Resumo:
A novel self-assembled dual-layer film as apotential excellent lubricant for micromachines was successfully prepared on single-crystal silicon substrate by chemical adsorption of stearic acid (STA) molecules on self-assembled monolayer of 3-aminopropyltri
Resumo:
The deformation microstructure of face-centered cubic cobalt subjected to surface mechanical attrition treatment was studied as a function of strain levels. Strain-induced gamma --> epsilon transformation and twinning deformation were evidenced by transmission electron microscopy and were found to progress continuously in ultrafine and nanocrystalline grains as the strain increased.
Resumo:
The microstructural evolution in localized shear deformation was investigated in an 8090 Al-Li alloy by split Hopkinson pressure bar (strain rate of approximately 10(3) s(-1)) at ambient temperature and 77 K. The alloy was tested in the peak-, over-, under-, and natural-aged conditions, that provide a wide range of microstructural parameters and mechanical properties. Two types of localized shear bands were distinguished by optical microscopy: the deformed shear band and the white-etching shear band. They form at different stages of deformation during localization. There are critical strains for the occurrence of deformed and white-etching localized shear deformation, at the imposed strain rate. Observations by transmission electron microscopy reveal that the white-etching bands contain fine equiaxed grains; it is proposed that they are the result of recrystallization occurring during localization. The deformed-type bands are observed after testing at 77 K in all heat treatment conditions, but they are not as well defined as those developed at ambient temperature. Cracking often occurs along the localized shear at ambient temperature. The decrement in temperature is favorable for the nucleation, growth and coalescence of the microcracks along the shear bands, inducing fracture.
Resumo:
A finite element study has been performed on the effects of holes and rigid inclusions on the elastic modulus and yield strength of regular honeycombs under biaxial loading. The focus is on honeycombs that have already been weakened by a small degree of geometrical imperfection, such as a random distribution of fractured cell walls, as these imperfect honeycombs resemble commercially available metallic foams. Hashin-Shtrikman lower and upper bounds and self-consistent estimates of elastic moduli are derived to provide reference solutions to the finite element calculations. It is found that the strength of an imperfect honeycomb is relatively insensitive to the presence of holes and inclusions, consistent with recent experimental observations on commercial aluminum alloy foams.
Resumo:
The influence of each of the six different types of morphological imperfection - waviness, non-uniform cell wall thickness, cell-size variations, fractured cell walls, cell-wall misalignments, and missing cells - on the yielding of 2D cellular solids has been studied systematically for biaxial loading. Emphasis is placed on quantifying the knock-down effect of these defects on the hydrostatic yield strength and upon understanding the associated deformation mechanisms. The simulations in the present study indicate that the high hydrostatic strength, characteristic of ideal honeycombs, is reduced to a level comparable with the deviatoric strength by several types of defect. The common source of this large knock-down is a switch in deformation mode from cell wall stretching to cell wall bending under hydrostatic loading. Fractured cell edges produce the largest knock-down effect on the yield strength of 2D foams, followed in order by missing cells, wavy cell edges, cell edge misalignments, Γ Voronoi cells, δ Voronoi cells, and non-uniform wall thickness. A simple elliptical yield function with two adjustable material parameters successfully fits the numerically predicted yield surfaces for the imperfect 2D foams, and shows potential as a phenomenological constitutive law to guide the design of structural components made from metallic foams.
Resumo:
利用超声波探测法对节理裂隙岩体进行了声波测试,对不同的节理裂隙岩体进行了质量评估,通过对节理裂隙岩体进行爆破漏斗试验,分析了节理裂隙对岩体中爆炸应力波传播、岩石破碎及爆破漏斗形成的影响.结果表明,节理裂隙等结构弱面的存在严重阻碍了爆炸能量均匀分布,因此在爆破设计和施工中,应尽量使炮孔与结构弱面垂直布置,如果遇到含有夹层情况宜加大装药量;炮孔与结构弱面平行时,应尽量减小炮眼孔距和最小抵抗线,尽量采用单孔螺旋掏槽.
