961 resultados para heat pump. thermo-chemical storage


Relevância:

20.00% 20.00%

Publicador:

Resumo:

An investigation was conducted on pollutants emitted from steady-state, steady-flow gasification and combustion of polyethylene (PE) in a two-stage furnace. The polymer, in pulverized form, was first pyrolyzed at 1000 degrees C, and subsequently, its gaseous pyrolyzates were burned, upon mixing with air at high temperatures (900-1100 degrees C). The motivation for this indirect type of burning PE was to attain nominally premixed combustion of the pyrolyzate gases with air, thereby achieving lower pollutant emissions than those emanating from the direct burning of the solid PE polymer. This work assessed the effluents of the two-stage furnace and examined the effects of the combustion temperature, as well as the polymer feed rate and the associated fuel/air equivalence ratio (0.3 < phi < 1.4). It was found that, whereas the yield of pyrolysis gas decreased with an increasing polymer feed rate, its composition was nearly independent of the feed rate. CO2 emissions peaked at an equivalence ratio near unity, while the CO emissions increased with an increasing equivalence ratio. The total light volatile hydrocarbon and semivolatile polycyclic aromatic hydrocarbon (PAH) emissions of combustion increased with an increasing equivalence ratio. The generated particulates were mostly submicrometer in size. Overall, PAH and soot emissions from this indirect burning of PE were an order of magnitude lower than corresponding emissions from the direct burning of the solid polymer, obtained previously in this laboratory using identical sampling and analytical techniques. Because pyrolysis of this polymer requires a nominal heat input that amounts to only a diminutive fraction of the heat released during its combustion, implementation of this technique is deemed advantageous.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The effect of different microstructures on the polarization resistance (Rp) and the hydrogen-induced cracking (HIC) of a micro-alloyed steel austenitized and submitted to different cooling rates was studied. Samples 19.1 x 6 x 2 mm, containing the whole thickness of the plate were extracted from a 20 mm plate and heat treated on a quenching dilatometer, were submitted to Rp and HIC corrosion tests. Both Rp and HIC tests followed as close as possible ASTM G59 and NACE standard TM0284-2003, in this case, modified only with regard to the size of the samples. Steel samples transformed from austenite by a slow cooling (cooling rate of 0.5 degrees C.s(-1)) showed higher susceptibility to hydrogen-induced cracking, with large cracks in the middle of the sample propagating along segregation bands, corresponding to the centerline of the plate thickness. For cooling rates of 10 degrees C.s(-1), only small cracks were found in the matrix and micro cracks nucleated at non-metallic inclusions. For higher cooling rates (40 degrees C.s(-1)) very few small cracks were detected, linked to non-metallic inclusions. This result suggests that structures formed by polygonal structures and segregation bands (were cutectoid microconstituents predominate) have higher susceptibility to HIC. Structures predominantly formed by acicular ferrite make it difficult to propagate the cracks among non-oriented and interlaced acicular ferrite crystals. Smaller segregation bands containing eutectoid products also help inhibit cracking and crack propagation; segregation bands can function as pipelines for hydrogen diffusion and offer a path of stress concentration for the propagation of cracks, frequently associated to non-metallic inclusions. Polarization resistance essays performed on the steel in theas received condition, prior to any heat treatment, showed larger differences between the regions of the plate, with a considerably lower Rp in the centerline. The austenitization heat treatments followed by cooling rates of 0.5 e 10 degrees C.s(-1) made more uniform the corrosion resistance along the thickness of the plate. The effects of heat treatments on the corrosion resistance are probably related to the microconstituent formed, allied to the chemical homogenization of the impurities concentrated on the centerline of the plate.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The goal of this work is to investigate the reduction of chromium from a quaternary slag by carbon dissolved in liquid steel. Laboratory scale experiments were conducted to study the reduction of chromium oxides in the slag by carbon dissolved in the melt. These experiments were made under different conditions of slag basicity and amount of added carbon. Thermodynamic calculations based on Double Sublattice model were applied using the commercial software Thermo-Calc, with the IRSID database. The results obtained showed good correlation with practical and calculated results, making it possible to predict equilibrium conditions of the system and to determine the activities of chromium oxides in the slag.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The distribution of Cr and N in a high-temperature gas-nitrided stainless steel was measured by using a scanning electron microscope-coupled wavelength-dispersive X-ray spectrometer and the results were related to the microhardness profile of the hardened case. The experimental spectrometric procedure was optimized to consistently measure N contents varying between 0.1 and 0.8 wt.% in martensite and between 18.3 and 21.6 wt.% in nitrides, as well as Cr contents ranging from 11.5 to 17.0 wt.%. (C) 2010 Acta Materialia Inc. Published by Elsevier Ltd. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Heat treated electrical steel laminations have shown evidence of low ductility behavior, characterized by a small number of bends till fracture, on repeated bending tests. The laminations were produced using a new grade of electrical steel with much lower aluminum content than usual. The problem happens when the oxygen potential (measured by the dew point of the atmosphere) of the heat treatment atmosphere is abnormally high. Furthermore, ductility can be restored by a low-oxygen potential heat treatment. Although the heat treatment resulted in a loss of ductility, the magnetic properties were not deteriorated. The low ductility samples always show intergranular fracture, whereas the un-treated laminations fracture by cleavage. The low ductility is associated with the formation of silicon manganese nitride precipitates formed at grain boundaries, although they are not the cause of the low ductility. Ductility could be restored by a low dew point heat treatment but the inclusions remained in the grain boundaries. The low ductility and its recovery must be ascribed to the presence of nitrogen atoms segregated to the grain boundaries when the heat treatment atmosphere has a high oxygen potential. The lack of aluminum in the composition of the steel hinders the scavenging effect of this element on nitrogen atoms in solution in the steel. (C) 2009 Elsevier Ltd. