864 resultados para Titanium mesh
Resumo:
Tribocorrosion plays an important role in the lifetime of metallic implants. Once implanted, biomaterials are subjected to micro-movements in aggressive biological fluids. Titanium is widely used as an implant material because it spontaneously forms a compact and protective nanometric thick oxide layer, mainly TiO2, in ambient air. That layer provides good corrosion resistance, and very low toxicity, but its low wear resistance is a concern. In this work, an anodizing treatment was performed on commercial pure titanium to form a homogeneous thick oxide surface layer in order to provide bioactivity and improve the biological, chemical and mechanical properties. Anodizing was performed in an electrolyte containing β-glycerophosphate and calcium acetate. The influence of the calcium acetate content on the tribocorrosion behaviour of the anodized material was studied. The concentration of calcium acetate in the electrolyte was found to largely affect the crystallographic structure of the resulting oxide layer. Better tribocorrosion behaviour was noticed on increasing the calcium acetate concentration. © 2013 IOP Publishing Ltd.
Resumo:
Pós-graduação em Engenharia Elétrica - FEIS
Resumo:
Pós-graduação em Reabilitação Oral - FOAR
Resumo:
Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)
Resumo:
The purpose of this study was nondecalcified histologic analysis of titanium implants modified by laser with and without hydroxyapatite. Implants with three modified surfaces were inserted into rabbit tibias: group 1, machined surface; group 2, irradiated (laser); and group 3, irradiated and hydroxyapatite coated (biomimetic method). The mean surface roughness (Ra) scores of groups 2 and 3 were higher than that of group 1. Bone-implant contact measurements at 30 and 60 days for groups 2 and 3 were higher than for group 1. Bone area at 30 and 60 days for group 2 was higher than for groups 1 and 3. Titanium implants modified by laser with and without hydroxyapatite exhibit increased early osseointegration.
Resumo:
Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)
Resumo:
Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)
Resumo:
Conselho Nacional de Desenvolvimento Científico e Tecnológico (CNPq)
Resumo:
Coordenação de Aperfeiçoamento de Pessoal de Nível Superior (CAPES)
Resumo:
Coordenação de Aperfeiçoamento de Pessoal de Nível Superior (CAPES)
Resumo:
Conselho Nacional de Desenvolvimento Científico e Tecnológico (CNPq)
Resumo:
Statement of problem. An imprecise fit between frameworks and supporting dental implants in loaded protocols increases the strain transferred to the periimplant bone, which may impair healing or generate microgaps.Purpose. The purpose of this study was to investigate the microstrain between premachined 1-piece screw-retained frameworks (group STF) and screw-retained frameworks fabricated by cementing titanium cylinders to the prefabricated framework (group CTF). This procedure was developed to correct the misfit between frameworks and loaded implants.Material and methods. Four internal hexagon cylindrical implants were placed 10 mm apart in a polyurethane block by using the surgical guides of the corresponding implant system. Previously fabricated titanium frameworks (n=10) were divided into 2 groups. In group STF, prefabricated machined frameworks were used (n=5), and, in group CTF, the frameworks were fabricated by using a passive fit procedure, which was developed to correct the misfit between the cast titanium frameworks and supporting dental implants (n=5). Both groups were screw-retained under torque control (10 Ncm). Six strain gauges were placed on the upper surface of the polyurethane block, and 3 strain measurements were recorded for each framework. Data were analyzed with the Student t test (alpha=.05).Results. The mean microstrain values between the framework and the implants were significantly higher for group STF (2517 me) than for group CTF (844 me) (P<.05).Conclusions. Complete-arch implant frameworks designed for load application and fabricated by using the passive fit procedure decreased the strain between the frameworks and implants more than 1 piece prefabricated machined frameworks.
Resumo:
Statement of problem. Removable partial dentures are affected by fatigue because of the cyclic mechanism of the masticatory system ansi frequent insertion and removal. Titanium and its alloys have been used in the manufacture of denture frameworks; however, preventive agents with fluorides are thought to attack titanium alloy surfaces.Purpose. This study evaluated, compared, analyzed the corrosion-fatigue life of commercially pure titanium and Ti-6Al-4V alloy in different storage environments.Material and methods. For each metal, 33 dumbbell rods, 2.3 mm in diameter at the central segment, were cast in the Rematitan system. Corrosion-fatigue strength test was carried out through a universal testing machine with a load 30% lon er than the 0.2% offset yield strength and a combined influence of different: environments: in air at room temperature, with synthetic saliva, and with fluoride synthetic saliva. After failure, the number of cycles were recorded, and fracture surfaces were examined with on SEM.Results. ANOVA and Tukey's multiple comparison rest indicated that Ti-6Al-4V alloy achieved 21,269 cycles (SD = 8,355) against 19,157 cycles (SD = 3,624) for the commercially purr Ti. There were no significant differences between either metal in the corrosion-fatigue life for dry specimens, but when the solutions were present, the fatigue life was significantly reduced, probably because of the product-ion of corrosion pits caused by superficial reactions.
Resumo:
The Polymeric Precursor Method has proved suitable for synthesizing reactive powders using low temperatures of calcination, especially when compared with conventional methods. However, during the thermal decomposition of the polymeric precursor the combustion event can be releases an additional heat that raises the temperature of the sample in several tens of degrees Celsius above the set temperature of the oven. This event may be detrimental to some material types, such as the titanium dioxide semiconductor. This ceramic material has a phase transition at around 600 ° C, which involves the irreversible structural rearrangement, characterized by the phase transition from anatase to rutile TiO2 phase. The control of the calcination step then becomes very important because the efficiency of the photocatalyst is dependent on the amount of anatase phase in the material. Furthermore, use of dopant in the material aims to improve various properties, such as increasing the absorption of radiation and in the time of the excited state, shifting of the absorption edge to the visible region, and increasing of the thermal stability of anatase. In this work, samples of titanium dioxide were synthesized by the Polymeric Precursor Method in order to investigate the effect of Fe (III) doping on the calcination stages. Thermal analysis has demonstrated that the Fe (III) insertion at 1 mol% anticipates the organic decomposition, reducing the combustion event in the final calcination. Furthermore, FTIR-PAS, XRD and SEM results showed that organic matter amount was reduced in the Fe (III)-doped TiO2 sample, which reduced the rutile phase amount and increased the reactivity and crystallinity of the powder samples.
Resumo:
Nickel-titanium rotatory systems should remove dentin during the root canal preparation to promote the enlargement and tapered shape with continuously narrowing towards the apex. Objective: The aim of this study was to analyze the cutting ability of three NiTi rotatory systems (n = 12): ProTaper (group 1), Mtwo (group 2), and K3 (group 3). Material and methods: Thirty six maxillary molar teeth were weighted on an analytical balance before and after the rotatory preparation of the mesio-buccal root canal. Data was statistically analyzed by ANOVA and Tukey s test with a significance level of 5%. Results: The results revealed the following mass differences (g) before and after the root canal preparation: ProTaper (group 1 – 0.0159 ± 0.004), Mtwo (group 2 – 0.0125 ± 0.002), and K3 (group 3 – 0.007 ± 0.003). Conclusion: ProTaper showed the highest cutting ability among the three tested nickel-titanium rotatory systems followed by Mtwo and K3.