961 resultados para caries-affected dentin
Resumo:
The objective of this study was to evaluate the use of a two-step total etch and rinse adhesive, the correlation between the hyybrid layer thickness (HL) and bond strength (BS), and between resin tag length (RT) and bond strength in the same teeth, and also to evaluate the fracture patterns of the tested specimens. Ten human molars were used for the restorative procedure and then sectioned in two halves (mesio-distally). The materials used were Adper Single Bond 2, 3M ESPE, Ultra etch gel, Ultradent and Filtek Z250, 3M ESPE. One half were utilized to measure the HL thickness and RT length through light microscopy analysis (400x), and the other half was subject to a microtensile test to measure the BS. The fractured surfaces were analyzed by scanning electron microscopy and fracture patterns classified. The Pearson correlation test was applied (p = 0.05). The results of the analyses of each specimen then were correlated: mean HL thickness = 4.39 (0.48) microm, mean length of RT = 9.94 (1.69) microm, mean BS = 23.98 (10.24) MPa. A statistically significant correlation between HL thickness and bond strength was found (r = 0.93). The two step etch and rinse adhesive system, showed a strong correlation between HL thickness and bond strength. The most common fractures were adhesive, followed by cohesive in resin.
Resumo:
The family Piperaceae contains nearly 2000 species, most of them distributed in two genera, Piper and Peperomia. In Brazil circa 170 Piper species are found, mainly in tropical areas Their use ranges from flavoring and culinary to raw material for pharmaceutical and cosmetic industry. One of these species, Piper callosum, is used in folk medicine in the Amazon area. The objective of this study was to evaluate the production of biomass (aerial parts) as well as yield and composition of the essential oil from the leaves, according to different spacing between cultivated plants at Embrapa Western Amazon, in Manaus, State of Amazonas, Brazil. The experimental design was randomized blocks, with four treatments and seven replicates with six plants. Biomass production was inversely proportional to the spatial arrangements, with the greatest biomass production (1034.93 kg/ha) in the shortest spacing (E1), although no statistical difference was verified between E3 and E4. The same response was observed for the production of essential oil. The chemical composition of the oil was not affected by spacing, and major compounds found were safrole (59.1%), beta-pinene (8.3%), alpha-pinene (6.5%), methyl eugenol (6.3%) and 1,8-cineole (4.1).
Resumo:
The aim of this study was to evaluate effect of bleaching agents on sound enamel (SE) and enamel with early artificial caries lesions (CL) using confocal laser scanning microscopy (CLSM). Eighty blocks (4 × 5 × 5 mm) of bovine enamel were used and half of them were submitted to a pH cycling model to induce CL. Eight experimental groups were obtained from the treatments and mineralization level of the enamel (SE or CL) (n=10). SE groups: G1 - unbleached (control); G2 - 4% hydrogen peroxide (4 HP); G3 - 4 HP containing 0.05% Ca (Ca); G4 - 7.5% hydrogen peroxide (7.5 HP) containing amorphous calcium phosphate (ACP). CL groups: G5 - unbleached; G6 - 4 HP; G7 - 4 HP containing Ca; G8 - 7.5 HP ACP. G2, G3, G6, G7 were treated with the bleaching agents for 8 h/day during 14 days, while G4 and G8 were exposed to the bleaching agents for 30 min twice a day during 14 days. The enamel blocks were stained with 0.1 mM rhodamine B solution and the demineralization was quantified using fluorescence intensity detected by CLSM. Data were analyzed using ANOVA and Fisher's tests (α=0.05). For the SE groups, the bleaching treatments increased significantly the demineralization area when compared with the unbleached group. In the CL groups, no statistically significant difference was observed (p>0.05). The addition of ACP or Ca in the composition of the whitening products did not overcome the effects caused by bleaching treatments on SE and neither was able to promote remineralization of CL.