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Nanomaterials have triggered excitement in both fundamental science and technological applications in several fields However, the same characteristic high interface area that is responsible for their unique properties causes unconventional instability, often leading to local collapsing during application Thermodynamically, this can be attributed to an increased contribution of the interface to the free energy, activating phenomena such as sintering and grain growth The lack of reliable interface energy data has restricted the development of conceptual models to allow the control of nanoparticle stability on a thermodynamic basis. Here we introduce a novel and accessible methodology to measure interface energy of nanoparticles exploiting the heat released during sintering to establish a quantitative relation between the solid solid and solid vapor interface energies. We exploited this method in MgO and ZnO nanoparticles and determined that the ratio between the solid solid and solid vapor interface energy is 11 for MgO and 0.7 for ZnO. We then discuss that this ratio is responsible for a thermodynamic metastable state that may prevent collapsing of nanoparticles and, therefore, may be used as a tool to design long-term stable nanoparticles.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The premature failure of a horizontal heat-exchanger, which occurred after service exposure at 580 degrees C for 50,000 h, revealed the occurrence of extensive through-thickness cracking in approximately 40% of the tube/stationary tube-sheet welds. Additionally, the internal surface of the welded joint featured intensive secondary intergranular cracking (up to 250 mu m deep), preferential formation of a 150 mu m thick layer of (Fe, Cr)(3)O-4 and internal intergranular oxidation (40 mu m deep). The welded region also showed intense carbon pick-up and, as consequence, severe precipitation of intergranular M7C3 and M23C6 carbides. The fracture surface was composed of two distinct regions: a ""planar"" region of 250 mu m, formed due to the stable crack growth along by the intergranular oxidation; and a slant region with radial marks, formed by the fast crack growth along the network of intergranular carbides. The association of intergranular oxidation pre-cracks with microstructural embrittlement promoted the premature failure, which took place by an overload mechanism, probably due to the jamming of the floating tube-sheet during the maintenance halt (cooling operation). (C) 2007 Elsevier Ltd. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Dynamic experiments in a nonadiabatic packed bed were carried out to evaluate the response to disturbances in wall temperature and inlet airflow rate and temperature. A two-dimensional, pseudo-homogeneous, axially dispersed plug-flow model was numerically solved and used to interpret the results. The model parameters were fitted in distinct stages: effective radial thermal conductivity (K (r)) and wall heat transfer coefficient (h (w)) were estimated from steady-state data and the characteristic packed bed time constant (tau) from transient data. A new correlation for the K (r) in packed beds of cylindrical particles was proposed. It was experimentally proved that temperature measurements using radially inserted thermocouples and a ring-shaped sensor were not distorted by heat conduction across the thermocouple or by the thermal inertia effect of the temperature sensors.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Steady-state and time-resolved fluorescence measurements are reported for several crude oils and their saturates, aromatics, resins, and asphaltenes (SARA) fractions (saturates, aromatics and resins), isolated from maltene after pentane precipitation of the asphaltenes. There is a clear relationship between the American Petroleum Institute (API) grade of the crude oils and their fluorescence emission intensity and maxima. Dilution of the crude oil samples with cyclohexane results in a significant increase of emission intensity and a blue shift, which is a clear indication of the presence of energy-transfer processes between the emissive chromophores present in the crude oil. Both the fluorescence spectra and the mean fluorescence lifetimes of the three SARA fractions and their mixtures indicate that the aromatics and resins are the major contributors to the emission of crude oils. Total synchronous fluorescence scan (TSFS) spectral maps are preferable to steady-state fluorescence spectra for discriminating between the fractions, making TSFS maps a particularly interesting choice for the development of fluorescence-based methods for the characterization and classification of crude oils. More detailed studies, using a much wider range of excitation and emission wavelengths, are necessary to determine the utility of time-resolved fluorescence (TRF) data for this purpose. Preliminary models constructed using TSFS spectra from 21 crude oil samples show a very good correlation (R(2) > 0.88) between the calculated and measured values of API and the SARA fraction concentrations. The use of models based on a fast fluorescence measurement may thus be an alternative to tedious and time-consuming chemical analysis in refineries.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Static mixers with improved performance were developed from CFD simulations in a stepwise approach. The relevant geometric features of simple mixer designs and the corresponding mixing mechanisms-laminar shear, elongational flow, and distributive mixing-were identified first. This information was used to formulate guidelines for the development of new geometries. The solid elements of the static mixer should: (a) provide restrictions to the flow; (b) deflect the flow; (c) be sequentially rotated around the flow direction to provide symmetry; (d) extend from the center of the pipe to the vicinity of the walls to avoid short-circuiting; and (e) distribute and remix the flow. Based on these guidelines, two improved mixer designs were developed: the DS A-I mixer has a good mixing efficiency and an acceptable pressure drop; the Fins 35 degrees mixer is more efficient and compact, but requires a larger pressure drop. Their performance indicates that their use is possible on industrial applications.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

