903 resultados para BLENDS


Relevância:

10.00% 10.00%

Publicador:

Resumo:

Communication: Conducting semi-interpenetrating network composites with low conductivity percolation threshold were synthesized from waterborne conducting polyaniline (cPAn) and melamine-urea resin, A perfect network of cPAn in the composite was observed by means of TEM (see Figure). The conductivity stability of cPAn in water was improved by confining the chain mobility of cPAn via in-situ crosslinking of melamine-urea resin. Cyclic voltammetry of the composites reveals electrochemical activities and reversibilities similarly to those of pure cPAn.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

A series of novel nitrogen- and sulfur-containing conjugated polymers with well-defined conjugation length have been synthesized via an acid-induced self-polycondensation of functional monomers with methylsulfinyl groups. Synthesized polymers exhibit good solubility in common solvents, such as CHCl3, THF, DMF, DMSO, and NMP. With increased numbers of aminophenyl groups, these polymers have shown similar electrical properties to polyaniline (PAn), and these are demonstrated by UV-vis spectroscopy and cyclic voltammetry (CV) measurements on the polymers. The conductivity of preliminarily protonic-doped poly[phenylene sulfide-alt-tetrakis(aniline)] (PPSTEA) is up to 10(-1) S cm(-1).

Relevância:

10.00% 10.00%

Publicador:

Resumo:

In this study, we established a correlation between cavitations volume and the brittle-ductile transition (BDT) for particle toughened thermoplastics. The brittle-ductile transition temperature (T-BD) was calculated as a function of T* and interparticle distance (ED), respectively, where T* was a parameter related to the volume of cavitations. The results showed that the smaller the cavitations volume, the higher the brittle-ductile transition temperature. The calculations correlated well with the experimental data. With respect to rubber particle, the rigid particle was too hard to be voided during deformation, thereby the TED of the blend was much higher than that of rubber particle toughened thermoplastic. This was a main reason that rubber particle could toughen thermoplastics effectively, whereas rigid particle could not.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Nanometre-sized poly(vinylidene fluoride) (PVDF) particle domains in a confined space were obtained by blending PVDF with excess poly(methyl methacrylate) (PMMA). When these particles were small enough they showed beta -form structure, which was different from the structure of bigger particles or PVDF bulk. However, the beta -form was thermodynamically metastable because it could eventually be transformed to a more stable phase by annealing at a certain temperature. Larger particle domains were of identical phase to the bulk, indicating that small size favours the formation of the beta -form. (C) 2000 Society of Chemical Industry.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Polyamide (PA)1010 is blended with a saturated polyolefin elastomer, ethylene-cu-olefin copolymer (EOCP). To improve the compatibility of PA1010 with EOCP, different grafting rates of EOCP with maleic anhydride (MA) are used. The reaction between PA1010 and EOCP-g-MA during extrusion is verified through an extraction test. Mechanical properties, such as notched Izod impact strength, elongation at break, etc., are examined as a function of grafting rate and weight fraction of elastomer. It was found that in the scale of grafting rate (0.13-0.92 wt %), 0.51 wt % is an extreme point for several mechanical properties. Elastomer domains of PA1010/ EOCP-g-MA blends show a finer and more uniform dispersion in the matrix than that of PA1010/EOCP blends. For the same grafting rate, the average sizes of elastomer particles are almost independent on the contents of elastomer, but for different grafting rates, the particle sizes are decreased with increasing grafting rate. The copolymer formed during extrusion strengthens the interfacial adhesion and acts as an emulsifier to prevent the aggregation of elastomer in the process of blending. (C) 2000 John Wiley & Sons, Inc.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

This paper studies the radiation properties of the immiscible blend of nylon1010 and HIPS. The gel fraction increased with increasing radiation dose. The network was found mostly in nylon1010, the networks were also found in both nylon1010 and HIPS when the dose reaches 0.85 MGy or more. We used the Charleby-Pinner equation and the modified Zhang-Sun-Qian equation to simulate the relationship with the dose and the sol fraction. The latter equation fits well with these polymer blends and the relationship used by it showed better linearity than the one by the Charleby-Pinner equation. We also studied the conditions of formation of the network by the mathematical expectation theorem for the binary system. Thermal properties of polymer blend were observed by DSC curves. The crystallization temperature decreases with increasing dose because the cross-linking reaction inhibited the crystallization procession and destroyed the crystals. The melting temperature also reduced with increasing radiation dose. The dual melting peak gradually shifted to single peak and the high melting peak disappeared at high radiation dose. However, the radiation-induced crystallization was observed by the heat of fusion increasing at low radiation dose. On the other hand, the crystal will be damaged by radiation. A similar conclusion may be drawn by the DSC traces when the polymer blends were crystallized. When the radiation dose increases, the heat of fusion reduces dramatically and so does the heat of crystallization. (C) 1999 Elsevier Science Ltd. All rights reserved.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Isotactic polypropylene in its a modification (alpha iPP) crystallises epitaxially on polytetrafluoroethylene (PTFE) and several hemiacids or salts of substituted benzoic acids via a novel contact plane, namely (110): so far, the only known contact plane involved in alpha iPP homo- and hetero-epitaxies was (010). In spite of its complicated architecture (alternation of antichiral helices with different azimuthal settings), the (110)(alpha iPP) contact plane displays well defined, if not prominent, rows of methyl side chains parallel to the crystallographic (112) direction (at 57 degrees to the c-axis) and approximate to 5.5 Angstrom apart. The matching contact planes of the substrates display linear gratings made of rows of e.g. chlorine atoms or PTFE chains with similar approximate to 5.5 Angstrom inter-row or interchain distances. Various morphologies are observed in iPP thin films crystallised at different cooling rates in the presence of PTFE; they can be analysed in terms of a succession and interplay of successive epitaxies: initial alpha iPP/PTFE heteroepitaxy, followed by alpha iPP/alpha iPP and gamma iPP/alpha iPP homoepitaxies. (C) 1999 Published by Elsevier Science Ltd. All rights reserved.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Poly(ethylene oxide) (PEO) and silica (SiO2) organic-inorganic hybrid materials have been synthesized by sol-gel approach. The crystallization behavior of PEO in silica networks has been investigated by differential scanning calorimeter (DSC) and scanning electron micrograph (SEM). The degree of PEO crystallinity in PEO/SiO2 hybrid networks reduces with the increase of SiO2. PEO is in amorphous state when the concentration of PEO is lower than 50 wt% in the hybrid materials. The melting points of PEO in the networks are lower than that of pure PEG, but the melting point of PEO in the networks almost has the same melting point. WAXD and SEM results show that the crystalline behavior of PEO in PEO/SiO2 hybrid system is sternly confined. (C) 1999 Elsevier Science Ltd. All rights reserved.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