Resumo:
With the arrival of self-etch adhesives systems, there has been a rise in interest among clinicians, making it imperative for health professionals to have knowledge of the properties, characteristics, the association as well as the dental structures of these materials, in order to select them and use them correctly. The self-etch adhesive systems show good values of bond strength, microleakage and performance, and have therefore become an option in direct adhesive restorations. In the regard, this case study aims to describe the technique involving the use of selfetch adhesives system for direct restoration of anterior teeth.
Resumo:
The aim of this study was to evaluate the effects of different irrigants on sealer-dentin bond strength when using Real Seal. Thirty single-rooted teeth were divided into 3 groups. In one group, the teeth were irrigated with 3 mL of 2.5% NaOCl after each file change, flushed with 17% EDTA for 3 min and finally rinsed with 3 mL of 2.5% NaOCl. In the other two groups, rinse with NaOCl was replaced with 2% chlorhexidine gluconate (CHX) and 0.9% saline, respectively. Each root was sectioned transversally into apical, middle and coronal thirds to obtain 2-mm-thick slices. Each slice was filled with Real Seal and Resilon. Push-out test was used to analyze bond strength and failure modes were classified as adhesive, cohesive or mixed, according to SEM observations. The push-out test did not reveal any statistically significant difference (p>0.05) between the irrigants. However, the groups exhibited significantly different (p<0.05) bond strengths in terms of the root canal third. Higher bond strength was observed at the apical third when compared with coronal third, while middle third presented intermediary values. Fifteen specimens were analyzed by SEM (5 per group). Eleven specimens exhibited adhesive failures (5 in saline, 4 in NaOCl and 2 in CHX group); 2 cohesive failures were observed in the CHX group, and 1 mixed failure each was observed in the CHX and NaOCl groups. The tested irrigants did not influence the bond strength of Resilon and Real Seal to dentin. The apical third exhibited higher mean bond strengths and adhesive failures were predominant.
Resumo:
Objectives: The objective of this study was to evaluate the clinical performance of 124 non-carious cervical lesion restorations at 12 months. Materials And Methods: Three study groups were formed according to the material and technique used. All teeth received 37% phosphoric acid etching in enamel and dentin. The teeth of Group I received the conventional adhesive system Scotch Bond Multi Purpose, followed by resin composite Filtek Z350; teeth of Group II were restored with resin-modified glassionomer cement Fuji II LC; teeth of Group III were restored with the same resin-modified glass-ionomer cement-however, before it was inserted, 2 coats of primer of the Scotch Bond Multi Purpose adhesive system were applied to dentinal tissue. The teeth were evaluated by 2 examiners with regard to the factors of retention, marginal adaptation, marginal discoloration, color alteration, presence of marginal caries lesion, anatomic shape, and sensitivity. Results: Application of the Kruskal-Wallis test showed no statistically significant difference for anatomic shape, marginal discoloration, color alteration, caries lesion, marginal adaptation, and sensitivity among the three study groups, but the variable retention presented statistically significant difference at 12 months, with Group III presenting a behavior superior to that of Group II but similar to that of Group I. Conclusion: The analyzed restorations of non-carious cervical lesions presented a good clinical performance at 12 months. © 2012 Nova Science Publishers, Inc.
Resumo:
Aim: This study analyzed and compared the experience of dental caries in 300 children aged 0 to 48 months, who were participants and non-participants of a preventive program 'Dentistry for babies', as well as the correlation between assiduity of dental visits and experience of dental caries. Methods: The subjects were randomly selected and divided into two groups: G1 'Non participant children of the Program' (n=100) and G2 'Participant Children of the Program' (n=200). Each group was subdivided in two subgroups: 0-24 months and 25-48 months. The collected data from G2 were analyzed, relating the variation of the dmft index (dmft refers to primary teeth: d = decayed, m = missing/extracted due to caries, f = filled, t = teeth) (C) and dental caries prevalence (P) with the influence of assiduity factor in each subgroup. To collect data, clinical examinations were performed using tactile and visual criteria by a single calibrated examiner. The data were statistically analyzed using the 'paired t-test', 'Mann-Whitney' and 'Chi-Squared' tests (p<0.05). Results: It was found that prevalence and dmft index were statistically significant (P=0.0001) with the greatest values observed in G1 (p=0.0001). The values were: PG1 (73%), PG2 (22%), CG1 (3.45±3.84), CG2 (0.66±1.57). Assiduity was significant in G2 (p=0.0001). The values observed were: P-Assiduous (2%), P-Non-assiduous (42%), C-Assiduous (0.04±0.31), and C-Non-assiduous (1.29±2.01). Conclusions: The participation in the program had a positive influence on the oral health of babies. Complete assiduity to the program resulted in the lowest rates and prevalence of dental caries.
