothiophenol (4-ATP) has been investigated by in situ electrochemical surface-enhanced Raman scattering spectroscopy (SERS). The repeat units and possible structures of the electrodeposited polyaniline (PANI) film were proposed; i.e., aniline monomer is coupled in head-to-tail predominately at the C-4 of aniline and amine of 4-ATP, and the thin PANI film is orientated vertically to substrate surface. Simultaneous Raman spectra during potential scanning indicate clearly that the ultrathin PANI film (in initial growth of the film) consists of semiquinone radical cation (IP+), para-disubstituted benzene (IP and IP+) and quinine diimine (NP) while it is oxidized, and without quinine diimine and semiquinone radical cation while reduced. Meanwhile, the results confirm that 4-ATP monolayer shows a strong promotion on the electrodeposition of aniline monomer, and a possible polymerization mechanism was proposed.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

The blends of low molecular weight triacetin (TAC) and oligomeric poly(1,3-butylene glycol adipate) (PBGA) were used as multiple plasticizers to lubricate poly(lactic acid) (PLA) in this study. The thermal and mechanical properties of plasticized polymers were investigated by means of dynamic mechanical analysis and differential scanning calorimetry. Atomic force microscopy (AFM) was used to analyze the morphologies of the blends. Multiple plasticizers were effective in lowering the glass transition temperature (T-g) and the melting temperature (T-m) of PLA. Moreover, crystallinity of PLA increased with increasing the con-tent of multiple plasticizers. Tensile strength of the blends decreased following the increasing of the plasticizers, but increased in elongation at break. AFM topographic images showed that the multiple plasticizers dispersed between interfibrillar regions. Moreover, the fibrillar crystallite formed the quasicrosslinkings, which is another cause for the increase in elongation at break.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Polymerizing 1,3-butadiene into syndiotactic 1,2-polybutadiene with art iron(III) catalyst system has been investigated. Activity of the catalyst was affected by the type of cocatalyst alkylaluminum and the phosphorus compound as an electron donor, molar ratio of catalyst components, and their aging sequence and aging time of the catalyst. The microstructure and configuration of the polymer was decided by the catalyst components, the higher [Al]/[Fe] molar ratio tending to yield syndiotactic 1,2-polybutadiene, while the higher [P]/[Fe] molar ratio favors the formation of amorphous 1,2-polybutadiene.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

In the title compound, C16H13NO4S, the phthalimide ring system makes a dihedral angle of 56.7 (1)degrees with the phenyl ring.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

FTIR spectroscopy was used to verify the presence of intermolecular hydrogen bond (inter-H-bond) between poly-(3-hydroxybutyrate co-3-hydroxyvalerate) (PHBV) and bisphenol A (BPA). By monitoring the spectral changes during PHBV crystallization and blends dissociation, the absorptivity ratio of C=O bonds in crystalline and amorphous regions in PHBV and that of H-bonded and free C=O in PHBV/BPA blends were experimentally determined as 1.40 and 1.68, respectively. Using curve-fitting program, the C=O absorptions in spectra of blends were ascribed to three types of bonds: amorphous, crystalline and H-bonded C=O. The crystallinity of PHBV and the fraction of H-bonded C=O were calculated. These results indicated that the H-bond clearly suppressed the PHBV crystallization. Furthermore, the fraction of BPA molecules that simultaneously formed two hydrogen bonds (H-bonds) with C=O was estimated. It revealed that there existed a H-bond network in PHBV/BPA blends. This network was compared with the covalent network by estimating the number of atoms between every two adjacent crosslink points in chain. Up to the high density of H-bond discussed in this paper, there was always a certain part in PHBV that crystallized due to the dynamic character of hydrogen bonds; however, the hydrogen bonds significantly reduced the crystallization rate of PHBV.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Graft copolymerization of maleic anhydride (MA) onto poly(3-hydroxybutyrate) (PHB) was carried out by use of benzoyl peroxide as initiator. The effects of various polymerization conditions on graft degree were investigated, including solvents, monomer and initiator concentrations, reaction temperature, and time. The monomer and initiator concentrations played an important role in graft copolymerization, and graft degree could be controlled in the range from 0.2 to 0.85% by changing the reaction conditions. The crystallization behavior and the thermal stability of PHB and maleated PHB were studied by DSC, WAXD, optical microscopy, and TGA. The results showed that, after grafting MA, the crystallization behavior of PHB was obviously changed. The cold crystallization temperature from the glass state increased, the crystallization temperature from the melted state decreased, and the growth rate of spherulite decreased. With the increase in graft degree, the banding texture of spherulites became more distinct and orderly. Moreover, the thermal stability of maleated PHB was obviously improved, compared with that of pure PHB.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Isothermal crystallization behavior of poly(3-hydroxybutyrate-co-3-hydroxyvalerate) (PHBV) was investigated by means of differential scanning calorimetry and polarized optical microscopy (POM). The Avrami analysis can be used successfully to describe the isothermal crystallization kinetics of PHBV, which indicates that the Avrami exponent n = 3 is good for all the temperatures investigated. The spherulitic growth rate, G, was determined by POM. The result shows that the G has a maximum value at about 353 K. Using the equilibrium melting temperature (448 K) determined by the Flory equation for melting point depression together with U-* = 1500 cal mol(-1), T-infinity = 30 K and T-g = 278 K, the nucleation parameter K-g was determined, which was found to be 3.14+/-0.07 x 10(5) (K-2), lower than that for pure PHB. The surface-free energy sigma = 2.55 x 10(-2) J m(-2) and sigma(e) = 2.70+/-0.06 x 10-2 J m(-2) were estimated and the work of chain-folding (q = 12.5+/-0.2 kJ mol(-1)) was derived from sigma(e), and found to be lower than that for PHB. This implies that the chains of PHBV are more flexible than that of PHB.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

In order to improve its thermal stability, poly(propylene carbonate)(PPC) was end-capped by different active agents. Thermogravimetric data show that the degradation temperature of uncapped PPC was lower than that of end-capped PPC. The kinetic parameters of thermal degradation of uncapped and end-capped PPC were calculated according to Chang's method. The results show that different mechanisms operate during the whole degradation temperature range for uncapped PPC. In the first stage, chain unzipping dominates the degradation. With increasing temperature, competing multi-step reactions occur. In the last stage, random chain scission plays an important role in degradation. For end-capped PPC, random chain scission dominates the whole degradation process.