Resumo:
The magnetic moment of square planar melt processed YBa2Cu3O7-δ thick films is observed to scale with the cube of the sample width at 4.2 K, suggesting that current flow on the length scale of the film determines its magnetization at this temperature. A well-defined discontinuity in slope in the scaling data at a sample width corresponding to the average grain size (≈2 mm) implies the coexistence of distinct intra- and inter-grain critical current densities of 1.1 × 105Acm-2 and 0.4 × 105Acm-2 at 1 T and 4.2 K. The presence of a critical state in the films at 4.2T is confirmed by removing the central section from a specimen. The observed change in magnetic moment is in excellent agreement with theory for fields greater than ≈2 T. A critical state is not observed at 77 K which suggests that the grains are only weakly coupled at the higher temperature. © 1994.
Resumo:
Transport critical current measurements have been carried out on melt-processed thick films of YBa2Cu3O7-δ on yttria-stabilized zirconia in fields of up to 8 T both within grains and across grain boundaries. These measurements yield Jc values of ∼3000 A cm-2 at 4.2 K and zero magnetic field and 400 A cm -2 at 77 K and zero magnetic field, taking the entire sample width as the definitive dimension. Optical and scanning electron microscopy reveals that the thick-film grains consist typically of a central "hub" region ∼50 μm in diameter, which is well connected to radial subgrains or "spokes" which extend ∼1 mm to define the complete grain structure. Attempts have been made to correlate the transport measurements of inter- and intra-hub-and-spoke (H-S) critical current with values of this parameter derived previously from magnetization measurements. Analysis of the transport measurements indicates that current flow through H-S grains is constrained to paths along the spokes via the grain hub. Taking the size of the hub as the definitive dimension yields an intra-H-S grain Jc of ∼60 000 A cm-2 at 4.2 K and 0 T, which is in reasonable agreement with the magnetization data. Experiments in which the hub is removed from individual grains confirm that this feature determines critically the J c of the film.
Resumo:
A gray, fine-grained arkosic sandstone tablet bearing an inscription in ancient Hebrew from the First Temple Period contains a rich assemblage of particles accumulated in the covering patina. Two types of patina cover the tablet: a thin layer of black to orange iron-oxide-rich layer, a product of micro-biogenic processes, and a light beige patina that contains feldspars, carbonate, iron oxide, subangular quartz grains, carbon ash particles and gold globules (1 to 4 microns [1 micron = 0.001 millimeter] in diameter). The patina covers the rock surface as well as the engraved lettering grooves and blankets and thus post-dates the incised inscription as well as a crack that runs across the stone and several of the engraved letters. Radiocarbon analyses of the carbon particles in the patina yield a calibrated radiocarbon age of 2340 to 2150 Cal BP. The presence of microcolonial fungi and associated pitting in the patina indicates slow growth over many years. The occurrence of pure gold globules and carbon ash particles is evidence of a thermal event in close proximity to the tablet (above 1000 degrees Celsius). This study supports the antiquity of the patina, which in turn, strengthens the contention that the inscription is authentic.
Resumo:
The microstructural evolution during surface mechanical attrition treatment of cobalt (a mixture of hexagonal close packed (hep) and face-centered cubic (fcc) phases) was investigated. In order to reveal the mechanism of grain refinement and strain accommodation. The microstructure was systematically characterized by both cross-sectional and planar-view transmission electron microscopy. In the hcp phase, the process of grain refinement. Accompanied by an increase in strain imposed in the surface layer. Involved: (1) the onset of 110 111 deformation twinning, (2) the operation of (1 120) 110 1 0} prismatic and (1 120) (000 1) basal slip, leading to the formation of low-angle dislocation boundaries, and (3) the successive subdivision of grains to a finer and finer scale. Ressulting in the formation of highly misoriented nanocrystalline grains. Moreover. The formation of nanocrystalliies at the grain boundary and triple junction was also observed to occur concurrently with straining. By contrast. The fec phase accommodated strain in a sequence as follows: (1) slip of dislocations by forming intersecting planar arrays of dislocations, (2) {1 1 1} deformation twinning, and (3) the gamma(fcc) --> epsilon(hcp) martensitic phase transformation. The mechanism of grain refinement was interpreted in terms of the structural subdivision of grains together with dynamic recrystallization occurring in the hep phase and the gamma --> E: martensitic transformation in the fcc phase as well.