Resumo:
The purpose of this in vitro study was to quantify the alterations on human root dentin permeability after exposure to different acid fruit juices and to evaluate the effect of toothbrushing with electric or sonic toothbrush after acid exposure. The root dentin of 50 extracted third molars was exposed with a high speed bur. Crowns were sectioned above the cementoenamel junction and root fragments were used to prepare dentin specimens. Specimens were randomly assigned to 5 groups according to the fruit juice (kiwifruit, starfruit, green apple, pineapple and acerolla). Each specimen was connected to a hydraulic pressure apparatus to measure root dentin permeability using fluid filtration method after the following sequential steps: I) conditioning with 37% phosphoric acid for 30 s, II) root scaling, III) exposure to acid fruit juices for 5 min and IV) electric or sonic toothbrushing without dentifrice for 3 min. Data were analyzed statistically by the Wilcoxon and Mann-Whitney tests at 5% significance level. All fruit juices promoted a significant increase of dentin permeability while toothbrushing decreased it significantly (p<0.05). It may be concluded that all acid fruit juices increased root dentin permeability, while toothbrushing without dentifrice after acid exposure decreased the permeability. The toothbrush mechanism (electric or sonic) had no influence on the decrease of root dentin permeability.
Resumo:
The aim of this study was to investigate the effects of some acidic drinks on dentin erosion, using methods of surface profile (SP) analysis and energy-dispersive X-ray fluorescence spectrometry (EDXRF). One hundred standardized dentin slabs obtained from bovine incisor roots were used. Dentin slabs measuring 5x5 mm were ground flat, polished and half of each specimen surface was protected with nail polish. For 60 min, the dentin surfaces were immersed in 50 mL of 5 different drinks (Gatorade®, Del Valle Mais orange juice®, Coca-Cola®, Red Bull® and white wine), 20 blocks in each drink. The pH of each beverage was measured. After the erosive challenge, the nail polish was removed and SP was analyzed. The mineral concentration of dentin surfaces was determined by means of EDXRF. Data were analyzed statistically by ANOVA and Tukey's test (α=0.05). SP analysis showed that Red-Bull had the highest erosive potential (p<0.05). EDXRF results exhibited a decrease in phosphate in the groups immersed in Red-Bull, orange juice and white wine (p<0.05), and no significant difference in calcium content between the reference surface and eroded surface. In conclusion, this study demonstrated that all studied beverages promoted erosion on root dentin and Red Bull had the highest erosive potential. There was no correlation between pH of beverages and their erosive potential and only the P content changed after erosive challenge.
Resumo:
The presence of residual endodontic sealer in the pulp chamber may cause discoloration of the dental crown and interfere with the adhesion of restorative materials. The aim of this study was to compare the efficacy of different solvents in removing residues of an epoxy resin-based sealer (AH Plus) from the dentin walls of the pulp chamber, by scanning electron microscopy (SEM). Forty-four bovine incisor dental crown fragments were treated with 17% EDTA and 2.5% NaOCl. Specimens received a coating of AH Plus and were left undisturbed for 5 min. Then, specimens were divided in four groups (n = 10) and cleaned with one of the following solutions: isopropyl alcohol, 95% ethanol, acetone solution, or amyl acetate solution. Negative controls (n = 2) did not receive AH Plus, while in positive controls (n = 2) the sealer was not removed. AH Plus removal was evaluated by SEM, and a score system was applied. Data were analyzed by Kruskal-Wallis and Dunn tests. None of the solutions tested was able to completely remove AH Plus from the dentin of the pulp chamber. Amyl acetate performed better than 95% ethanol and isopropyl alcohol (p < 0.05), but not better than acetone (p > 0.05) in removing the sealer from dentin. No significant differences were observed between acetone, 95% ethanol, and isopropyl alcohol (p > 0.05). It was concluded that amyl acetate and acetone may be good options for cleaning the pulp chamber after obturation with AH Plus. SCANNING 35:17-21, 2013. © 2012 Wiley Periodicals, Inc. © Wiley Periodicals, Inc.