This work aims to characterize corrosion products formed on copper samples exposed to synthetic rainwater of Rio Janeiro and Sao Paulo. XRD and XPS were employed to determine their composition, while electrochemical techniques were used to evaluate their protective properties. XRD and XPS indicated the thickening of the corrosion layer with time. Electrochemical results showed that the protectiveness of the corrosion layer depends on the solution composition. Based on our findings a corrosion mechanism for copper in simulated rainwater is proposed where the role of NH(4)(+) ions in the cuprite layer partial regeneration is taken into account. (C) 2009 Elsevier Ltd. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

An experimental investigation of the kinetics of cationic polymerization of beta-pinene was performed using two different initiator systems under two different operating conditions (shot additions of initiator, and continuous feeding of monomer). The experiments were done using calorimetric measurements under isoperibolic conditions. The heat of polymerization of beta-pinene was found to be -30.6 kcal . mol(-1). A simple kinetic model was tentatively proposed, and the model fit reasonably well to the different experimental runs. Different values of the fitting parameters were obtained for runs carried out under different conditions, which can probably be ascribed to the presence of adventitious impurities in the commercial-grade monomer used.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

P>Coconut water is an isotonic beverage naturally obtained from the green coconut. After extracted and exposed to air, it is rapidly degraded by enzymes peroxidase (POD) and polyphenoloxidase (PPO). To study the effect of thermal processing on coconut water enzymatic activity, batch process was conducted at three different temperatures, and at eight holding times. The residual activity values suggest the presence of two isoenzymes with different thermal resistances, at least, and a two-component first-order model was considered to model the enzymatic inactivation parameters. The decimal reduction time at 86.9 degrees C (D(86.9 degrees C)) determined were 6.0 s and 11.3 min for PPO heat labile and heat resistant fractions, respectively, with average z-value = 5.6 degrees C (temperature difference required for tenfold change in D). For POD, D(86.9 degrees C) = 8.6 s (z = 3.4 degrees C) for the heat labile fraction was obtained and D(86.9 degrees C) = 26.3 min (z = 6.7 degrees C) for the heat resistant one.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The objective was to study the flow pattern in a plate heat exchanger (PHE) through residence time distribution (RTD) experiments. The tested PHE had flat plates and it was part of a laboratory scale pasteurization unit. Series flow and parallel flow configurations were tested with a variable number of passes and channels per pass. Owing to the small scale of the equipment and the short residence times, it was necessary to take into account the influence of the tracer detection unit on the RID data. Four theoretical RID models were adjusted: combined, series combined, generalized convection and axial dispersion. The combined model provided the best fit and it was useful to quantify the active and dead space volumes of the PHE and their dependence on its configuration. Results suggest that the axial dispersion model would present good results for a larger number of passes because of the turbulence associated with the changes of pass. This type of study can be useful to compare the hydraulic performance of different plates or to provide data for the evaluation of heat-induced changes that occur in the processing of heat-sensitive products. (C) 2011 Elsevier Ltd. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

In this work, we have studied the influence of the substrate surface condition on the roughness and the structure of the nanostructured DLC films deposited by High Density Plasma Chemical Vapor Deposition. Four methods were used to modify the silicon wafers surface before starting the deposition processes of the nanostructured DLC films: micro-diamond powder dispersion, micro-graphite powder dispersion, and roughness generation by wet chemical etching and roughness generation by plasma etching. The reference wafer was only submitted to a chemical cleaning. It was possible to see that the final roughness and the sp(3) hybridization degree strongly depend on the substrate surface conditions. The surface roughness was observed by AFM and SEM and the hybridization degree of the DLC films was analyzed by Raman Spectroscopy. In these samples, the final roughness and the sp(3) hybridization quantity depend strongly on the substrate surface condition. Thus, the effects of the substrate surface on the DLC film structure were confirmed. These phenomena can be explained by the fact that the locally higher surface energy and the sharp edges may induce local defects promoting the nanostructured characteristics in the DLC films. (C) 2008 Elsevier B.V. All rights reserved.