Resumo:
The nanocrystalline (nc) formation was studied in cobalt (a mixture of c (hexagonal close packed) and gamma (face-centered cubic) phases) subjected to surface mechanical attrition treatment. Electron microscopy revealed the operation of {10(1) over bar 0}< 11(2) over bar 0 > prismatic and {0001}< 11(2) over bar 0 > basal slip in the E phase, leading to the successive subdivision of grains to nanoscale. In particular, the dislocation splitting into the stacking faults was observed to occur in ultrafine and nc grains. By contrast, the planar dislocation arrays, twins and martensites were evidenced in the gamma phase. The strain-induced gamma ->epsilon martensitic transformation was found to progress continuously in ultrafine and nc grains as the strain increased. The nc formation in the gamma phase was interpreted in terms of the martensitic transformation and twinning.
Resumo:
Thin films of inorganic materials are used in diverse applications, typically in polycrystalline form due to their relatively simple production. We have used enhanced piezoresponse force microscopy to investigate the domain distribution within neighbouring grains in thin polycrystalline films of the ferroelectric-ferroelastic system lead zirconate titanate (PZT). We demonstrate that domains are organized into areas with a correlated alignment of the ferroelastic and ferroelectric domains, spanning multiple grain boundaries. We present five typical arrangements of such structures: azimuthal, radial, gradient, and short- and long- range linear domain organizations. Moreover, we discuss the mechanical and electrical constraints that dictate these structures. Copyright © 2011 WILEY-VCH Verlag GmbH & Co. KGaA, Weinheim.
Resumo:
An investigation has been made into the plastic deformation behavior of a Monel alloy deformed at high strain rate of 10(5) s(-1) by split Hopkinson bar. The results reveal that there are some equiaxed grains with an average size of 150 nm in diameter in the center of the shear bands, suggesting that this microstructure characteristics be developed by dynamic recrystallization, arising from the deformation and the rapid temperature rise in the band. Analysis shows that the plastic strain rate and the mobile dislocation density play a key role in the new crystallized grain formation and growth. Based on grain boundary energy change and diffusion mechanism, the grain growth kinetics is developed for plastic deformation at a high strain rate.
Resumo:
Deformation microstructures have been investigated in nanocrystalline (nc) Ni with grain sizes in the 50-100 nm range. It was found that deformation twinning started to occur in grains of similar to 90 nm, and its propensity increased with decreasing grain size. In most of the nc grains dislocations were observed as well, in the form of individual dislocations and dipoles. It is concluded that dislocation-mediated plasticity dominates for grain sizes in the upper half, i.e. 50-100 nm, of the nanocrystalline regime. (C) 2007 Published by Elsevier B.V.
Resumo:
The response of porous Al2O3 to nanoindentation was investigated at microscopic scales (nm-mu m) and under ultra-low loads from 5 to 90 mN with special attention paid to the dependence of the load-depth behaviour to sample porosity. It was found that the load-depth curves manifest local responses typical of the various porous structures investigated. This is particularly clear for the residual deformation after load removal. Similarly, the limited mean pressure of the sample containing small grains and interconnected pores is consistent with its porous structure. By comparison, the samples with larger grain size and various porous structures exhibit higher pressures and smaller residual deformations that can be attributed to the mechanical response of the solid phase. (C) 2007 Elsevier B.V. All rights reserved.