Resumo:
Objective: To evaluate the effects of simulated aging in bond strength and nanoleakage of class II restorations using three different restorative techniques. Materials and methods: Class II preparations (n = 12) were restored using: FS - composite resin Filtek Supreme Plus (3M/ESPE); RMGIC + FS - resin-modified glass ionomer cement Vitrebond Plus (3M/ESPE) + FS; and FFS + FS - flowable composite resin Filtek Supreme Plus Flowable (3M ESPE) + FS. The teeth were assigned into two groups: Control and Simulated Aging - Thermal/Mechanical cycling (3,000 cycles, 20-80 °C/500,000 cycles, 50 N). From each tooth, two slabs were assessed to microtensile bond strength test (μTBS) (MPa), and two slabs were prepared for nanoleakage assessment, calculated as penetration along the restoration margin considering the penetration length (%) and as the area of silver nitrate particle deposition (μm2). Data were analyzed by two-way analysis of variance (ANOVA) followed by Tukey's post hoc test (p < 0. 05). Results: FS presented the highest μTBS to dentin (22. 39 ± 7. 55 MPa) after simulated aging, while the presence of flowable resin significantly decreased μTBS (14. 53 ± 11. 65 MPa) when compared to no aging condition. Both control and aging groups of RMGIC + FS presented the highest values of silver nitrate penetration (89. 90 ± 16. 31 % and 97. 14 ± 5. 76 %) and deposition area (33. 05 ± 12. 49 and 28. 08 ± 9. 76 μm2). Nanoleakage was not affected by simulated aging. Conclusions: FS presented higher bond strength and lower nanoleakage and was not affected by simulated aging. Use of flowable resin compromised the bond strength after simulated aging. Clinical relevance: The use of an intermediate layer did not improve the dentin bond strength neither reduced nanoleakage at the gingival margins of class II restorations under simulated aging conditions. © 2012 Springer-Verlag.
Resumo:
This study determined if dentin proteases are denatured by phosphoric acid (PA) used in etch-and-rinse dentin adhesives. Dentin beams were completely demineralized with EDTA for 30 days. We acid-etched experimental groups by exposing the demineralized dentin beams to 1, 10, or 37 mass% PA for 15 sec or 15 min. Control beams were not exposed to PA but were incubated in simulated body fluid for 3 days to assay their total endogenous telopeptidase activity, by their ability to solubilize C-terminal crosslinked telopeptides ICTP and CTX from insoluble dentin collagen. Control beams released 6.1 ± 0.8 ng ICTP and 0.6 ± 0.1 ng CTX/mg dry-wt/3 days. Positive control beams pre-incubated in p-aminophenylmercuric acetate, a compound known to activate proMMPs, released about the same amount of ICTP peptides, but released significantly less CTX. Beams immersed in 1, 10, or 37 mass% PA for 15 sec or 15 min released amounts of ICTP and CTX similar to that released by the controls (p > 0.05). Beams incubated in galardin, an MMP inhibitor, or E-64, a cathepsin inhibitor, blocked most of the release of ICTP and CTX, respectively. It is concluded that PA does not denature endogenous MMP and cathepsin activities of dentin matrices. © 2013 International & American Associations for Dental Research.
