Ytterbium-doped calcium pyroniobate single crystal has been grown for the first time. Spectral properties of Yb: Ca2Nb2O7 were investigated by emission and absorption spectra. Its cooperative luminescence and fluorescence lifetime were also studied. Yb ions in Ca2Nb2O7 showed very broad absorption and emission bandwidth and relatively large absorption and emission cross-sections. Along with other optical properties, this Yb-doped crystal would be a potential self-frequency doubling femtosecond laser gain material. (C) 2007 Published by Elsevier B.V.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

A bulk crystal of Yb:Sc2SiO5 (Yb:SSO) with favorable thermal properties was successfully obtained by the Czochralski method. The energy level diagrams for Yb:SSO crystal were determined by optical spectroscopic analysis and semi-empirical crystal-field calculations using the simple overlap model. The full width at half maximum of the absorption band centering at 976 nm was calculated to be 24 nm with a peak absorption cross-section of 9.2x10(-21) cm(2). The largest ground-state splitting of Yb3+ ions is up to 1027 cm(-1) in a SSO crystal host. Efficient diode-pumped laser performance of Yb:SSO was primarily demonstrated with a slope efficiency of 45% and output power of 3.55 W.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

以高纯α-Al2O3和石墨为原料,采用温梯法生长了α-Al2O3:C晶体,使用RisΦTL/OSL-DA-15型热释光和光释光仪研究了其热释光和光释光特性.α-Al2O3:C晶体在462K附近有单一热释光峰,发射波长位于410nm.随着辐照剂量的增加,热释光强度逐渐增强,462K的热释光特征峰位置保持不变.α-Al2O3:C晶体的光释光衰减曲线由快衰减和慢衰减两个部分组成,随着辐照剂量的增加,快衰减部分衰减速率变化不大,而慢衰减部分衰减速率加快.在5×10-6—10Gy剂量范围内,α-Al2O3:C晶体的热释光剂量响应呈现良好的线性关系,30Gy时达到饱和;光释光剂量响应在5×10-6—60Gy剂量范围内呈现良好的线性关系,100Gy时达到饱和.与热释光相比,光释光剂量响应具有更高的灵敏度和更宽的线性剂量响应范围.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The electronic structures and absorption spectra for the perfect PbMoO4 crystal and the crystal containing lead vacancy V-Pb(2-) with lattice structure optimized are calculated using density functional theory code CASTEP. The calculated absorption spectra of the PbMoO4 crystal containing V-Pb(2-) exhibit three absorption bands peaking at 2.0 eV (620 nm), 3.0 eV (413 run) and 3.3 eV (375 nm), which are in good agreement with experimental values. The theory predicts that the 390 nm, 430 nm and 580 run absorption bands are related to the existence of V-Pb(2-) in the PbMoO4 crystal.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

An Ho3+-doped YAlO3 (Ho : YAP) single crystal has been grown by the Czochralski technique. The polarized absorption spectra, polarized fluorescence spectra and fluorescence decay curve of the crystal are measured at room temperature. The spectroscopic parameters are calculated based on Judd-Ofelt theory, and the effective phenomenological intensity parameters Omega(2,eff), Omega(4,eff) and Omega(6,eff) are obtained to be 2.89 x 10(-20), 2.92 x 10(-20) and 1.32 x 10(-20) cm(2), respectively. The room-temperature fluorescence lifetime of the Ho3+ 5I(7) -> I-5(8) transition is measured to be 8.1 ms. Values of the absorption and emission cross-sections with different polarizations are presented for the I-5(7) manifold, and the polarized gain cross-section curves are also provided and discussed.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The Ho:YAP crystal is grown by the Czochralski technique. The room-temperature polarized absorption spectra of Ho:YAP crystal was measured on a c-cut sample with 1 at% holmium. According to the obtained Judd-Ofelt intensity parameters Omega(2) = 1.42 x 10(-20) cm(2), Omega(4) = 2.92 x 10(-20) cm(2), and Omega(6) = 1.71 x 10(-20) cm(2), this paper calculated the fluorescence lifetime to be 6 ms for I-5(7) -> I-5(8) transition, and the integrated emission cross section to be 2.24 x 10(-18) cm(2). It investigates the room-temperature Ho:YAP laser end-pumped by a 1.91-mu m Tm:YLF laser. The maximum output power was 4.1 W when the incident 1.91-mu m pump power was 14.4W. The slope efficiency is 40.8%, corresponding to an optical-to-optical conversion efficiency of 28.4%. The Ho:YAP output wavelength was centred at 2118 nm with full width at half maximum of about 0.8 nm.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The 2 at.% Sm:GdVO4 crystal was grown by the Czochralski method. The segregation coefficient of Sm3+ ion in this crystal is 0.98. The crystal structure of the Sm:GdVO4 crystal was determined by X-ray diffraction analysis. Judd-Ofelt theory was used to calculate the intensity parameters (Omega(i)), the spontaneous emission probability, the luminary branching ratio and the radiative lifetime of the state (4)G(5/2). The stimulated emission cross-sections at 567, 604 and 646 nm are calculated to be 5.92 x 10(-21), 7.62 x 10(-21) and 5.88 x 10(-21) cm(2), respectively. The emission cross-section at 604 nm is 4.4 times lager than that in Sm: YAP at 607 nm. (C) 2007 Elsevier B.V. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Mg0.4Al2.4O4 single crystals with good optical quality were successfully grown by the Czochralski method. The transmission spectrum indicated that the absorption edge of the crystal was at 220nm, while no apparent absorption peaks were found. The X-ray diffraction and DSC curve analysis showed that Mg0.4Al2.4O4 crystal was stable at room temperature. While after annealing in the air and hydrogen atmosphere at about 1200 degrees C,Mg0.4Al2.4O4 decomposed into Al2O3 and (MgO)(0.4)(Al2O3)(x) (0.4 < x < 1.2). The reaction mainly occurred on the crystal surface, barely inside. (C) 2008 Elsevier B.V. All rights reserved.