A novel conducting polymer poly(phenylene sulfide-tetraaniline) (PPSTEA), with tetraaniline (TA) and phenylene sulfide (PS) segments in its repeat unit, has been synthesized through an acid-induced polycondensation reaction of 4-methylsulfinylphenyl-capped tetraaniline. The new polymer, which represents the first soluble conducting polyaniline analogue with well-defined structure, has high molecular weight, good solubility in common solvents, and good film-forming properties. Its electrical property is analogous to polyaniline. The conductivity of preliminarily, protonic-doping PPSTEA is up to 10 degrees S/cm. This synthetic strategy appears to be general for developing novel well-defined polyaniline analogue containing much longer fixed conjugation length.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

A hybrid material with a conductive organic network in an inorganic matrix has been prepared by in-situ hydrolysis/polycondensation of TEOS in an aqueous solution of a solubilized polyaniline. Due to intense hydrogen bonding (indicated by Si-29 NMR and FTIR) the conductive polymer is very well dispersed in the silica matrix. The Figure shows SEM images of a 46/54 wt.-% hybrid at two temperatures (left 20 degreesC, right 100 degreesC).

Relevância:

10.00% 10.00%

Publicador:

Resumo:

The homoepitaxial crystallization in the films of a thermotropic liquid crystalline chloro-ply(aryl ether ketone) is studied by transmission electron microscopy (TEM) and electron diffraction (ED). The homoepitaxy takes place in the temperature range 330-320 degreesC, in which a highly-ordered smectic crystalline phase of the copolymer with a single-crystal-like banded structure is formed during the cooling process from the isotropic melt. The homoepitaxial crystallizations with angles of 32 degrees and 122 degrees between the two b axes are the major populations observed, and possess epitaxial contact planes of (100)(I)-(210)(II) and (010)(I)-(210)(II); respectively.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

The thermal stability, crystallization behavior and biodegradability of poly(beta -hydroxybutyrate) (PHB) grafted with maleic anhydride (MA) were studied by DSC,TGA, optical microscopy and WAXD. The results showed that thermal stability of maleated PHB was obviously improved, comparing with that of pure PHB. The temperature of decomposition was enhanced about 20 degreesC After grafting MA, the crystallization behavior of PHB changed evidently. The rate of spherulite growth decreased, the crystallization temperature from the melt state reduced, and the cold crystallization temperature from the glass state increased. With the increase in graft degree, the banding texture of spherulite became more distinct and orderly. Moreover, the introduction of MA groups promoted the biodegradation of PHB.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

The nonisothermal crystallization behavior of polyethylene oxide (PEO) in poly(ethylene terephthalate)poly(ethylene oxide) (PETPEO) segmented copolymer and PEO homopolymer has been studied by means of differential scanning calorimetry, as well as transmission electron microscope. The kinetics of PEO in copolymer and PEO homopolymer under nonisothermal crystallization condition has been analyzed by Ozawa equation. The results show that Ozawa equation only describes the crystallization behavior of PEO-6000 homopolymer successfully, but fails to describe the whole crystallization process of PEO in copolymer because the secondary crystallization in the later stage could not be neglected. Due to the constraint of PET segments imposed on the PEO segments, a distinct two stage of crystallization of PEO in copolymer has been investigated by using Avrami equation modified by Jeziorny to deal with the nonisothermal crystallization data. In the case of PEO-6000 homopolymer, good linear relation for the whole crystallization process is obtained owing to the secondary crystallization does not occur under our experimental condition. (C) 2001 Elsevier Science Ltd. All rights reserved.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

In this paper, blends of Nylon 6,6 with the liquid crystal polymer Vectra A950 are considered; specifically we focused our attention on Nylon 6,6 modifications by interchange reactions that can occur in the melt, as a function of mixing conditions and blend compositions. Two matrix samples have been used, characterised by a slightly different relative amount of amine and carboxylic end groups, being the latter predominant in both cases. The dried polymers Nylon 6,6/Vectra, combined in weight ratios between 95/5 and 50/50, were subjected to reactive blending with different methods (single-screw extruder, Brabender, pyrex reactor). Pure Nylon samples have been also investigated as reference materials. The soluble Nylon 6,6-rich fraction of each blend was separated from the insoluble Vectra-rich one and used for molecular and spectroscopic characterisations. Thermal and morphological analyses, as well as testing of tensile properties, were carried out on the blends. Evidences of the occurrence of interchange reactions are given and the most probable ones are suggested. (C) 2001 Elsevier Science Ltd. All rights reserved.