Nanoindentation and nanoscratch tests were performed for titanium nitride (TiN) coatings on different tool steel substrates to investigate the indentation/scratch induced deformation behavior of the coatings and the adhesion of the coating–substrate interfaces and their tribological property. In this work, TiN coatings with a thickness of about 500 nm were grown on GT35, 9Cr18 and 40CrNiMo steels using vacuum magnetic-filtering arc plasma deposition. In the nanoindentation tests, the hardness and modulus curves for TiN/GT35 reduced the slowest around the film thickness 500 nm with the increase of indentation depth, followed by TiN/9Cr18 and TiN/40CrNiMo. Improving adhesion properties of coating and substrate can decrease the differences of internal stress field. The scratch tests showed that the scratch response was controlled by plastic deformation in the substrate. The substrate plays an important role in determining the mechanical properties and wear resistance of such coatings. TiN/GT35 exhibited the best load-carrying capacity and scratch/wear resistance. As a consequence, GT35 is the best substrate for TiN coatings of the substrate materials tested.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

对经不同扩散工艺处理的热浸镀铝层高温抗氧化性进行了研究,通过SEM、TEM、XRD分析了经扩散处理后,热浸镀铝层高温氧化过程中组织结构的变化情况,分析了热浸镀铝层高温抗氧化性能和微观结构的关系,确定了提高热浸镀铝层高温抗氧化性的适宜扩散温度.结果表明,经750℃扩散处理,热浸镀铝层结构由较厚的外表层(Fe2Al5+FeAl2)及内层(FeAl+条状FeAl2)组成,条状FeAl2的形成为氧提供了扩散通道,其抗氧化性较差;经950℃扩散处理,镀层外表层变薄,外表层转为单一FeAl2、内层为FeAl,并出现早期内氧化裂纹,其抗氧化性较差:当扩散处理温度为850℃时,镀层外表层变薄,结构转为FeAl2+少量Fe2Al5,而内层增厚,其结构为FeAl+球状FeAl2,而内层FeAl2球化,增强了氧由内层向基体扩散的阻碍作用,使氧只能逐层形成Al2O3+Fe2O3的氧化膜,提高了镀层的高温抗氧化性.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Titanium carbide particle (TiCp) reinforced Ni alloy composite coatings were synthesized by laser cladding using a cw 3 kW CO2 laser. Two kinds of coatings were present in terms of TiCp origins, i.e. undissolved and in situ reacted TiCp, respectively. The former came from the TiCp pre-coated on the sample, whereas the latter from in situ reaction between titanium and graphite in the molten pool during laser irradiation. Conventional and high-resolution transmission electron microscope observations showed the epitaxial growth of TiC, the precipitation of CrB, and the chemical reaction between Ti and B elements around phase interfaces of undissolved TiCp. The hardness, H, and elastic modulus, E, were measured by nanoindentation of the matrix near the TiCp interface. For undissolved TiCp, the loading curve revealed pop-in phenomena caused by the plastic deformation of the crack formation or debounding of TiCp from the matrix. As for in situ generated TiCp, no pop-in mark appears. On the other hand, in situ reacted TiCp led to much higher hardness and modulus than that in the case of undissolved TiCp. The coating reinforced by in situ generated TiCp displayed the highest impact wear resistance at both low and high impact conditions, as compared with coatings with undissolved TiCp and without TiCp. The impact wear resistance of the coating reinforced by undissolved TiCp increases at a low impact work but decreases at a high impact work, as compared with the single Ni alloy coating. The degree of wear for the composite coating depends primarily on the debonding removal of TiCp.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

采用激光相变硬化的方法在电镀前对基体表层预先进行处理,以改善镀层与基体的结合强度,提高其承载能力。借助扫描电镜(SEM)分析镀铬层的组织和界面,对镀层、相变硬化区和基体的硬度变化进行分析,对镀层抗高温烧蚀能力进行测试。结果表明,基体经激光相变硬化处理后,既可以促进镀层外延生长,又可以在镀层和基体之间实现硬度的梯度过渡,从而可以改善结合,缓解应力,提高承载能力,镀层的抗剥落能力和使用寿命得到显著提高。激光相变硬化得到细小的淬火马氏体,位错密度显著增加,表面活性增强,是促进镀层外延生长的主要原因。

Relevância:

10.00% 10.00%

Publicador:

Resumo:

