This paper presents experimental tests carried out on steel fibre reinforced concrete samples, including mechanical tests as well as non-destructive technique (electrical resistivity) and non destructive technique on cores (X-ray). Electrical resistivity measurements are done as a blind test, to characterise the electrical anisotropy and deduce the distribution and the orientation of fibres. These results are compared to X-ray imaging to check the quality of the non destructive evaluation. Then, flexural and compressive strength are measured on specimens to assess the influence of fibre distribution on the concrete properties.
Resumo:
Fibre distribution and orientation in a series of round panel specimens of ultra high performance fibre reinforced concrete (UHPFRC) was investigated using electrical resistivity measurements and confirmed by X-ray CT imaging. By pouring specimens in different ways, the orientation of steel fibres was influenced and the sensitivity of the electrical resistivity technique was investigated. The round panels were tested in flexure and the results are discussed in relation to the observed orientation of fibres in the panels. It was found that the fibres tended to align perpendicular to the direction of flow. As a result, panels poured from the centre were significantly stronger than panels poured by other methods because the alignment of fibres led to more fibres bridging the radial cracks formed during mechanical testing.
Resumo:
The ductility of concrete made with commercially available steel and synthetic fibres has been investigated. Flexural stress–deflection relationships have been used to determine: flexural strength, flexural toughness, equivalent flexural strength, and equivalent flexural strength ratio. The flexural toughness of concrete was found to increase considerably when steel and synthetic fibres were used. However, equal dosages of different fibres did not result in specimens with the same flexural toughness. Flexural toughness differences of almost 35 J existed even at the same fibre dosage. This also resulted in considerable differences in the minimum required ground supported slab thickness.