Resumo:
A better understanding of the differential growth of upland rice (Oryza sativa L.) cultivars with increasing soil S availability could help improve rice yield under upland conditions. The objective of this study was to evaluate root and shoot growth and nutrition of upland traditional and modern rice cultivars as affected by S availability. The experimental design was completely randomized in a 3 (rates of S) × 3 (cultivars) factorial with four replications. Low availability of S in the soil reduces root and shoot development and the efficiency of N, P, and S uptake, as well as the concentration and content of these nutrients in rice cultivars. At 0 mg dm-3 of S, rice cultivars prioritize root growth over shoots, and the traditional cultivar does so with greater intensity. Our results suggested that more development of traditional cultivars under low S availability facilitates its adaptation in soils under this condition. On the other hand, the intermediate and modern cultivars are more responsive to S fertilization. Moreover, S fertilization allows significant increases in upland rice growth and must be considered in cropping systems aiming for high yields. © Soil Science Society of America.
Resumo:
Aim: This study evaluates bond strength between dentin and composite using adhesives with different solvents to dry and wet dentin. Materials and methods: Ninety bovine incisors were used; the vestibular surfaces were worn by the exposure of an area with a diameter of 4 mm of dentin. The specimens were divided into 6 groups, according to the type of adhesive used and hydratation stals: Group SB-wet: Single Bond 2 in wet dentin, Group SBdry: Single Bond 2 in dry dentin, Group SL-wet: Solobond M in wet dentin, Group SL-dry: Solobond M in dentin dry. Group XPwet: XP Bond in wet dentin, Group XP-dry: XP Bond in dentin dry. They were cut to obtain specimens in the shape of stick with 1 × 1 mm and subjected to microtensile test in universal testing machine with a cross speed of 1mm/min. The data were analyzed with ANOVA and Tukey's tests (5%). Results: ANOVA showed significant differences for surface treatment and interaction, but no difference was found for adhesive factor. The Tukey's test showed that the samples with wet dentin shown higher values of bond strength. Conclusion: The adhesive did not influence in the bond strength. The groups with wet dentin showed higher values of bond strength than groups with dry dentin.
Resumo:
Aim: The aim of this study was to compare the microtensile bond strength of three adhesive systems, using different methods of dentin preparation. Materials and methods: A hundred and eight bovine teeth were used. The dentin from buccal face was exposed and prepared with three different methods, divided in 3 groups: Group 1 (DT)- diamond tip on a high-speed handpiece; Group 2 (CVD)-CVD tip on a ultrasonic handpiece; Group 3 (LA)-Er: YAG laser. The teeth were divided into 3 subgroups, according adhesive systems used: Subgroup 1-Adper Single Bond Plus/3M ESPE (SB) total-etch adhesive; Subgroup 2-Adper Scotchbond SE/3M ESPE (AS) selfetching adhesive; Subgroup 3-Clearfil SE Bond/Kuraray (CS) selfetching adhesive. Blocks of composite (Filtek Z250-3M ESPE) 4 mm high were built up and specimens were stored in deionized water for 24 hours at 37°C. Serial mesiodistal and buccolingual cuts were made and stick-like specimens were obtained, with transversal section of 1.0 mm2. The samples were submitted to microtensile test at 1 mm/min and load of 10 kg in a universal testing machine. Data (MPa) were subjected to ANOVA and Tukey's tests (p < 0.05). Results and conclusion: Surface treatment with Diamond or CVD tips associated with Clearfil SE Bond adhesive produced significantly lower bond strength values compared to other groups. Surface treatment with Er: YAG laser associated with Single Bond Plus or Clearfil SE Bond adhesives and surface treatment with CVD tip associated with Adper Scotchbond SE adhesive produced significantly lower bond strength values compared to surface treatment with diamond or CVD tips associated with Single Bond Plus or Adper Scotchbond SE adhesives. Clinical significance: Interactions between laser and the CVD tip technologies and the different adhesive systems can produce a satisfactory bonding strength result, so that these associations may be beneficial and enhance the clinical outcomes.