A brief analysis is presented of how heat transfer takes place in porous materials of various types. The emphasis is on materials able to withstand extremes of temperature, gas pressure, irradiation, etc., i.e. metals and ceramics, rather than polymers. A primary aim is commonly to maximize either the thermal resistance (i.e. provide insulation) or the rate of thermal equilibration between the material and a fluid passing through it (i.e. to facilitate heat exchange). The main structural characteristics concern porosity (void content), anisotropy, pore connectivity and scale. The effect of scale is complex, since the permeability decreases as the structure is refined, but the interfacial area for fluid-solid heat exchange is, thereby, raised. The durability of the pore structure may also be an issue, with a possible disadvantage of finer scale structures being poor microstructural stability under service conditions. Finally, good mechanical properties may be required, since the development of thermal gradients, high fluid fluxes, etc. can generate substantial levels of stress. There are, thus, some complex interplays between service conditions, pore architecture/scale, fluid permeation characteristics, convective heat flow, thermal conduction and radiative heat transfer. Such interplays are illustrated with reference to three examples: (i) a thermal barrier coating in a gas turbine engine; (ii) a Space Shuttle tile; and (iii) a Stirling engine heat exchanger. Highly porous, permeable materials are often made by bonding fibres together into a network structure and much of the analysis presented here is oriented towards such materials. © 2005 The Royal Society.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Recently ZnO nanowire films have been used in very promising and inexpensive dye-sensitized solar cells (DSSC). It was found that the performance of the devices can be enhanced by functionalising the nanowires with a thin metal oxide coating. This nm-scale shell is believed to tailor the electronic structure of the nanowire, and help the absorption of the dye. Core-shell ZnO nanowire structures are synthesised at low temperature (below 120°C) by consecutive hydrothermal growth steps. Different materials are investigated for the coating, including Mg, Al, Cs and Zr oxides. High resolution TEM is used to characterise the quality of both the nanowire core and the shell, and to monitor the thickness and the degree of crystallisation of the oxide coating. The interface between the nanowire core and the outer shell is investigated in order to understand the adhesion of the coating, and give valuable feedback for the synthesis process. Nanowire films are packaged into dye-sensitised solar cell prototypes; samples coated with ZrO2 and MgO show the largest enhancement in the photocurrent and open-circuit voltage and look very promising for further improvement. © 2010 IOP Publishing Ltd.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Nano-sized TiNi powder with an average size of 50nm was consolidated using spark plasma sintering (SPS) at 800 °C for 5min. A layer of anatase TiO 2 coating was formed on the sintered TiNi by chemical reaction with a hydrogen peroxide (H2O2) solution at 60 °C followed by heat treatment at 400 °C to enhance the bioactivity of the metal surface. Cell culture using osteoblast cells and a biomimetic test in simulated body fluid proved the biocompatibility of the chemically treated SPS TiNi. © IOP Publishing Ltd.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Surface coatings and treatments have been used to reduce material loss of components in bubbling fluidized bed combustors (FBCs). The performance of protective coatings in FBC boilers and laboratory simulations is reviewed. Important coating properties to minimize wastage appear to be high hardness, low oxidation rate, low porosity, high adhesion and sufficient thickness to maintain protection for a long period. Economic considerations and criteria for choosing a suitable coating or treatment are discussed for the different types of bubbling FBC. © 1995.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

The aim of this study was to investigate the effect of temperature on tribological properties of plasma-sprayed Al-Cu-Fe quasicrystal (QC) coating after laser re-melting treatment. The laser treatment resulted in a more uniform, denser and harder microstructure than that of the as-sprayed coatings. Tribological experiments on the coatings were conducted under reciprocating motion at high frequency in the temperature range from 25 to 650 degreesC. Remarkable influence of temperature on the friction behavior of the coating was recorded and analyzed. Microstructural analysis indicated that the wear mechanisms of the re-melted QC coatings changed from abrasive wear at room temperature, to adhesive wear at 400 degreesC and severe adhesive wear at 650 degreesC owing to the material transfer of the counterpart ball. It was also observed that the ratio of the icosahedral (i)-phase to beta-Al-50(Fe,CU)(50) phase in the coating was higher after test at 400 'C than that at 650 'C. The variation of the ratio UP of coating and of the property of the counterpart ball and coating with the temperature are the two main factors influencing the wear mechanisms and value of the friction coefficient.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

An electron cyclotron wave resonant methane plasma discharge was used for the high rate deposition of hydrogenated amorphous carbon (a-C:H). Deposition rates of up to ∼400 Å/min were obtained over substrates up to 2.5 in. in diameter with a film thickness uniformity of ∼±10%. The deposited films were characterised in terms of their mass density, sp3 and hydrogen contents, C-H bonding, intrinsic stress, scratch resistance and friction properties. The deposited films possessed an average sp3 content, mass density and refractive index of ∼58%, 1.76 g/cm3 and 2.035 respectively.Mechanical characterisation indicated that the films possessed very low steady-state coefficients of friction (ca. 0.06) and a moderate shear strength of ∼141 MPa. Nano-indentation measurements also indicated a hardness and elastic modulus of ∼16.1 and 160 GPa respectively. The critical loads required to induce coating failure were also observed to increase with ion energy as a consequence of the increase in degree of ion mixing at the interface. Furthermore, coating failure under scratch test conditions was observed to take place via fracture within the silicon substrate itself, rather than either in the coating or at the film/substrate interface. © 2003 Elsevier B.V. All rights reserved.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Silent and stable long laminar plasma jets can be generated in a rather wide range of working parameters. The laminar flow state can be maintained even if considerable parameter fluctuations exist in the laminar plasma jet or if there is an impact of laterally injected particulate matter and its carrier gas. The attractive special features of laminar plasma jets include extremely low noise level, less entrainment of ambient air, much longer and adjustable high-temperature region length, and smaller axial gradient of plasma parameters. Modeling results show that the laminar plasma jet length increases with increasing jet inlet velocity or temperature and the effect of natural convection on laminar plasma jet characteristics can be ignored, consistent with experimental observations. The large difference between laminar and turbulent plasma jet characteristics is revealed to be due to their different laws of surrounding gas entrainment. Besides the promising applications of the laminar plasma jet to remelting and cladding strengthening of the metallic surface and to thermal barrier coating preparation, it is expected that the laminar plasma jet can become a rather ideal object for the basic studies of thermal plasma science owing to the nonexistence of the complexity caused by turbulence.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

某型发动机的火焰筒表面采用高温陶瓷涂层防护.该涂层用添加少量高岭土的玻璃料熔烧而成.由于批量生产时曾出现涂层与金属基体结合强度以及涂层耐酸性降低的问题,追溯工艺流程,发现高岭土原料存在问题.实际上,由于原料不合格导致的涂层质量问题在工艺试制时也偶有发生,但以前主要关注主料玻璃料,较少关注辅料高岭土的问题.本文对涂层的制备工艺及高岭土的作用进行了分析,针对原高岭土存在的问题以及新型高岭土的试用效果,探讨了选用新型高岭土的依据,力图解决当前发动机火焰筒陶瓷涂层的质量控制和提高新机火焰筒组件的性能等问题.……

Relevância:

10.00% 10.00%

Publicador:

Resumo:

钢基身管镀铬层在高温腐蚀性气体中服役,采用YAG激光器对身管内表面作螺旋线状离散淬火预处理后再电镀铬的复合工艺,形成了基体界面呈激光淬火区/激光未处理区周期性变化的铬层/基体结构.对该身管进行高温腐蚀介质为火药气体的靶场实验.对实验后的基体界面腐蚀形貌与铬层剥落的关系研究表明:次界面裂纹的形成是基体界面高温气体腐蚀的根本原因,基体界面腐蚀的结果是形成基体烧蚀坑,烧蚀坑上的铬层以断裂形式剥落.激光淬火预处理钢基体通过抑制次界面裂纹的形成避免了基体界面高温气体腐蚀损伤,提高了铬层的抗剥落能力.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

The finite element method is used to analyze the elastodynamic response of a columnar thermal barrier coating due to normal impact and oblique impact by an erosive particle. An assessment is made of the erosion by crack growth from preexisting flaws at the edge of each column: it is demonstrated that particle impacts can be sufficiently severe to give rise to columnar cracking. First, the transient stress state induced by the normal impact of a circular cylinder or a sphere is calculated in order to assess whether a 2D calculation adequately captures the more realistic 3D behavior. It is found that the transient stress states for the plane strain and axisymmetric models are similar. The sensitivity of response to particle diameter and to impact velocity is determined for both the cylinder and the sphere. Second, the transient stress state is explored for 2D oblique impact by a circular cylindrical particle and by an angular cylindrical particle. The sensitivity of transient tensile stress within the columns to particle shape (circular and angular), impact angle, impact location, orientation of the angular particle, and to the level of friction is explored in turn. The paper concludes with an evaluation of the effect of inclining the thermal barrier coating columns upon their erosion resistance. © 2011 The American Ceramic Society.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

热浸镀铝钢材在铝铁界面处易产成FeAl冶金结合层。本文就FeAl层对铝镀层等离子体电解氧化(PEO)陶瓷层的表面形貌、截面组织、相结构和元素分布的影响进行了研究。结果表明:由于FeAl参与,PEO陶瓷层局部区域出现了50μm~80μm的贯穿性孔洞,在孔洞/FeAl界面处出现了许多微观裂纹。EDS结果显示孔洞周围的Fe、Na元素含量增高了近8倍。陶瓷层主要由γ-Al_2O_3、莫来石相、α-Al_2O_3和Fe_3O_4相组成。与FeAl层相比,PEO陶瓷层具有较高的硬度和塑性变形能力。